Flame-retardant polyurethane repair adhesive and repair method

The invention relates to a flame-retardant polyurethane repair adhesive and a repair method. The flame-retardant polyurethane repair adhesive comprises a polyurethane prepolymer, a chain extender and a primer which are independently packaged, the chain extender comprises solid amines playing a cross...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WU XINCHENG, MA KE, WU JIANGUO, LI MINGHUI, MENG YANG, GU ZHENGYU, JO SUNGUL, PAN JUN, HAN MEICHEN, ZHOU XUCHEN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WU XINCHENG
MA KE
WU JIANGUO
LI MINGHUI
MENG YANG
GU ZHENGYU
JO SUNGUL
PAN JUN
HAN MEICHEN
ZHOU XUCHEN
description The invention relates to a flame-retardant polyurethane repair adhesive and a repair method. The flame-retardant polyurethane repair adhesive comprises a polyurethane prepolymer, a chain extender and a primer which are independently packaged, the chain extender comprises solid amines playing a crosslinking role, liquid amines playing a crosslinking role, a polyurethane catalyst, a defoaming agent, a flame retardant and ethyl acetate; the mass ratio of the chain extender to the prepolymer is (25-45): 100. The repairing method comprises the following steps: polishing the rubber surface, dissolving trichloroisocyanuric acid urea in ethyl acetate, smearing the mixture on the rubber surface, coating the primer, uniformly mixing the chain extender with the prepolymer, and pouring. The operation waiting time for repairing the conveying belt can be shortened, and standby consumption is reduced; the chain extender reacts with the polyurethane prepolymer to generate polyurethane, and the service life can be prolonged a
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117887406A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117887406A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117887406A3</originalsourceid><addsrcrecordid>eNrjZLBzy0nMTdUtSi1JLEpJzCtRKMjPqSwFcjMS81IVilILEjOLFBJTMlKLM8tSFRLzUmBiuUAl-Sk8DKxpiTnFqbxQmptB0c01xNlDN7UgPz61uCAxOTUvtSTe2c_Q0NzCwtzEwMzRmBg1AIbWMPM</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Flame-retardant polyurethane repair adhesive and repair method</title><source>esp@cenet</source><creator>WU XINCHENG ; MA KE ; WU JIANGUO ; LI MINGHUI ; MENG YANG ; GU ZHENGYU ; JO SUNGUL ; PAN JUN ; HAN MEICHEN ; ZHOU XUCHEN</creator><creatorcontrib>WU XINCHENG ; MA KE ; WU JIANGUO ; LI MINGHUI ; MENG YANG ; GU ZHENGYU ; JO SUNGUL ; PAN JUN ; HAN MEICHEN ; ZHOU XUCHEN</creatorcontrib><description>The invention relates to a flame-retardant polyurethane repair adhesive and a repair method. The flame-retardant polyurethane repair adhesive comprises a polyurethane prepolymer, a chain extender and a primer which are independently packaged, the chain extender comprises solid amines playing a crosslinking role, liquid amines playing a crosslinking role, a polyurethane catalyst, a defoaming agent, a flame retardant and ethyl acetate; the mass ratio of the chain extender to the prepolymer is (25-45): 100. The repairing method comprises the following steps: polishing the rubber surface, dissolving trichloroisocyanuric acid urea in ethyl acetate, smearing the mixture on the rubber surface, coating the primer, uniformly mixing the chain extender with the prepolymer, and pouring. The operation waiting time for repairing the conveying belt can be shortened, and standby consumption is reduced; the chain extender reacts with the polyurethane prepolymer to generate polyurethane, and the service life can be prolonged a</description><language>chi ; eng</language><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE ; ADHESIVES ; CHEMISTRY ; COMPOSITIONS BASED THEREON ; DYES ; MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS ; METALLURGY ; MISCELLANEOUS APPLICATIONS OF MATERIALS ; MISCELLANEOUS COMPOSITIONS ; NATURAL RESINS ; NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL ; ORGANIC MACROMOLECULAR COMPOUNDS ; PAINTS ; POLISHES ; THEIR PREPARATION OR CHEMICAL WORKING-UP ; USE OF MATERIALS AS ADHESIVES</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240416&amp;DB=EPODOC&amp;CC=CN&amp;NR=117887406A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25546,76297</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240416&amp;DB=EPODOC&amp;CC=CN&amp;NR=117887406A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WU XINCHENG</creatorcontrib><creatorcontrib>MA KE</creatorcontrib><creatorcontrib>WU JIANGUO</creatorcontrib><creatorcontrib>LI MINGHUI</creatorcontrib><creatorcontrib>MENG YANG</creatorcontrib><creatorcontrib>GU ZHENGYU</creatorcontrib><creatorcontrib>JO SUNGUL</creatorcontrib><creatorcontrib>PAN JUN</creatorcontrib><creatorcontrib>HAN MEICHEN</creatorcontrib><creatorcontrib>ZHOU XUCHEN</creatorcontrib><title>Flame-retardant polyurethane repair adhesive and repair method</title><description>The invention relates to a flame-retardant polyurethane repair adhesive and a repair method. The flame-retardant polyurethane repair adhesive comprises a polyurethane prepolymer, a chain extender and a primer which are independently packaged, the chain extender comprises solid amines playing a crosslinking role, liquid amines playing a crosslinking role, a polyurethane catalyst, a defoaming agent, a flame retardant and ethyl acetate; the mass ratio of the chain extender to the prepolymer is (25-45): 100. The repairing method comprises the following steps: polishing the rubber surface, dissolving trichloroisocyanuric acid urea in ethyl acetate, smearing the mixture on the rubber surface, coating the primer, uniformly mixing the chain extender with the prepolymer, and pouring. The operation waiting time for repairing the conveying belt can be shortened, and standby consumption is reduced; the chain extender reacts with the polyurethane prepolymer to generate polyurethane, and the service life can be prolonged a</description><subject>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</subject><subject>ADHESIVES</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS BASED THEREON</subject><subject>DYES</subject><subject>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</subject><subject>METALLURGY</subject><subject>MISCELLANEOUS APPLICATIONS OF MATERIALS</subject><subject>MISCELLANEOUS COMPOSITIONS</subject><subject>NATURAL RESINS</subject><subject>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</subject><subject>ORGANIC MACROMOLECULAR COMPOUNDS</subject><subject>PAINTS</subject><subject>POLISHES</subject><subject>THEIR PREPARATION OR CHEMICAL WORKING-UP</subject><subject>USE OF MATERIALS AS ADHESIVES</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLBzy0nMTdUtSi1JLEpJzCtRKMjPqSwFcjMS81IVilILEjOLFBJTMlKLM8tSFRLzUmBiuUAl-Sk8DKxpiTnFqbxQmptB0c01xNlDN7UgPz61uCAxOTUvtSTe2c_Q0NzCwtzEwMzRmBg1AIbWMPM</recordid><startdate>20240416</startdate><enddate>20240416</enddate><creator>WU XINCHENG</creator><creator>MA KE</creator><creator>WU JIANGUO</creator><creator>LI MINGHUI</creator><creator>MENG YANG</creator><creator>GU ZHENGYU</creator><creator>JO SUNGUL</creator><creator>PAN JUN</creator><creator>HAN MEICHEN</creator><creator>ZHOU XUCHEN</creator><scope>EVB</scope></search><sort><creationdate>20240416</creationdate><title>Flame-retardant polyurethane repair adhesive and repair method</title><author>WU XINCHENG ; MA KE ; WU JIANGUO ; LI MINGHUI ; MENG YANG ; GU ZHENGYU ; JO SUNGUL ; PAN JUN ; HAN MEICHEN ; ZHOU XUCHEN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117887406A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE</topic><topic>ADHESIVES</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS BASED THEREON</topic><topic>DYES</topic><topic>MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS</topic><topic>METALLURGY</topic><topic>MISCELLANEOUS APPLICATIONS OF MATERIALS</topic><topic>MISCELLANEOUS COMPOSITIONS</topic><topic>NATURAL RESINS</topic><topic>NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL</topic><topic>ORGANIC MACROMOLECULAR COMPOUNDS</topic><topic>PAINTS</topic><topic>POLISHES</topic><topic>THEIR PREPARATION OR CHEMICAL WORKING-UP</topic><topic>USE OF MATERIALS AS ADHESIVES</topic><toplevel>online_resources</toplevel><creatorcontrib>WU XINCHENG</creatorcontrib><creatorcontrib>MA KE</creatorcontrib><creatorcontrib>WU JIANGUO</creatorcontrib><creatorcontrib>LI MINGHUI</creatorcontrib><creatorcontrib>MENG YANG</creatorcontrib><creatorcontrib>GU ZHENGYU</creatorcontrib><creatorcontrib>JO SUNGUL</creatorcontrib><creatorcontrib>PAN JUN</creatorcontrib><creatorcontrib>HAN MEICHEN</creatorcontrib><creatorcontrib>ZHOU XUCHEN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WU XINCHENG</au><au>MA KE</au><au>WU JIANGUO</au><au>LI MINGHUI</au><au>MENG YANG</au><au>GU ZHENGYU</au><au>JO SUNGUL</au><au>PAN JUN</au><au>HAN MEICHEN</au><au>ZHOU XUCHEN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Flame-retardant polyurethane repair adhesive and repair method</title><date>2024-04-16</date><risdate>2024</risdate><abstract>The invention relates to a flame-retardant polyurethane repair adhesive and a repair method. The flame-retardant polyurethane repair adhesive comprises a polyurethane prepolymer, a chain extender and a primer which are independently packaged, the chain extender comprises solid amines playing a crosslinking role, liquid amines playing a crosslinking role, a polyurethane catalyst, a defoaming agent, a flame retardant and ethyl acetate; the mass ratio of the chain extender to the prepolymer is (25-45): 100. The repairing method comprises the following steps: polishing the rubber surface, dissolving trichloroisocyanuric acid urea in ethyl acetate, smearing the mixture on the rubber surface, coating the primer, uniformly mixing the chain extender with the prepolymer, and pouring. The operation waiting time for repairing the conveying belt can be shortened, and standby consumption is reduced; the chain extender reacts with the polyurethane prepolymer to generate polyurethane, and the service life can be prolonged a</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117887406A
source esp@cenet
subjects ADHESIVE PROCESSES NOT PROVIDED FOR ELSEWHERE
ADHESIVES
CHEMISTRY
COMPOSITIONS BASED THEREON
DYES
MACROMOLECULAR COMPOUNDS OBTAINED OTHERWISE THAN BY REACTIONSONLY INVOLVING UNSATURATED CARBON-TO-CARBON BONDS
METALLURGY
MISCELLANEOUS APPLICATIONS OF MATERIALS
MISCELLANEOUS COMPOSITIONS
NATURAL RESINS
NON-MECHANICAL ASPECTS OF ADHESIVE PROCESSES IN GENERAL
ORGANIC MACROMOLECULAR COMPOUNDS
PAINTS
POLISHES
THEIR PREPARATION OR CHEMICAL WORKING-UP
USE OF MATERIALS AS ADHESIVES
title Flame-retardant polyurethane repair adhesive and repair method
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-17T10%3A48%3A10IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WU%20XINCHENG&rft.date=2024-04-16&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117887406A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true