Hard-face welding wire for continuous casting roller of horizontal section of continuous casting machine

The invention discloses a hard-face welding wire for a horizontal section continuous casting roller of a continuous casting machine. The hard-face welding wire comprises the following components in percentage by weight: 0.05-0.07% of C, 4.0-6.0% of Mg, 0.03-0.10% of Mn, 0.05-0.10% of Cr, less than o...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU XIN, ZHAO XU, ZENG XINZHE, JIANG CHENGWEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LIU XIN
ZHAO XU
ZENG XINZHE
JIANG CHENGWEI
description The invention discloses a hard-face welding wire for a horizontal section continuous casting roller of a continuous casting machine. The hard-face welding wire comprises the following components in percentage by weight: 0.05-0.07% of C, 4.0-6.0% of Mg, 0.03-0.10% of Mn, 0.05-0.10% of Cr, less than or equal to 0.25% of Si, less than or equal to 0.40% of Cu, less than or equal to 0.20% of Cu, less than or equal to 0.20% of Zn, less than or equal to 0.0003% of Be, 0.10-0.15% of Cr and the balance of Al and other inevitable impurities. In order to reach a high strength grade, a certain content of C is essential, but the content of C cannot be too high, otherwise, the toughness of deposited metal is seriously influenced, so that the content of C is controlled to be 0.06, a certain strength guarantee is provided for the deposited metal by properly adding Mn, and meanwhile, Mn has desulfurization and deoxidation effects in a molten pool process, so that the toughness of the deposited metal is greatly improved. The c
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118417759A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118417759A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118417759A3</originalsourceid><addsrcrecordid>eNrjZMjwSCxK0U1LTE5VKE_NScnMS1cozyxKVUjLL1JIzs8rycwrzS8tVkhOLC4ByRXl5-SkFinkpylk5BdlVgEVJOYoFKcml2Tm54FEsWjJTUzOyMxL5WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFQBfkpZbEO_sZGlqYGJqbm1o6GhOjBgA7AED2</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Hard-face welding wire for continuous casting roller of horizontal section of continuous casting machine</title><source>esp@cenet</source><creator>LIU XIN ; ZHAO XU ; ZENG XINZHE ; JIANG CHENGWEI</creator><creatorcontrib>LIU XIN ; ZHAO XU ; ZENG XINZHE ; JIANG CHENGWEI</creatorcontrib><description>The invention discloses a hard-face welding wire for a horizontal section continuous casting roller of a continuous casting machine. The hard-face welding wire comprises the following components in percentage by weight: 0.05-0.07% of C, 4.0-6.0% of Mg, 0.03-0.10% of Mn, 0.05-0.10% of Cr, less than or equal to 0.25% of Si, less than or equal to 0.40% of Cu, less than or equal to 0.20% of Cu, less than or equal to 0.20% of Zn, less than or equal to 0.0003% of Be, 0.10-0.15% of Cr and the balance of Al and other inevitable impurities. In order to reach a high strength grade, a certain content of C is essential, but the content of C cannot be too high, otherwise, the toughness of deposited metal is seriously influenced, so that the content of C is controlled to be 0.06, a certain strength guarantee is provided for the deposited metal by properly adding Mn, and meanwhile, Mn has desulfurization and deoxidation effects in a molten pool process, so that the toughness of the deposited metal is greatly improved. The c</description><language>chi ; eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240802&amp;DB=EPODOC&amp;CC=CN&amp;NR=118417759A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240802&amp;DB=EPODOC&amp;CC=CN&amp;NR=118417759A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIU XIN</creatorcontrib><creatorcontrib>ZHAO XU</creatorcontrib><creatorcontrib>ZENG XINZHE</creatorcontrib><creatorcontrib>JIANG CHENGWEI</creatorcontrib><title>Hard-face welding wire for continuous casting roller of horizontal section of continuous casting machine</title><description>The invention discloses a hard-face welding wire for a horizontal section continuous casting roller of a continuous casting machine. The hard-face welding wire comprises the following components in percentage by weight: 0.05-0.07% of C, 4.0-6.0% of Mg, 0.03-0.10% of Mn, 0.05-0.10% of Cr, less than or equal to 0.25% of Si, less than or equal to 0.40% of Cu, less than or equal to 0.20% of Cu, less than or equal to 0.20% of Zn, less than or equal to 0.0003% of Be, 0.10-0.15% of Cr and the balance of Al and other inevitable impurities. In order to reach a high strength grade, a certain content of C is essential, but the content of C cannot be too high, otherwise, the toughness of deposited metal is seriously influenced, so that the content of C is controlled to be 0.06, a certain strength guarantee is provided for the deposited metal by properly adding Mn, and meanwhile, Mn has desulfurization and deoxidation effects in a molten pool process, so that the toughness of the deposited metal is greatly improved. The c</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZMjwSCxK0U1LTE5VKE_NScnMS1cozyxKVUjLL1JIzs8rycwrzS8tVkhOLC4ByRXl5-SkFinkpylk5BdlVgEVJOYoFKcml2Tm54FEsWjJTUzOyMxL5WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFQBfkpZbEO_sZGlqYGJqbm1o6GhOjBgA7AED2</recordid><startdate>20240802</startdate><enddate>20240802</enddate><creator>LIU XIN</creator><creator>ZHAO XU</creator><creator>ZENG XINZHE</creator><creator>JIANG CHENGWEI</creator><scope>EVB</scope></search><sort><creationdate>20240802</creationdate><title>Hard-face welding wire for continuous casting roller of horizontal section of continuous casting machine</title><author>LIU XIN ; ZHAO XU ; ZENG XINZHE ; JIANG CHENGWEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118417759A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>LIU XIN</creatorcontrib><creatorcontrib>ZHAO XU</creatorcontrib><creatorcontrib>ZENG XINZHE</creatorcontrib><creatorcontrib>JIANG CHENGWEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIU XIN</au><au>ZHAO XU</au><au>ZENG XINZHE</au><au>JIANG CHENGWEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Hard-face welding wire for continuous casting roller of horizontal section of continuous casting machine</title><date>2024-08-02</date><risdate>2024</risdate><abstract>The invention discloses a hard-face welding wire for a horizontal section continuous casting roller of a continuous casting machine. The hard-face welding wire comprises the following components in percentage by weight: 0.05-0.07% of C, 4.0-6.0% of Mg, 0.03-0.10% of Mn, 0.05-0.10% of Cr, less than or equal to 0.25% of Si, less than or equal to 0.40% of Cu, less than or equal to 0.20% of Cu, less than or equal to 0.20% of Zn, less than or equal to 0.0003% of Be, 0.10-0.15% of Cr and the balance of Al and other inevitable impurities. In order to reach a high strength grade, a certain content of C is essential, but the content of C cannot be too high, otherwise, the toughness of deposited metal is seriously influenced, so that the content of C is controlled to be 0.06, a certain strength guarantee is provided for the deposited metal by properly adding Mn, and meanwhile, Mn has desulfurization and deoxidation effects in a molten pool process, so that the toughness of the deposited metal is greatly improved. The c</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN118417759A
source esp@cenet
subjects CLADDING OR PLATING BY SOLDERING OR WELDING
CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
PERFORMING OPERATIONS
SOLDERING OR UNSOLDERING
TRANSPORTING
WELDING
WORKING BY LASER BEAM
title Hard-face welding wire for continuous casting roller of horizontal section of continuous casting machine
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-04T20%3A45%3A11IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIU%20XIN&rft.date=2024-08-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118417759A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true