Method for forming ohmic contact to semiconductor

The present invention provides a system and method for creating self-doping contacts to silicon devices in which the contact metal is coated with a layer of dopant and subjected to high temperature, thereby alloying the silver with the silicon and simultaneously doping the silicon substrate and form...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
1. Verfasser: DANIEL L. MEIER,HUBERT P. DAVIS,RUTH A. GARCIA
Format: Patent
Sprache:eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator DANIEL L. MEIER,HUBERT P. DAVIS,RUTH A. GARCIA
description The present invention provides a system and method for creating self-doping contacts to silicon devices in which the contact metal is coated with a layer of dopant and subjected to high temperature, thereby alloying the silver with the silicon and simultaneously doping the silicon substrate and forming a low-resistance ohmic contact to it. A self-doping negative contact may be formed from unalloyed silver which may be applied to the silicon substrate by either sputtering, screen printing a paste or evaporation. The silver is coated with a layer of dopant. Once applied, the silver, substrate and dopant are heated to a temperature above the Ag-Si eutectic temperature (but below the melting point of silicon). The silver liquefies more than a eutectic proportion of the silicon substrate. The temperature is then decreased towards the eutectic temperature. As the temperature is decreased, the molten silicon reforms through liquid-phase epitaxy and while so doing dopant atoms are incorporated into the re-grown silicon lattice. Once the temperature drops below the silver-silicon eutectic temperature the silicon which has not already been reincorporated into the substrate through epitaxial re-growth forms a solid-phase alloy with the silver. This alloy of silver and silicon is the final contact material, and is composed of eutectic proportions of silicon and silver. Under eutectic proportions there is significantly more silver than silicon in the final contact material, thereby insuring good electrical conductivity of the final contact material.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN1260830CC</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN1260830CC</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN1260830CC3</originalsourceid><addsrcrecordid>eNrjZDD0TS3JyE9RSMsvAuHczLx0hfyM3MxkheT8vJLE5BKFknyF4lSgQH5eSmlySX4RDwNrWmJOcSovlOZmUHBzDXH20E0tyI9PLS5ITE7NSy2Jd_YzNDIzsDA2cHY2JkIJAEn5K4A</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for forming ohmic contact to semiconductor</title><source>esp@cenet</source><creator>DANIEL L. MEIER,HUBERT P. DAVIS,RUTH A. GARCIA</creator><creatorcontrib>DANIEL L. MEIER,HUBERT P. DAVIS,RUTH A. GARCIA</creatorcontrib><description>The present invention provides a system and method for creating self-doping contacts to silicon devices in which the contact metal is coated with a layer of dopant and subjected to high temperature, thereby alloying the silver with the silicon and simultaneously doping the silicon substrate and forming a low-resistance ohmic contact to it. A self-doping negative contact may be formed from unalloyed silver which may be applied to the silicon substrate by either sputtering, screen printing a paste or evaporation. The silver is coated with a layer of dopant. Once applied, the silver, substrate and dopant are heated to a temperature above the Ag-Si eutectic temperature (but below the melting point of silicon). The silver liquefies more than a eutectic proportion of the silicon substrate. The temperature is then decreased towards the eutectic temperature. As the temperature is decreased, the molten silicon reforms through liquid-phase epitaxy and while so doing dopant atoms are incorporated into the re-grown silicon lattice. Once the temperature drops below the silver-silicon eutectic temperature the silicon which has not already been reincorporated into the substrate through epitaxial re-growth forms a solid-phase alloy with the silver. This alloy of silver and silicon is the final contact material, and is composed of eutectic proportions of silicon and silver. Under eutectic proportions there is significantly more silver than silicon in the final contact material, thereby insuring good electrical conductivity of the final contact material.</description><language>eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR ; ELECTRICITY ; SEMICONDUCTOR DEVICES</subject><creationdate>2006</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20060621&amp;DB=EPODOC&amp;CC=CN&amp;NR=1260830C$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20060621&amp;DB=EPODOC&amp;CC=CN&amp;NR=1260830C$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DANIEL L. MEIER,HUBERT P. DAVIS,RUTH A. GARCIA</creatorcontrib><title>Method for forming ohmic contact to semiconductor</title><description>The present invention provides a system and method for creating self-doping contacts to silicon devices in which the contact metal is coated with a layer of dopant and subjected to high temperature, thereby alloying the silver with the silicon and simultaneously doping the silicon substrate and forming a low-resistance ohmic contact to it. A self-doping negative contact may be formed from unalloyed silver which may be applied to the silicon substrate by either sputtering, screen printing a paste or evaporation. The silver is coated with a layer of dopant. Once applied, the silver, substrate and dopant are heated to a temperature above the Ag-Si eutectic temperature (but below the melting point of silicon). The silver liquefies more than a eutectic proportion of the silicon substrate. The temperature is then decreased towards the eutectic temperature. As the temperature is decreased, the molten silicon reforms through liquid-phase epitaxy and while so doing dopant atoms are incorporated into the re-grown silicon lattice. Once the temperature drops below the silver-silicon eutectic temperature the silicon which has not already been reincorporated into the substrate through epitaxial re-growth forms a solid-phase alloy with the silver. This alloy of silver and silicon is the final contact material, and is composed of eutectic proportions of silicon and silver. Under eutectic proportions there is significantly more silver than silicon in the final contact material, thereby insuring good electrical conductivity of the final contact material.</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR</subject><subject>ELECTRICITY</subject><subject>SEMICONDUCTOR DEVICES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2006</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDD0TS3JyE9RSMsvAuHczLx0hfyM3MxkheT8vJLE5BKFknyF4lSgQH5eSmlySX4RDwNrWmJOcSovlOZmUHBzDXH20E0tyI9PLS5ITE7NSy2Jd_YzNDIzsDA2cHY2JkIJAEn5K4A</recordid><startdate>20060621</startdate><enddate>20060621</enddate><creator>DANIEL L. MEIER,HUBERT P. DAVIS,RUTH A. GARCIA</creator><scope>EVB</scope></search><sort><creationdate>20060621</creationdate><title>Method for forming ohmic contact to semiconductor</title><author>DANIEL L. MEIER,HUBERT P. DAVIS,RUTH A. GARCIA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN1260830CC3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>eng</language><creationdate>2006</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR</topic><topic>ELECTRICITY</topic><topic>SEMICONDUCTOR DEVICES</topic><toplevel>online_resources</toplevel><creatorcontrib>DANIEL L. MEIER,HUBERT P. DAVIS,RUTH A. GARCIA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DANIEL L. MEIER,HUBERT P. DAVIS,RUTH A. GARCIA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for forming ohmic contact to semiconductor</title><date>2006-06-21</date><risdate>2006</risdate><abstract>The present invention provides a system and method for creating self-doping contacts to silicon devices in which the contact metal is coated with a layer of dopant and subjected to high temperature, thereby alloying the silver with the silicon and simultaneously doping the silicon substrate and forming a low-resistance ohmic contact to it. A self-doping negative contact may be formed from unalloyed silver which may be applied to the silicon substrate by either sputtering, screen printing a paste or evaporation. The silver is coated with a layer of dopant. Once applied, the silver, substrate and dopant are heated to a temperature above the Ag-Si eutectic temperature (but below the melting point of silicon). The silver liquefies more than a eutectic proportion of the silicon substrate. The temperature is then decreased towards the eutectic temperature. As the temperature is decreased, the molten silicon reforms through liquid-phase epitaxy and while so doing dopant atoms are incorporated into the re-grown silicon lattice. Once the temperature drops below the silver-silicon eutectic temperature the silicon which has not already been reincorporated into the substrate through epitaxial re-growth forms a solid-phase alloy with the silver. This alloy of silver and silicon is the final contact material, and is composed of eutectic proportions of silicon and silver. Under eutectic proportions there is significantly more silver than silicon in the final contact material, thereby insuring good electrical conductivity of the final contact material.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language eng
recordid cdi_epo_espacenet_CN1260830CC
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRIC SOLID STATE DEVICES NOT OTHERWISE PROVIDED FOR
ELECTRICITY
SEMICONDUCTOR DEVICES
title Method for forming ohmic contact to semiconductor
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-25T14%3A03%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DANIEL%20L.%20MEIER,HUBERT%20P.%20DAVIS,RUTH%20A.%20GARCIA&rft.date=2006-06-21&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN1260830CC%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true