Solution-treated Sr, Zr, Ti and Y quaternary composite microalloyed as-cast high-strength high-plasticity as-cast Al-Si-Mg cast aluminum alloy and preparation method thereof

The invention relates to a solution treated Sr, Zr, Ti and Y quaternary composite microalloyed high-strength and high-plasticity Al-Si-Mg cast aluminum alloy, which is characterized by mainly comprising the following components in percentage by mass: 7.43 to 7.45 percent of aluminum (Al), 0.47 to 0....

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DAI SONG, CHEN JUN, LIU XUN, SHENG JIANGFENG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator DAI SONG
CHEN JUN
LIU XUN
SHENG JIANGFENG
description The invention relates to a solution treated Sr, Zr, Ti and Y quaternary composite microalloyed high-strength and high-plasticity Al-Si-Mg cast aluminum alloy, which is characterized by mainly comprising the following components in percentage by mass: 7.43 to 7.45 percent of aluminum (Al), 0.47 to 0.486 percent of silicon (Si), 0.03 to 0.0385 percent of magnesium (Mg), 0.03 to 0.0385 percent of strontium (Sr), 0.253 to 0.257 percent of zirconium (Zr), 0.0597 to 0.0676 percent of titanium (Ti) and the balance of yttrium (Y). The mass percent of yttrium (Y) is 0.2% (nominal), the balance is aluminum and a small amount of impurity elements, and the sum of all the components is 100%. The preparation process of the alloy comprises casting and solution treatment. The Si phase of the cast aluminum alloy is highly dispersed fine spheres with the size of 2-5 microns, the tensile strength can reach 271.01 MPa, and meanwhile the percentage elongation after fracture is 18.75%. 一种固溶处理的Sr,Zr,Ti,Y四元复合微合金化的高强度高塑性Al-Si-Mg铸造铝合金
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118389914A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118389914A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118389914A3</originalsourceid><addsrcrecordid>eNqNTrtuwzAM9NKhaPsPzF4NRjokYxC06JIszpIuASHTFgFJVCV68Ef1H6s4QecOxOEePPKx-enET8oSjWZCpR66_ApfdU4MGHs4w_dU9Rwxz2AlJCmsBIFtFvRe5rqCxVgsCo5HZ0otiqO6G0u-GmxZ57_UzpuOzWGEhaGfAscpwFK2nEyZEma8fgWB1EkP6iiTDM_Nw4C-0Msdn5rVx_tp_2koyYVKQkuR9LI_tu1mvdlu27fd-j-ZX334WYw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Solution-treated Sr, Zr, Ti and Y quaternary composite microalloyed as-cast high-strength high-plasticity as-cast Al-Si-Mg cast aluminum alloy and preparation method thereof</title><source>esp@cenet</source><creator>DAI SONG ; CHEN JUN ; LIU XUN ; SHENG JIANGFENG</creator><creatorcontrib>DAI SONG ; CHEN JUN ; LIU XUN ; SHENG JIANGFENG</creatorcontrib><description>The invention relates to a solution treated Sr, Zr, Ti and Y quaternary composite microalloyed high-strength and high-plasticity Al-Si-Mg cast aluminum alloy, which is characterized by mainly comprising the following components in percentage by mass: 7.43 to 7.45 percent of aluminum (Al), 0.47 to 0.486 percent of silicon (Si), 0.03 to 0.0385 percent of magnesium (Mg), 0.03 to 0.0385 percent of strontium (Sr), 0.253 to 0.257 percent of zirconium (Zr), 0.0597 to 0.0676 percent of titanium (Ti) and the balance of yttrium (Y). The mass percent of yttrium (Y) is 0.2% (nominal), the balance is aluminum and a small amount of impurity elements, and the sum of all the components is 100%. The preparation process of the alloy comprises casting and solution treatment. The Si phase of the cast aluminum alloy is highly dispersed fine spheres with the size of 2-5 microns, the tensile strength can reach 271.01 MPa, and meanwhile the percentage elongation after fracture is 18.75%. 一种固溶处理的Sr,Zr,Ti,Y四元复合微合金化的高强度高塑性Al-Si-Mg铸造铝合金</description><language>chi ; eng</language><subject>ALLOYS ; CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240726&amp;DB=EPODOC&amp;CC=CN&amp;NR=118389914A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25566,76549</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240726&amp;DB=EPODOC&amp;CC=CN&amp;NR=118389914A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DAI SONG</creatorcontrib><creatorcontrib>CHEN JUN</creatorcontrib><creatorcontrib>LIU XUN</creatorcontrib><creatorcontrib>SHENG JIANGFENG</creatorcontrib><title>Solution-treated Sr, Zr, Ti and Y quaternary composite microalloyed as-cast high-strength high-plasticity as-cast Al-Si-Mg cast aluminum alloy and preparation method thereof</title><description>The invention relates to a solution treated Sr, Zr, Ti and Y quaternary composite microalloyed high-strength and high-plasticity Al-Si-Mg cast aluminum alloy, which is characterized by mainly comprising the following components in percentage by mass: 7.43 to 7.45 percent of aluminum (Al), 0.47 to 0.486 percent of silicon (Si), 0.03 to 0.0385 percent of magnesium (Mg), 0.03 to 0.0385 percent of strontium (Sr), 0.253 to 0.257 percent of zirconium (Zr), 0.0597 to 0.0676 percent of titanium (Ti) and the balance of yttrium (Y). The mass percent of yttrium (Y) is 0.2% (nominal), the balance is aluminum and a small amount of impurity elements, and the sum of all the components is 100%. The preparation process of the alloy comprises casting and solution treatment. The Si phase of the cast aluminum alloy is highly dispersed fine spheres with the size of 2-5 microns, the tensile strength can reach 271.01 MPa, and meanwhile the percentage elongation after fracture is 18.75%. 一种固溶处理的Sr,Zr,Ti,Y四元复合微合金化的高强度高塑性Al-Si-Mg铸造铝合金</description><subject>ALLOYS</subject><subject>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNTrtuwzAM9NKhaPsPzF4NRjokYxC06JIszpIuASHTFgFJVCV68Ef1H6s4QecOxOEePPKx-enET8oSjWZCpR66_ApfdU4MGHs4w_dU9Rwxz2AlJCmsBIFtFvRe5rqCxVgsCo5HZ0otiqO6G0u-GmxZ57_UzpuOzWGEhaGfAscpwFK2nEyZEma8fgWB1EkP6iiTDM_Nw4C-0Msdn5rVx_tp_2koyYVKQkuR9LI_tu1mvdlu27fd-j-ZX334WYw</recordid><startdate>20240726</startdate><enddate>20240726</enddate><creator>DAI SONG</creator><creator>CHEN JUN</creator><creator>LIU XUN</creator><creator>SHENG JIANGFENG</creator><scope>EVB</scope></search><sort><creationdate>20240726</creationdate><title>Solution-treated Sr, Zr, Ti and Y quaternary composite microalloyed as-cast high-strength high-plasticity as-cast Al-Si-Mg cast aluminum alloy and preparation method thereof</title><author>DAI SONG ; CHEN JUN ; LIU XUN ; SHENG JIANGFENG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118389914A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>ALLOYS</topic><topic>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>DAI SONG</creatorcontrib><creatorcontrib>CHEN JUN</creatorcontrib><creatorcontrib>LIU XUN</creatorcontrib><creatorcontrib>SHENG JIANGFENG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DAI SONG</au><au>CHEN JUN</au><au>LIU XUN</au><au>SHENG JIANGFENG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Solution-treated Sr, Zr, Ti and Y quaternary composite microalloyed as-cast high-strength high-plasticity as-cast Al-Si-Mg cast aluminum alloy and preparation method thereof</title><date>2024-07-26</date><risdate>2024</risdate><abstract>The invention relates to a solution treated Sr, Zr, Ti and Y quaternary composite microalloyed high-strength and high-plasticity Al-Si-Mg cast aluminum alloy, which is characterized by mainly comprising the following components in percentage by mass: 7.43 to 7.45 percent of aluminum (Al), 0.47 to 0.486 percent of silicon (Si), 0.03 to 0.0385 percent of magnesium (Mg), 0.03 to 0.0385 percent of strontium (Sr), 0.253 to 0.257 percent of zirconium (Zr), 0.0597 to 0.0676 percent of titanium (Ti) and the balance of yttrium (Y). The mass percent of yttrium (Y) is 0.2% (nominal), the balance is aluminum and a small amount of impurity elements, and the sum of all the components is 100%. The preparation process of the alloy comprises casting and solution treatment. The Si phase of the cast aluminum alloy is highly dispersed fine spheres with the size of 2-5 microns, the tensile strength can reach 271.01 MPa, and meanwhile the percentage elongation after fracture is 18.75%. 一种固溶处理的Sr,Zr,Ti,Y四元复合微合金化的高强度高塑性Al-Si-Mg铸造铝合金</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN118389914A
source esp@cenet
subjects ALLOYS
CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Solution-treated Sr, Zr, Ti and Y quaternary composite microalloyed as-cast high-strength high-plasticity as-cast Al-Si-Mg cast aluminum alloy and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-17T19%3A54%3A22IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DAI%20SONG&rft.date=2024-07-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118389914A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true