Verfahren zur Beseitigung von Molybdaenverunreinigungen aus nickel-,eisen- und schwefelhaltigen Produkten

1319503 Removal of Mo from Ni-containing residues SHERRITT GORDON MINES Ltd 16 Nov 1970 [7 Jan 1970 18 Sept 1970] 54459/70 Heading C1A Molybdenum is removed from residues containing Ni, Fe and S and possibly Cu, Co, Cr or W by mixing with the latter, before and/or during pelletizing of the same usin...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: MEHL.ERNEST, KAWULKA,PAUL, WEIZENBACH,BAUKE
Format: Patent
Sprache:ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator MEHL.ERNEST
KAWULKA,PAUL
WEIZENBACH,BAUKE
description 1319503 Removal of Mo from Ni-containing residues SHERRITT GORDON MINES Ltd 16 Nov 1970 [7 Jan 1970 18 Sept 1970] 54459/70 Heading C1A Molybdenum is removed from residues containing Ni, Fe and S and possibly Cu, Co, Cr or W by mixing with the latter, before and/or during pelletizing of the same using water, an alkali in an amount equivalent to a residue-to- NaOH weight ratio of from 20 : 1 to 3 : 1; roasting the pellets at 540‹-870‹C. with a source of oxygen (e.g. air or steam) present to convert substantially all of the Mo into watersoluble alkali metal molybdates; quenching the roasted, pelletized mixture in water and agitating the slurry to extract and dissolve the molybdates; and finally separating the solution from the Ni-containing residue. Tungsten, if present in the original residue, may also be removed as water-soluble tungstates. The alkali to be used is preferably NaOH, KOH, Na 2 CO 3 , K 2 CO 3 or Na 2 S or mixtures of these.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_DE2060516A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>DE2060516A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_DE2060516A13</originalsourceid><addsrcrecordid>eNqNzLEKwjAUheEuDqK-w30AC61i96oVF8FBXEtsT5rQcFOSpqJPbxAfwOkM_8eZJ_oOJ4VyYHoHR3t46FF3gTuaLNPFmtejFeAJLrCD5m-LWgRPrJseJl1De3BKgVvyjXpCwihh4k10V2fb0I_gZTKTwnisfrtI6FTdDucUg63hB9GAMdbHapMV2S4vynz7B_kASLFBEg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Verfahren zur Beseitigung von Molybdaenverunreinigungen aus nickel-,eisen- und schwefelhaltigen Produkten</title><source>esp@cenet</source><creator>MEHL.ERNEST ; KAWULKA,PAUL ; WEIZENBACH,BAUKE</creator><creatorcontrib>MEHL.ERNEST ; KAWULKA,PAUL ; WEIZENBACH,BAUKE</creatorcontrib><description>1319503 Removal of Mo from Ni-containing residues SHERRITT GORDON MINES Ltd 16 Nov 1970 [7 Jan 1970 18 Sept 1970] 54459/70 Heading C1A Molybdenum is removed from residues containing Ni, Fe and S and possibly Cu, Co, Cr or W by mixing with the latter, before and/or during pelletizing of the same using water, an alkali in an amount equivalent to a residue-to- NaOH weight ratio of from 20 : 1 to 3 : 1; roasting the pellets at 540‹-870‹C. with a source of oxygen (e.g. air or steam) present to convert substantially all of the Mo into watersoluble alkali metal molybdates; quenching the roasted, pelletized mixture in water and agitating the slurry to extract and dissolve the molybdates; and finally separating the solution from the Ni-containing residue. Tungsten, if present in the original residue, may also be removed as water-soluble tungstates. The alkali to be used is preferably NaOH, KOH, Na 2 CO 3 , K 2 CO 3 or Na 2 S or mixtures of these.</description><language>ger</language><subject>CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; FERROUS OR NON-FERROUS ALLOYS ; INORGANIC CHEMISTRY ; METALLURGY ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; SEPARATION ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>1971</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19711118&amp;DB=EPODOC&amp;CC=DE&amp;NR=2060516A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25569,76552</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19711118&amp;DB=EPODOC&amp;CC=DE&amp;NR=2060516A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>MEHL.ERNEST</creatorcontrib><creatorcontrib>KAWULKA,PAUL</creatorcontrib><creatorcontrib>WEIZENBACH,BAUKE</creatorcontrib><title>Verfahren zur Beseitigung von Molybdaenverunreinigungen aus nickel-,eisen- und schwefelhaltigen Produkten</title><description>1319503 