Preparation method of alkaline total-iron flow battery electrode material

The invention discloses a preparation method of an alkaline all-iron flow battery electrode material, which comprises the following steps: uniformly mixing ferrous salt, a surfactant and water according to a certain proportion range, then soaking a graphite felt pretreated by nitric acid in the mixe...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HU LU, WU HONGGUAN, XU FEI, QU LISHENG, LI HAIFENG, XU XUNDA, WANG QINGQING, YU GUOXIAN, PAN WEI, CHEN HE
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HU LU
WU HONGGUAN
XU FEI
QU LISHENG
LI HAIFENG
XU XUNDA
WANG QINGQING
YU GUOXIAN
PAN WEI
CHEN HE
description The invention discloses a preparation method of an alkaline all-iron flow battery electrode material, which comprises the following steps: uniformly mixing ferrous salt, a surfactant and water according to a certain proportion range, then soaking a graphite felt pretreated by nitric acid in the mixed liquid, adding a sodium hydroxide solution to adjust the pH value to 8-9, adding an oxidant for oxidation, and finally, carrying out vacuum drying to obtain the alkaline all-iron flow battery electrode material. And adjusting the pH value of the impregnated mixture to 10-13 by using a sodium hydroxide solution at 90-100 DEG C, refluxing for 1-3 hours, finally taking out the graphite felt, washing, and carrying out vacuum drying, thereby obtaining the ferroferric oxide modified graphite felt electrode material. And reaction active sites of positive and negative electrode electrolyte active substances on the surface of the electrode are obviously increased. The preparation method has the advantages of easily availa
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117996093A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117996093A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117996093A3</originalsourceid><addsrcrecordid>eNqNijEKwkAQRbexEPUO4wEChoCSUoKijVjYhzH5SxYnO8tmQLy9KTyA1YP33tJd7xmJM1vQSCNs0J7UE8uLJUSQqbEUIc_Vi77pyWbIH4Kgs6w9aORZBJa1W3iWCZsfV257Pj2aS4GkLabEHSKsbW5leajr_a6ujtU_zxcSNTUo</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of alkaline total-iron flow battery electrode material</title><source>esp@cenet</source><creator>HU LU ; WU HONGGUAN ; XU FEI ; QU LISHENG ; LI HAIFENG ; XU XUNDA ; WANG QINGQING ; YU GUOXIAN ; PAN WEI ; CHEN HE</creator><creatorcontrib>HU LU ; WU HONGGUAN ; XU FEI ; QU LISHENG ; LI HAIFENG ; XU XUNDA ; WANG QINGQING ; YU GUOXIAN ; PAN WEI ; CHEN HE</creatorcontrib><description>The invention discloses a preparation method of an alkaline all-iron flow battery electrode material, which comprises the following steps: uniformly mixing ferrous salt, a surfactant and water according to a certain proportion range, then soaking a graphite felt pretreated by nitric acid in the mixed liquid, adding a sodium hydroxide solution to adjust the pH value to 8-9, adding an oxidant for oxidation, and finally, carrying out vacuum drying to obtain the alkaline all-iron flow battery electrode material. And adjusting the pH value of the impregnated mixture to 10-13 by using a sodium hydroxide solution at 90-100 DEG C, refluxing for 1-3 hours, finally taking out the graphite felt, washing, and carrying out vacuum drying, thereby obtaining the ferroferric oxide modified graphite felt electrode material. And reaction active sites of positive and negative electrode electrolyte active substances on the surface of the electrode are obviously increased. The preparation method has the advantages of easily availa</description><language>chi ; eng</language><subject>BASIC ELECTRIC ELEMENTS ; ELECTRICITY ; PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240507&amp;DB=EPODOC&amp;CC=CN&amp;NR=117996093A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25547,76298</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240507&amp;DB=EPODOC&amp;CC=CN&amp;NR=117996093A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HU LU</creatorcontrib><creatorcontrib>WU HONGGUAN</creatorcontrib><creatorcontrib>XU FEI</creatorcontrib><creatorcontrib>QU LISHENG</creatorcontrib><creatorcontrib>LI HAIFENG</creatorcontrib><creatorcontrib>XU XUNDA</creatorcontrib><creatorcontrib>WANG QINGQING</creatorcontrib><creatorcontrib>YU GUOXIAN</creatorcontrib><creatorcontrib>PAN WEI</creatorcontrib><creatorcontrib>CHEN HE</creatorcontrib><title>Preparation method of alkaline total-iron flow battery electrode material</title><description>The invention discloses a preparation method of an alkaline all-iron flow battery electrode material, which comprises the following steps: uniformly mixing ferrous salt, a surfactant and water according to a certain proportion range, then soaking a graphite felt pretreated by nitric acid in the mixed liquid, adding a sodium hydroxide solution to adjust the pH value to 8-9, adding an oxidant for oxidation, and finally, carrying out vacuum drying to obtain the alkaline all-iron flow battery electrode material. And adjusting the pH value of the impregnated mixture to 10-13 by using a sodium hydroxide solution at 90-100 DEG C, refluxing for 1-3 hours, finally taking out the graphite felt, washing, and carrying out vacuum drying, thereby obtaining the ferroferric oxide modified graphite felt electrode material. And reaction active sites of positive and negative electrode electrolyte active substances on the surface of the electrode are obviously increased. The preparation method has the advantages of easily availa</description><subject>BASIC ELECTRIC ELEMENTS</subject><subject>ELECTRICITY</subject><subject>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNijEKwkAQRbexEPUO4wEChoCSUoKijVjYhzH5SxYnO8tmQLy9KTyA1YP33tJd7xmJM1vQSCNs0J7UE8uLJUSQqbEUIc_Vi77pyWbIH4Kgs6w9aORZBJa1W3iWCZsfV257Pj2aS4GkLabEHSKsbW5leajr_a6ujtU_zxcSNTUo</recordid><startdate>20240507</startdate><enddate>20240507</enddate><creator>HU LU</creator><creator>WU HONGGUAN</creator><creator>XU FEI</creator><creator>QU LISHENG</creator><creator>LI HAIFENG</creator><creator>XU XUNDA</creator><creator>WANG QINGQING</creator><creator>YU GUOXIAN</creator><creator>PAN WEI</creator><creator>CHEN HE</creator><scope>EVB</scope></search><sort><creationdate>20240507</creationdate><title>Preparation method of alkaline total-iron flow battery electrode material</title><author>HU LU ; WU HONGGUAN ; XU FEI ; QU LISHENG ; LI HAIFENG ; XU XUNDA ; WANG QINGQING ; YU GUOXIAN ; PAN WEI ; CHEN HE</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117996093A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>BASIC ELECTRIC ELEMENTS</topic><topic>ELECTRICITY</topic><topic>PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY</topic><toplevel>online_resources</toplevel><creatorcontrib>HU LU</creatorcontrib><creatorcontrib>WU HONGGUAN</creatorcontrib><creatorcontrib>XU FEI</creatorcontrib><creatorcontrib>QU LISHENG</creatorcontrib><creatorcontrib>LI HAIFENG</creatorcontrib><creatorcontrib>XU XUNDA</creatorcontrib><creatorcontrib>WANG QINGQING</creatorcontrib><creatorcontrib>YU GUOXIAN</creatorcontrib><creatorcontrib>PAN WEI</creatorcontrib><creatorcontrib>CHEN HE</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HU LU</au><au>WU HONGGUAN</au><au>XU FEI</au><au>QU LISHENG</au><au>LI HAIFENG</au><au>XU XUNDA</au><au>WANG QINGQING</au><au>YU GUOXIAN</au><au>PAN WEI</au><au>CHEN HE</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of alkaline total-iron flow battery electrode material</title><date>2024-05-07</date><risdate>2024</risdate><abstract>The invention discloses a preparation method of an alkaline all-iron flow battery electrode material, which comprises the following steps: uniformly mixing ferrous salt, a surfactant and water according to a certain proportion range, then soaking a graphite felt pretreated by nitric acid in the mixed liquid, adding a sodium hydroxide solution to adjust the pH value to 8-9, adding an oxidant for oxidation, and finally, carrying out vacuum drying to obtain the alkaline all-iron flow battery electrode material. And adjusting the pH value of the impregnated mixture to 10-13 by using a sodium hydroxide solution at 90-100 DEG C, refluxing for 1-3 hours, finally taking out the graphite felt, washing, and carrying out vacuum drying, thereby obtaining the ferroferric oxide modified graphite felt electrode material. And reaction active sites of positive and negative electrode electrolyte active substances on the surface of the electrode are obviously increased. The preparation method has the advantages of easily availa</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117996093A
source esp@cenet
subjects BASIC ELECTRIC ELEMENTS
ELECTRICITY
PROCESSES OR MEANS, e.g. BATTERIES, FOR THE DIRECT CONVERSIONOF CHEMICAL INTO ELECTRICAL ENERGY
title Preparation method of alkaline total-iron flow battery electrode material
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-16T07%3A05%3A04IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HU%20LU&rft.date=2024-05-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117996093A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true