Preparation and strengthening method of transparent cover plate glass

The invention discloses a preparation strengthening method of transparent cover plate glass, which comprises the following steps: mixing SiO2, Al2O3, P2O5, ZrO2, ZnO and other substances, melting, forming and annealing to obtain precursor glass, then carrying out three-stage heat treatment, includin...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: CHEN YAZHOU, LIANG XINHUI, ZHANG QUANGUANG, WU XIANGPING, LIAO QIBING, LI SHUZHI, HE HAOBO, WANG YUBO, TANG ZHONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator CHEN YAZHOU
LIANG XINHUI
ZHANG QUANGUANG
WU XIANGPING
LIAO QIBING
LI SHUZHI
HE HAOBO
WANG YUBO
TANG ZHONG
description The invention discloses a preparation strengthening method of transparent cover plate glass, which comprises the following steps: mixing SiO2, Al2O3, P2O5, ZrO2, ZnO and other substances, melting, forming and annealing to obtain precursor glass, then carrying out three-stage heat treatment, including two-stage heating treatment and one-stage rapid cooling treatment, and finally polishing to obtain the transparent cover plate glass. Wherein the second-stage heating treatment needs to be carried out in an SO2 atmosphere. In addition, the method also comprises the following steps: performing low-temperature ion exchange treatment by using NaNO3/KNO3 molten salt, and quickly cooling in an SO2 atmosphere after treatment, thereby finishing surface strengthening of the transparent cover plate glass. Through three-section heat treatment and neutralization and/or enhanced cooling in the SO2 atmosphere, the surface strength is enhanced, and the cleaning difficulty of residues is reduced. 本发明公开了一种透明盖板玻璃的制备强化方法,将SiO2、Al2
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118619562A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118619562A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118619562A3</originalsourceid><addsrcrecordid>eNqNyzEKwkAQRuFtLES9w3gAi1UMppQQsRIL-zAkfzaBdWbZHTy_KTyA1Wu-t3btMyNxZptViGWgYhkSbILMEugNm3QgHckyS1kkxKjXDzKlyAYKkUvZutXIsWD368btb-2ruR-QtMOy9RBY1zy8v1S-PlfH6-kf8wU8gjPJ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation and strengthening method of transparent cover plate glass</title><source>esp@cenet</source><creator>CHEN YAZHOU ; LIANG XINHUI ; ZHANG QUANGUANG ; WU XIANGPING ; LIAO QIBING ; LI SHUZHI ; HE HAOBO ; WANG YUBO ; TANG ZHONG</creator><creatorcontrib>CHEN YAZHOU ; LIANG XINHUI ; ZHANG QUANGUANG ; WU XIANGPING ; LIAO QIBING ; LI SHUZHI ; HE HAOBO ; WANG YUBO ; TANG ZHONG</creatorcontrib><description>The invention discloses a preparation strengthening method of transparent cover plate glass, which comprises the following steps: mixing SiO2, Al2O3, P2O5, ZrO2, ZnO and other substances, melting, forming and annealing to obtain precursor glass, then carrying out three-stage heat treatment, including two-stage heating treatment and one-stage rapid cooling treatment, and finally polishing to obtain the transparent cover plate glass. Wherein the second-stage heating treatment needs to be carried out in an SO2 atmosphere. In addition, the method also comprises the following steps: performing low-temperature ion exchange treatment by using NaNO3/KNO3 molten salt, and quickly cooling in an SO2 atmosphere after treatment, thereby finishing surface strengthening of the transparent cover plate glass. Through three-section heat treatment and neutralization and/or enhanced cooling in the SO2 atmosphere, the surface strength is enhanced, and the cleaning difficulty of residues is reduced. 本发明公开了一种透明盖板玻璃的制备强化方法,将SiO2、Al2</description><language>chi ; eng</language><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS ; CHEMISTRY ; GLASS ; JOINING GLASS TO GLASS OR OTHER MATERIALS ; MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES ; METALLURGY ; MINERAL OR SLAG WOOL ; SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS ; SURFACE TREATMENT OF GLASS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240910&amp;DB=EPODOC&amp;CC=CN&amp;NR=118619562A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240910&amp;DB=EPODOC&amp;CC=CN&amp;NR=118619562A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CHEN YAZHOU</creatorcontrib><creatorcontrib>LIANG XINHUI</creatorcontrib><creatorcontrib>ZHANG QUANGUANG</creatorcontrib><creatorcontrib>WU XIANGPING</creatorcontrib><creatorcontrib>LIAO QIBING</creatorcontrib><creatorcontrib>LI SHUZHI</creatorcontrib><creatorcontrib>HE HAOBO</creatorcontrib><creatorcontrib>WANG YUBO</creatorcontrib><creatorcontrib>TANG ZHONG</creatorcontrib><title>Preparation and strengthening method of transparent cover plate glass</title><description>The invention discloses a preparation strengthening method of transparent cover plate glass, which comprises the following steps: mixing SiO2, Al2O3, P2O5, ZrO2, ZnO and other substances, melting, forming and annealing to obtain precursor glass, then carrying out three-stage heat treatment, including two-stage heating treatment and one-stage rapid cooling treatment, and finally polishing to obtain the transparent cover plate glass. Wherein the second-stage heating treatment needs to be carried out in an SO2 atmosphere. In addition, the method also comprises the following steps: performing low-temperature ion exchange treatment by using NaNO3/KNO3 molten salt, and quickly cooling in an SO2 atmosphere after treatment, thereby finishing surface strengthening of the transparent cover plate glass. Through three-section heat treatment and neutralization and/or enhanced cooling in the SO2 atmosphere, the surface strength is enhanced, and the cleaning difficulty of residues is reduced. 