Interwoven blanket
The making process of interwoven blanket includes: dyeing acrylon yarn of 25-40 Nm/2 with thermal shrinking performance, vapor steaming at 130 deg.c in a steaming box for 10-15 min, cooling naturally, stoving with hot blast below 130 deg.c to water content below 2 % to shrink to 80 % of original yar...
Gespeichert in:
Hauptverfasser: | , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
Zusammenfassung: | The making process of interwoven blanket includes: dyeing acrylon yarn of 25-40 Nm/2 with thermal shrinking performance, vapor steaming at 130 deg.c in a steaming box for 10-15 min, cooling naturally, stoving with hot blast below 130 deg.c to water content below 2 % to shrink to 80 % of original yarn size and loss the thermal shrinking performance within 130 deg.c, interweaving the treated yarn with un-treated yarn to form blanket blank, cutting in a breadth cutter to form even surface, and steaming and finishing the blanket blank in a steaming box at 130 deg.c to make the yarn with thermal shrinking performance shrink to form the embossed surface. Thus made blanket has stereo pattern.
一种交织毛毯的生产方法,将具有热收缩性能的25-40Nm/2晴纶纱线进行染色,在130℃蒸箱内汽蒸10-15分钟,自然降温至常温,用130℃以下的热风烘干至含水量2%以下,使其缩至原纱的80%,并丧失130℃以内的热收缩性,与未蒸化处理的纱线进行交织,所织坯毯经剖幅机割绒后,坯毯表面平整无凹凸现象,将坯毯置于130℃蒸箱内蒸化整理后,具有热收缩性能的纱线收缩形成毛毯花纹的凹部分,丧失热收缩性能的纱线形成毛毯花纹的凸部分,凹凸部分的绒面按一定规律排列时,即形成了凹凸不平,具有立体花纹的绒面的毛毯。 |
---|