Synthesis process of nanometer mesoporous gold complex

The present invention relates to the synthesis process of nanometer mesoporous gold complex. The synthesis process includes: dissolving chlorauric acid in solution prepared with template agent, water and hydrochloric acid via strirring at 0-60 deg.c for 0.3-1 hr; dropping ethyl silicate into the sol...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: GAOMENG,QI LU
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GAOMENG,QI LU
description The present invention relates to the synthesis process of nanometer mesoporous gold complex. The synthesis process includes: dissolving chlorauric acid in solution prepared with template agent, water and hydrochloric acid via strirring at 0-60 deg.c for 0.3-1 hr; dropping ethyl silicate into the solution to obtain the sol of nanometer mesoporous gold complex and crystallizing statically at 0-160 deg.c for 24-72 hr; filtering, washing and drying to obtain nanometer Ag/SiO2 mesoporous complex cake; and roasting at 450-600 deg.c in air atmosphere for eliminating the template agent to obtain the nanometer mesoporous gold complex. The present invention has simple reaction process, simple operation, low reaction temperature, wide temperature range, etc. and the prepared nanometer metal particle has size of 2.5-20 nm.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN1318298CC</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN1318298CC</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN1318298CC3</originalsourceid><addsrcrecordid>eNrjZDALrswryUgtzixWKCjKT04tLlbIT1PIS8zLz00tSS1SyE0tzi_IL8ovLVZIz89JUUjOzy3ISa3gYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxzn6GxoYWRpYWzs7GRCgBAJn7LgY</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Synthesis process of nanometer mesoporous gold complex</title><source>esp@cenet</source><creator>GAOMENG,QI LU</creator><creatorcontrib>GAOMENG,QI LU</creatorcontrib><description>The present invention relates to the synthesis process of nanometer mesoporous gold complex. The synthesis process includes: dissolving chlorauric acid in solution prepared with template agent, water and hydrochloric acid via strirring at 0-60 deg.c for 0.3-1 hr; dropping ethyl silicate into the solution to obtain the sol of nanometer mesoporous gold complex and crystallizing statically at 0-160 deg.c for 24-72 hr; filtering, washing and drying to obtain nanometer Ag/SiO2 mesoporous complex cake; and roasting at 450-600 deg.c in air atmosphere for eliminating the template agent to obtain the nanometer mesoporous gold complex. The present invention has simple reaction process, simple operation, low reaction temperature, wide temperature range, etc. and the prepared nanometer metal particle has size of 2.5-20 nm.</description><language>eng</language><subject>CHEMISTRY ; COMPOUNDS THEREOF ; INORGANIC CHEMISTRY ; METALLURGY ; NON-METALLIC ELEMENTS</subject><creationdate>2007</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20070530&amp;DB=EPODOC&amp;CC=CN&amp;NR=1318298C$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76290</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20070530&amp;DB=EPODOC&amp;CC=CN&amp;NR=1318298C$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GAOMENG,QI LU</creatorcontrib><title>Synthesis process of nanometer mesoporous gold complex</title><description>The present invention relates to the synthesis process of nanometer mesoporous gold complex. The synthesis process includes: dissolving chlorauric acid in solution prepared with template agent, water and hydrochloric acid via strirring at 0-60 deg.c for 0.3-1 hr; dropping ethyl silicate into the solution to obtain the sol of nanometer mesoporous gold complex and crystallizing statically at 0-160 deg.c for 24-72 hr; filtering, washing and drying to obtain nanometer Ag/SiO2 mesoporous complex cake; and roasting at 450-600 deg.c in air atmosphere for eliminating the template agent to obtain the nanometer mesoporous gold complex. The present invention has simple reaction process, simple operation, low reaction temperature, wide temperature range, etc. and the prepared nanometer metal particle has size of 2.5-20 nm.</description><subject>CHEMISTRY</subject><subject>COMPOUNDS THEREOF</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>NON-METALLIC ELEMENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2007</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDALrswryUgtzixWKCjKT04tLlbIT1PIS8zLz00tSS1SyE0tzi_IL8ovLVZIz89JUUjOzy3ISa3gYWBNS8wpTuWF0twMCm6uIc4euqkF-fGpxQWJyal5qSXxzn6GxoYWRpYWzs7GRCgBAJn7LgY</recordid><startdate>20070530</startdate><enddate>20070530</enddate><creator>GAOMENG,QI LU</creator><scope>EVB</scope></search><sort><creationdate>20070530</creationdate><title>Synthesis process of nanometer mesoporous gold complex</title><author>GAOMENG,QI LU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN1318298CC3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2007</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS THEREOF</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>NON-METALLIC ELEMENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>GAOMENG,QI LU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GAOMENG,QI LU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Synthesis process of nanometer mesoporous gold complex</title><date>2007-05-30</date><risdate>2007</risdate><abstract>The present invention relates to the synthesis process of nanometer mesoporous gold complex. The synthesis process includes: dissolving chlorauric acid in solution prepared with template agent, water and hydrochloric acid via strirring at 0-60 deg.c for 0.3-1 hr; dropping ethyl silicate into the solution to obtain the sol of nanometer mesoporous gold complex and crystallizing statically at 0-160 deg.c for 24-72 hr; filtering, washing and drying to obtain nanometer Ag/SiO2 mesoporous complex cake; and roasting at 450-600 deg.c in air atmosphere for eliminating the template agent to obtain the nanometer mesoporous gold complex. The present invention has simple reaction process, simple operation, low reaction temperature, wide temperature range, etc. and the prepared nanometer metal particle has size of 2.5-20 nm.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_CN1318298CC
source esp@cenet
subjects CHEMISTRY
COMPOUNDS THEREOF
INORGANIC CHEMISTRY
METALLURGY
NON-METALLIC ELEMENTS
title Synthesis process of nanometer mesoporous gold complex
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-01T18%3A35%3A40IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GAOMENG,QI%20LU&rft.date=2007-05-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN1318298CC%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true