Asphalt mixture compositely modified by ethylene-vinyl acetate copolymer, naphthenic oil and polyphosphoric acid and preparation method thereof
The invention provides an asphalt mixture compositely modified by an ethylene-vinyl acetate copolymer, naphthenic oil and polyphosphoric acid and a preparation method of the asphalt mixture, and aims to solve the technical problems of improving high and low temperature diseases and aging resistance...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , , , , , , , , , , , , , , , , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | CHEN YUANZHAO ZHANG GUIFEN JIN YUNGUANG LI ZHEN LI QIANGQIANG LIU QI WANG XING LYU HAIJIANG WANG LONG LI BO SHANG YUN ZHANG ZHIYONG CUI LONGFEI ZHANG CHUANG HAO ZHUO CHEN QI WANG JINGXIANG SHAO DAN ZHANG HONGHAI LIU XIAONAN YANG GUOHONG DU PENG MENG LINCHAO AN JIN HU YUPING ZHAO CHEN'AO FAN ZHICHAO PAN YILUN HOU CHENGCHENG WANG CHAO BAO XUN LIU XUN YU SHUYIN |
description | The invention provides an asphalt mixture compositely modified by an ethylene-vinyl acetate copolymer, naphthenic oil and polyphosphoric acid and a preparation method of the asphalt mixture, and aims to solve the technical problems of improving high and low temperature diseases and aging resistance of an asphalt pavement while ensuring the pavement performance of the asphalt mixture. The composite modified asphalt mixture is prepared from the following raw materials in parts by weight: 100 parts of mineral aggregate, 5 to 7 parts of asphalt, 0.24 to 0.49 part of ethylene-vinyl acetate copolymer, 0.1 to 0.21 part of naphthenic oil and 0.025 to 0.105 part of polyphosphoric acid. The composite modified asphalt mixture provided by the invention belongs to an environment-friendly, non-toxic and non-corrosive composite asphalt mixture, is excellent in pavement performance, can enhance the high-temperature stability, low-temperature crack resistance and water stability of an asphalt pavement, has great significance |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN118084397A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN118084397A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN118084397A3</originalsourceid><addsrcrecordid>eNqNjcEKwjAQRHvxIOo_rHcLlgrWYymKJ0_eJTZbspBkQ7qK-Qp_2RT9AE8DM29m5sW7HYNRVsDRSx4RoWcXeCRBm8CxpoFQwz0BikkWPZZP8smC6lGUTHhgmxzGDXgVjBj01ANTJryGKQuG8wXHbKue9NePGFRUQuzB5WXWkJsReVgWs0HZEVc_XRTr0_HanUsMfMMx5F-PcusuVdVsm1192Lf1P8wHElNQRA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Asphalt mixture compositely modified by ethylene-vinyl acetate copolymer, naphthenic oil and polyphosphoric acid and preparation method thereof</title><source>esp@cenet</source><creator>CHEN YUANZHAO ; ZHANG GUIFEN ; JIN YUNGUANG ; LI ZHEN ; LI QIANGQIANG ; LIU QI ; WANG XING ; LYU HAIJIANG ; WANG LONG ; LI BO ; SHANG YUN ; ZHANG ZHIYONG ; CUI LONGFEI ; ZHANG CHUANG ; HAO ZHUO ; CHEN QI ; WANG JINGXIANG ; SHAO DAN ; ZHANG HONGHAI ; LIU XIAONAN ; YANG GUOHONG ; DU PENG ; MENG LINCHAO ; AN JIN ; HU YUPING ; ZHAO CHEN'AO ; FAN ZHICHAO ; PAN YILUN ; HOU CHENGCHENG ; WANG CHAO ; BAO XUN ; LIU XUN ; YU SHUYIN</creator><creatorcontrib>CHEN YUANZHAO ; ZHANG GUIFEN ; JIN YUNGUANG ; LI ZHEN ; LI QIANGQIANG ; LIU QI ; WANG XING ; LYU HAIJIANG ; WANG LONG ; LI BO ; SHANG YUN ; ZHANG ZHIYONG ; CUI LONGFEI ; ZHANG CHUANG ; HAO ZHUO ; CHEN QI ; WANG JINGXIANG ; SHAO DAN ; ZHANG HONGHAI ; LIU XIAONAN ; YANG GUOHONG ; DU PENG ; MENG LINCHAO ; AN JIN ; HU YUPING ; ZHAO CHEN'AO ; FAN ZHICHAO ; PAN YILUN ; HOU CHENGCHENG ; WANG CHAO ; BAO XUN ; LIU XUN ; YU SHUYIN</creatorcontrib><description>The invention provides an asphalt mixture compositely modified by an ethylene-vinyl acetate copolymer, naphthenic oil and polyphosphoric acid and a preparation method of the asphalt mixture, and aims to solve the technical problems of improving high and low temperature diseases and aging resistance of an asphalt pavement while ensuring the pavement performance of the asphalt mixture. The composite modified asphalt mixture is prepared from the following raw materials in parts by weight: 100 parts of mineral aggregate, 5 to 7 parts of asphalt, 0.24 to 0.49 part of ethylene-vinyl acetate copolymer, 0.1 to 0.21 part of naphthenic oil and 0.025 to 0.105 part of polyphosphoric acid. The composite modified asphalt mixture provided by the invention belongs to an environment-friendly, non-toxic and non-corrosive composite asphalt mixture, is excellent in pavement performance, can enhance the high-temperature stability, low-temperature crack resistance and water stability of an asphalt pavement, has great significance</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240528&DB=EPODOC&CC=CN&NR=118084397A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240528&DB=EPODOC&CC=CN&NR=118084397A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>CHEN YUANZHAO</creatorcontrib><creatorcontrib>ZHANG GUIFEN</creatorcontrib><creatorcontrib>JIN YUNGUANG</creatorcontrib><creatorcontrib>LI ZHEN</creatorcontrib><creatorcontrib>LI QIANGQIANG</creatorcontrib><creatorcontrib>LIU QI</creatorcontrib><creatorcontrib>WANG XING</creatorcontrib><creatorcontrib>LYU HAIJIANG</creatorcontrib><creatorcontrib>WANG LONG</creatorcontrib><creatorcontrib>LI BO</creatorcontrib><creatorcontrib>SHANG YUN</creatorcontrib><creatorcontrib>ZHANG ZHIYONG</creatorcontrib><creatorcontrib>CUI LONGFEI</creatorcontrib><creatorcontrib>ZHANG CHUANG</creatorcontrib><creatorcontrib>HAO ZHUO</creatorcontrib><creatorcontrib>CHEN QI</creatorcontrib><creatorcontrib>WANG JINGXIANG</creatorcontrib><creatorcontrib>SHAO DAN</creatorcontrib><creatorcontrib>ZHANG HONGHAI</creatorcontrib><creatorcontrib>LIU XIAONAN</creatorcontrib><creatorcontrib>YANG GUOHONG</creatorcontrib><creatorcontrib>DU PENG</creatorcontrib><creatorcontrib>MENG LINCHAO</creatorcontrib><creatorcontrib>AN JIN</creatorcontrib><creatorcontrib>HU YUPING</creatorcontrib><creatorcontrib>ZHAO CHEN'AO</creatorcontrib><creatorcontrib>FAN ZHICHAO</creatorcontrib><creatorcontrib>PAN YILUN</creatorcontrib><creatorcontrib>HOU CHENGCHENG</creatorcontrib><creatorcontrib>WANG CHAO</creatorcontrib><creatorcontrib>BAO XUN</creatorcontrib><creatorcontrib>LIU XUN</creatorcontrib><creatorcontrib>YU SHUYIN</creatorcontrib><title>Asphalt mixture compositely modified by ethylene-vinyl acetate copolymer, naphthenic oil and polyphosphoric acid and preparation method thereof</title><description>The invention provides an asphalt mixture compositely modified by an ethylene-vinyl acetate copolymer, naphthenic oil and polyphosphoric acid and a preparation method of the asphalt mixture, and aims to solve the technical problems of improving high and low temperature diseases and aging resistance of an asphalt pavement while