本发明公开了一种透明盖板玻璃的制备强化方法,将SiO2、Al2</description><subject>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</subject><subject>CHEMISTRY</subject><subject>GLASS</subject><subject>JOINING GLASS TO GLASS OR OTHER MATERIALS</subject><subject>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</subject><subject>METALLURGY</subject><subject>MINERAL OR SLAG WOOL</subject><subject>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</subject><subject>SURFACE TREATMENT OF GLASS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyzEKwkAQRuFtLES9w3gAi1UMppQQsRIL-zAkfzaBdWbZHTy_KTyA1Wu-t3btMyNxZptViGWgYhkSbILMEugNm3QgHckyS1kkxKjXDzKlyAYKkUvZutXIsWD368btb-2ruR-QtMOy9RBY1zy8v1S-PlfH6-kf8wU8gjPJ</recordid><startdate>20240910</startdate><enddate>20240910</enddate><creator>CHEN YAZHOU</creator><creator>LIANG XINHUI</creator><creator>ZHANG QUANGUANG</creator><creator>WU XIANGPING</creator><creator>LIAO QIBING</creator><creator>LI SHUZHI</creator><creator>HE HAOBO</creator><creator>WANG YUBO</creator><creator>TANG ZHONG</creator><scope>EVB</scope></search><sort><creationdate>20240910</creationdate><title>Preparation and strengthening method of transparent cover plate glass</title><author>CHEN YAZHOU ; LIANG XINHUI ; ZHANG QUANGUANG ; WU XIANGPING ; LIAO QIBING ; LI SHUZHI ; HE HAOBO ; WANG YUBO ; TANG ZHONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118619562A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS</topic><topic>CHEMISTRY</topic><topic>GLASS</topic><topic>JOINING GLASS TO GLASS OR OTHER MATERIALS</topic><topic>MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES</topic><topic>METALLURGY</topic><topic>MINERAL OR SLAG WOOL</topic><topic>SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS</topic><topic>SURFACE TREATMENT OF GLASS</topic><toplevel>online_resources</toplevel><creatorcontrib>CHEN YAZHOU</creatorcontrib><creatorcontrib>LIANG XINHUI</creatorcontrib><creatorcontrib>ZHANG QUANGUANG</creatorcontrib><creatorcontrib>WU XIANGPING</creatorcontrib><creatorcontrib>LIAO QIBING</creatorcontrib><creatorcontrib>LI SHUZHI</creatorcontrib><creatorcontrib>HE HAOBO</creatorcontrib><creatorcontrib>WANG YUBO</creatorcontrib><creatorcontrib>TANG ZHONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CHEN YAZHOU</au><au>LIANG XINHUI</au><au>ZHANG QUANGUANG</au><au>WU XIANGPING</au><au>LIAO QIBING</au><au>LI SHUZHI</au><au>HE HAOBO</au><au>WANG YUBO</au><au>TANG ZHONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation and strengthening method of transparent cover plate glass</title><date>2024-09-10</date><risdate>2024</risdate><abstract>The invention discloses a preparation strengthening method of transparent cover plate glass, which comprises the following steps: mixing SiO2, Al2O3, P2O5, ZrO2, ZnO and other substances, melting, forming and annealing to obtain precursor glass, then carrying out three-stage heat treatment, including two-stage heating treatment and one-stage rapid cooling treatment, and finally polishing to obtain the transparent cover plate glass. Wherein the second-stage heating treatment needs to be carried out in an SO2 atmosphere. In addition, the method also comprises the following steps: performing low-temperature ion exchange treatment by using NaNO3/KNO3 molten salt, and quickly cooling in an SO2 atmosphere after treatment, thereby finishing surface strengthening of the transparent cover plate glass. Through three-section heat treatment and neutralization and/or enhanced cooling in the SO2 atmosphere, the surface strength is enhanced, and the cleaning difficulty of residues is reduced. 本发明公开了一种透明盖板玻璃的制备强化方法,将SiO2、Al2</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN118619562A
source esp@cenet
subjects CHEMICAL COMPOSITION OF GLASSES, GLAZES, OR VITREOUSENAMELS
CHEMISTRY
GLASS
JOINING GLASS TO GLASS OR OTHER MATERIALS
MANUFACTURE, SHAPING, OR SUPPLEMENTARY PROCESSES
METALLURGY
MINERAL OR SLAG WOOL
SURFACE TREATMENT OF FIBRES OR FILAMENTS MADE FROM GLASS,MINERALS OR SLAGS
SURFACE TREATMENT OF GLASS
title Preparation and strengthening method of transparent cover plate glass
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-23T13%3A03%3A55IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CHEN%20YAZHOU&rft.date=2024-09-10&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118619562A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true