VERFAHREN ZUR HERSTELLUNG EINES RISSFREIEN HOCH MOLEKULARORIENTIERTEN GEBLASENEN BEHAELTERS

Mfr. of molecularly highly oriented blow-moulded containers e.g. bottles, free from cracks, from nitrile-contg. polymer, comprises (a) shaping a seamless comparison closed at 1 end, in an injection-mould with an extrusion die that has a cavity surrounding a coaxial core pin; (b) injecting polymer me...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MILA BELIVAKICI,ILIE, RICHARD YOUNG,ROBERT
Format: Patent
Sprache:ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MILA BELIVAKICI,ILIE
RICHARD YOUNG,ROBERT
description Mfr. of molecularly highly oriented blow-moulded containers e.g. bottles, free from cracks, from nitrile-contg. polymer, comprises (a) shaping a seamless comparison closed at 1 end, in an injection-mould with an extrusion die that has a cavity surrounding a coaxial core pin; (b) injecting polymer melt under pressure into the extrusion die cavity; removing the parison from the core pin; and (c) transferring the hot parison immediately to a temp. controlled conditioning pin in contact with the inner surface with the inner surface of the parison and a temp. controlled cavity in contact with the outer surface of the parison. Thus the parison is temp. conditioned within the orientation temp. range for the polymer. The so-conditioned parison is then blow-moulded, the polymer an orientation relaxation stress (sic), in a circumferential direction, of at least 35.2 kg/cm. Used e.g. in mfr. of plastics bottles for carbonated beverages. The prods. are free from stress cracks and unsightly stress marks.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_DE2702495A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>DE2702495A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_DE2702495A13</originalsourceid><addsrcrecordid>eNqNjDEKAjEURNNYiHqHXEDQVRHL7DrZH4wJ_CQWWiyLxEp0Yb0_pvAAVjPMe8xU3C5grYjh5DWxJHCIsDa5VsI4BMkmBM0wRSDfkDx7i1Oyij2XLRpwLKhFbVWAK7UGKdhYjuZi8uifY178ciakRmxomYd3l8ehv-dX_nRHVPtVtT3s1Hrzh_IFfQMyQg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>VERFAHREN ZUR HERSTELLUNG EINES RISSFREIEN HOCH MOLEKULARORIENTIERTEN GEBLASENEN BEHAELTERS</title><source>esp@cenet</source><creator>MILA BELIVAKICI,ILIE ; RICHARD YOUNG,ROBERT</creator><creatorcontrib>MILA BELIVAKICI,ILIE ; RICHARD YOUNG,ROBERT</creatorcontrib><description>Mfr. of molecularly highly oriented blow-moulded containers e.g. bottles, free from cracks, from nitrile-contg. polymer, comprises (a) shaping a seamless comparison closed at 1 end, in an injection-mould with an extrusion die that has a cavity surrounding a coaxial core pin; (b) injecting polymer melt under pressure into the extrusion die cavity; removing the parison from the core pin; and (c) transferring the hot parison immediately to a temp. controlled conditioning pin in contact with the inner surface with the inner surface of the parison and a temp. controlled cavity in contact with the outer surface of the parison. Thus the parison is temp. conditioned within the orientation temp. range for the polymer. The so-conditioned parison is then blow-moulded, the polymer an orientation relaxation stress (sic), in a circumferential direction, of at least 35.2 kg/cm. Used e.g. in mfr. of plastics bottles for carbonated beverages. The prods. are free from stress cracks and unsightly stress marks.</description><edition>2</edition><language>ger</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; MAKING GRANULES OR PREFORMS ; PERFORMING OPERATIONS ; PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED ; RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>1977</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19770728&amp;DB=EPODOC&amp;CC=DE&amp;NR=2702495A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19770728&amp;DB=EPODOC&amp;CC=DE&amp;NR=2702495A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MILA BELIVAKICI,ILIE</creatorcontrib><creatorcontrib>RICHARD YOUNG,ROBERT</creatorcontrib><title>VERFAHREN ZUR HERSTELLUNG EINES RISSFREIEN HOCH MOLEKULARORIENTIERTEN GEBLASENEN BEHAELTERS</title><description>Mfr. of molecularly highly oriented blow-moulded containers e.g. bottles, free from cracks, from nitrile-contg. polymer, comprises (a) shaping a seamless comparison closed at 1 end, in an injection-mould with an extrusion die that has a