ensuring the pavement performance of the asphalt mixture. The composite modified asphalt mixture is prepared from the following raw materials in parts by weight: 100 parts of mineral aggregate, 5 to 7 parts of asphalt, 0.24 to 0.49 part of ethylene-vinyl acetate copolymer, 0.1 to 0.21 part of naphthenic oil and 0.025 to 0.105 part of polyphosphoric acid. The composite modified asphalt mixture provided by the invention belongs to an environment-friendly, non-toxic and non-corrosive composite asphalt mixture, is excellent in pavement performance, can enhance the high-temperature stability, low-temperature crack resistance and water stability of an asphalt pavement, has great significance</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjcEKwjAQRHvxIOo_rHcLlgrWYymKJ0_eJTZbspBkQ7qK-Qp_2RT9AE8DM29m5sW7HYNRVsDRSx4RoWcXeCRBm8CxpoFQwz0BikkWPZZP8smC6lGUTHhgmxzGDXgVjBj01ANTJryGKQuG8wXHbKue9NePGFRUQuzB5WXWkJsReVgWs0HZEVc_XRTr0_HanUsMfMMx5F-PcusuVdVsm1192Lf1P8wHElNQRA</recordid><startdate>20240528</startdate><enddate>20240528</enddate><creator>CHEN YUANZHAO</creator><creator>ZHANG GUIFEN</creator><creator>JIN YUNGUANG</creator><creator>LI ZHEN</creator><creator>LI QIANGQIANG</creator><creator>LIU QI</creator><creator>WANG XING</creator><creator>LYU HAIJIANG</creator><creator>WANG LONG</creator><creator>LI BO</creator><creator>SHANG YUN</creator><creator>ZHANG ZHIYONG</creator><creator>CUI LONGFEI</creator><creator>ZHANG CHUANG</creator><creator>HAO ZHUO</creator><creator>CHEN QI</creator><creator>WANG JINGXIANG</creator><creator>SHAO DAN</creator><creator>ZHANG HONGHAI</creator><creator>LIU XIAONAN</creator><creator>YANG GUOHONG</creator><creator>DU PENG</creator><creator>MENG LINCHAO</creator><creator>AN JIN</creator><creator>HU YUPING</creator><creator>ZHAO CHEN'AO</creator><creator>FAN ZHICHAO</creator><creator>PAN YILUN</creator><creator>HOU CHENGCHENG</creator><creator>WANG CHAO</creator><creator>BAO XUN</creator><creator>LIU XUN</creator><creator>YU SHUYIN</creator><scope>EVB</scope></search><sort><creationdate>20240528</creationdate><title>Asphalt mixture compositely modified by ethylene-vinyl acetate copolymer, naphthenic oil and polyphosphoric acid and preparation method thereof</title><author>CHEN YUANZHAO ; ZHANG GUIFEN ; JIN YUNGUANG ; LI ZHEN ; LI QIANGQIANG ; LIU QI ; WANG XING ; LYU HAIJIANG ; WANG LONG ; LI BO ; SHANG YUN ; ZHANG ZHIYONG ; CUI LONGFEI ; ZHANG CHUANG ; HAO ZHUO ; CHEN QI ; WANG JINGXIANG ; SHAO DAN ; ZHANG HONGHAI ; LIU XIAONAN ; YANG GUOHONG ; DU PENG ; MENG LINCHAO ; AN JIN ; HU YUPING ; ZHAO CHEN'AO ; FAN ZHICHAO ; PAN YILUN ; HOU CHENGCHENG ; WANG CHAO ; BAO XUN ; LIU XUN ; YU SHUYIN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN118084397A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>CHEN YUANZHAO</creatorcontrib><creatorcontrib>ZHANG GUIFEN</creatorcontrib><creatorcontrib>JIN YUNGUANG</creatorcontrib><creatorcontrib>LI ZHEN</creatorcontrib><creatorcontrib>LI QIANGQIANG</creatorcontrib><creatorcontrib>LIU QI</creatorcontrib><creatorcontrib>WANG XING</creatorcontrib><creatorcontrib>LYU HAIJIANG</creatorcontrib><creatorcontrib>WANG LONG</creatorcontrib><creatorcontrib>LI BO</creatorcontrib><creatorcontrib>SHANG YUN</creatorcontrib><creatorcontrib>ZHANG ZHIYONG</creatorcontrib><creatorcontrib>CUI LONGFEI</creatorcontrib><creatorcontrib>ZHANG CHUANG</creatorcontrib><creatorcontrib>HAO