Method for recovering zinc through combined treatment of zinc-containing waste residues and aluminum electrolysis overhaul residues
The invention discloses a method for recovering zinc through combined treatment of zinc-containing waste residues and aluminum electrolysis overhaul residues, which comprises the following steps of: mixing the zinc-containing waste residues, the overhaul residues and a fluorine fixing agent, heating...
Gespeichert in:
Hauptverfasser: | , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | LUO, YINGTAO LUO ZHONGSHENG SU ZIWEI ZHANG DINGCHUAN YUAN CONGCONG LIU JIANJUN DU TINGTING LI RUONAN |
description | The invention discloses a method for recovering zinc through combined treatment of zinc-containing waste residues and aluminum electrolysis overhaul residues, which comprises the following steps of: mixing the zinc-containing waste residues, the overhaul residues and a fluorine fixing agent, heating in a muffle furnace, reacting the mixed material at high temperature, reducing zinc into simple substances, and exchanging the simple substances; and then reacting with oxygen in the air to generate zinc oxide so as to realize zinc recovery. According to the method, the zinc-containing waste residues and the aluminum electrolysis overhaul residues are combined, efficient recovery of zinc is effectively achieved, meanwhile, harmful substances such as soluble fluoride and cyanide in the aluminum electrolysis overhaul residues are converted into stable compounds or decomposed into harmless substances in the high-temperature roasting process, harmless treatment of the aluminum electrolysis overhaul residues is achieve |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118421956A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118421956A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118421956A3</originalsourceid><addsrcrecordid>eNqNzTsOwjAQBNA0FAi4w3KAFOEnKFEEooGKPjLOJrZk70b2GgQtF4cgRE01zZuZYfY8ohiuoeEAATVfMVhq4WFJg5jAqTWg2V8sYQ0SUIlHEuDmQ3LNJMpSX7mpKPjeiLZOGEFRDcolbyl5QIdaArt7tBH6D6OS-9lxNmiUizj55iib7nfn8pBjxxXGTmkklKo8FcV6MSs2y9V2_o95AfZGS-k</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for recovering zinc through combined treatment of zinc-containing waste residues and aluminum electrolysis overhaul residues</title><source>esp@cenet</source><creator>LUO, YINGTAO ; LUO ZHONGSHENG ; SU ZIWEI ; ZHANG DINGCHUAN ; YUAN CONGCONG ; LIU JIANJUN ; DU TINGTING ; LI RUONAN</creator><creatorcontrib>LUO, YINGTAO ; LUO ZHONGSHENG ; SU ZIWEI ; ZHANG DINGCHUAN ; YUAN CONGCONG ; LIU JIANJUN ; DU TINGTING ; LI RUONAN</creatorcontrib><description>The invention discloses a method for recovering zinc through combined treatment of zinc-containing waste residues and aluminum electrolysis overhaul residues, which comprises the following steps of: mixing the zinc-containing waste residues, the overhaul residues and a fluorine fixing agent, heating in a muffle furnace, reacting the mixed material at high temperature, reducing zinc into simple substances, and exchanging the simple substances; and then reacting with oxygen in the air to generate zinc oxide so as to realize zinc recovery. According to the method, the zinc-containing waste residues and the aluminum electrolysis overhaul residues are combined, efficient recovery of zinc is effectively achieved, meanwhile, harmful substances such as soluble fluoride and cyanide in the aluminum electrolysis overhaul residues are converted into stable compounds or decomposed into harmless substances in the high-temperature roasting process, harmless treatment of the aluminum electrolysis overhaul residues is achieve</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS ; DISPOSAL OF SOLID WASTE ; FERROUS OR NON-FERROUS ALLOYS ; INORGANIC CHEMISTRY ; METALLURGY ; PERFORMING OPERATIONS ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; RECLAMATION OF CONTAMINED SOIL SOIL ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240802&DB=EPODOC&CC=CN&NR=118421956A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25566,76549</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240802&DB=EPODOC&CC=CN&NR=118421956A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LUO, YINGTAO</creatorcontrib><creatorcontrib>LUO ZHONGSHENG</creatorcontrib><creatorcontrib>SU ZIWEI</creatorcontrib><creatorcontrib>ZHANG DINGCHUAN</creatorcontrib><creatorcontrib>YUAN CONGCONG</creatorcontrib><creatorcontrib>LIU JIANJUN</creatorcontrib><creatorcontrib>DU TINGTING</creatorcontrib><creatorcontrib>LI RUONAN</creatorcontrib><title>Method for recovering zinc through combined treatment of zinc-containing waste residues and aluminum electrolysis overhaul residues</title><description>The invention discloses a method for recovering zinc through combined treatment of zinc-containing waste residues and aluminum electrolysis overhaul residues, which comprises the following steps of: mixing the zinc-containing waste residues, the overhaul residues and a fluorine fixing agent, heating in a muffle furnace, reacting the mixed material at high temperature, reducing zinc into simple substances, and exchanging the simple substances; and then reacting with oxygen in the air to generate zinc oxide so as to realize zinc recovery. According to the method, the zinc-containing waste residues and the aluminum electrolysis overhaul residues are combined, efficient recovery of zinc is effectively achieved, meanwhile, harmful substances such as soluble fluoride and cyanide in the aluminum electrolysis overhaul residues are converted into stable compounds or decomposed into harmless substances in the high-temperature roasting process, harmless treatment of the aluminum electrolysis overhaul residues is achieve</description><subject>CHEMISTRY</subject><subject>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</subject><subject>DISPOSAL OF SOLID WASTE</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>RECLAMATION OF CONTAMINED SOIL SOIL</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNzTsOwjAQBNA0FAi4w3KAFOEnKFEEooGKPjLOJrZk70b2GgQtF4cgRE01zZuZYfY8ohiuoeEAATVfMVhq4WFJg5jAqTWg2V8sYQ0SUIlHEuDmQ3LNJMpSX7mpKPjeiLZOGEFRDcolbyl5QIdaArt7tBH6D6OS-9lxNmiUizj55iib7nfn8pBjxxXGTmkklKo8FcV6MSs2y9V2_o95AfZGS-k</recordid><startdate>20240802</startdate><enddate>20240802</enddate><creator>LUO, YINGTAO</creator><creator>LUO ZHONGSHENG</creator><creator>SU ZIWEI</creator><creator>ZHANG DINGCHUAN</creator><creator>YUAN CONGCONG</creator><creator>LIU JIANJUN</creator><creator>DU TINGTING</creator><creator>LI RUONAN</creator><scope>EVB</scope></search><sort><creationdate>20240802</creationdate><title>Method for recovering zinc through combined treatment of zinc-containing waste residues and aluminum electrolysis overhaul residues</title><author>LUO, YINGTAO ; LUO ZHONGSHENG ; SU ZIWEI ; ZHANG DINGCHUAN ; YUAN CONGCONG ; LIU JIANJUN ; DU TINGTING ; LI RUONAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118421956A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</topic><topic>DISPOSAL OF SOLID WASTE</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>RECLAMATION OF CONTAMINED SOIL SOIL</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>LUO, YINGTAO</creatorcontrib><creatorcontrib>LUO ZHONGSHENG</creatorcontrib><creatorcontrib>SU ZIWEI</creatorcontrib><creatorcontrib>ZHANG DINGCHUAN</creatorcontrib><creatorcontrib>YUAN CONGCONG</creatorcontrib><creatorcontrib>LIU JIANJUN</creatorcontrib><creatorcontrib>DU TINGTING</creatorcontrib><creatorcontrib>LI RUONAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LUO, YINGTAO</au><au>LUO ZHONGSHENG</au><au>SU ZIWEI</au><au>ZHANG DINGCHUAN</au><au>YUAN CONGCONG</au><au>LIU JIANJUN</au><au>DU TINGTING</au><au>LI RUONAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for recovering zinc through combined treatment of zinc-containing waste residues and aluminum electrolysis overhaul residues</title><date>2024-08-02</date><risdate>2024</risdate><abstract>The invention discloses a method for recovering zinc through combined treatment of zinc-containing waste residues and aluminum electrolysis overhaul residues, which comprises the following steps of: mixing the zinc-containing waste residues, the overhaul residues and a fluorine fixing agent, heating in a muffle furnace, reacting the mixed material at high temperature, reducing zinc into simple substances, and exchanging the simple substances; and then reacting with oxygen in the air to generate zinc oxide so as to realize zinc recovery. According to the method, the zinc-containing waste residues and the aluminum electrolysis overhaul residues are combined, efficient recovery of zinc is effectively achieved, meanwhile, harmful substances such as soluble fluoride and cyanide in the aluminum electrolysis overhaul residues are converted into stable compounds or decomposed into harmless substances in the high-temperature roasting process, harmless treatment of the aluminum electrolysis overhaul residues is achieve</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN118421956A |
source | esp@cenet |
subjects | CHEMISTRY COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS DISPOSAL OF SOLID WASTE FERROUS OR NON-FERROUS ALLOYS INORGANIC CHEMISTRY METALLURGY PERFORMING OPERATIONS PRETREATMENT OF RAW MATERIALS PRODUCTION AND REFINING OF METALS RECLAMATION OF CONTAMINED SOIL SOIL TRANSPORTING TREATMENT OF ALLOYS OR NON-FERROUS METALS |
title | Method for recovering zinc through combined treatment of zinc-containing waste residues and aluminum electrolysis overhaul residues |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-17T22%3A31%3A54IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LUO,%20YINGTAO&rft.date=2024-08-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118421956A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |