Method for preparing ferro-nickel alloy through step-by-step reduction of laterite-nickel ore in rotary kiln

The invention discloses a method for preparing ferro-nickel alloy through step-by-step reduction of laterite-nickel ore in a rotary kiln. The method comprises the following steps: screening a carbon reducing agent into an oversize reducing agent and an undersize reducing agent; the method comprises...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG DUODONG, BAO JIN, YANG ZEPING, ZHANG JIHONG, XU JIKANG, CAI JIANYONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WANG DUODONG
BAO JIN
YANG ZEPING
ZHANG JIHONG
XU JIKANG
CAI JIANYONG
description The invention discloses a method for preparing ferro-nickel alloy through step-by-step reduction of laterite-nickel ore in a rotary kiln. The method comprises the following steps: screening a carbon reducing agent into an oversize reducing agent and an undersize reducing agent; the method comprises the following steps: screening, crushing and drying laterite-nickel ore, feeding the laterite-nickel ore into a rotary kiln, adding an oversize reducing agent at the kiln tail of the rotary kiln, carrying out pre-reduction roasting, adding an undersize reducing agent from the kiln head of the rotary kiln after roasting, mixing with a pre-reduction roasting product roasted product, feeding the mixture into a charging bucket for caching, and smelting by an electric furnace, thereby obtaining the product. The addition amount of the carbon reducing agent is 3-5.5% of the mass of the dry laterite-nickel ore; and the particle size of the oversize reducing agent is greater than or equal to 20mm. According to the method, a
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118345241A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118345241A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118345241A3</originalsourceid><addsrcrecordid>eNqNy7EOgjAURmEWB6O-w_UBOiCYuBqicdHJnVT4Cw1Nb3N7GXh7Y6K707ecsy7CHTpyT46FkiBZ8XEgBxE20XcTAtkQeCEdhedhpKxI5rWYjyTo5049R2JHwSrEK34fC8hHElYrC00-xG2xcjZk7L5uiv318mxuBolb5GQ7RGjbPMryVNXHQ12eq3-aN0UjQfg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing ferro-nickel alloy through step-by-step reduction of laterite-nickel ore in rotary kiln</title><source>esp@cenet</source><creator>WANG DUODONG ; BAO JIN ; YANG ZEPING ; ZHANG JIHONG ; XU JIKANG ; CAI JIANYONG</creator><creatorcontrib>WANG DUODONG ; BAO JIN ; YANG ZEPING ; ZHANG JIHONG ; XU JIKANG ; CAI JIANYONG</creatorcontrib><description>The invention discloses a method for preparing ferro-nickel alloy through step-by-step reduction of laterite-nickel ore in a rotary kiln. The method comprises the following steps: screening a carbon reducing agent into an oversize reducing agent and an undersize reducing agent; the method comprises the following steps: screening, crushing and drying laterite-nickel ore, feeding the laterite-nickel ore into a rotary kiln, adding an oversize reducing agent at the kiln tail of the rotary kiln, carrying out pre-reduction roasting, adding an undersize reducing agent from the kiln head of the rotary kiln after roasting, mixing with a pre-reduction roasting product roasted product, feeding the mixture into a charging bucket for caching, and smelting by an electric furnace, thereby obtaining the product. The addition amount of the carbon reducing agent is 3-5.5% of the mass of the dry laterite-nickel ore; and the particle size of the oversize reducing agent is greater than or equal to 20mm. According to the method, a</description><language>chi ; eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; METALLURGY OF IRON ; PRETREATMENT OF RAW MATERIALS ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; PRODUCTION AND REFINING OF METALS ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240716&amp;DB=EPODOC&amp;CC=CN&amp;NR=118345241A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240716&amp;DB=EPODOC&amp;CC=CN&amp;NR=118345241A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG DUODONG</creatorcontrib><creatorcontrib>BAO JIN</creatorcontrib><creatorcontrib>YANG ZEPING</creatorcontrib><creatorcontrib>ZHANG JIHONG</creatorcontrib><creatorcontrib>XU JIKANG</creatorcontrib><creatorcontrib>CAI JIANYONG</creatorcontrib><title>Method for preparing ferro-nickel alloy through step-by-step reduction of laterite-nickel ore in rotary kiln</title><description>The invention discloses a method for preparing ferro-nickel alloy through step-by-step reduction of laterite-nickel ore in a rotary kiln. The method comprises the following steps: screening a carbon reducing agent into an oversize reducing agent and an undersize reducing agent; the method comprises the following steps: screening, crushing and drying laterite-nickel ore, feeding the laterite-nickel ore into a rotary kiln, adding an oversize reducing agent at the kiln tail of the rotary kiln, carrying out pre-reduction roasting, adding an undersize reducing agent from the kiln head of the rotary kiln after roasting, mixing with a pre-reduction roasting product roasted product, feeding the mixture into a charging bucket for caching, and smelting by an electric furnace, thereby obtaining the product. The addition amount of the carbon reducing agent is 3-5.5% of the mass of the dry laterite-nickel ore; and the particle size of the oversize reducing agent is greater than or equal to 20mm. According to the method, a</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNy7EOgjAURmEWB6O-w_UBOiCYuBqicdHJnVT4Cw1Nb3N7GXh7Y6K707ecsy7CHTpyT46FkiBZ8XEgBxE20XcTAtkQeCEdhedhpKxI5rWYjyTo5049R2JHwSrEK34fC8hHElYrC00-xG2xcjZk7L5uiv318mxuBolb5GQ7RGjbPMryVNXHQ12eq3-aN0UjQfg</recordid><startdate>20240716</startdate><enddate>20240716</enddate><creator>WANG DUODONG</creator><creator>BAO JIN</creator><creator>YANG ZEPING</creator><creator>ZHANG JIHONG</creator><creator>XU JIKANG</creator><creator>CAI JIANYONG</creator><scope>EVB</scope></search><sort><creationdate>20240716</creationdate><title>Method for preparing ferro-nickel alloy through step-by-step reduction of laterite-nickel ore in rotary kiln</title><author>WANG DUODONG ; BAO JIN ; YANG ZEPING ; ZHANG JIHONG ; XU JIKANG ; CAI JIANYONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118345241A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG DUODONG</creatorcontrib><creatorcontrib>BAO JIN</creatorcontrib><creatorcontrib>YANG ZEPING</creatorcontrib><creatorcontrib>ZHANG JIHONG</creatorcontrib><creatorcontrib>XU JIKANG</creatorcontrib><creatorcontrib>CAI JIANYONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG DUODONG</au><au>BAO JIN</au><au>YANG ZEPING</au><au>ZHANG JIHONG</au><au>XU JIKANG</au><au>CAI JIANYONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing ferro-nickel alloy through step-by-step reduction of laterite-nickel ore in rotary kiln</title><date>2024-07-16</date><risdate>2024</risdate><abstract>The invention discloses a method for preparing ferro-nickel alloy through step-by-step reduction of laterite-nickel ore in a rotary kiln. The method comprises the following steps: screening a carbon reducing agent into an oversize reducing agent and an undersize reducing agent; the method comprises the following steps: screening, crushing and drying laterite-nickel ore, feeding the laterite-nickel ore into a rotary kiln, adding an oversize reducing agent at the kiln tail of the rotary kiln, carrying out pre-reduction roasting, adding an undersize reducing agent from the kiln head of the rotary kiln after roasting, mixing with a pre-reduction roasting product roasted product, feeding the mixture into a charging bucket for caching, and smelting by an electric furnace, thereby obtaining the product. The addition amount of the carbon reducing agent is 3-5.5% of the mass of the dry laterite-nickel ore; and the particle size of the oversize reducing agent is greater than or equal to 20mm. According to the method, a</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN118345241A
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
METALLURGY OF IRON
PRETREATMENT OF RAW MATERIALS
PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL
PRODUCTION AND REFINING OF METALS
TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Method for preparing ferro-nickel alloy through step-by-step reduction of laterite-nickel ore in rotary kiln
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-29T10%3A29%3A41IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20DUODONG&rft.date=2024-07-16&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118345241A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true