Low-temperature high-construction steel thick plate welding method
The invention provides a low-temperature high-construction steel thick plate welding method, which belongs to the technical field of thick plate welding, and comprises the following steps: carrying out special welding process evaluation, compiling an operation instruction book, and determining weldi...
Gespeichert in:
Hauptverfasser: | , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | GUO FAQIANG WANG HONGJUN WU YUE NIU HUIYONG LIAO RUIZHI ZHANG XINHE MA XIN JIANG YAO |
description | The invention provides a low-temperature high-construction steel thick plate welding method, which belongs to the technical field of thick plate welding, and comprises the following steps: carrying out special welding process evaluation, compiling an operation instruction book, and determining welding process parameters; a protective shed is erected in the welding area; preheating before welding: preheating a welding area through a heating piece, wherein the lowest preheating temperature is 60 DEG C; a multi-layer and multi-pass welding method is adopted, and the interlayer temperature ranges from 100 DEG C to 150 DEG C; and post-welding heat preservation, wherein after welding is finished, post-heating heat preservation treatment is conducted on a weld joint. Through the process steps of arrangement of the protective shed, preheating before welding, interlayer temperature welding and heat preservation after welding, the quality of a welding seam is improved to the maximum extent, welding residual stress and |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118478069A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118478069A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118478069A3</originalsourceid><addsrcrecordid>eNrjZHDyyS_XLUnNLUgtSiwpLUpVyMhMz9BNzs8rLikqTS7JzM9TKC5JTc1RKMnITM5WKMhJLElVKE_NScnMS1fITS3JyE_hYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GhhYm5hYGZpaOxsSoAQCOIzK3</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Low-temperature high-construction steel thick plate welding method</title><source>esp@cenet</source><creator>GUO FAQIANG ; WANG HONGJUN ; WU YUE ; NIU HUIYONG ; LIAO RUIZHI ; ZHANG XINHE ; MA XIN ; JIANG YAO</creator><creatorcontrib>GUO FAQIANG ; WANG HONGJUN ; WU YUE ; NIU HUIYONG ; LIAO RUIZHI ; ZHANG XINHE ; MA XIN ; JIANG YAO</creatorcontrib><description>The invention provides a low-temperature high-construction steel thick plate welding method, which belongs to the technical field of thick plate welding, and comprises the following steps: carrying out special welding process evaluation, compiling an operation instruction book, and determining welding process parameters; a protective shed is erected in the welding area; preheating before welding: preheating a welding area through a heating piece, wherein the lowest preheating temperature is 60 DEG C; a multi-layer and multi-pass welding method is adopted, and the interlayer temperature ranges from 100 DEG C to 150 DEG C; and post-welding heat preservation, wherein after welding is finished, post-heating heat preservation treatment is conducted on a weld joint. Through the process steps of arrangement of the protective shed, preheating before welding, interlayer temperature welding and heat preservation after welding, the quality of a welding seam is improved to the maximum extent, welding residual stress and</description><language>chi ; eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240813&DB=EPODOC&CC=CN&NR=118478069A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240813&DB=EPODOC&CC=CN&NR=118478069A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GUO FAQIANG</creatorcontrib><creatorcontrib>WANG HONGJUN</creatorcontrib><creatorcontrib>WU YUE</creatorcontrib><creatorcontrib>NIU HUIYONG</creatorcontrib><creatorcontrib>LIAO RUIZHI</creatorcontrib><creatorcontrib>ZHANG XINHE</creatorcontrib><creatorcontrib>MA XIN</creatorcontrib><creatorcontrib>JIANG YAO</creatorcontrib><title>Low-temperature high-construction steel thick plate welding method</title><description>The invention provides a low-temperature high-construction steel thick plate welding method, which belongs to the technical field of thick plate welding, and comprises the following steps: carrying out special welding process evaluation, compiling an operation instruction book, and determining welding process parameters; a protective shed is erected in the welding area; preheating before welding: preheating a welding area through a heating piece, wherein the lowest preheating temperature is 60 DEG C; a multi-layer and multi-pass welding method is adopted, and the interlayer temperature ranges from 100 DEG C to 150 DEG C; and post-welding heat preservation, wherein after welding is finished, post-heating heat preservation treatment is conducted on a weld joint. Through the process steps of arrangement of the protective shed, preheating before welding, interlayer temperature welding and heat preservation after welding, the quality of a welding seam is improved to the maximum extent, welding residual stress and</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHDyyS_XLUnNLUgtSiwpLUpVyMhMz9BNzs8rLikqTS7JzM9TKC5JTc1RKMnITM5WKMhJLElVKE_NScnMS1fITS3JyE_hYWBNS8wpTuWF0twMim6uIc4euqkF-fGpxQWJyal5qSXxzn6GhhYm5hYGZpaOxsSoAQCOIzK3</recordid><startdate>20240813</startdate><enddate>20240813</enddate><creator>GUO FAQIANG</creator><creator>WANG HONGJUN</creator><creator>WU YUE</creator><creator>NIU HUIYONG</creator><creator>LIAO RUIZHI</creator><creator>ZHANG XINHE</creator><creator>MA XIN</creator><creator>JIANG YAO</creator><scope>EVB</scope></search><sort><creationdate>20240813</creationdate><title>Low-temperature high-construction steel thick plate welding method</title><author>GUO FAQIANG ; WANG HONGJUN ; WU YUE ; NIU HUIYONG ; LIAO RUIZHI ; ZHANG XINHE ; MA XIN ; JIANG YAO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118478069A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>GUO FAQIANG</creatorcontrib><creatorcontrib>WANG HONGJUN</creatorcontrib><creatorcontrib>WU YUE</creatorcontrib><creatorcontrib>NIU HUIYONG</creatorcontrib><creatorcontrib>LIAO RUIZHI</creatorcontrib><creatorcontrib>ZHANG XINHE</creatorcontrib><creatorcontrib>MA XIN</creatorcontrib><creatorcontrib>JIANG YAO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GUO FAQIANG</au><au>WANG HONGJUN</au><au>WU YUE</au><au>NIU HUIYONG</au><au>LIAO RUIZHI</au><au>ZHANG XINHE</au><au>MA XIN</au><au>JIANG YAO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Low-temperature high-construction steel thick plate welding method</title><date>2024-08-13</date><risdate>2024</risdate><abstract>The invention provides a low-temperature high-construction steel thick plate welding method, which belongs to the technical field of thick plate welding, and comprises the following steps: carrying out special welding process evaluation, compiling an operation instruction book, and determining welding process parameters; a protective shed is erected in the welding area; preheating before welding: preheating a welding area through a heating piece, wherein the lowest preheating temperature is 60 DEG C; a multi-layer and multi-pass welding method is adopted, and the interlayer temperature ranges from 100 DEG C to 150 DEG C; and post-welding heat preservation, wherein after welding is finished, post-heating heat preservation treatment is conducted on a weld joint. Through the process steps of arrangement of the protective shed, preheating before welding, interlayer temperature welding and heat preservation after welding, the quality of a welding seam is improved to the maximum extent, welding residual stress and</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN118478069A |
source | esp@cenet |
subjects | CLADDING OR PLATING BY SOLDERING OR WELDING CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING MACHINE TOOLS METAL-WORKING NOT OTHERWISE PROVIDED FOR PERFORMING OPERATIONS SOLDERING OR UNSOLDERING TRANSPORTING WELDING WORKING BY LASER BEAM |
title | Low-temperature high-construction steel thick plate welding method |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-18T20%3A34%3A23IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GUO%20FAQIANG&rft.date=2024-08-13&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118478069A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |