Coprecipitation preparation method of nanoscale yttrium-stabilized zirconia powder

The invention relates to a coprecipitation preparation method of nanoscale yttrium-stabilized zirconia powder. The preparation method comprises the following steps: weighing a certain amount of ZrOCl2. 8H2O, adding a certain amount of Y2O3 according to the stoichiometric ratio of Y0. 06Zr0. 94O1. 97...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU JIAXIANG, CHANG JINGXIAN, XU XIAOJUN, ZHOU YUEZHI, GAN XUEXIAN, YANG YANNA
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LIU JIAXIANG
CHANG JINGXIAN
XU XIAOJUN
ZHOU YUEZHI
GAN XUEXIAN
YANG YANNA
description The invention relates to a coprecipitation preparation method of nanoscale yttrium-stabilized zirconia powder. The preparation method comprises the following steps: weighing a certain amount of ZrOCl2. 8H2O, adding a certain amount of Y2O3 according to the stoichiometric ratio of Y0. 06Zr0. 94O1. 97, stirring and dissolving, and preparing a mixed salt solution with the concentration of 0.1-1 mol/L; the method comprises the following steps: weighing a certain amount of NaOH, KOH, ammonia water or ammonium carbonate, and preparing an alkali solution with the concentration of 0.1-1 mol/L; dropwise adding the mixed salt solution into an alkaline solution which is magnetically stirred at the constant temperature of 60-80 DEG C, and titrating until a certain pH value (7-12) is reached; after the reaction is finished, aging the flocculent precipitate for 0.5-4 hours, washing with water, washing with absolute ethyl alcohol, filtering and drying to obtain a white precursor; and calcining the precursor for 2-4 hours at
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118561320A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118561320A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118561320A3</originalsourceid><addsrcrecordid>eNqNijEKAjEQANNYiPqH9QEHxkOxlaBYWYj9sSZ7uJDLhmRFvNcr6AOsZgZmai5OciHPmRWVJcGnMpavD6R3CSA9JExSPUaCl2rhx9BUxRtHHinAyMVLYoQsz0BlbiY9xkqLH2dmeTxc3amhLB3VjJ4SaefO1u42W9uuV_v2n-cNw3o5UQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Coprecipitation preparation method of nanoscale yttrium-stabilized zirconia powder</title><source>esp@cenet</source><creator>LIU JIAXIANG ; CHANG JINGXIAN ; XU XIAOJUN ; ZHOU YUEZHI ; GAN XUEXIAN ; YANG YANNA</creator><creatorcontrib>LIU JIAXIANG ; CHANG JINGXIAN ; XU XIAOJUN ; ZHOU YUEZHI ; GAN XUEXIAN ; YANG YANNA</creatorcontrib><description>The invention relates to a coprecipitation preparation method of nanoscale yttrium-stabilized zirconia powder. The preparation method comprises the following steps: weighing a certain amount of ZrOCl2. 8H2O, adding a certain amount of Y2O3 according to the stoichiometric ratio of Y0. 06Zr0. 94O1. 97, stirring and dissolving, and preparing a mixed salt solution with the concentration of 0.1-1 mol/L; the method comprises the following steps: weighing a certain amount of NaOH, KOH, ammonia water or ammonium carbonate, and preparing an alkali solution with the concentration of 0.1-1 mol/L; dropwise adding the mixed salt solution into an alkaline solution which is magnetically stirred at the constant temperature of 60-80 DEG C, and titrating until a certain pH value (7-12) is reached; after the reaction is finished, aging the flocculent precipitate for 0.5-4 hours, washing with water, washing with absolute ethyl alcohol, filtering and drying to obtain a white precursor; and calcining the precursor for 2-4 hours at</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS ; INORGANIC CHEMISTRY ; MANUFACTURE OR TREATMENT OF NANOSTRUCTURES ; MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES ; METALLURGY ; NANOTECHNOLOGY ; PERFORMING OPERATIONS ; SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES ; TRANSPORTING</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240830&amp;DB=EPODOC&amp;CC=CN&amp;NR=118561320A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76318</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240830&amp;DB=EPODOC&amp;CC=CN&amp;NR=118561320A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIU JIAXIANG</creatorcontrib><creatorcontrib>CHANG JINGXIAN</creatorcontrib><creatorcontrib>XU XIAOJUN</creatorcontrib><creatorcontrib>ZHOU YUEZHI</creatorcontrib><creatorcontrib>GAN XUEXIAN</creatorcontrib><creatorcontrib>YANG YANNA</creatorcontrib><title>Coprecipitation preparation method of nanoscale yttrium-stabilized zirconia powder</title><description>The invention relates to a coprecipitation preparation method of nanoscale yttrium-stabilized zirconia powder. The preparation method comprises the following steps: weighing a certain amount of ZrOCl2. 