Furfuryl alcohol prepn. by furfurol reduction - with gas from ammonia synthesis in medium contg. demineralised water

Continuous furfuryl alcohol (I) prepn. by catalytic reduction of furfurol with gas from NH3-synthesis at atmos. press. takes place in a 1-3% medium of demineralised water at a specific filling wt. of 0.1-0.05 (0.07)kg. furfurol/l. catalyst/hr., pref. at 115-135 degrees C. By this process, furfuryl a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GROS, IOSIF., VICTORIA, SFINTESCU, CLAUDIU GHEORGHE ION, COICA, ION, VOICU, MARIA MAGDALENA, KNALL, LEO, MIHORDEA, CORNELIA, CORLATEANU, ELENA AURELIA, LUPESCU, ANA MARIA., VICTORIA, HERSCOVICI, JUSTIN, BOTA, DUMITRU TEOFIL, IUGA, VIRGIL
Format: Patent
Sprache:eng ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GROS, IOSIF., VICTORIA
SFINTESCU, CLAUDIU GHEORGHE ION
COICA, ION
VOICU, MARIA MAGDALENA
KNALL, LEO
MIHORDEA, CORNELIA
CORLATEANU, ELENA AURELIA
LUPESCU, ANA MARIA., VICTORIA
HERSCOVICI, JUSTIN
BOTA, DUMITRU TEOFIL
IUGA, VIRGIL
description Continuous furfuryl alcohol (I) prepn. by catalytic reduction of furfurol with gas from NH3-synthesis at atmos. press. takes place in a 1-3% medium of demineralised water at a specific filling wt. of 0.1-0.05 (0.07)kg. furfurol/l. catalyst/hr., pref. at 115-135 degrees C. By this process, furfuryl alcohol yields are increased to 95%. Wear of catalyst is slight and its activity can be maintained unchanged for 1500 hrs. Mol. ratio furfurol:synthesis gas is esp.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_DE2401603A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>DE2401603A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_DE2401603A13</originalsourceid><addsrcrecordid>eNqNiksKwjAQQLtxIeod5gItrRX3oi0ewH0Zk4kdSCYhH0pvr4gHcPXgvbet8liiKXG1gFb52VsIkYI08FzBfNNHRdJFZfYCNSycZ3hhAhO9A3TOCyOkVfJMiROwgCPNxYHykl8NaHIsFNFyIg0LZor7amPQJjr8uKtgHB7Xe03BT5QCKhLK0204ntru3PaXrv9jeQP07kQ6</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Furfuryl alcohol prepn. by furfurol reduction - with gas from ammonia synthesis in medium contg. demineralised water</title><source>esp@cenet</source><creator>GROS, IOSIF., VICTORIA ; SFINTESCU, CLAUDIU GHEORGHE ION ; COICA, ION ; VOICU, MARIA MAGDALENA ; KNALL, LEO ; MIHORDEA, CORNELIA ; CORLATEANU, ELENA AURELIA ; LUPESCU, ANA MARIA., VICTORIA ; HERSCOVICI, JUSTIN ; BOTA, DUMITRU TEOFIL ; IUGA, VIRGIL</creator><creatorcontrib>GROS, IOSIF., VICTORIA ; SFINTESCU, CLAUDIU GHEORGHE ION ; COICA, ION ; VOICU, MARIA MAGDALENA ; KNALL, LEO ; MIHORDEA, CORNELIA ; CORLATEANU, ELENA AURELIA ; LUPESCU, ANA MARIA., VICTORIA ; HERSCOVICI, JUSTIN ; BOTA, DUMITRU TEOFIL ; IUGA, VIRGIL</creatorcontrib><description>Continuous furfuryl alcohol (I) prepn. by catalytic reduction of furfurol with gas from NH3-synthesis at atmos. press. takes place in a 1-3% medium of demineralised water at a specific filling wt. of 0.1-0.05 (0.07)kg. furfurol/l. catalyst/hr., pref. at 115-135 degrees C. By this process, furfuryl alcohol yields are increased to 95%. Wear of catalyst is slight and its activity can be maintained unchanged for 1500 hrs. Mol. ratio furfurol:synthesis gas is esp.</description><edition>2</edition><language>eng ; ger</language><subject>CHEMISTRY ; HETEROCYCLIC COMPOUNDS ; METALLURGY ; ORGANIC CHEMISTRY</subject><creationdate>1975</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19750717&amp;DB=EPODOC&amp;CC=DE&amp;NR=2401603A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19750717&amp;DB=EPODOC&amp;CC=DE&amp;NR=2401603A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GROS, IOSIF., VICTORIA</creatorcontrib><creatorcontrib>SFINTESCU, CLAUDIU GHEORGHE ION</creatorcontrib><creatorcontrib>COICA, ION</creatorcontrib><creatorcontrib>VOICU, MARIA MAGDALENA</creatorcontrib><creatorcontrib>KNALL, LEO</creatorcontrib><creatorcontrib>MIHORDEA, CORNELIA</creatorcontrib><creatorcontrib>CORLATEANU, ELENA AURELIA</creatorcontrib><creatorcontrib>LUPESCU, ANA MARIA., VICTORIA</creatorcontrib><creatorcontrib>HERSCOVICI, JUSTIN</creatorcontrib><creatorcontrib>BOTA, DUMITRU TEOFIL</creatorcontrib><creatorcontrib>IUGA, VIRGIL</creatorcontrib><title>Furfuryl alcohol prepn. by furfurol reduction - with gas from ammonia synthesis in medium contg. demineralised water</title><description>Continuous furfuryl alcohol (I) prepn. by catalytic reduction of furfurol with gas from NH3-synthesis at atmos. press. takes place in a 1-3% medium of demineralised water at a specific filling wt. of 0.1-0.05 (0.07)kg. furfurol/l. catalyst/hr., pref. at 115-135 degrees C. By this process, furfuryl alcohol yields are increased to 95%. Wear of catalyst is slight and its activity can be maintained unchanged for 1500 hrs. Mol. ratio furfurol:synthesis gas is esp.</description><subject>CHEMISTRY</subject><subject>HETEROCYCLIC COMPOUNDS</subject><subject>METALLURGY</subject><subject>ORGANIC CHEMISTRY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1975</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNiksKwjAQQLtxIeod5gItrRX3oi0ewH0Zk4kdSCYhH0pvr4gHcPXgvbet8liiKXG1gFb52VsIkYI08FzBfNNHRdJFZfYCNSycZ3hhAhO9A3TOCyOkVfJMiROwgCPNxYHykl8NaHIsFNFyIg0LZor7amPQJjr8uKtgHB7Xe03BT5QCKhLK0204ntru3PaXrv9jeQP07kQ6</recordid><startdate>19750717</startdate><enddate>19750717</enddate><creator>GROS, IOSIF., VICTORIA</creator><creator>SFINTESCU, CLAUDIU GHEORGHE ION</creator><creator>COICA, ION</creator><creator>VOICU, MARIA MAGDALENA</creator><creator>KNALL, LEO</creator><creator>MIHORDEA, CORNELIA</creator><creator>CORLATEANU, ELENA AURELIA</creator><creator>LUPESCU, ANA MARIA., VICTORIA</creator><creator>HERSCOVICI, JUSTIN</creator><creator>BOTA, DUMITRU TEOFIL</creator><creator>IUGA, VIRGIL</creator><scope>EVB</scope></search><sort><creationdate>19750717</creationdate><title>Furfuryl alcohol prepn. by furfurol reduction - with gas from ammonia synthesis in medium contg. demineralised water</title><author>GROS, IOSIF., VICTORIA ; SFINTESCU, CLAUDIU GHEORGHE ION ; COICA, ION ; VOICU, MARIA MAGDALENA ; KNALL, LEO ; MIHORDEA, CORNELIA ; CORLATEANU, ELENA AURELIA ; LUPESCU, ANA MARIA., VICTORIA ; HERSCOVICI, JUSTIN ; BOTA, DUMITRU TEOFIL ; IUGA, VIRGIL</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_DE2401603A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; ger</language><creationdate>1975</creationdate><topic>CHEMISTRY</topic><topic>HETEROCYCLIC COMPOUNDS</topic><topic>METALLURGY</topic><topic>ORGANIC CHEMISTRY</topic><toplevel>online_resources</toplevel><creatorcontrib>GROS, IOSIF., VICTORIA</creatorcontrib><creatorcontrib>SFINTESCU, CLAUDIU GHEORGHE ION</creatorcontrib><creatorcontrib>COICA, ION</creatorcontrib><creatorcontrib>VOICU, MARIA MAGDALENA</creatorcontrib><creatorcontrib>KNALL, LEO</creatorcontrib><creatorcontrib>MIHORDEA, CORNELIA</creatorcontrib><creatorcontrib>CORLATEANU, ELENA AURELIA</creatorcontrib><creatorcontrib>LUPESCU, ANA MARIA., VICTORIA</creatorcontrib><creatorcontrib>HERSCOVICI, JUSTIN</creatorcontrib><creatorcontrib>BOTA, DUMITRU TEOFIL</creatorcontrib><creatorcontrib>IUGA, VIRGIL</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GROS, IOSIF., VICTORIA</au><au>SFINTESCU, CLAUDIU GHEORGHE ION</au><au>COICA, ION</au><au>VOICU, MARIA MAGDALENA</au><au>KNALL, LEO</au><au>MIHORDEA, CORNELIA</au><au>CORLATEANU, ELENA AURELIA</au><au>LUPESCU, ANA MARIA., VICTORIA</au><au>HERSCOVICI, JUSTIN</au><au>BOTA, DUMITRU TEOFIL</au><au>IUGA, VIRGIL</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Furfuryl alcohol prepn. by furfurol reduction - with gas from ammonia synthesis in medium contg. demineralised water</title><date>1975-07-17</date><risdate>1975</risdate><abstract>Continuous furfuryl alcohol (I) prepn. by catalytic reduction of furfurol with gas from NH3-synthesis at atmos. press. takes place in a 1-3% medium of demineralised water at a specific filling wt. of 0.1-0.05 (0.07)kg. furfurol/l. catalyst/hr., pref. at 115-135 degrees C. By this process, furfuryl alcohol yields are increased to 95%. Wear of catalyst is slight and its activity can be maintained unchanged for 1500 hrs. Mol. ratio furfurol:synthesis gas is esp.</abstract><edition>2</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; ger
recordid cdi_epo_espacenet_DE2401603A1
source esp@cenet
subjects CHEMISTRY
HETEROCYCLIC COMPOUNDS
METALLURGY
ORGANIC CHEMISTRY
title Furfuryl alcohol prepn. by furfurol reduction - with gas from ammonia synthesis in medium contg. demineralised water
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-05T12%3A31%3A41IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GROS,%20IOSIF.,%20VICTORIA&rft.date=1975-07-17&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EDE2401603A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true