Preparation method and application of organic long-afterglow polyurethane elastic fiber with high quantum yield

The invention provides a preparation method and application of a high-quantum-yield organic long-afterglow polyurethane elastic fiber, and the preparation method comprises the following steps: (1) carrying out reaction on oligomer polyol and excessive diisocyanate to form an NCO-terminated prepolyme...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG XIAOYAN, ZHANG JIAXIN, DU JINMEI, XIAO GUOWEI, YANG SHUKANG, JIANG YANG, XU CHANGHAI, MIAO DAGANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WANG XIAOYAN
ZHANG JIAXIN
DU JINMEI
XIAO GUOWEI
YANG SHUKANG
JIANG YANG
XU CHANGHAI
MIAO DAGANG
description The invention provides a preparation method and application of a high-quantum-yield organic long-afterglow polyurethane elastic fiber, and the preparation method comprises the following steps: (1) carrying out reaction on oligomer polyol and excessive diisocyanate to form an NCO-terminated prepolymer solution, and dropwise adding ethylenediamine into the prepolymer solution to carry out chain extension reaction to obtain a polyurethane spinning solution; (2) adding a fluorescent dye into the polyurethane spinning solution prepared in the step (1), and uniformly stirring at room temperature to form a polyurethane-fluorescent dye spinning solution; and (3) carrying out wet spinning on the polyurethane-fluorescent dye spinning solution to prepare the organic long afterglow polyurethane elastic fiber with high quantum yield. According to the invention, the problems of poor flexibility, low quantum yield, short service life, non-uniform luminescence, unstable luminescence and the like of the existing long-afterglo
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118600588A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118600588A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118600588A3</originalsourceid><addsrcrecordid>eNqNizEKwkAQRdNYiHqH8QCBBFHSSlCsxMI-jMns7sBkZ91sCLm9AT2AxefB4_11po9IASMmVg89JacdoF8WgnD71WpAo0XPLYh6m6NJFK3oBEFlHuPyQk9AgkNaGsMvijBxcuDYOniP6NPYw8wk3TZbGZSBdj9usv318qxvOQVtaAjYkqfU1PeyrE5Fcayq8-Gf5gN2JUO4</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method and application of organic long-afterglow polyurethane elastic fiber with high quantum yield</title><source>esp@cenet</source><creator>WANG XIAOYAN ; ZHANG JIAXIN ; DU JINMEI ; XIAO GUOWEI ; YANG SHUKANG ; JIANG YANG ; XU CHANGHAI ; MIAO DAGANG</creator><creatorcontrib>WANG XIAOYAN ; ZHANG JIAXIN ; DU JINMEI ; XIAO GUOWEI ; YANG SHUKANG ; JIANG YANG ; XU CHANGHAI ; MIAO DAGANG</creatorcontrib><description>The invention provides a preparation method and application of a high-quantum-yield organic long-afterglow polyurethane elastic fiber, and the preparation method comprises the following steps: (1) carrying out reaction on oligomer polyol and excessive diisocyanate to form an NCO-terminated prepolymer solution, and dropwise adding ethylenediamine into the prepolymer solution to carry out chain extension reaction to obtain a polyurethane spinning solution; (2) adding a fluorescent dye into the polyurethane spinning solution prepared in the step (1), and uniformly stirring at room temperature to form a polyurethane-fluorescent dye spinning solution; and (3) carrying out wet spinning on the polyurethane-fluorescent dye spinning solution to prepare the organic long afterglow polyurethane elastic fiber with high quantum yield. According to the invention, the problems of poor flexibility, low quantum yield, short service life, non-uniform luminescence, unstable luminescence and the like of the existing long-afterglo</description><language>chi ; eng</language><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS ; CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS ; MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OFARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES ORRIBBONS ; NATURAL OR ARTIFICIAL THREADS OR FIBRES ; SPINNING ; TEXTILES</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240906&amp;DB=EPODOC&amp;CC=CN&amp;NR=118600588A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240906&amp;DB=EPODOC&amp;CC=CN&amp;NR=118600588A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG XIAOYAN</creatorcontrib><creatorcontrib>ZHANG JIAXIN</creatorcontrib><creatorcontrib>DU JINMEI</creatorcontrib><creatorcontrib>XIAO GUOWEI</creatorcontrib><creatorcontrib>YANG SHUKANG</creatorcontrib><creatorcontrib>JIANG YANG</creatorcontrib><creatorcontrib>XU CHANGHAI</creatorcontrib><creatorcontrib>MIAO DAGANG</creatorcontrib><title>Preparation method and application of organic long-afterglow polyurethane elastic fiber with high quantum yield</title><description>The invention provides a preparation method and application of a high-quantum-yield organic long-afterglow polyurethane elastic fiber, and the preparation method comprises the following steps: (1) carrying out reaction on oligomer polyol and excessive diisocyanate to form an NCO-terminated prepolymer solution, and dropwise adding ethylenediamine into the prepolymer solution to carry out chain extension reaction to obtain a polyurethane spinning solution; (2) adding a fluorescent dye into the polyurethane spinning solution prepared in the step (1), and uniformly stirring at room temperature to form a polyurethane-fluorescent dye spinning solution; and (3) carrying out wet spinning on the polyurethane-fluorescent dye spinning solution to prepare the organic long afterglow polyurethane elastic fiber with high quantum yield. According to the invention, the problems of poor flexibility, low quantum yield, short service life, non-uniform luminescence, unstable luminescence and the like of the existing long-afterglo</description><subject>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</subject><subject>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</subject><subject>MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OFARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES ORRIBBONS</subject><subject>NATURAL OR ARTIFICIAL THREADS OR FIBRES</subject><subject>SPINNING</subject><subject>TEXTILES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNizEKwkAQRdNYiHqH8QCBBFHSSlCsxMI-jMns7sBkZ91sCLm9AT2AxefB4_11po9IASMmVg89JacdoF8WgnD71WpAo0XPLYh6m6NJFK3oBEFlHuPyQk9AgkNaGsMvijBxcuDYOniP6NPYw8wk3TZbGZSBdj9usv318qxvOQVtaAjYkqfU1PeyrE5Fcayq8-Gf5gN2JUO4</recordid><startdate>20240906</startdate><enddate>20240906</enddate><creator>WANG XIAOYAN</creator><creator>ZHANG JIAXIN</creator><creator>DU JINMEI</creator><creator>XIAO GUOWEI</creator><creator>YANG SHUKANG</creator><creator>JIANG YANG</creator><creator>XU CHANGHAI</creator><creator>MIAO DAGANG</creator><scope>EVB</scope></search><sort><creationdate>20240906</creationdate><title>Preparation method and application of organic long-afterglow polyurethane elastic fiber with high quantum yield</title><author>WANG XIAOYAN ; ZHANG JIAXIN ; DU JINMEI ; XIAO GUOWEI ; YANG SHUKANG ; JIANG YANG ; XU CHANGHAI ; MIAO DAGANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118600588A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS</topic><topic>CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS</topic><topic>MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OFARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES ORRIBBONS</topic><topic>NATURAL OR ARTIFICIAL THREADS OR FIBRES</topic><topic>SPINNING</topic><topic>TEXTILES</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG XIAOYAN</creatorcontrib><creatorcontrib>ZHANG JIAXIN</creatorcontrib><creatorcontrib>DU JINMEI</creatorcontrib><creatorcontrib>XIAO GUOWEI</creatorcontrib><creatorcontrib>YANG SHUKANG</creatorcontrib><creatorcontrib>JIANG YANG</creatorcontrib><creatorcontrib>XU CHANGHAI</creatorcontrib><creatorcontrib>MIAO DAGANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG XIAOYAN</au><au>ZHANG JIAXIN</au><au>DU JINMEI</au><au>XIAO GUOWEI</au><au>YANG SHUKANG</au><au>JIANG YANG</au><au>XU CHANGHAI</au><au>MIAO DAGANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method and application of organic long-afterglow polyurethane elastic fiber with high quantum yield</title><date>2024-09-06</date><risdate>2024</risdate><abstract>The invention provides a preparation method and application of a high-quantum-yield organic long-afterglow polyurethane elastic fiber, and the preparation method comprises the following steps: (1) carrying out reaction on oligomer polyol and excessive diisocyanate to form an NCO-terminated prepolymer solution, and dropwise adding ethylenediamine into the prepolymer solution to carry out chain extension reaction to obtain a polyurethane spinning solution; (2) adding a fluorescent dye into the polyurethane spinning solution prepared in the step (1), and uniformly stirring at room temperature to form a polyurethane-fluorescent dye spinning solution; and (3) carrying out wet spinning on the polyurethane-fluorescent dye spinning solution to prepare the organic long afterglow polyurethane elastic fiber with high quantum yield. According to the invention, the problems of poor flexibility, low quantum yield, short service life, non-uniform luminescence, unstable luminescence and the like of the existing long-afterglo</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN118600588A
source esp@cenet
subjects APPARATUS SPECIALLY ADAPTED FOR THE MANUFACTURE OF CARBONFILAMENTS
CHEMICAL FEATURES IN THE MANUFACTURE OF ARTIFICIAL FILAMENTS,THREADS, FIBRES, BRISTLES OR RIBBONS
MECHANICAL METHODS OR APPARATUS IN THE MANUFACTURE OFARTIFICIAL FILAMENTS, THREADS, FIBRES, BRISTLES ORRIBBONS
NATURAL OR ARTIFICIAL THREADS OR FIBRES
SPINNING
TEXTILES
title Preparation method and application of organic long-afterglow polyurethane elastic fiber with high quantum yield
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T14%3A21%3A14IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20XIAOYAN&rft.date=2024-09-06&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118600588A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true