Preparation method of lanthanum-loaded artificial wetland filler for deep phosphorus removal

A preparation method of a lanthanum-loaded artificial wetland filler for deep phosphorus removal comprises the following steps: preparing an artificial wetland pre-filler which is prepared from the following components in parts by weight: 65-75 parts of lake sediment, 10 parts of canna biomass powde...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HE XUEMEI, XIAO JINGJIANG, XU QIAOLING
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HE XUEMEI
XIAO JINGJIANG
XU QIAOLING
description A preparation method of a lanthanum-loaded artificial wetland filler for deep phosphorus removal comprises the following steps: preparing an artificial wetland pre-filler which is prepared from the following components in parts by weight: 65-75 parts of lake sediment, 10 parts of canna biomass powder, 10-20 parts of soluble starch/attapulgite and 5-10 parts of magnesium carbonate; the method comprises the following steps: magnetically stirring a lanthanum chloride solution with the concentration of 0.02-0.1 mol.L at 25-85 DEG C for 5-10 minutes, adding a constructed wetland pre-filling material, then adding magnesium salt, carrying out ultrasonic treatment for 10-30 minutes, and continuously stirring for 10-20 minutes to obtain a mixed solution; and dropwise adding a sodium bicarbonate solution into the mixed solution, continuously stirring, aging for 15-30 minutes, cooling, carrying out suction filtration, washing with distilled water, and drying to obtain the lanthanum-loaded artificial wetland filler
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118239603A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118239603A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118239603A3</originalsourceid><addsrcrecordid>eNqNijEKAjEQAK-xEPUP6wMOPAOipRyKlVhYCsdy2ZDAJhs2Of2-V_gAi2GKmWXzeihlVKxBEkSqXiyIA8ZUPaYptixoyQJqDS6MARk-VOdswQVmUnCiYIkyZC9lRqcCSlHeyOtm4ZALbX5eNdvr5dnfWsoyUMk4UqI69PeuO-7N6bAzZ_PP8wUFHDx5</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of lanthanum-loaded artificial wetland filler for deep phosphorus removal</title><source>esp@cenet</source><creator>HE XUEMEI ; XIAO JINGJIANG ; XU QIAOLING</creator><creatorcontrib>HE XUEMEI ; XIAO JINGJIANG ; XU QIAOLING</creatorcontrib><description>A preparation method of a lanthanum-loaded artificial wetland filler for deep phosphorus removal comprises the following steps: preparing an artificial wetland pre-filler which is prepared from the following components in parts by weight: 65-75 parts of lake sediment, 10 parts of canna biomass powder, 10-20 parts of soluble starch/attapulgite and 5-10 parts of magnesium carbonate; the method comprises the following steps: magnetically stirring a lanthanum chloride solution with the concentration of 0.02-0.1 mol.L &lt;-1 &gt; at 25-85 DEG C for 5-10 minutes, adding a constructed wetland pre-filling material, then adding magnesium salt, carrying out ultrasonic treatment for 10-30 minutes, and continuously stirring for 10-20 minutes to obtain a mixed solution; and dropwise adding a sodium bicarbonate solution into the mixed solution, continuously stirring, aging for 15-30 minutes, cooling, carrying out suction filtration, washing with distilled water, and drying to obtain the lanthanum-loaded artificial wetland filler</description><language>chi ; eng</language><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY ; CHEMISTRY ; METALLURGY ; PERFORMING OPERATIONS ; PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL ; THEIR RELEVANT APPARATUS ; TRANSPORTING ; TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240625&amp;DB=EPODOC&amp;CC=CN&amp;NR=118239603A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240625&amp;DB=EPODOC&amp;CC=CN&amp;NR=118239603A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HE XUEMEI</creatorcontrib><creatorcontrib>XIAO JINGJIANG</creatorcontrib><creatorcontrib>XU QIAOLING</creatorcontrib><title>Preparation method of lanthanum-loaded artificial wetland filler for deep phosphorus removal</title><description>A preparation method of a lanthanum-loaded artificial wetland filler for deep phosphorus removal comprises the following steps: preparing an artificial wetland pre-filler which is prepared from the following components in parts by weight: 65-75 parts of lake sediment, 10 parts of canna biomass powder, 10-20 parts of soluble starch/attapulgite and 5-10 parts of magnesium carbonate; the method comprises the following steps: magnetically stirring a lanthanum chloride solution with the concentration of 0.02-0.1 mol.L &lt;-1 &gt; at 25-85 DEG C for 5-10 minutes, adding a constructed wetland pre-filling material, then adding magnesium salt, carrying out ultrasonic treatment for 10-30 minutes, and continuously stirring for 10-20 minutes to obtain a mixed solution; and dropwise adding a sodium bicarbonate solution into the mixed solution, continuously stirring, aging for 15-30 minutes, cooling, carrying out suction filtration, washing with distilled water, and drying to obtain the lanthanum-loaded artificial wetland filler</description><subject>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</subject><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</subject><subject>THEIR RELEVANT APPARATUS</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNijEKAjEQAK-xEPUP6wMOPAOipRyKlVhYCsdy2ZDAJhs2Of2-V_gAi2GKmWXzeihlVKxBEkSqXiyIA8ZUPaYptixoyQJqDS6MARk-VOdswQVmUnCiYIkyZC9lRqcCSlHeyOtm4ZALbX5eNdvr5dnfWsoyUMk4UqI69PeuO-7N6bAzZ_PP8wUFHDx5</recordid><startdate>20240625</startdate><enddate>20240625</enddate><creator>HE XUEMEI</creator><creator>XIAO JINGJIANG</creator><creator>XU QIAOLING</creator><scope>EVB</scope></search><sort><creationdate>20240625</creationdate><title>Preparation method of lanthanum-loaded artificial wetland filler for deep phosphorus removal</title><author>HE XUEMEI ; XIAO JINGJIANG ; XU QIAOLING</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118239603A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY</topic><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL</topic><topic>THEIR RELEVANT APPARATUS</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE</topic><toplevel>online_resources</toplevel><creatorcontrib>HE XUEMEI</creatorcontrib><creatorcontrib>XIAO JINGJIANG</creatorcontrib><creatorcontrib>XU QIAOLING</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HE XUEMEI</au><au>XIAO JINGJIANG</au><au>XU QIAOLING</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of lanthanum-loaded artificial wetland filler for deep phosphorus removal</title><date>2024-06-25</date><risdate>2024</risdate><abstract>A preparation method of a lanthanum-loaded artificial wetland filler for deep phosphorus removal comprises the following steps: preparing an artificial wetland pre-filler which is prepared from the following components in parts by weight: 65-75 parts of lake sediment, 10 parts of canna biomass powder, 10-20 parts of soluble starch/attapulgite and 5-10 parts of magnesium carbonate; the method comprises the following steps: magnetically stirring a lanthanum chloride solution with the concentration of 0.02-0.1 mol.L &lt;-1 &gt; at 25-85 DEG C for 5-10 minutes, adding a constructed wetland pre-filling material, then adding magnesium salt, carrying out ultrasonic treatment for 10-30 minutes, and continuously stirring for 10-20 minutes to obtain a mixed solution; and dropwise adding a sodium bicarbonate solution into the mixed solution, continuously stirring, aging for 15-30 minutes, cooling, carrying out suction filtration, washing with distilled water, and drying to obtain the lanthanum-loaded artificial wetland filler</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN118239603A
source esp@cenet
subjects CHEMICAL OR PHYSICAL PROCESSES, e.g. CATALYSIS OR COLLOIDCHEMISTRY
CHEMISTRY
METALLURGY
PERFORMING OPERATIONS
PHYSICAL OR CHEMICAL PROCESSES OR APPARATUS IN GENERAL
THEIR RELEVANT APPARATUS
TRANSPORTING
TREATMENT OF WATER, WASTE WATER, SEWAGE, OR SLUDGE
title Preparation method of lanthanum-loaded artificial wetland filler for deep phosphorus removal
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-27T00%3A18%3A40IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HE%20XUEMEI&rft.date=2024-06-25&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118239603A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true