Kautschukmischung für Reifenlaufstreifen

Sulphur vulcanised rubber mixture comprises: (a) 100 pph diene elastomer(s) from natural rubber, synthetic polyisoprene, polybutadiene, acrylonitrile-butadiene and/or butadiene-styrene; (b) 35-100 pph of filler comprising (b1) 12-97% carbon back of average particle size 20-40 nm, dibutyl phthalate (...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WILHELM, ULF, 30827 GARBSEN, DE, BUSMANN, DIRK, 30165 HANNOVER, DE, STEVENS, HENDRIK., 30419 HANNOVER, DE
Format: Patent
Sprache:ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WILHELM, ULF, 30827 GARBSEN, DE
BUSMANN, DIRK, 30165 HANNOVER, DE
STEVENS, HENDRIK., 30419 HANNOVER, DE
description Sulphur vulcanised rubber mixture comprises: (a) 100 pph diene elastomer(s) from natural rubber, synthetic polyisoprene, polybutadiene, acrylonitrile-butadiene and/or butadiene-styrene; (b) 35-100 pph of filler comprising (b1) 12-97% carbon back of average particle size 20-40 nm, dibutyl phthalate (DBP)/cetyl trimethyl ammonium bromide (CTAB) ratio > 1.5, DBP number > 145 ml/100 g, CTAB number 70-100 m /g and CDBP number > 100 mg/100 g and (b2) 3-88% finely divided sillicic acid of BET surface area 145-270 m /g, CTAB number 120-285 m /g and pore vol. 0.7-1.7 m/g; and (c) other additives. Also claimed are tyres made using the above rubber mixture. Preferably the mixture contains at least 60 pph natural rubber and 30-65 pph filler. Alternatively, it contains at least 60 pph diene elastomer from synthetic polyisoprene, polybutadiene, acrylonitrile-butadiene and/or butadiene-styrene and 60-100 pph filler. Preferably the filer comprises 50-80% carbon black and also non-activated silicic acid. The mixture contains bis-3(triethoxy-silylpropy)tetrasulphide (TESPT).
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_DE19644888A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>DE19644888A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_DE19644888A13</originalsourceid><addsrcrecordid>eNrjZND0TiwtKU7OKM3OzQRReekKaYf3FCkEpWampeblJJamFZcUgdk8DKxpiTnFqbxQmptB0c01xNlDN7UgPz61uCAxOTUvtSTexdXQ0szExMLCwtHQmBg1AJ8YKis</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Kautschukmischung für Reifenlaufstreifen</title><source>esp@cenet</source><creator>WILHELM, ULF, 30827 GARBSEN, DE ; BUSMANN, DIRK, 30165 HANNOVER, DE ; STEVENS, HENDRIK., 30419 HANNOVER, DE</creator><creatorcontrib>WILHELM, ULF, 30827 GARBSEN, DE ; BUSMANN, DIRK, 30165 HANNOVER, DE ; STEVENS, HENDRIK., 30419 HANNOVER, DE</creatorcontrib><description>Sulphur vulcanised rubber mixture comprises: (a) 100 pph diene elastomer(s) from natural rubber, synthetic polyisoprene, polybutadiene, acrylonitrile-butadiene and/or butadiene-styrene; (b) 35-100 pph of filler comprising (b1) 12-97% carbon back of average particle size 20-40 nm, dibutyl phthalate (DBP)/cetyl trimethyl ammonium bromide (CTAB) ratio &gt; 1.5, DBP number &gt; 145 ml/100 g, CTAB number 70-100 m /g and CDBP number &gt; 100 mg/100 g and (b2) 3-88% finely divided sillicic acid of BET surface area 145-270 m /g, CTAB number 120-285 m /g and pore vol. 0.7-1.7 m/g; and (c) other additives. Also claimed are tyres made using the above rubber mixture. Preferably the mixture contains at least 60 pph natural rubber and 30-65 pph filler. Alternatively, it contains at least 60 pph diene elastomer from synthetic polyisoprene, polybutadiene, acrylonitrile-butadiene and/or butadiene-styrene and 60-100 pph filler. Preferably the filer comprises 50-80% carbon black and also non-activated silicic acid. The mixture contains bis-3(triethoxy-silylpropy)tetrasulphide (TESPT).</description><edition>6</edition><language>ger</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; DEVICES OR ARRANGEMENTS RELATED TO TYRES ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; PERFORMING OPERATIONS ; REPAIRING, OR CONNECTING VALVES TO, INFLATABLE ELASTIC BODIESIN GENERAL ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; TRANSPORTING ; TYRE CHANGING OR REPAIRING ; TYRE INFLATION ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS ; VEHICLE TYRES ; VEHICLES IN GENERAL</subject><creationdate>1998</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19980430&amp;DB=EPODOC&amp;CC=DE&amp;NR=19644888A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25551,76302</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=19980430&amp;DB=EPODOC&amp;CC=DE&amp;NR=19644888A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WILHELM, ULF, 30827 GARBSEN, DE</creatorcontrib><creatorcontrib>BUSMANN, DIRK, 30165 HANNOVER, DE</creatorcontrib><creatorcontrib>STEVENS, HENDRIK., 30419 HANNOVER, DE</creatorcontrib><title>Kautschukmischung für Reifenlaufstreifen</title><description>Sulphur vulcanised rubber mixture comprises: (a) 100 pph diene elastomer(s) from natural rubber, synthetic polyisoprene, polybutadiene, acrylonitrile-butadiene and/or butadiene-styrene; (b) 35-100 pph of filler comprising (b1) 12-97% carbon back of average particle size 20-40 nm, dibutyl phthalate (DBP)/cetyl trimethyl ammonium bromide (CTAB) ratio &gt; 1.5, DBP number &gt; 145 ml/100 g, CTAB number 70-100 m /g and CDBP number &gt; 100 mg/100 g and (b2) 3-88% finely divided sillicic acid of BET surface area 145-270 m /g, CTAB number 120-285 m /g and pore vol. 0.7-1.7 m/g; and (c) other additives. Also claimed are tyres made using the above rubber mixture. Preferably the mixture contains at least 60 pph natural rubber and 30-65 pph filler. Alternatively, it contains at least 60 pph diene elastomer from synthetic polyisoprene, polybutadiene, acrylonitrile-butadiene and/or butadiene-styrene and 60-100 pph filler. Preferably the filer comprises 50-80% carbon black and also non-activated silicic acid. The mixture contains bis-3(triethoxy-silylpropy)tetrasulphide (TESPT).</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>DEVICES OR ARRANGEMENTS RELATED TO TYRES</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PERFORMING OPERATIONS</subject><subject>REPAIRING, OR CONNECTING VALVES TO, INFLATABLE ELASTIC BODIESIN GENERAL</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>TRANSPORTING</subject><subject>TYRE CHANGING OR REPAIRING</subject><subject>TYRE INFLATION</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><subject>VEHICLE TYRES</subject><subject>VEHICLES IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>1998</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZND0TiwtKU7OKM3OzQRReekKaYf3FCkEpWampeblJJamFZcUgdk8DKxpiTnFqbxQmptB0c01xNlDN7UgPz61uCAxOTUvtSTexdXQ0szExMLCwtHQmBg1AJ8YKis</recordid><startdate>19980430</startdate><enddate>19980430</enddate><creator>WILHELM, ULF, 30827 GARBSEN, DE</creator><creator>BUSMANN, DIRK, 30165 HANNOVER, DE</creator><creator>STEVENS, HENDRIK., 30419 HANNOVER, DE</creator><scope>EVB</scope></search><sort><creationdate>19980430</creationdate><title>Kautschukmischung für Reifenlaufstreifen</title><author>WILHELM, ULF, 30827 GARBSEN, DE ; BUSMANN, DIRK, 30165 HANNOVER, DE ; STEVENS, HENDRIK., 30419 HANNOVER, DE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_DE19644888A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>ger</language><creationdate>1998</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>DEVICES OR ARRANGEMENTS RELATED TO TYRES</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PERFORMING OPERATIONS</topic><topic>REPAIRING, OR CONNECTING VALVES TO, INFLATABLE ELASTIC BODIESIN GENERAL</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>TRANSPORTING</topic><topic>TYRE CHANGING OR REPAIRING</topic><topic>TYRE INFLATION</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><topic>VEHICLE TYRES</topic><topic>VEHICLES IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>WILHELM, ULF, 30827 GARBSEN, DE</creatorcontrib><creatorcontrib>BUSMANN, DIRK, 30165 HANNOVER, DE</creatorcontrib><creatorcontrib>STEVENS, HENDRIK., 30419 HANNOVER, DE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WILHELM, ULF, 30827 GARBSEN, DE</au><au>BUSMANN, DIRK, 30165 HANNOVER, DE</au><au>STEVENS, HENDRIK., 30419 HANNOVER, DE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Kautschukmischung für Reifenlaufstreifen</title><date>1998-04-30</date><risdate>1998</risdate><abstract>Sulphur vulcanised rubber mixture comprises: (a) 100 pph diene elastomer(s) from natural rubber, synthetic polyisoprene, polybutadiene, acrylonitrile-butadiene and/or butadiene-styrene; (b) 35-100 pph of filler comprising (b1) 12-97% carbon back of average particle size 20-40 nm, dibutyl phthalate (DBP)/cetyl trimethyl ammonium bromide (CTAB) ratio &gt; 1.5, DBP number &gt; 145 ml/100 g, CTAB number 70-100 m /g and CDBP number &gt; 100 mg/100 g and (b2) 3-88% finely divided sillicic acid of BET surface area 145-270 m /g, CTAB number 120-285 m /g and pore vol. 0.7-1.7 m/g; and (c) other additives. Also claimed are tyres made using the above rubber mixture. Preferably the mixture contains at least 60 pph natural rubber and 30-65 pph filler. Alternatively, it contains at least 60 pph diene elastomer from synthetic polyisoprene, polybutadiene, acrylonitrile-butadiene and/or butadiene-styrene and 60-100 pph filler. Preferably the filer comprises 50-80% carbon black and also non-activated silicic acid. The mixture contains bis-3(triethoxy-silylpropy)tetrasulphide (TESPT).</abstract><edition>6</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language ger
recordid cdi_epo_espacenet_DE19644888A1
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
DEVICES OR ARRANGEMENTS RELATED TO TYRES
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
PERFORMING OPERATIONS
REPAIRING, OR CONNECTING VALVES TO, INFLATABLE ELASTIC BODIESIN GENERAL
THEIR PREPARATION OR CHEMICAL WORKING-UP
TRANSPORTING
TYRE CHANGING OR REPAIRING
TYRE INFLATION
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS
VEHICLE TYRES
VEHICLES IN GENERAL
title Kautschukmischung für Reifenlaufstreifen
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-16T03%3A20%3A02IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WILHELM,%20ULF,%2030827%20GARBSEN,%20DE&rft.date=1998-04-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EDE19644888A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true