Removal of Mo from Ni-containing residues SHERRITT GORDON MINES Ltd 16 Nov 1970 [7 Jan 1970 18 Sept 1970] 54459/70 Heading C1A Molybdenum is removed from residues containing Ni, Fe and S and possibly Cu, Co, Cr or W by mixing with the latter, before and/or during pelletizing of the same using water, an alkali in an amount equivalent to a residue-to- NaOH weight ratio of from 20 : 1 to 3 : 1; roasting the pellets at 540‹-870‹C. with a source of oxygen (e.g. air or steam) present to convert substantially all of the Mo into watersoluble alkali metal molybdates; quenching the roasted, pelletized mixture in water and agitating the slurry to extract and dissolve the molybdates; and finally separating the solution from the Ni-containing residue. Tungsten, if present in the original residue, may also be removed as water-soluble tungstates. The alkali to be used is preferably NaOH, KOH, Na 2 CO 3 , K 2 CO 3 or Na 2 S or mixtures of these.</description><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>SEPARATION</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1971</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNzLEKwjAUheEuDqK-w30AC61i96oVF8FBXEtsT5rQcFOSpqJPbxAfwOkM_8eZJ_oOJ4VyYHoHR3t46FF3gTuaLNPFmtejFeAJLrCD5m-LWgRPrJseJl1De3BKgVvyjXpCwihh4k10V2fb0I_gZTKTwnisfrtI6FTdDucUg63hB9GAMdbHapMV2S4vynz7B_kASLFBEg</recordid><startdate>19711118</startdate><enddate>19711118</enddate><creator>MEHL.ERNEST</creator><creator>KAWULKA,PAUL</creator><creator>WEIZENBACH,BAUKE</creator><scope>EVB</scope></search><sort><creationdate>19711118</creationdate><title>Verfahren zur Beseitigung von Molybdaenverunreinigungen aus nickel-,eisen- und schwefelhaltigen Produkten</title><author>MEHL.ERNEST ; KAWULKA,PAUL ; WEIZENBACH,BAUKE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_DE2060516A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>ger</language><creationdate>1971</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>SEPARATION</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>MEHL.ERNEST</creatorcontrib><creatorcontrib>KAWULKA,PAUL</creatorcontrib><creatorcontrib>WEIZENBACH,BAUKE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>MEHL.ERNEST</au><au>KAWULKA,PAUL</au><au>WEIZENBACH,BAUKE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Verfahren zur Beseitigung von Molybdaenverunreinigungen aus nickel-,eisen- und schwefelhaltigen Produkten</title><date>1971-11-18</date><risdate>1971</risdate><abstract>1319503 Removal of Mo from Ni-containing residues SHERRITT GORDON MINES Ltd 16 Nov 1970 [7 Jan 1970 18 Sept 1970] 54459/70 Heading C1A Molybdenum is removed from residues containing Ni, Fe and S and possibly Cu, Co, Cr or W by mixing with the latter, before and/or during pelletizing of the same using water, an alkali in an amount equivalent to a residue-to- NaOH weight ratio of from 20 : 1 to 3 : 1; roasting the pellets at 540‹-870‹C. with a source of oxygen (e.g. air or steam) present to convert substantially all of the Mo into watersoluble alkali metal molybdates; quenching the roasted, pelletized mixture in water and agitating the slurry to extract and dissolve the molybdates; and finally separating the solution from the Ni-containing residue. Tungsten, if present in the original residue, may also be removed as water-soluble tungstates. The alkali to be used is preferably NaOH, KOH, Na 2 CO 3 , K 2 CO 3 or Na 2 S or mixtures of these.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language ger
recordid cdi_epo_espacenet_DE2060516A1
source esp@cenet
subjects CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
FERROUS OR NON-FERROUS ALLOYS
INORGANIC CHEMISTRY
METALLURGY
PERFORMING OPERATIONS
PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
SEPARATION
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Verfahren zur Beseitigung von Molybdaenverunreinigungen aus nickel-,eisen- und schwefelhaltigen Produkten
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-15T19%3A38%3A36IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=MEHL.ERNEST&rft.date=1971-11-18&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EDE2060516A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true