ZHUO</creatorcontrib><creatorcontrib>CHEN QI</creatorcontrib><creatorcontrib>WANG JINGXIANG</creatorcontrib><creatorcontrib>SHAO DAN</creatorcontrib><creatorcontrib>ZHANG HONGHAI</creatorcontrib><creatorcontrib>LIU XIAONAN</creatorcontrib><creatorcontrib>YANG GUOHONG</creatorcontrib><creatorcontrib>DU PENG</creatorcontrib><creatorcontrib>MENG LINCHAO</creatorcontrib><creatorcontrib>AN JIN</creatorcontrib><creatorcontrib>HU YUPING</creatorcontrib><creatorcontrib>ZHAO CHEN'AO</creatorcontrib><creatorcontrib>FAN ZHICHAO</creatorcontrib><creatorcontrib>PAN YILUN</creatorcontrib><creatorcontrib>HOU CHENGCHENG</creatorcontrib><creatorcontrib>WANG CHAO</creatorcontrib><creatorcontrib>BAO XUN</creatorcontrib><creatorcontrib>LIU XUN</creatorcontrib><creatorcontrib>YU SHUYIN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>CHEN YUANZHAO</au><au>ZHANG GUIFEN</au><au>JIN YUNGUANG</au><au>LI ZHEN</au><au>LI QIANGQIANG</au><au>LIU QI</au><au>WANG XING</au><au>LYU HAIJIANG</au><au>WANG LONG</au><au>LI BO</au><au>SHANG YUN</au><au>ZHANG ZHIYONG</au><au>CUI LONGFEI</au><au>ZHANG CHUANG</au><au>HAO ZHUO</au><au>CHEN QI</au><au>WANG JINGXIANG</au><au>SHAO DAN</au><au>ZHANG HONGHAI</au><au>LIU XIAONAN</au><au>YANG GUOHONG</au><au>DU PENG</au><au>MENG LINCHAO</au><au>AN JIN</au><au>HU YUPING</au><au>ZHAO CHEN'AO</au><au>FAN ZHICHAO</au><au>PAN YILUN</au><au>HOU CHENGCHENG</au><au>WANG CHAO</au><au>BAO XUN</au><au>LIU XUN</au><au>YU SHUYIN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Asphalt mixture compositely modified by ethylene-vinyl acetate copolymer, naphthenic oil and polyphosphoric acid and preparation method thereof</title><date>2024-05-28</date><risdate>2024</risdate><abstract>The invention provides an asphalt mixture compositely modified by an ethylene-vinyl acetate copolymer, naphthenic oil and polyphosphoric acid and a preparation method of the asphalt mixture, and aims to solve the technical problems of improving high and low temperature diseases and aging resistance of an asphalt pavement while ensuring the pavement performance of the asphalt mixture. The composite modified asphalt mixture is prepared from the following raw materials in parts by weight: 100 parts of mineral aggregate, 5 to 7 parts of asphalt, 0.24 to 0.49 part of ethylene-vinyl acetate copolymer, 0.1 to 0.21 part of naphthenic oil and 0.025 to 0.105 part of polyphosphoric acid. The composite modified asphalt mixture provided by the invention belongs to an environment-friendly, non-toxic and non-corrosive composite asphalt mixture, is excellent in pavement performance, can enhance the high-temperature stability, low-temperature crack resistance and water stability of an asphalt pavement, has great significance</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN118084397A |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE LIME, MAGNESIA METALLURGY REFRACTORIES SLAG TREATMENT OF NATURAL STONE |
title | Asphalt mixture compositely modified by ethylene-vinyl acetate copolymer, naphthenic oil and polyphosphoric acid and preparation method thereof |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-29T16%3A13%3A45IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=CHEN%20YUANZHAO&rft.date=2024-05-28&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN118084397A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |