Graphite particles, for cathodes of e.g. lithium ion batteries, comprise natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values

Graphite particles comprises natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values. Graphite particles comprise natural veined graphite or flake graphite particle clusters having a D50 diameter of 8-22 Micro as measu...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SHIRAHIGE, MINORU, OHZEKI, KATSUTOMO
Format: Patent
Sprache:eng ; ger
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SHIRAHIGE, MINORU
OHZEKI, KATSUTOMO
description Graphite particles comprises natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values. Graphite particles comprise natural veined graphite or flake graphite particle clusters having a D50 diameter of 8-22 Micro as measured by laser beam diffraction, a specific surface of 2.5-6 m2>/g as measured by nitrogen gas adsorption and an apparent density of >= 0.25 g/cm3> before compaction and >= 0.55 g/cm3> after compaction, the apparent density after compaction being 1.8-2.5 times that before compaction. Graphite particles comprises natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values. Graphite particles comprise natural veined graphite or flake graphite particle clusters having a D50 diameter of 8-22 microns as measured by laser beam diffraction, a specific surface of 2.5-6 m /g as measured by nitrogen gas adsorption and an apparent density of \- 0.25 g/cm before compaction and \- 0.55 g/cm after compaction, the apparent density after compaction being 1.8-2.5 times that before compaction. Es werden Graphitteilchen bereitgestellt, die für die Herstellung einer negativen Elektrode einer nicht-wäßrigen Sammelbatterie zu dem Zweck eingesetzt werden, um die Eigenschaften zum raschen Laden/Entladen und die Eigenschaften hinsichtlich der Zykluslebensdauer zu verbessern und die irreversible Kapazität im ersten Zyklus zu verringern, wobei die Graphitteilchen klumpige Graphitteilchen sind, die aus natürlichen gemaserten Graphitteilchen oder Flockengraphitteilchen gebildet und dadurch gekennzeichnet sind, daß der Teilchendurchmesser mit einer Wahrscheinlichkeit von 50% (D50-Durchmesser), die spezifische Oberfläche und die apparente Dichte dieser Teilchen auf jeweils spezifische Bereiche eingeschränkt sind.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_DE10012963A1</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>DE10012963A1</sourcerecordid><originalsourceid>FETCH-epo_espacenet_DE10012963A13</originalsourceid><addsrcrecordid>eNqNjUFKBDEQRXvjQtQ7lPtxmHZgwKXoqAdwP5Tpn-7CdBJSlRav6YmMYOPWVcH_7786776eC-dJDJS5mLgA3ZBPhRzblAYoJU_YjlsKYpPUmSRFemMzFPlhXZpzEQVFtlo40AKJGGhcvc3lA7_jL1k_kQtVm0fpo7lJM5x4aVteUHgEDcIzGrBZO0dai2cH4tiw3EyIRgOiin3SwqFCL7szz0Fx9Xsvuuun4-vDyw1yOkFzm0fY6fHY73b97d1hf9_v_8N8A0mlaA4</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Graphite particles, for cathodes of e.g. lithium ion batteries, comprise natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values</title><source>esp@cenet</source><creator>SHIRAHIGE, MINORU ; OHZEKI, KATSUTOMO</creator><creatorcontrib>SHIRAHIGE, MINORU ; OHZEKI, KATSUTOMO</creatorcontrib><description>Graphite particles comprises natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values. Graphite particles comprise natural veined graphite or flake graphite particle clusters having a D50 diameter of 8-22 Micro as measured by laser beam diffraction, a specific surface of 2.5-6 m2&gt;/g as measured by nitrogen gas adsorption and an apparent density of &gt;= 0.25 g/cm3&gt; before compaction and &gt;= 0.55 g/cm3&gt; after compaction, the apparent density after compaction being 1.8-2.5 times that before compaction. Graphite particles comprises natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values. Graphite particles comprise natural veined graphite or flake graphite particle clusters having a D50 diameter of 8-22 microns as measured by laser beam diffraction, a specific surface of 2.5-6 m /g as measured by nitrogen gas adsorption and an apparent density of \- 0.25 g/cm before compaction and \- 0.55 g/cm after compaction, the apparent density after compaction being 1.8-2.5 times that before compaction. Es werden Graphitteilchen bereitgestellt, die für die Herstellung einer negativen Elektrode einer nicht-wäßrigen Sammelbatterie zu dem Zweck eingesetzt werden, um die Eigenschaften zum raschen Laden/Entladen und die Eigenschaften hinsichtlich der Zykluslebensdauer zu verbessern und die irreversible Kapazität im ersten Zyklus zu verringern, wobei die Graphitteilchen klumpige Graphitteilchen sind, die aus natürlichen gemaserten Graphitteilchen oder Flockengraphitteilchen gebildet und dadurch gekennzeichnet sind, daß der Teilchendurchmesser mit einer Wahrscheinlichkeit von 50% (D50-Durchmesser), die spezifische Oberfläche und die apparente Dichte dieser Teilchen auf jeweils spezifische Bereiche eingeschränkt sind.</description><edition>7</edition><language>eng ; ger</language><subject>BASIC ELECTRIC ELEMENTS ; CHEMISTRY ; COMPOUNDS THEREOF ; ELECTRICITY ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2000</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20001005&amp;DB=EPODOC&amp;CC=DE&amp;NR=10012963A1$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20001005&amp;DB=EPODOC&amp;CC=DE&amp;NR=10012963A1$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SHIRAHIGE, MINORU</creatorcontrib><creatorcontrib>OHZEKI, KATSUTOMO</creatorcontrib><title>Graphite particles, for cathodes of e.g. lithium ion batteries, comprise natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values</title><description>Graphite particles comprises natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values. Graphite particles comprise natural veined graphite or flake graphite particle