Metallische Bänder und deren Herstellungsverfahren

Producing a metal strip which, in addition to Fe, contains 0,01% to 0,2% C, 12% to 17% Cr, 4% to 8% Ni, 0% to 3,5% Cu, 0% to 0,5% Ti .0% to 1.8% Si and 0% to 2% Mn, includes the following steps: preparing a metal strip material with a predetermined thickness, width and length; heating until a prehea...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: Schuster, Roland
Format: Patent
Sprache:ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator Schuster, Roland
description Producing a metal strip which, in addition to Fe, contains 0,01% to 0,2% C, 12% to 17% Cr, 4% to 8% Ni, 0% to 3,5% Cu, 0% to 0,5% Ti .0% to 1.8% Si and 0% to 2% Mn, includes the following steps: preparing a metal strip material with a predetermined thickness, width and length; heating until a preheating temperature between 90 ° C and 150 ° C is reached; subsequent uniform heating from the preheating temperature to a temperature which is 5 ° C and 60 ° C lower than the predetermined target temperature for 2 h to 4 h, the target temperature is between 450 ° C and 700 ° C; subsequent uniform heating to the target temperature over 0.1 h and 1 h; endurance at target temperature for 0.5 h to 2.5 h ("endurance temperature"); cooling to an annealing temperature between 200 ° C and 400 ° C over 0.5 h to 2.5 h; subsequent cooling from the ignition temperature to room temperature.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_DE102015220591B8</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>DE102015220591B8</sourcerecordid><originalsourceid>FETCH-epo_espacenet_DE102015220591B83</originalsourceid><addsrcrecordid>eNrjZDD2TS1JzMnJLE7OSFVwOrwkLyW1SKE0L0UBSKfmKXikFhWXpObklOalF5elFqUlZgBFeRhY0xJzilN5oTQ3g6qba4izh25qQX58anFBYnJqXmpJvIuroYGRgaGpkZGBqaWhk4UxseoAz7gu7w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Metallische Bänder und deren Herstellungsverfahren</title><source>esp@cenet</source><creator>Schuster, Roland</creator><creatorcontrib>Schuster, Roland</creatorcontrib><description>Producing a metal strip which, in addition to Fe, contains 0,01% to 0,2% C, 12% to 17% Cr, 4% to 8% Ni, 0% to 3,5% Cu, 0% to 0,5% Ti .0% to 1.8% Si and 0% to 2% Mn, includes the following steps: preparing a metal strip material with a predetermined thickness, width and length; heating until a preheating temperature between 90 ° C and 150 ° C is reached; subsequent uniform heating from the preheating temperature to a temperature which is 5 ° C and 60 ° C lower than the predetermined target temperature for 2 h to 4 h, the target temperature is between 450 ° C and 700 ° C; subsequent uniform heating to the target temperature over 0.1 h and 1 h; endurance at target temperature for 0.5 h to 2.5 h ("endurance temperature"); cooling to an annealing temperature between 200 ° C and 400 ° C over 0.5 h to 2.5 h; subsequent cooling from the ignition temperature to room temperature.</description><language>ger</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2018</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180927&amp;DB=EPODOC&amp;CC=DE&amp;NR=102015220591B8$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20180927&amp;DB=EPODOC&amp;CC=DE&amp;NR=102015220591B8$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>Schuster, Roland</creatorcontrib><title>Metallische Bänder und deren Herstellungsverfahren</title><description>Producing a metal strip which, in addition to Fe, contains 0,01% to 0,2% C, 12% to 17% Cr, 4% to 8% Ni, 0% to 3,5% Cu, 0% to 0,5% Ti .0% to 1.8% Si and 0% to 2% Mn, includes the following steps: preparing a metal strip material with a predetermined thickness, width and length; heating until a preheating temperature between 90 ° C and 150 ° C is reached; subsequent uniform heating from the preheating temperature to a temperature which is 5 ° C and 60 ° C lower than the predetermined target temperature for 2 h to 4 h, the target temperature is between 450 ° C and 700 ° C; subsequent uniform heating to the target temperature over 0.1 h and 1 h; endurance at target temperature for 0.5 h to 2.5 h ("endurance temperature"); cooling to an annealing temperature between 200 ° C and 400 ° C over 0.5 h to 2.5 h; subsequent cooling from the ignition temperature to room temperature.</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2018</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDD2TS1JzMnJLE7OSFVwOrwkLyW1SKE0L0UBSKfmKXikFhWXpObklOalF5elFqUlZgBFeRhY0xJzilN5oTQ3g6qba4izh25qQX58anFBYnJqXmpJvIuroYGRgaGpkZGBqaWhk4UxseoAz7gu7w</recordid><startdate>20180927</startdate><enddate>20180927</enddate><creator>Schuster, Roland</creator><scope>EVB</scope></search><sort><creationdate>20180927</creationdate><title>Metallische Bänder und deren Herstellungsverfahren</title><author>Schuster, Roland</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_DE102015220591B83</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>ger</language><creationdate>2018</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>Schuster, Roland</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>Schuster, Roland</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Metallische Bänder und deren Herstellungsverfahren</title><date>2018-09-27</date><risdate>2018</risdate><abstract>Producing a metal strip which, in addition to Fe, contains 0,01% to 0,2% C, 12% to 17% Cr, 4% to 8% Ni, 0% to 3,5% Cu, 0% to 0,5% Ti .0% to 1.8% Si and 0% to 2% Mn, includes the following steps: preparing a metal strip material with a predetermined thickness, width and length; heating until a preheating temperature between 90 ° C and 150 ° C is reached; subsequent uniform heating from the preheating temperature to a temperature which is 5 ° C and 60 ° C lower than the predetermined target temperature for 2 h to 4 h, the target temperature is between 450 ° C and 700 ° C; subsequent uniform heating to the target temperature over 0.1 h and 1 h; endurance at target temperature for 0.5 h to 2.5 h ("endurance temperature"); cooling to an annealing temperature between 200 ° C and 400 ° C over 0.5 h to 2.5 h; subsequent cooling from the ignition temperature to room temperature.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language ger
recordid cdi_epo_espacenet_DE102015220591B8
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Metallische Bänder und deren Herstellungsverfahren
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T05%3A42%3A08IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=Schuster,%20Roland&rft.date=2018-09-27&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EDE102015220591B8%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true