8H2O, adding a certain amount of Y2O3 according to the stoichiometric ratio of Y0. 06Zr0. 94O1. 97, stirring and dissolving, and preparing a mixed salt solution with the concentration of 0.1-1 mol/L; the method comprises the following steps: weighing a certain amount of NaOH, KOH, ammonia water or ammonium carbonate, and preparing an alkali solution with the concentration of 0.1-1 mol/L; dropwise adding the mixed salt solution into an alkaline solution which is magnetically stirred at the constant temperature of 60-80 DEG C, and titrating until a certain pH value (7-12) is reached; after the reaction is finished, aging the flocculent precipitate for 0.5-4 hours, washing with water, washing with absolute ethyl alcohol, filtering and drying to obtain a white precursor; and calcining the precursor for 2-4 hours at</description><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</subject><subject>INORGANIC CHEMISTRY</subject><subject>MANUFACTURE OR TREATMENT OF NANOSTRUCTURES</subject><subject>MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES</subject><subject>METALLURGY</subject><subject>NANOTECHNOLOGY</subject><subject>PERFORMING OPERATIONS</subject><subject>SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNijEKAjEQANNYiPqH9QEHxkOxlaBYWYj9sSZ7uJDLhmRFvNcr6AOsZgZmai5OciHPmRWVJcGnMpavD6R3CSA9JExSPUaCl2rhx9BUxRtHHinAyMVLYoQsz0BlbiY9xkqLH2dmeTxc3amhLB3VjJ4SaefO1u42W9uuV_v2n-cNw3o5UQ</recordid><startdate>20240830</startdate><enddate>20240830</enddate><creator>LIU JIAXIANG</creator><creator>CHANG JINGXIAN</creator><creator>XU XIAOJUN</creator><creator>ZHOU YUEZHI</creator><creator>GAN XUEXIAN</creator><creator>YANG YANNA</creator><scope>EVB</scope></search><sort><creationdate>20240830</creationdate><title>Coprecipitation preparation method of nanoscale yttrium-stabilized zirconia powder</title><author>LIU JIAXIANG ; CHANG JINGXIAN ; XU XIAOJUN ; ZHOU YUEZHI ; GAN XUEXIAN ; YANG YANNA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118561320A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</topic><topic>INORGANIC CHEMISTRY</topic><topic>MANUFACTURE OR TREATMENT OF NANOSTRUCTURES</topic><topic>MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES</topic><topic>METALLURGY</topic><topic>NANOTECHNOLOGY</topic><topic>PERFORMING OPERATIONS</topic><topic>SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>LIU JIAXIANG</creatorcontrib><creatorcontrib>CHANG JINGXIAN</creatorcontrib><creatorcontrib>XU XIAOJUN</creatorcontrib><creatorcontrib>ZHOU YUEZHI</creatorcontrib><creatorcontrib>GAN XUEXIAN</creatorcontrib><creatorcontrib>YANG YANNA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIU JIAXIANG</au><au>CHANG JINGXIAN</au><au>XU XIAOJUN</au><au>ZHOU YUEZHI</au><au>GAN XUEXIAN</au><au>YANG YANNA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Coprecipitation preparation method of nanoscale yttrium-stabilized zirconia powder</title><date>2024-08-30</date><risdate>2024</risdate><abstract>The invention relates to a coprecipitation preparation method of nanoscale yttrium-stabilized zirconia powder. The preparation method comprises the following steps: weighing a certain amount of ZrOCl2. 8H2O, adding a certain amount of Y2O3 according to the stoichiometric ratio of Y0. 06Zr0. 94O1. 97, stirring and dissolving, and preparing a mixed salt solution with the concentration of 0.1-1 mol/L; the method comprises the following steps: weighing a certain amount of NaOH, KOH, ammonia water or ammonium carbonate, and preparing an alkali solution with the concentration of 0.1-1 mol/L; dropwise adding the mixed salt solution into an alkaline solution which is magnetically stirred at the constant temperature of 60-80 DEG C, and titrating until a certain pH value (7-12) is reached; after the reaction is finished, aging the flocculent precipitate for 0.5-4 hours, washing with water, washing with absolute ethyl alcohol, filtering and drying to obtain a white precursor; and calcining the precursor for 2-4 hours at</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN118561320A
source esp@cenet
subjects CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS
INORGANIC CHEMISTRY
MANUFACTURE OR TREATMENT OF NANOSTRUCTURES
MEASUREMENT OR ANALYSIS OF NANOSTRUCTURES
METALLURGY
NANOTECHNOLOGY
PERFORMING OPERATIONS
SPECIFIC USES OR APPLICATIONS OF NANOSTRUCTURES
TRANSPORTING
title Coprecipitation preparation method of nanoscale yttrium-stabilized zirconia powder
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-12T01%3A13%3A16IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIU%20JIAXIANG&rft.date=2024-08-30&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118561320A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true