clusters having a D50 diameter of 8-22 Micro as measured by laser beam diffraction, a specific surface of 2.5-6 m2&gt;/g as measured by nitrogen gas adsorption and an apparent density of &gt;= 0.25 g/cm3&gt; before compaction and &gt;= 0.55 g/cm3&gt; after compaction, the apparent density after compaction being 1.8-2.5 times that before compaction. Graphite particles comprises natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values. Graphite particles comprise natural veined graphite or flake graphite particle clusters having a D50 diameter of 8-22 microns as measured by laser beam diffraction, a specific surface of 2.5-6 m /g as measured by nitrogen gas adsorption and an apparent density of \- 0.25 g/cm before compaction and \- 0.55 g/cm after compaction, the apparent density after compaction being 1.8-2.5 times that before compaction. Es werden Graphitteilchen bereitgestellt, die für die Herstellung einer negativen Elektrode einer nicht-wäßrigen Sammelbatterie zu dem Zweck eingesetzt werden, um die Eigenschaften zum raschen Laden/Entladen und die Eigenschaften hinsichtlich der Zykluslebensdauer zu verbessern und die irreversible Kapazität im ersten Zyklus zu verringern, wobei die Graphitteilchen klumpige Graphitteilchen sind, die aus natürlichen gemaserten Graphitteilchen oder Flockengraphitteilchen gebildet und dadurch gekennzeichnet sind, daß der Teilchendurchmesser mit einer Wahrscheinlichkeit von 50% (D50-Durchmesser), die spezifische Oberfläche und die apparente Dichte dieser Teilchen auf jeweils spezifische Bereiche eingeschränkt sind.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>CHEMISTRY</subject><subject>COMPOUNDS THEREOF</subject><subject>ELECTRICITY</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2000</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjUFKBDEQRXvjQtQ7lPtxmHZgwKXoqAdwP5Tpn-7CdBJSlRav6YmMYOPWVcH_7786776eC-dJDJS5mLgA3ZBPhRzblAYoJU_YjlsKYpPUmSRFemMzFPlhXZpzEQVFtlo40AKJGGhcvc3lA7_jL1k_kQtVm0fpo7lJM5x4aVteUHgEDcIzGrBZO0dai2cH4tiw3EyIRgOiin3SwqFCL7szz0Fx9Xsvuuun4-vDyw1yOkFzm0fY6fHY73b97d1hf9_v_8N8A0mlaA4</recordid><startdate>20001005</startdate><enddate>20001005</enddate><creator>SHIRAHIGE, MINORU</creator><creator>OHZEKI, KATSUTOMO</creator><scope>EVB</scope></search><sort><creationdate>20001005</creationdate><title>Graphite particles, for cathodes of e.g. lithium ion batteries, comprise natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values</title><author>SHIRAHIGE, MINORU ; OHZEKI, KATSUTOMO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_DE10012963A13</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng ; ger</language><creationdate>2000</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>CHEMISTRY</topic><topic>COMPOUNDS THEREOF</topic><topic>ELECTRICITY</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>SHIRAHIGE, MINORU</creatorcontrib><creatorcontrib>OHZEKI, KATSUTOMO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SHIRAHIGE, MINORU</au><au>OHZEKI, KATSUTOMO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Graphite particles, for cathodes of e.g. lithium ion batteries, comprise natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values</title><date>2000-10-05</date><risdate>2000</risdate><abstract>Graphite particles comprises natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values. Graphite particles comprise natural veined graphite or flake graphite particle clusters having a D50 diameter of 8-22 Micro as measured by laser beam diffraction, a specific surface of 2.5-6 m2&gt;/g as measured by nitrogen gas adsorption and an apparent density of &gt;= 0.25 g/cm3&gt; before compaction and &gt;= 0.55 g/cm3&gt; after compaction, the apparent density after compaction being 1.8-2.5 times that before compaction. Graphite particles comprises natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values. Graphite particles comprise natural veined graphite or flake graphite particle clusters having a D50 diameter of 8-22 microns as measured by laser beam diffraction, a specific surface of 2.5-6 m /g as measured by nitrogen gas adsorption and an apparent density of \- 0.25 g/cm before compaction and \- 0.55 g/cm after compaction, the apparent density after compaction being 1.8-2.5 times that before compaction. Es werden Graphitteilchen bereitgestellt, die für die Herstellung einer negativen Elektrode einer nicht-wäßrigen Sammelbatterie zu dem Zweck eingesetzt werden, um die Eigenschaften zum raschen Laden/Entladen und die Eigenschaften hinsichtlich der Zykluslebensdauer zu verbessern und die irreversible Kapazität im ersten Zyklus zu verringern, wobei die Graphitteilchen klumpige Graphitteilchen sind, die aus natürlichen gemaserten Graphitteilchen oder Flockengraphitteilchen gebildet und dadurch gekennzeichnet sind, daß der Teilchendurchmesser mit einer Wahrscheinlichkeit von 50% (D50-Durchmesser), die spezifische Oberfläche und die apparente Dichte dieser Teilchen auf jeweils spezifische Bereiche eingeschränkt sind.</abstract><edition>7</edition><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng ; ger
recordid cdi_epo_espacenet_DE10012963A1
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
CHEMISTRY
COMPOUNDS THEREOF
ELECTRICITY
INORGANIC CHEMISTRY
METALLURGY
NON-METALLIC ELEMENTS
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title Graphite particles, for cathodes of e.g. lithium ion batteries, comprise natural veined graphite or flake graphite particle clusters with specified average diameter, specific surface and apparent density values
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T07%3A35%3A13IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SHIRAHIGE,%20MINORU&rft.date=2000-10-05&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3EDE10012963A1%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true