Ceramsite proppant preparation method
The invention discloses a preparation method of a ceramsite proppant, the ceramsite proppant contains 35-40 parts of aluminum ash, 30-38 parts of flint clay, 20-25 parts of kaolin, 10-20 parts of perlite, 8-15 parts of manganese ore, 5-8 parts of straw and 3-5 parts of 2, 5-furandicarboxylic acid (F...
Gespeichert in:
Hauptverfasser: | , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | XIE QIUBO CHEN PINWEI ZHENG LI WU JINGJING GAO YUNJIE ZHENG PENG CHEN PEIYAO |
description | The invention discloses a preparation method of a ceramsite proppant, the ceramsite proppant contains 35-40 parts of aluminum ash, 30-38 parts of flint clay, 20-25 parts of kaolin, 10-20 parts of perlite, 8-15 parts of manganese ore, 5-8 parts of straw and 3-5 parts of 2, 5-furandicarboxylic acid (FDCA), and the preparation method comprises the following steps: firstly carrying out coarse crushing on the straw, and then carrying out ball milling to obtain 500-mesh powder; the flint clay, the kaolin, the perlite, the manganese ore and the FDCA are subjected to ball milling to obtain 500-mesh raw materials, then the raw materials are mixed in proportion, granulated and formed, the raw materials are dried through a belt dryer and then transferred to a rotary kiln to be fired, and the finished product is obtained.The ceramsite proppant prepared through the method has the advantages of being high in strength, low in density, good in stability and low in crushing rate, recycled raw materials are adopted, energy is |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118125854A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118125854A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118125854A3</originalsourceid><addsrcrecordid>eNrjZFB1Ti1KzC3OLElVKCjKLyhIzCsBMlILEosSSzLz8xRyU0sy8lN4GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8s5-hoYWhkamFqYmjMTFqAHK7J6k</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Ceramsite proppant preparation method</title><source>esp@cenet</source><creator>XIE QIUBO ; CHEN PINWEI ; ZHENG LI ; WU JINGJING ; GAO YUNJIE ; ZHENG PENG ; CHEN PEIYAO</creator><creatorcontrib>XIE QIUBO ; CHEN PINWEI ; ZHENG LI ; WU JINGJING ; GAO YUNJIE ; ZHENG PENG ; CHEN PEIYAO</creatorcontrib><description>The invention discloses a preparation method of a ceramsite proppant, the ceramsite proppant contains 35-40 parts of aluminum ash, 30-38 parts of flint clay, 20-25 parts of kaolin, 10-20 parts of perlite, 8-15 parts of manganese ore, 5-8 parts of straw and 3-5 parts of 2, 5-furandicarboxylic acid (FDCA), and the preparation method comprises the following steps: firstly carrying out coarse crushing on the straw, and then carrying out ball milling to obtain 500-mesh powder; the flint clay, the kaolin, the perlite, the manganese ore and the FDCA are subjected to ball milling to obtain 500-mesh raw materials, then the raw materials are mixed in proportion, granulated and formed, the raw materials are dried through a belt dryer and then transferred to a rotary kiln to be fired, and the finished product is obtained.The ceramsite proppant prepared through the method has the advantages of being high in strength, low in density, good in stability and low in crushing rate, recycled raw materials are adopted, energy is</description><language>chi ; eng</language><subject>ADHESIVES ; ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; DYES ; LIME, MAGNESIA ; MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; PAINTS ; POLISHES ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240604&DB=EPODOC&CC=CN&NR=118125854A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240604&DB=EPODOC&CC=CN&NR=118125854A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>XIE QIUBO</creatorcontrib><creatorcontrib>CHEN PINWEI</creatorcontrib><creatorcontrib>ZHENG LI</creatorcontrib><creatorcontrib>WU JINGJING</creatorcontrib><creatorcontrib>GAO YUNJIE</creatorcontrib><creatorcontrib>ZHENG PENG</creatorcontrib><creatorcontrib>CHEN PEIYAO</creatorcontrib><title>Ceramsite proppant preparation method</title><description>The invention discloses a preparation method of a ceramsite proppant, the ceramsite proppant contains 35-40 parts of aluminum ash, 30-38 parts of flint clay, 20-25 parts of kaolin, 10-20 parts of perlite, 8-15 parts of manganese ore, 5-8 parts of straw and 3-5 parts of 2, 5-furandicarboxylic acid (FDCA), and the preparation method comprises the following steps: firstly carrying out coarse crushing on the straw, and then carrying out ball milling to obtain 500-mesh powder; the flint clay, the kaolin, the perlite, the manganese ore and the FDCA are subjected to ball milling to obtain 500-mesh raw materials, then the raw materials are mixed in proportion, granulated and formed, the raw materials are dried through a belt dryer and then transferred to a rotary kiln to be fired, and the finished product is obtained.The ceramsite proppant prepared through the method has the advantages of being high in strength, low in density, good in stability and low in crushing rate, recycled raw materials are adopted, energy is</description><subject>ADHESIVES</subject><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>DYES</subject><subject>LIME, MAGNESIA</subject><subject>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZFB1Ti1KzC3OLElVKCjKLyhIzCsBMlILEosSSzLz8xRyU0sy8lN4GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8s5-hoYWhkamFqYmjMTFqAHK7J6k</recordid><startdate>20240604</startdate><enddate>20240604</enddate><creator>XIE QIUBO</creator><creator>CHEN PINWEI</creator><creator>ZHENG LI</creator><creator>WU JINGJING</creator><creator>GAO YUNJIE</creator><creator>ZHENG PENG</creator><creator>CHEN PEIYAO</creator><scope>EVB</scope></search><sort><creationdate>20240604</creationdate><title>Ceramsite proppant preparation method</title><author>XIE QIUBO ; CHEN PINWEI ; ZHENG LI ; WU JINGJING ; GAO YUNJIE ; ZHENG PENG ; CHEN PEIYAO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118125854A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>ADHESIVES</topic><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>DYES</topic><topic>LIME, MAGNESIA</topic><topic>MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>XIE QIUBO</creatorcontrib><creatorcontrib>CHEN PINWEI</creatorcontrib><creatorcontrib>ZHENG LI</creatorcontrib><creatorcontrib>WU JINGJING</creatorcontrib><creatorcontrib>GAO YUNJIE</creatorcontrib><creatorcontrib>ZHENG PENG</creatorcontrib><creatorcontrib>CHEN PEIYAO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>XIE QIUBO</au><au>CHEN PINWEI</au><au>ZHENG LI</au><au>WU JINGJING</au><au>GAO YUNJIE</au><au>ZHENG PENG</au><au>CHEN PEIYAO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Ceramsite proppant preparation method</title><date>2024-06-04</date><risdate>2024</risdate><abstract>The invention discloses a preparation method of a ceramsite proppant, the ceramsite proppant contains 35-40 parts of aluminum ash, 30-38 parts of flint clay, 20-25 parts of kaolin, 10-20 parts of perlite, 8-15 parts of manganese ore, 5-8 parts of straw and 3-5 parts of 2, 5-furandicarboxylic acid (FDCA), and the preparation method comprises the following steps: firstly carrying out coarse crushing on the straw, and then carrying out ball milling to obtain 500-mesh powder; the flint clay, the kaolin, the perlite, the manganese ore and the FDCA are subjected to ball milling to obtain 500-mesh raw materials, then the raw materials are mixed in proportion, granulated and formed, the raw materials are dried through a belt dryer and then transferred to a rotary kiln to be fired, and the finished product is obtained.The ceramsite proppant prepared through the method has the advantages of being high in strength, low in density, good in stability and low in crushing rate, recycled raw materials are adopted, energy is</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN118125854A |
source | esp@cenet |
subjects | ADHESIVES ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE DYES LIME, MAGNESIA MATERIALS FOR MISCELLANEOUS APPLICATIONS, NOT PROVIDED FORELSEWHERE METALLURGY MISCELLANEOUS APPLICATIONS OF MATERIALS MISCELLANEOUS COMPOSITIONS NATURAL RESINS PAINTS POLISHES REFRACTORIES SLAG TREATMENT OF NATURAL STONE |
title | Ceramsite proppant preparation method |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-22T19%3A17%3A48IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=XIE%20QIUBO&rft.date=2024-06-04&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118125854A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |