Pre-lithiation method of silicon negative electrode and assembling method of lithium ion battery

The invention relates to the field of lithium ion batteries, and discloses a pre-lithiation method of a silicon negative electrode and an assembling method of a lithium ion battery. The pre-lithiation treatment of the silicon negative electrode plate is realized by directly contacting the metal lith...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: CHEN NANTAO, ZHANG ZHENG, CHU GUANGHUI, YUAN DONGYA, GAO JIAOYANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator CHEN NANTAO
ZHANG ZHENG
CHU GUANGHUI
YUAN DONGYA
GAO JIAOYANG
description The invention relates to the field of lithium ion batteries, and discloses a pre-lithiation method of a silicon negative electrode and an assembling method of a lithium ion battery. The pre-lithiation treatment of the silicon negative electrode plate is realized by directly contacting the metal lithium plate with the silicon negative electrode plate under the infiltration of the electrolyte, and the pre-lithiation degree is controlled by controlling the contact time. According to the invention, simple and convenient pre-lithiation treatment can be carried out on the silicon negative electrode piece, impurities are not introduced, the original morphology of silicon negative electrode active particles is preserved, the internal resistance of the battery is reduced, and the first coulombic efficiency is obviously improved; therefore, better rate capability and cycle performance are obtained. 本申请涉及锂离子电池领域,公开了一种硅负极的预锂化方法以及锂离子电池的组装方法。本申请通过让金属锂片与硅负极极片在电解液的浸润下直接接触,来实现对硅负极极片的预锂化处理,并通过控制接触时间来控制预锂化的程度。通过本申请可以实现对硅负极极片进行简
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118738296A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118738296A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118738296A3</originalsourceid><addsrcrecordid>eNrjZEgIKErVzcksychMLMnMz1PITS3JyE9RyE9TKM7MyUwGiuSlpgOlylIVUnNSk0uK8lNSFRLzUhQSi4tTc5NyMvPSkfSADSrNVQCZlJRYUpJaVMnDwJqWmFOcyguluRkU3VxDnD10Uwvy41OLCxKTU_NSS-Kd_QwNLcyNLYwszRyNiVEDAObqPaY</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Pre-lithiation method of silicon negative electrode and assembling method of lithium ion battery</title><source>esp@cenet</source><creator>CHEN NANTAO ; ZHANG ZHENG ; CHU GUANGHUI ; YUAN DONGYA ; GAO JIAOYANG</creator><creatorcontrib>CHEN NANTAO ; ZHANG ZHENG ; CHU GUANGHUI ; YUAN DONGYA ; GAO JIAOYANG</creatorcontrib><description>The invention relates to the field of lithium ion batteries, and discloses a pre-lithiation method of a silicon negative electrode and an assembling method of a lithium ion battery. The pre-lithiation treatment of the silicon negative electrode plate is realized by directly contacting the metal lithium plate with the silicon negative electrode plate under the infiltration of the electrolyte, and the pre-lithiation degree is controlled by controlling the contact time. According to the invention, simple and convenient pre-lithiation treatment can be carried out on the silicon negative electrode piece, impurities are not introduced, the original morphology of silicon negative electrode active particles is preserved, the internal resistance of the battery is reduced, and the first coulombic efficiency is obviously improved; therefore, better rate capability and cycle performance are obtained. 本申请涉及锂离子电池领域,公开了一种硅负极的预锂化方法以及锂离子电池的组装方法。本申请通过让金属锂片与硅负极极片在电解液的浸润下直接接触,来实现对硅负极极片的预锂化处理,并通过控制接触时间来控制预锂化的程度。通过本申请可以实现对硅负极极片进行简</description><language>chi ; eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20241001&amp;DB=EPODOC&amp;CC=CN&amp;NR=118738296A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20241001&amp;DB=EPODOC&amp;CC=CN&amp;NR=118738296A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CHEN NANTAO</creatorcontrib><creatorcontrib>ZHANG ZHENG</creatorcontrib><creatorcontrib>CHU GUANGHUI</creatorcontrib><creatorcontrib>YUAN DONGYA</creatorcontrib><creatorcontrib>GAO JIAOYANG</creatorcontrib><title>Pre-lithiation method of silicon negative electrode and assembling method of lithium ion battery</title><description>The invention relates to the field of lithium ion batteries, and discloses a pre-lithiation method of a silicon negative electrode and an assembling method of a lithium ion battery. The pre-lithiation treatment of the silicon negative electrode plate is realized by directly contacting the metal lithium plate with the silicon negative electrode plate under the infiltration of the electrolyte, and the pre-lithiation degree is controlled by controlling the contact time. According to the invention, simple and convenient pre-lithiation treatment can be carried out on the silicon negative electrode piece, impurities are not introduced, the original morphology of silicon negative electrode active particles is preserved, the internal resistance of the battery is reduced, and the first coulombic efficiency is obviously improved; therefore, better rate capability and cycle performance are obtained. 本申请涉及锂离子电池领域,公开了一种硅负极的预锂化方法以及锂离子电池的组装方法。本申请通过让金属锂片与硅负极极片在电解液的浸润下直接接触,来实现对硅负极极片的预锂化处理,并通过控制接触时间来控制预锂化的程度。通过本申请可以实现对硅负极极片进行简</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZEgIKErVzcksychMLMnMz1PITS3JyE9RyE9TKM7MyUwGiuSlpgOlylIVUnNSk0uK8lNSFRLzUhQSi4tTc5NyMvPSkfSADSrNVQCZlJRYUpJaVMnDwJqWmFOcyguluRkU3VxDnD10Uwvy41OLCxKTU_NSS-Kd_QwNLcyNLYwszRyNiVEDAObqPaY</recordid><startdate>20241001</startdate><enddate>20241001</enddate><creator>CHEN NANTAO</creator><creator>ZHANG ZHENG</creator><creator>CHU GUANGHUI</creator><creator>YUAN DONGYA</creator><creator>GAO JIAOYANG</creator><scope>EVB</scope></search><sort><creationdate>20241001</creationdate><title>Pre-lithiation method of silicon negative electrode and assembling method of lithium ion battery</title><author>CHEN NANTAO ; ZHANG ZHENG ; CHU GUANGHUI ; YUAN DONGYA ; GAO JIAOYANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118738296A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>CHEN NANTAO</creatorcontrib><creatorcontrib>ZHANG ZHENG</creatorcontrib><creatorcontrib>CHU GUANGHUI</creatorcontrib><creatorcontrib>YUAN DONGYA</creatorcontrib><creatorcontrib>GAO JIAOYANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CHEN NANTAO</au><au>ZHANG ZHENG</au><au>CHU GUANGHUI</au><au>YUAN DONGYA</au><au>GAO JIAOYANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Pre-lithiation method of silicon negative electrode and assembling method of lithium ion battery</title><date>2024-10-01</date><risdate>2024</risdate><abstract>The invention relates to the field of lithium ion batteries, and discloses a pre-lithiation method of a silicon negative electrode and an assembling method of a lithium ion battery. The pre-lithiation treatment of the silicon negative electrode plate is realized by directly contacting the metal lithium plate with the silicon negative electrode plate under the infiltration of the electrolyte, and the pre-lithiation degree is controlled by controlling the contact time. According to the invention, simple and convenient pre-lithiation treatment can be carried out on the silicon negative electrode piece, impurities are not introduced, the original morphology of silicon negative electrode active particles is preserved, the internal resistance of the battery is reduced, and the first coulombic efficiency is obviously improved; therefore, better rate capability and cycle performance are obtained. 本申请涉及锂离子电池领域,公开了一种硅负极的预锂化方法以及锂离子电池的组装方法。本申请通过让金属锂片与硅负极极片在电解液的浸润下直接接触,来实现对硅负极极片的预锂化处理,并通过控制接触时间来控制预锂化的程度。通过本申请可以实现对硅负极极片进行简</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN118738296A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRICITY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title Pre-lithiation method of silicon negative electrode and assembling method of lithium ion battery
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-07T01%3A45%3A57IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CHEN%20NANTAO&rft.date=2024-10-01&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118738296A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true