Three-component different-fineness wet spunlace non-woven fabric and preparation method thereof

The invention relates to a three-component different-fineness wet spunlaced non-woven fabric and a preparation method thereof, and relates to the technical field of non-woven fabrics, the three-component different-fineness wet spunlaced non-woven fabric comprises a body, the body comprises viscose f...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YANG ZIQIANG, CHEN YANG, QIN RUIYUAN, CHEN JIAFAN, QIN CAIHONG, YU YI, XU SHIXUE, GAN YI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
Beschreibung
Zusammenfassung:The invention relates to a three-component different-fineness wet spunlaced non-woven fabric and a preparation method thereof, and relates to the technical field of non-woven fabrics, the three-component different-fineness wet spunlaced non-woven fabric comprises a body, the body comprises viscose fibers, lyocell fibers and wood pulp fibers, the ratio of the viscose fibers to the lyocell fibers to the wood pulp fibers is A: B: C, the value range of A and B is 5-18, the value range of C is 70-80, the length-diameter ratio of the viscose fibers is 350-1000, and the length-diameter ratio of the lyocell fibers to the wood pulp fibers is 350-1000. The length-diameter ratio of the lyocell fibers is 500-1500, and the length-diameter ratio of the wood pulp fibers is 50-110. The water-based paint has the advantages of being good in wet strength and flushability. 本申请涉及一种三组份异纤度湿法水刺非织造布及其制备方法,涉及非织造布的技术领域,包括本体,本体包括粘胶纤维、莱赛尔纤维和木浆纤维,三者的比例为A:B:C,A和B的取值范围均为5-18,C的取值范围为70-80,粘胶纤维的长径比为350-1000,莱赛尔纤维的长径比为500-1500,木浆纤维的长径比为50-110。