High-temperature stable high-entropy ceramic material with excellent energy storage performance and preparation method of high-temperature stable high-entropy ceramic material

The invention discloses a high-temperature stable high-entropy ceramic material with excellent energy storage performance and a preparation method thereof.The preparation method comprises the steps that firstly, according to the molar ratio of (Ba0. 3Sr0. 7) TiO3, (Na0. 5Bi0. 5) TiO3 and (K0. 5Bi0....

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU SENWEI, LI XIN, CUI YONGFEI, WANG ZHUO
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LIU SENWEI
LI XIN
CUI YONGFEI
WANG ZHUO
description The invention discloses a high-temperature stable high-entropy ceramic material with excellent energy storage performance and a preparation method thereof.The preparation method comprises the steps that firstly, according to the molar ratio of (Ba0. 3Sr0. 7) TiO3, (Na0. 5Bi0. 5) TiO3 and (K0. 5Bi0. 5) TiO3, raw materials, absolute ethyl alcohol and zirconium oxide ballstone are subjected to ball milling and mixing, after drying and calcining are conducted respectively, (Ba0. 3Sr0. 7) TiO3 powder, (Na0. 5Bi0. 5) TiO3 powder and (K0. 5Bi0. 5) TiO3 powder are obtained, according to the molar ratio of (Ba0. 12Sr0. 28K0. 3xBi0. 3Nax) TiO3 (x is larger than or equal to 0.125 and smaller than or equal to 0.2 The preparation method comprises the following steps: drying the raw materials to obtain final material powder, pre-pressing the material powder through a mold, carrying out cold isostatic pressing, and sintering at 1220-1250 DEG C for 4 hours to obtain the high-entropy perovskite ceramic, the high-entropy perov
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118878319A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118878319A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118878319A3</originalsourceid><addsrcrecordid>eNqVTjsOgkAUpLEw6h2eB6AgFGJpiIbKyp48lwE22V8ea5RTeUXX6AG0mmT-y-zZ6GHMI2yAcLwJaIp8NaDxzcNF8WEmlUSrFVmOEM2G7jqOhIeCMclDcJBhTlEvPIBSV-_FslMgdh0FQeBUr70jizj6jnz_Wfh3eZ0tejYTNl9cZdvT8VI3OYJvMQVW6Uts63NRVNWuKov9ofzF8wLxdVx_</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>High-temperature stable high-entropy ceramic material with excellent energy storage performance and preparation method of high-temperature stable high-entropy ceramic material</title><source>esp@cenet</source><creator>LIU SENWEI ; LI XIN ; CUI YONGFEI ; WANG ZHUO</creator><creatorcontrib>LIU SENWEI ; LI XIN ; CUI YONGFEI ; WANG ZHUO</creatorcontrib><description>The invention discloses a high-temperature stable high-entropy ceramic material with excellent energy storage performance and a preparation method thereof.The preparation method comprises the steps that firstly, according to the molar ratio of (Ba0. 3Sr0. 7) TiO3, (Na0. 5Bi0. 5) TiO3 and (K0. 5Bi0. 5) TiO3, raw materials, absolute ethyl alcohol and zirconium oxide ballstone are subjected to ball milling and mixing, after drying and calcining are conducted respectively, (Ba0. 3Sr0. 7) TiO3 powder, (Na0. 5Bi0. 5) TiO3 powder and (K0. 5Bi0. 5) TiO3 powder are obtained, according to the molar ratio of (Ba0. 12Sr0. 28K0. 3xBi0. 3Nax) TiO3 (x is larger than or equal to 0.125 and smaller than or equal to 0.2 The preparation method comprises the following steps: drying the raw materials to obtain final material powder, pre-pressing the material powder through a mold, carrying out cold isostatic pressing, and sintering at 1220-1250 DEG C for 4 hours to obtain the high-entropy perovskite ceramic, the high-entropy perov</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20241101&amp;DB=EPODOC&amp;CC=CN&amp;NR=118878319A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20241101&amp;DB=EPODOC&amp;CC=CN&amp;NR=118878319A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIU SENWEI</creatorcontrib><creatorcontrib>LI XIN</creatorcontrib><creatorcontrib>CUI YONGFEI</creatorcontrib><creatorcontrib>WANG ZHUO</creatorcontrib><title>High-temperature stable high-entropy ceramic material with excellent energy storage performance and preparation method of high-temperature stable high-entropy ceramic material</title><description>The invention discloses a high-temperature stable high-entropy ceramic material with excellent energy storage performance and a preparation method thereof.The preparation method comprises the steps that firstly, according to the molar ratio of (Ba0. 3Sr0. 7) TiO3, (Na0. 5Bi0. 5) TiO3 and (K0. 5Bi0. 5) TiO3, raw materials, absolute ethyl alcohol and zirconium oxide ballstone are subjected to ball milling and mixing, after drying and calcining are conducted respectively, (Ba0. 3Sr0. 7) TiO3 powder, (Na0. 5Bi0. 5) TiO3 powder and (K0. 5Bi0. 5) TiO3 powder are obtained, according to the molar ratio of (Ba0. 12Sr0. 28K0. 3xBi0. 3Nax) TiO3 (x is larger than or equal to 0.125 and smaller than or equal to 0.2 The preparation method comprises the following steps: drying the raw materials to obtain final material powder, pre-pressing the material powder through a mold, carrying out cold isostatic pressing, and sintering at 1220-1250 DEG C for 4 hours to obtain the high-entropy perovskite ceramic, the high-entropy perov</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqVTjsOgkAUpLEw6h2eB6AgFGJpiIbKyp48lwE22V8ea5RTeUXX6AG0mmT-y-zZ6GHMI2yAcLwJaIp8NaDxzcNF8WEmlUSrFVmOEM2G7jqOhIeCMclDcJBhTlEvPIBSV-_FslMgdh0FQeBUr70jizj6jnz_Wfh3eZ0tejYTNl9cZdvT8VI3OYJvMQVW6Uts63NRVNWuKov9ofzF8wLxdVx_</recordid><startdate>20241101</startdate><enddate>20241101</enddate><creator>LIU SENWEI</creator><creator>LI XIN</creator><creator>CUI YONGFEI</creator><creator>WANG ZHUO</creator><scope>EVB</scope></search><sort><creationdate>20241101</creationdate><title>High-temperature stable high-entropy ceramic material with excellent energy storage performance and preparation method of high-temperature stable high-entropy ceramic material</title><author>LIU SENWEI ; LI XIN ; CUI YONGFEI ; WANG ZHUO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118878319A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>LIU SENWEI</creatorcontrib><creatorcontrib>LI XIN</creatorcontrib><creatorcontrib>CUI YONGFEI</creatorcontrib><creatorcontrib>WANG ZHUO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIU SENWEI</au><au>LI XIN</au><au>CUI YONGFEI</au><au>WANG ZHUO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>High-temperature stable high-entropy ceramic material with excellent energy storage performance and preparation method of high-temperature stable high-entropy ceramic material</title><date>2024-11-01</date><risdate>2024</risdate><abstract>The invention discloses a high-temperature stable high-entropy ceramic material with excellent energy storage performance and a preparation method thereof.The preparation method comprises the steps that firstly, according to the molar ratio of (Ba0. 3Sr0. 7) TiO3, (Na0. 5Bi0. 5) TiO3 and (K0. 5Bi0. 5) TiO3, raw materials, absolute ethyl alcohol and zirconium oxide ballstone are subjected to ball milling and mixing, after drying and calcining are conducted respectively, (Ba0. 3Sr0. 7) TiO3 powder, (Na0. 5Bi0. 5) TiO3 powder and (K0. 5Bi0. 5) TiO3 powder are obtained, according to the molar ratio of (Ba0. 12Sr0. 28K0. 3xBi0. 3Nax) TiO3 (x is larger than or equal to 0.125 and smaller than or equal to 0.2 The preparation method comprises the following steps: drying the raw materials to obtain final material powder, pre-pressing the material powder through a mold, carrying out cold isostatic pressing, and sintering at 1220-1250 DEG C for 4 hours to obtain the high-entropy perovskite ceramic, the high-entropy perov</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN118878319A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title High-temperature stable high-entropy ceramic material with excellent energy storage performance and preparation method of high-temperature stable high-entropy ceramic material
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-13T23%3A37%3A14IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIU%20SENWEI&rft.date=2024-11-01&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118878319A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true