SBS modified asphalt and preparation method thereof

The invention provides SBS (Styrene Butadiene Styrene) modified asphalt which comprises the following components in parts by weight: 100 parts of matrix asphalt, 3-10 parts of modified SBS and 0.1-0.5 part of a sulfur stabilizer, the modified SBS is prepared from the following components in parts by...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: SUN YINGUO, YU JIANHUA, SONG LIMING, YI HONGYU, SI TE, FENG WEI, CHEN HONGFEI, CHEN FUJUN, FU RUIMING, ZHONG SHENGRAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator SUN YINGUO
YU JIANHUA
SONG LIMING
YI HONGYU
SI TE
FENG WEI
CHEN HONGFEI
CHEN FUJUN
FU RUIMING
ZHONG SHENGRAN
description The invention provides SBS (Styrene Butadiene Styrene) modified asphalt which comprises the following components in parts by weight: 100 parts of matrix asphalt, 3-10 parts of modified SBS and 0.1-0.5 part of a sulfur stabilizer, the modified SBS is prepared from the following components in parts by weight: 20 to 30 parts of SBS, 15 to 20 parts of propylene and 0.2 to 0.5 part of a Grubbs II catalyst; the preparation method of the SBS modified asphalt comprises the following steps: S1, heating and melting the matrix asphalt, adding the modified SBS into the matrix asphalt, uniformly mixing, heating, adding the sulfur stabilizer, and continuously stirring until the modified SBS is swelled and developed to obtain prefabricated asphalt; s2, carrying out constant-temperature heat preservation on the obtained prefabricated asphalt, and meanwhile, carrying out vibration homogenization, so as to finally prepare the SBS modified asphalt. According to the present invention, the blending ability of the modified SBS and
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118515981A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118515981A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118515981A3</originalsourceid><addsrcrecordid>eNrjZDAOdgpWyM1PyUzLTE1RSCwuyEjMKVFIzEtRKChKLUgsSizJzM9TyE0tychPUSjJSC1KzU_jYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GhhamhqaWFoaOxsSoAQDbOyxE</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>SBS modified asphalt and preparation method thereof</title><source>esp@cenet</source><creator>SUN YINGUO ; YU JIANHUA ; SONG LIMING ; YI HONGYU ; SI TE ; FENG WEI ; CHEN HONGFEI ; CHEN FUJUN ; FU RUIMING ; ZHONG SHENGRAN</creator><creatorcontrib>SUN YINGUO ; YU JIANHUA ; SONG LIMING ; YI HONGYU ; SI TE ; FENG WEI ; CHEN HONGFEI ; CHEN FUJUN ; FU RUIMING ; ZHONG SHENGRAN</creatorcontrib><description>The invention provides SBS (Styrene Butadiene Styrene) modified asphalt which comprises the following components in parts by weight: 100 parts of matrix asphalt, 3-10 parts of modified SBS and 0.1-0.5 part of a sulfur stabilizer, the modified SBS is prepared from the following components in parts by weight: 20 to 30 parts of SBS, 15 to 20 parts of propylene and 0.2 to 0.5 part of a Grubbs II catalyst; the preparation method of the SBS modified asphalt comprises the following steps: S1, heating and melting the matrix asphalt, adding the modified SBS into the matrix asphalt, uniformly mixing, heating, adding the sulfur stabilizer, and continuously stirring until the modified SBS is swelled and developed to obtain prefabricated asphalt; s2, carrying out constant-temperature heat preservation on the obtained prefabricated asphalt, and meanwhile, carrying out vibration homogenization, so as to finally prepare the SBS modified asphalt. According to the present invention, the blending ability of the modified SBS and</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOSITIONS BASED THEREON ; COMPOSITIONS OF MACROMOLECULAR COMPOUNDS ; METALLURGY ; ORGANIC MACROMOLECULAR COMPOUNDS ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240820&amp;DB=EPODOC&amp;CC=CN&amp;NR=118515981A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240820&amp;DB=EPODOC&amp;CC=CN&amp;NR=118515981A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>SUN YINGUO</creatorcontrib><creatorcontrib>YU JIANHUA</creatorcontrib><creatorcontrib>SONG LIMING</creatorcontrib><creatorcontrib>YI HONGYU</creatorcontrib><creatorcontrib>SI TE</creatorcontrib><creatorcontrib>FENG WEI</creatorcontrib><creatorcontrib>CHEN HONGFEI</creatorcontrib><creatorcontrib>CHEN FUJUN</creatorcontrib><creatorcontrib>FU RUIMING</creatorcontrib><creatorcontrib>ZHONG SHENGRAN</creatorcontrib><title>SBS modified asphalt and preparation method thereof</title><description>The invention provides SBS (Styrene Butadiene Styrene) modified asphalt which comprises the following components in parts by weight: 100 parts of matrix asphalt, 3-10 parts of modified SBS and 0.1-0.5 part of a sulfur stabilizer, the modified SBS is prepared from the following components in parts by weight: 20 to 30 parts of SBS, 15 to 20 parts of propylene and 0.2 to 0.5 part of a Grubbs II catalyst; the preparation method of the SBS modified asphalt comprises the following steps: S1, heating and melting the matrix asphalt, adding the modified SBS into the matrix asphalt, uniformly mixing, heating, adding the sulfur stabilizer, and continuously stirring until the modified SBS is swelled and developed to obtain prefabricated asphalt; s2, carrying out constant-temperature heat preservation on the obtained prefabricated asphalt, and meanwhile, carrying out vibration homogenization, so as to finally prepare the SBS modified asphalt. According to the present invention, the blending ability of the modified SBS and</description><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</subject><subject>METALLURGY</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZDAOdgpWyM1PyUzLTE1RSCwuyEjMKVFIzEtRKChKLUgsSizJzM9TyE0tychPUSjJSC1KzU_jYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GhhamhqaWFoaOxsSoAQDbOyxE</recordid><startdate>20240820</startdate><enddate>20240820</enddate><creator>SUN YINGUO</creator><creator>YU JIANHUA</creator><creator>SONG LIMING</creator><creator>YI HONGYU</creator><creator>SI TE</creator><creator>FENG WEI</creator><creator>CHEN HONGFEI</creator><creator>CHEN FUJUN</creator><creator>FU RUIMING</creator><creator>ZHONG SHENGRAN</creator><scope>EVB</scope></search><sort><creationdate>20240820</creationdate><title>SBS modified asphalt and preparation method thereof</title><author>SUN YINGUO ; YU JIANHUA ; SONG LIMING ; YI HONGYU ; SI TE ; FENG WEI ; CHEN HONGFEI ; CHEN FUJUN ; FU RUIMING ; ZHONG SHENGRAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118515981A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>COMPOSITIONS OF MACROMOLECULAR COMPOUNDS</topic><topic>METALLURGY</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS</topic><toplevel>online_resources</toplevel><creatorcontrib>SUN YINGUO</creatorcontrib><creatorcontrib>YU JIANHUA</creatorcontrib><creatorcontrib>SONG LIMING</creatorcontrib><creatorcontrib>YI HONGYU</creatorcontrib><creatorcontrib>SI TE</creatorcontrib><creatorcontrib>FENG WEI</creatorcontrib><creatorcontrib>CHEN HONGFEI</creatorcontrib><creatorcontrib>CHEN FUJUN</creatorcontrib><creatorcontrib>FU RUIMING</creatorcontrib><creatorcontrib>ZHONG SHENGRAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>SUN YINGUO</au><au>YU JIANHUA</au><au>SONG LIMING</au><au>YI HONGYU</au><au>SI TE</au><au>FENG WEI</au><au>CHEN HONGFEI</au><au>CHEN FUJUN</au><au>FU RUIMING</au><au>ZHONG SHENGRAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>SBS modified asphalt and preparation method thereof</title><date>2024-08-20</date><risdate>2024</risdate><abstract>The invention provides SBS (Styrene Butadiene Styrene) modified asphalt which comprises the following components in parts by weight: 100 parts of matrix asphalt, 3-10 parts of modified SBS and 0.1-0.5 part of a sulfur stabilizer, the modified SBS is prepared from the following components in parts by weight: 20 to 30 parts of SBS, 15 to 20 parts of propylene and 0.2 to 0.5 part of a Grubbs II catalyst; the preparation method of the SBS modified asphalt comprises the following steps: S1, heating and melting the matrix asphalt, adding the modified SBS into the matrix asphalt, uniformly mixing, heating, adding the sulfur stabilizer, and continuously stirring until the modified SBS is swelled and developed to obtain prefabricated asphalt; s2, carrying out constant-temperature heat preservation on the obtained prefabricated asphalt, and meanwhile, carrying out vibration homogenization, so as to finally prepare the SBS modified asphalt. According to the present invention, the blending ability of the modified SBS and</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN118515981A
source esp@cenet
subjects CHEMISTRY
COMPOSITIONS BASED THEREON
COMPOSITIONS OF MACROMOLECULAR COMPOUNDS
METALLURGY
ORGANIC MACROMOLECULAR COMPOUNDS
THEIR PREPARATION OR CHEMICAL WORKING-UP
USE OF INORGANIC OR NON-MACROMOLECULAR ORGANIC SUBSTANCES ASCOMPOUNDING INGREDIENTS
title SBS modified asphalt and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-20T07%3A17%3A09IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=SUN%20YINGUO&rft.date=2024-08-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118515981A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true