Process for preparing chromium oxide by recovering chromium-containing electroplating sludge

The invention discloses a process for preparing chromium oxide by recovering chromium-containing electroplating sludge, and belongs to the technical field of chromium-containing electroplating sludge treatment.The process comprises the following steps that sodium carbonate is added into dry sludge,...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG JUN, ZHAO HUANRAN, LI HAIYANG, LI SHUYAN, CAI HONGZHI, WU WENMING
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WANG JUN
ZHAO HUANRAN
LI HAIYANG
LI SHUYAN
CAI HONGZHI
WU WENMING
description The invention discloses a process for preparing chromium oxide by recovering chromium-containing electroplating sludge, and belongs to the technical field of chromium-containing electroplating sludge treatment.The process comprises the following steps that sodium carbonate is added into dry sludge, then roasting is conducted, clinker is obtained, deionized water is added into the clinker for water leaching treatment, and leachate is obtained after filtering; sulfuric acid is added into the leachate to adjust the pH value, then sodium metaaluminate is added, and purified liquid is obtained after evaporation and concentration; adding deionized water into the purified liquid, and then crystallizing at room temperature for 6-8 hours to obtain sodium dichromate; the method comprises the following steps: grinding sodium dichromate, adding carbon black into the ground sodium dichromate, heating to 500-550 DEG C, preserving heat for 2.5-3.0 hours, and grinding, washing and filtering a product to obtain chromic oxide.
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117699855A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117699855A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117699855A3</originalsourceid><addsrcrecordid>eNrjZIgJKMpPTi0uVkjLL1IoKEotSCzKzEtXSM4oys_NLM1VyK_ITElVSKpUKEpNzi9LRZHUTc7PK0nMzAOJpeakJpcU5RfkJJaAuMU5pSnpqTwMrGmJOcWpvFCam0HRzTXE2UM3tSA_PrW4IDE5NS-1JN7Zz9DQ3MzS0sLU1NGYGDUAQ5c9Hw</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Process for preparing chromium oxide by recovering chromium-containing electroplating sludge</title><source>esp@cenet</source><creator>WANG JUN ; ZHAO HUANRAN ; LI HAIYANG ; LI SHUYAN ; CAI HONGZHI ; WU WENMING</creator><creatorcontrib>WANG JUN ; ZHAO HUANRAN ; LI HAIYANG ; LI SHUYAN ; CAI HONGZHI ; WU WENMING</creatorcontrib><description>The invention discloses a process for preparing chromium oxide by recovering chromium-containing electroplating sludge, and belongs to the technical field of chromium-containing electroplating sludge treatment.The process comprises the following steps that sodium carbonate is added into dry sludge, then roasting is conducted, clinker is obtained, deionized water is added into the clinker for water leaching treatment, and leachate is obtained after filtering; sulfuric acid is added into the leachate to adjust the pH value, then sodium metaaluminate is added, and purified liquid is obtained after evaporation and concentration; adding deionized water into the purified liquid, and then crystallizing at room temperature for 6-8 hours to obtain sodium dichromate; the method comprises the following steps: grinding sodium dichromate, adding carbon black into the ground sodium dichromate, heating to 500-550 DEG C, preserving heat for 2.5-3.0 hours, and grinding, washing and filtering a product to obtain chromic oxide.</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; INORGANIC CHEMISTRY ; METALLURGY</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240315&amp;DB=EPODOC&amp;CC=CN&amp;NR=117699855A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25566,76549</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240315&amp;DB=EPODOC&amp;CC=CN&amp;NR=117699855A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG JUN</creatorcontrib><creatorcontrib>ZHAO HUANRAN</creatorcontrib><creatorcontrib>LI HAIYANG</creatorcontrib><creatorcontrib>LI SHUYAN</creatorcontrib><creatorcontrib>CAI HONGZHI</creatorcontrib><creatorcontrib>WU WENMING</creatorcontrib><title>Process for preparing chromium oxide by recovering chromium-containing electroplating sludge</title><description>The invention discloses a process for preparing chromium oxide by recovering chromium-containing electroplating sludge, and belongs to the technical field of chromium-containing electroplating sludge treatment.The process comprises the following steps that sodium carbonate is added into dry sludge, then roasting is conducted, clinker is obtained, deionized water is added into the clinker for water leaching treatment, and leachate is obtained after filtering; sulfuric acid is added into the leachate to adjust the pH value, then sodium metaaluminate is added, and purified liquid is obtained after evaporation and concentration; adding deionized water into the purified liquid, and then crystallizing at room temperature for 6-8 hours to obtain sodium dichromate; the method comprises the following steps: grinding sodium dichromate, adding carbon black into the ground sodium dichromate, heating to 500-550 DEG C, preserving heat for 2.5-3.0 hours, and grinding, washing and filtering a product to obtain chromic oxide.</description><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZIgJKMpPTi0uVkjLL1IoKEotSCzKzEtXSM4oys_NLM1VyK_ITElVSKpUKEpNzi9LRZHUTc7PK0nMzAOJpeakJpcU5RfkJJaAuMU5pSnpqTwMrGmJOcWpvFCam0HRzTXE2UM3tSA_PrW4IDE5NS-1JN7Zz9DQ3MzS0sLU1NGYGDUAQ5c9Hw</recordid><startdate>20240315</startdate><enddate>20240315</enddate><creator>WANG JUN</creator><creator>ZHAO HUANRAN</creator><creator>LI HAIYANG</creator><creator>LI SHUYAN</creator><creator>CAI HONGZHI</creator><creator>WU WENMING</creator><scope>EVB</scope></search><sort><creationdate>20240315</creationdate><title>Process for preparing chromium oxide by recovering chromium-containing electroplating sludge</title><author>WANG JUN ; ZHAO HUANRAN ; LI HAIYANG ; LI SHUYAN ; CAI HONGZHI ; WU WENMING</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117699855A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG JUN</creatorcontrib><creatorcontrib>ZHAO HUANRAN</creatorcontrib><creatorcontrib>LI HAIYANG</creatorcontrib><creatorcontrib>LI SHUYAN</creatorcontrib><creatorcontrib>CAI HONGZHI</creatorcontrib><creatorcontrib>WU WENMING</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG JUN</au><au>ZHAO HUANRAN</au><au>LI HAIYANG</au><au>LI SHUYAN</au><au>CAI HONGZHI</au><au>WU WENMING</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Process for preparing chromium oxide by recovering chromium-containing electroplating sludge</title><date>2024-03-15</date><risdate>2024</risdate><abstract>The invention discloses a process for preparing chromium oxide by recovering chromium-containing electroplating sludge, and belongs to the technical field of chromium-containing electroplating sludge treatment.The process comprises the following steps that sodium carbonate is added into dry sludge, then roasting is conducted, clinker is obtained, deionized water is added into the clinker for water leaching treatment, and leachate is obtained after filtering; sulfuric acid is added into the leachate to adjust the pH value, then sodium metaaluminate is added, and purified liquid is obtained after evaporation and concentration; adding deionized water into the purified liquid, and then crystallizing at room temperature for 6-8 hours to obtain sodium dichromate; the method comprises the following steps: grinding sodium dichromate, adding carbon black into the ground sodium dichromate, heating to 500-550 DEG C, preserving heat for 2.5-3.0 hours, and grinding, washing and filtering a product to obtain chromic oxide.</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117699855A
source esp@cenet
subjects CHEMISTRY
COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F
INORGANIC CHEMISTRY
METALLURGY
title Process for preparing chromium oxide by recovering chromium-containing electroplating sludge
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-17T17%3A58%3A24IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20JUN&rft.date=2024-03-15&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117699855A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true