cavity surrounding a coaxial core pin; (b) injecting polymer melt under pressure into the extrusion die cavity; removing the parison from the core pin; and (c) transferring the hot parison immediately to a temp. controlled conditioning pin in contact with the inner surface with the inner surface of the parison and a temp. controlled cavity in contact with the outer surface of the parison. Thus the parison is temp. conditioned within the orientation temp. range for the polymer. The so-conditioned parison is then blow-moulded, the polymer an orientation relaxation stress (sic), in a circumferential direction, of at least 35.2 kg/cm. Used e.g. in mfr. of plastics bottles for carbonated beverages. The prods. are free from stress cracks and unsightly stress marks.</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>MAKING GRANULES OR PREFORMS</subject><subject>PERFORMING OPERATIONS</subject><subject>PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED</subject><subject>RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1977</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjDEKAjEURNNYiHqHXEDQVRHL7DrZH4wJ_CQWWiyLxEp0Yb0_pvAAVjPMe8xU3C5grYjh5DWxJHCIsDa5VsI4BMkmBM0wRSDfkDx7i1Oyij2XLRpwLKhFbVWAK7UGKdhYjuZi8uifY178ciakRmxomYd3l8ehv-dX_nRHVPtVtT3s1Hrzh_IFfQMyQg</recordid><startdate>19770728</startdate><enddate>19770728</enddate><creator>MILA BELIVAKICI,ILIE</creator><creator>RICHARD YOUNG,ROBERT</creator><scope>EVB</scope></search><sort><creationdate>19770728</creationdate><title>VERFAHREN ZUR HERSTELLUNG EINES RISSFREIEN HOCH MOLEKULARORIENTIERTEN GEBLASENEN BEHAELTERS</title><author>MILA BELIVAKICI,ILIE ; RICHARD YOUNG,ROBERT</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_DE2702495A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>ger</language><creationdate>1977</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>MAKING GRANULES OR PREFORMS</topic><topic>PERFORMING OPERATIONS</topic><topic>PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED</topic><topic>RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>MILA BELIVAKICI,ILIE</creatorcontrib><creatorcontrib>RICHARD YOUNG,ROBERT</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MILA BELIVAKICI,ILIE</au><au>RICHARD YOUNG,ROBERT</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>VERFAHREN ZUR HERSTELLUNG EINES RISSFREIEN HOCH MOLEKULARORIENTIERTEN GEBLASENEN BEHAELTERS</title><date>1977-07-28</date><risdate>1977</risdate><abstract>Mfr. of molecularly highly oriented blow-moulded containers e.g. bottles, free from cracks, from nitrile-contg. polymer, comprises (a) shaping a seamless comparison closed at 1 end, in an injection-mould with an extrusion die that has a cavity surrounding a coaxial core pin; (b) injecting polymer melt under pressure into the extrusion die cavity; removing the parison from the core pin; and (c) transferring the hot parison immediately to a temp. controlled conditioning pin in contact with the inner surface with the inner surface of the parison and a temp. controlled cavity in contact with the outer surface of the parison. Thus the parison is temp. conditioned within the orientation temp. range for the polymer. The so-conditioned parison is then blow-moulded, the polymer an orientation relaxation stress (sic), in a circumferential direction, of at least 35.2 kg/cm. Used e.g. in mfr. of plastics bottles for carbonated beverages. The prods. are free from stress cracks and unsightly stress marks.</abstract><edition>2</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language ger
recordid cdi_epo_espacenet_DE2702495A1
source esp@cenet
subjects AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
MAKING GRANULES OR PREFORMS
PERFORMING OPERATIONS
PREPARATION OR PRETREATMENT OF THE MATERIAL TO BESHAPED
RECOVERY OF PLASTICS OR OTHER CONSTITUENTS OF WASTE MATERIALCONTAINING PLASTICS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
TRANSPORTING
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
title VERFAHREN ZUR HERSTELLUNG EINES RISSFREIEN HOCH MOLEKULARORIENTIERTEN GEBLASENEN BEHAELTERS
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-03T06%3A32%3A37IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MILA%20BELIVAKICI,ILIE&rft.date=1977-07-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EDE2702495A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true