Method for recovering iron through microwave roasting of copper tailings

The invention belongs to the technical field of extraction of valuable metals from non-ferrous metal tailings, and particularly relates to a method for recycling iron from copper tailings through microwave roasting. The method comprises the specific steps that copper tailings and a calcium material...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU FEI, WANG DAZHI, LIU YUANDONG, HE ZHICHENG, JIANG LEI, WU XIAOLI, WANG JINGHUI, LUO ANNENG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LIU FEI
WANG DAZHI
LIU YUANDONG
HE ZHICHENG
JIANG LEI
WU XIAOLI
WANG JINGHUI
LUO ANNENG
description The invention belongs to the technical field of extraction of valuable metals from non-ferrous metal tailings, and particularly relates to a method for recycling iron from copper tailings through microwave roasting. The method comprises the specific steps that copper tailings and a calcium material are mixed to be uniform, microwave roasting is adopted, oxygen is introduced, roasting is conducted at the temperature of 800-1000 DEG C, roasting slag is crushed and ground and then mixed with an acid solution for iron leaching, the iron leaching rate is not lower than 92%, and an iron chemical product is obtained after leaching liquid is subjected to concentration-cooling crystallization and recrystallization impurity removal. The method has the beneficial effects that the fayalite phase in the copper tailings can be effectively converted and decomposed at the temperature lower than 1000 DEG C, the energy consumption is low, the wet leaching iron leaching rate is high, the technological process is short, operatio
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117625948A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117625948A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117625948A3</originalsourceid><addsrcrecordid>eNrjZPDwTS3JyE9RSMsvUihKTc4vSy3KzEtXyCzKz1MoySjKL03PUMjNTC7KL08sS1Uoyk8sLgHJ56cpJOcXFKQWKZQkZuYARYp5GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8s5-hobmZkamliYWjMTFqAOOYNOc</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for recovering iron through microwave roasting of copper tailings</title><source>esp@cenet</source><creator>LIU FEI ; WANG DAZHI ; LIU YUANDONG ; HE ZHICHENG ; JIANG LEI ; WU XIAOLI ; WANG JINGHUI ; LUO ANNENG</creator><creatorcontrib>LIU FEI ; WANG DAZHI ; LIU YUANDONG ; HE ZHICHENG ; JIANG LEI ; WU XIAOLI ; WANG JINGHUI ; LUO ANNENG</creatorcontrib><description>The invention belongs to the technical field of extraction of valuable metals from non-ferrous metal tailings, and particularly relates to a method for recycling iron from copper tailings through microwave roasting. The method comprises the specific steps that copper tailings and a calcium material are mixed to be uniform, microwave roasting is adopted, oxygen is introduced, roasting is conducted at the temperature of 800-1000 DEG C, roasting slag is crushed and ground and then mixed with an acid solution for iron leaching, the iron leaching rate is not lower than 92%, and an iron chemical product is obtained after leaching liquid is subjected to concentration-cooling crystallization and recrystallization impurity removal. The method has the beneficial effects that the fayalite phase in the copper tailings can be effectively converted and decomposed at the temperature lower than 1000 DEG C, the energy consumption is low, the wet leaching iron leaching rate is high, the technological process is short, operatio</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; FERROUS OR NON-FERROUS ALLOYS ; LIME, MAGNESIA ; MANUFACTURE OF IRON OR STEEL ; METALLURGY ; METALLURGY OF IRON ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; REFRACTORIES ; SLAG ; TREATMENT OF ALLOYS OR NON-FERROUS METALS ; TREATMENT OF NATURAL STONE</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240301&amp;DB=EPODOC&amp;CC=CN&amp;NR=117625948A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240301&amp;DB=EPODOC&amp;CC=CN&amp;NR=117625948A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIU FEI</creatorcontrib><creatorcontrib>WANG DAZHI</creatorcontrib><creatorcontrib>LIU YUANDONG</creatorcontrib><creatorcontrib>HE ZHICHENG</creatorcontrib><creatorcontrib>JIANG LEI</creatorcontrib><creatorcontrib>WU XIAOLI</creatorcontrib><creatorcontrib>WANG JINGHUI</creatorcontrib><creatorcontrib>LUO ANNENG</creatorcontrib><title>Method for recovering iron through microwave roasting of copper tailings</title><description>The invention belongs to the technical field of extraction of valuable metals from non-ferrous metal tailings, and particularly relates to a method for recycling iron from copper tailings through microwave roasting. The method comprises the specific steps that copper tailings and a calcium material are mixed to be uniform, microwave roasting is adopted, oxygen is introduced, roasting is conducted at the temperature of 800-1000 DEG C, roasting slag is crushed and ground and then mixed with an acid solution for iron leaching, the iron leaching rate is not lower than 92%, and an iron chemical product is obtained after leaching liquid is subjected to concentration-cooling crystallization and recrystallization impurity removal. The method has the beneficial effects that the fayalite phase in the copper tailings can be effectively converted and decomposed at the temperature lower than 1000 DEG C, the energy consumption is low, the wet leaching iron leaching rate is high, the technological process is short, operatio</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>LIME, MAGNESIA</subject><subject>MANUFACTURE OF IRON OR STEEL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZPDwTS3JyE9RSMsvUihKTc4vSy3KzEtXyCzKz1MoySjKL03PUMjNTC7KL08sS1Uoyk8sLgHJ56cpJOcXFKQWKZQkZuYARYp5GFjTEnOKU3mhNDeDoptriLOHbmpBfnxqcUFicmpeakm8s5-hobmZkamliYWjMTFqAOOYNOc</recordid><startdate>20240301</startdate><enddate>20240301</enddate><creator>LIU FEI</creator><creator>WANG DAZHI</creator><creator>LIU YUANDONG</creator><creator>HE ZHICHENG</creator><creator>JIANG LEI</creator><creator>WU XIAOLI</creator><creator>WANG JINGHUI</creator><creator>LUO ANNENG</creator><scope>EVB</scope></search><sort><creationdate>20240301</creationdate><title>Method for recovering iron through microwave roasting of copper tailings</title><author>LIU FEI ; WANG DAZHI ; LIU YUANDONG ; HE ZHICHENG ; JIANG LEI ; WU XIAOLI ; WANG JINGHUI ; LUO ANNENG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117625948A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>LIME, MAGNESIA</topic><topic>MANUFACTURE OF IRON OR STEEL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>LIU FEI</creatorcontrib><creatorcontrib>WANG DAZHI</creatorcontrib><creatorcontrib>LIU YUANDONG</creatorcontrib><creatorcontrib>HE ZHICHENG</creatorcontrib><creatorcontrib>JIANG LEI</creatorcontrib><creatorcontrib>WU XIAOLI</creatorcontrib><creatorcontrib>WANG JINGHUI</creatorcontrib><creatorcontrib>LUO ANNENG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIU FEI</au><au>WANG DAZHI</au><au>LIU YUANDONG</au><au>HE ZHICHENG</au><au>JIANG LEI</au><au>WU XIAOLI</au><au>WANG JINGHUI</au><au>LUO ANNENG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for recovering iron through microwave roasting of copper tailings</title><date>2024-03-01</date><risdate>2024</risdate><abstract>The invention belongs to the technical field of extraction of valuable metals from non-ferrous metal tailings, and particularly relates to a method for recycling iron from copper tailings through microwave roasting. The method comprises the specific steps that copper tailings and a calcium material are mixed to be uniform, microwave roasting is adopted, oxygen is introduced, roasting is conducted at the temperature of 800-1000 DEG C, roasting slag is crushed and ground and then mixed with an acid solution for iron leaching, the iron leaching rate is not lower than 92%, and an iron chemical product is obtained after leaching liquid is subjected to concentration-cooling crystallization and recrystallization impurity removal. The method has the beneficial effects that the fayalite phase in the copper tailings can be effectively converted and decomposed at the temperature lower than 1000 DEG C, the energy consumption is low, the wet leaching iron leaching rate is high, the technological process is short, operatio</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117625948A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
FERROUS OR NON-FERROUS ALLOYS
LIME, MAGNESIA
MANUFACTURE OF IRON OR STEEL
METALLURGY
METALLURGY OF IRON
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
REFRACTORIES
SLAG
TREATMENT OF ALLOYS OR NON-FERROUS METALS
TREATMENT OF NATURAL STONE
title Method for recovering iron through microwave roasting of copper tailings
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-06T23%3A57%3A17IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIU%20FEI&rft.date=2024-03-01&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117625948A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true