Method for carrying out calcium treatment on low-silicon steel by adopting high-calcium wire

The invention discloses a method for performing calcium treatment on low-silicon steel by adopting a high-calcium wire, which is characterized in that the high-calcium wire is adopted for performing calcium treatment in the production of low-silicon aluminum-containing killed steel, the piece weight...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YUNXIA, MA XIAOGUANG, DIAO WANGCAI, TANG JIANPING, PANG ZHIJIE
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YUNXIA
MA XIAOGUANG
DIAO WANGCAI
TANG JIANPING
PANG ZHIJIE
description The invention discloses a method for performing calcium treatment on low-silicon steel by adopting a high-calcium wire, which is characterized in that the high-calcium wire is adopted for performing calcium treatment in the production of low-silicon aluminum-containing killed steel, the piece weight of the high-calcium wire is 288.78 g/m, the powder particle weight is 58.78 g/m, the diameter of a cored wire is 9.3-10.2 mm, and the thickness of an iron sheet is 1-1.2 mm; the smelting process before and after LF refining and wire feeding comprises the following steps: after the first furnace of steel is subjected to LF refining, firstly heating to melt slag and desulfurize, adjusting components to reach the standard, off-line measuring temperature and determining oxygen, then feeding a certain amount of aluminum wire according to the oxygen content of molten steel, then feeding the high-calcium wire, measuring temperature and determining oxygen after wire feeding, softly blowing for a certain time, and hoisting
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118147395A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118147395A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118147395A3</originalsourceid><addsrcrecordid>eNqNi7EKwjAURbM4iPoPzw_IEKpoRymKi06OQonpaxNI80LySunfW0F3p3MP3LMUzxuypQZaSmB0SpMLHdDAs3jjhh44oeYeAwMF8DTK7Lwz886M6OE1gW4o8iezrrPy140u4VosWu0zbr5cie3l_KiuEiPVmKM2GJDr6q7UUe0ORbk_Ff983rPVO98</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for carrying out calcium treatment on low-silicon steel by adopting high-calcium wire</title><source>esp@cenet</source><creator>YUNXIA ; MA XIAOGUANG ; DIAO WANGCAI ; TANG JIANPING ; PANG ZHIJIE</creator><creatorcontrib>YUNXIA ; MA XIAOGUANG ; DIAO WANGCAI ; TANG JIANPING ; PANG ZHIJIE</creatorcontrib><description>The invention discloses a method for performing calcium treatment on low-silicon steel by adopting a high-calcium wire, which is characterized in that the high-calcium wire is adopted for performing calcium treatment in the production of low-silicon aluminum-containing killed steel, the piece weight of the high-calcium wire is 288.78 g/m, the powder particle weight is 58.78 g/m, the diameter of a cored wire is 9.3-10.2 mm, and the thickness of an iron sheet is 1-1.2 mm; the smelting process before and after LF refining and wire feeding comprises the following steps: after the first furnace of steel is subjected to LF refining, firstly heating to melt slag and desulfurize, adjusting components to reach the standard, off-line measuring temperature and determining oxygen, then feeding a certain amount of aluminum wire according to the oxygen content of molten steel, then feeding the high-calcium wire, measuring temperature and determining oxygen after wire feeding, softly blowing for a certain time, and hoisting</description><language>chi ; eng</language><subject>CHEMISTRY ; METALLURGY ; METALLURGY OF IRON ; PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL ; TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240607&amp;DB=EPODOC&amp;CC=CN&amp;NR=118147395A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76419</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240607&amp;DB=EPODOC&amp;CC=CN&amp;NR=118147395A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YUNXIA</creatorcontrib><creatorcontrib>MA XIAOGUANG</creatorcontrib><creatorcontrib>DIAO WANGCAI</creatorcontrib><creatorcontrib>TANG JIANPING</creatorcontrib><creatorcontrib>PANG ZHIJIE</creatorcontrib><title>Method for carrying out calcium treatment on low-silicon steel by adopting high-calcium wire</title><description>The invention discloses a method for performing calcium treatment on low-silicon steel by adopting a high-calcium wire, which is characterized in that the high-calcium wire is adopted for performing calcium treatment in the production of low-silicon aluminum-containing killed steel, the piece weight of the high-calcium wire is 288.78 g/m, the powder particle weight is 58.78 g/m, the diameter of a cored wire is 9.3-10.2 mm, and the thickness of an iron sheet is 1-1.2 mm; the smelting process before and after LF refining and wire feeding comprises the following steps: after the first furnace of steel is subjected to LF refining, firstly heating to melt slag and desulfurize, adjusting components to reach the standard, off-line measuring temperature and determining oxygen, then feeding a certain amount of aluminum wire according to the oxygen content of molten steel, then feeding the high-calcium wire, measuring temperature and determining oxygen after wire feeding, softly blowing for a certain time, and hoisting</description><subject>CHEMISTRY</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</subject><subject>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNi7EKwjAURbM4iPoPzw_IEKpoRymKi06OQonpaxNI80LySunfW0F3p3MP3LMUzxuypQZaSmB0SpMLHdDAs3jjhh44oeYeAwMF8DTK7Lwz886M6OE1gW4o8iezrrPy140u4VosWu0zbr5cie3l_KiuEiPVmKM2GJDr6q7UUe0ORbk_Ff983rPVO98</recordid><startdate>20240607</startdate><enddate>20240607</enddate><creator>YUNXIA</creator><creator>MA XIAOGUANG</creator><creator>DIAO WANGCAI</creator><creator>TANG JIANPING</creator><creator>PANG ZHIJIE</creator><scope>EVB</scope></search><sort><creationdate>20240607</creationdate><title>Method for carrying out calcium treatment on low-silicon steel by adopting high-calcium wire</title><author>YUNXIA ; MA XIAOGUANG ; DIAO WANGCAI ; TANG JIANPING ; PANG ZHIJIE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118147395A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CHEMISTRY</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL</topic><topic>TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS</topic><toplevel>online_resources</toplevel><creatorcontrib>YUNXIA</creatorcontrib><creatorcontrib>MA XIAOGUANG</creatorcontrib><creatorcontrib>DIAO WANGCAI</creatorcontrib><creatorcontrib>TANG JIANPING</creatorcontrib><creatorcontrib>PANG ZHIJIE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YUNXIA</au><au>MA XIAOGUANG</au><au>DIAO WANGCAI</au><au>TANG JIANPING</au><au>PANG ZHIJIE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for carrying out calcium treatment on low-silicon steel by adopting high-calcium wire</title><date>2024-06-07</date><risdate>2024</risdate><abstract>The invention discloses a method for performing calcium treatment on low-silicon steel by adopting a high-calcium wire, which is characterized in that the high-calcium wire is adopted for performing calcium treatment in the production of low-silicon aluminum-containing killed steel, the piece weight of the high-calcium wire is 288.78 g/m, the powder particle weight is 58.78 g/m, the diameter of a cored wire is 9.3-10.2 mm, and the thickness of an iron sheet is 1-1.2 mm; the smelting process before and after LF refining and wire feeding comprises the following steps: after the first furnace of steel is subjected to LF refining, firstly heating to melt slag and desulfurize, adjusting components to reach the standard, off-line measuring temperature and determining oxygen, then feeding a certain amount of aluminum wire according to the oxygen content of molten steel, then feeding the high-calcium wire, measuring temperature and determining oxygen after wire feeding, softly blowing for a certain time, and hoisting</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN118147395A
source esp@cenet
subjects CHEMISTRY
METALLURGY
METALLURGY OF IRON
PROCESSING OF PIG-IRON, e.g. REFINING, MANUFACTURE OFWROUGHT-IRON OR STEEL
TREATMENT IN MOLTEN STATE OF FERROUS ALLOYS
title Method for carrying out calcium treatment on low-silicon steel by adopting high-calcium wire
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T17%3A20%3A48IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YUNXIA&rft.date=2024-06-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118147395A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true