Low-alkali ecological porous concrete and preparation method thereof
The invention relates to the technical field of concrete, and discloses low-alkali ecological porous concrete and a preparation method thereof. The ecological porous concrete is prepared from the following raw materials in parts by mass: 70 to 80 parts of gravel coarse aggregate, 17 to 22 parts of c...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | ZHOU PING OUYANG QI YE RUIQIN OUYANG XUE YIN JIAN HU YINBO LI SIJIAO LYU XIAOYONG QIN YUHANG ZENG YI |
description | The invention relates to the technical field of concrete, and discloses low-alkali ecological porous concrete and a preparation method thereof. The ecological porous concrete is prepared from the following raw materials in parts by mass: 70 to 80 parts of gravel coarse aggregate, 17 to 22 parts of cement, 1 to 2 parts of diatomite, 0.1 to 0.3 part of oxalic acid, 0.1 to 0.3 part of ferric sulfate, 0.01 to 0.03 part of water reducing agent and 4 to 6 parts of water, the pH value of a 28d pore aqueous solution of the obtained low-alkali ecological porous concrete is 9.0 or below, the 7d cubic compressive strength reaches 7-10 MPa, the 28d cubic compressive strength reaches 10-15 MPa, and the porosity is 25%-30%. The ecological porous concrete is simple in formula and low in cost, the lowest pH value of 28d is 8.79, the low alkalinity and the porous structure can retain water, ventilate and supply oxygen, the germination rate of plant seeds can be increased, the environment requirement for normal growth of plant |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117985976A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117985976A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117985976A3</originalsourceid><addsrcrecordid>eNqNyjEOwjAMBdAsDAi4gzlAhwpB6YgKiAExsVdW-ksjQmw5QVyfhQMwveXN3fEqn4rjk2MgeInyCJ4jqZi8M3lJ3lBAnAZSg7JxCZLohTLJQGWCQcalm40cM1Y_F259Pt27SwWVHlnZI6H03a2um3a_bZvdYfPP-QLgvTNV</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Low-alkali ecological porous concrete and preparation method thereof</title><source>esp@cenet</source><creator>ZHOU PING ; OUYANG QI ; YE RUIQIN ; OUYANG XUE ; YIN JIAN ; HU YINBO ; LI SIJIAO ; LYU XIAOYONG ; QIN YUHANG ; ZENG YI</creator><creatorcontrib>ZHOU PING ; OUYANG QI ; YE RUIQIN ; OUYANG XUE ; YIN JIAN ; HU YINBO ; LI SIJIAO ; LYU XIAOYONG ; QIN YUHANG ; ZENG YI</creatorcontrib><description>The invention relates to the technical field of concrete, and discloses low-alkali ecological porous concrete and a preparation method thereof. The ecological porous concrete is prepared from the following raw materials in parts by mass: 70 to 80 parts of gravel coarse aggregate, 17 to 22 parts of cement, 1 to 2 parts of diatomite, 0.1 to 0.3 part of oxalic acid, 0.1 to 0.3 part of ferric sulfate, 0.01 to 0.03 part of water reducing agent and 4 to 6 parts of water, the pH value of a 28d pore aqueous solution of the obtained low-alkali ecological porous concrete is 9.0 or below, the 7d cubic compressive strength reaches 7-10 MPa, the 28d cubic compressive strength reaches 10-15 MPa, and the porosity is 25%-30%. The ecological porous concrete is simple in formula and low in cost, the lowest pH value of 28d is 8.79, the low alkalinity and the porous structure can retain water, ventilate and supply oxygen, the germination rate of plant seeds can be increased, the environment requirement for normal growth of plant</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240507&DB=EPODOC&CC=CN&NR=117985976A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240507&DB=EPODOC&CC=CN&NR=117985976A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHOU PING</creatorcontrib><creatorcontrib>OUYANG QI</creatorcontrib><creatorcontrib>YE RUIQIN</creatorcontrib><creatorcontrib>OUYANG XUE</creatorcontrib><creatorcontrib>YIN JIAN</creatorcontrib><creatorcontrib>HU YINBO</creatorcontrib><creatorcontrib>LI SIJIAO</creatorcontrib><creatorcontrib>LYU XIAOYONG</creatorcontrib><creatorcontrib>QIN YUHANG</creatorcontrib><creatorcontrib>ZENG YI</creatorcontrib><title>Low-alkali ecological porous concrete and preparation method thereof</title><description>The invention relates to the technical field of concrete, and discloses low-alkali ecological porous concrete and a preparation method thereof. The ecological porous concrete is prepared from the following raw materials in parts by mass: 70 to 80 parts of gravel coarse aggregate, 17 to 22 parts of cement, 1 to 2 parts of diatomite, 0.1 to 0.3 part of oxalic acid, 0.1 to 0.3 part of ferric sulfate, 0.01 to 0.03 part of water reducing agent and 4 to 6 parts of water, the pH value of a 28d pore aqueous solution of the obtained low-alkali ecological porous concrete is 9.0 or below, the 7d cubic compressive strength reaches 7-10 MPa, the 28d cubic compressive strength reaches 10-15 MPa, and the porosity is 25%-30%. The ecological porous concrete is simple in formula and low in cost, the lowest pH value of 28d is 8.79, the low alkalinity and the porous structure can retain water, ventilate and supply oxygen, the germination rate of plant seeds can be increased, the environment requirement for normal growth of plant</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyjEOwjAMBdAsDAi4gzlAhwpB6YgKiAExsVdW-ksjQmw5QVyfhQMwveXN3fEqn4rjk2MgeInyCJ4jqZi8M3lJ3lBAnAZSg7JxCZLohTLJQGWCQcalm40cM1Y_F259Pt27SwWVHlnZI6H03a2um3a_bZvdYfPP-QLgvTNV</recordid><startdate>20240507</startdate><enddate>20240507</enddate><creator>ZHOU PING</creator><creator>OUYANG QI</creator><creator>YE RUIQIN</creator><creator>OUYANG XUE</creator><creator>YIN JIAN</creator><creator>HU YINBO</creator><creator>LI SIJIAO</creator><creator>LYU XIAOYONG</creator><creator>QIN YUHANG</creator><creator>ZENG YI</creator><scope>EVB</scope></search><sort><creationdate>20240507</creationdate><title>Low-alkali ecological porous concrete and preparation method thereof</title><author>ZHOU PING ; OUYANG QI ; YE RUIQIN ; OUYANG XUE ; YIN JIAN ; HU YINBO ; LI SIJIAO ; LYU XIAOYONG ; QIN YUHANG ; ZENG YI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117985976A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHOU PING</creatorcontrib><creatorcontrib>OUYANG QI</creatorcontrib><creatorcontrib>YE RUIQIN</creatorcontrib><creatorcontrib>OUYANG XUE</creatorcontrib><creatorcontrib>YIN JIAN</creatorcontrib><creatorcontrib>HU YINBO</creatorcontrib><creatorcontrib>LI SIJIAO</creatorcontrib><creatorcontrib>LYU XIAOYONG</creatorcontrib><creatorcontrib>QIN YUHANG</creatorcontrib><creatorcontrib>ZENG YI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHOU PING</au><au>OUYANG QI</au><au>YE RUIQIN</au><au>OUYANG XUE</au><au>YIN JIAN</au><au>HU YINBO</au><au>LI SIJIAO</au><au>LYU XIAOYONG</au><au>QIN YUHANG</au><au>ZENG YI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Low-alkali ecological porous concrete and preparation method thereof</title><date>2024-05-07</date><risdate>2024</risdate><abstract>The invention relates to the technical field of concrete, and discloses low-alkali ecological porous concrete and a preparation method thereof. The ecological porous concrete is prepared from the following raw materials in parts by mass: 70 to 80 parts of gravel coarse aggregate, 17 to 22 parts of cement, 1 to 2 parts of diatomite, 0.1 to 0.3 part of oxalic acid, 0.1 to 0.3 part of ferric sulfate, 0.01 to 0.03 part of water reducing agent and 4 to 6 parts of water, the pH value of a 28d pore aqueous solution of the obtained low-alkali ecological porous concrete is 9.0 or below, the 7d cubic compressive strength reaches 7-10 MPa, the 28d cubic compressive strength reaches 10-15 MPa, and the porosity is 25%-30%. The ecological porous concrete is simple in formula and low in cost, the lowest pH value of 28d is 8.79, the low alkalinity and the porous structure can retain water, ventilate and supply oxygen, the germination rate of plant seeds can be increased, the environment requirement for normal growth of plant</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN117985976A |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE LIME, MAGNESIA METALLURGY REFRACTORIES SLAG TREATMENT OF NATURAL STONE |
title | Low-alkali ecological porous concrete and preparation method thereof |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-27T17%3A01%3A17IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHOU%20PING&rft.date=2024-05-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117985976A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |