Preparation method of low-carbon spheroidized marine silicate and cement prepared from low-carbon spheroidized marine silicate

The invention provides a preparation method of low-carbon spheroidized maritime work silicate and cement prepared from the low-carbon spheroidized maritime work silicate. The low-carbon spheroidized maritime work silicate cement has the particle size and interval accumulative distribution as follows...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LUO MINGYANG, WU YUXIANG, WU HONG'AN, LIU ANQI, MA HAIJUN, MA ZHAOMU, SUN ZHISHENG, WANG XINGQIN, ZHU WENSHANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LUO MINGYANG
WU YUXIANG
WU HONG'AN
LIU ANQI
MA HAIJUN
MA ZHAOMU
SUN ZHISHENG
WANG XINGQIN
ZHU WENSHANG
description The invention provides a preparation method of low-carbon spheroidized maritime work silicate and cement prepared from the low-carbon spheroidized maritime work silicate. The low-carbon spheroidized maritime work silicate cement has the particle size and interval accumulative distribution as follows: 13%-23% of a part with the particle size smaller than 3 microns, 50%-70% of a part with the particle size smaller than 32 microns and 8%-18% of residues on a square hole sieve with the particle size smaller than 45 microns. The invention also provides a preparation method of the low-carbon spheroidized maritime work Portland cement. The mixed material is directly fed into a novel dry-process energy-saving vertical grinder for grinding and shaping. The particle size distribution of the low-carbon spheroidized cement is optimized, the circularity is improved, the length-diameter ratio is reduced, the distribution interval of the length-diameter ratio and the circularity of particles is small, the particle size dist
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117623650A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117623650A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117623650A3</originalsourceid><addsrcrecordid>eNqNjEEKwjAUBbtxIeodvgcoWIt1LUVxJS7cl2_yQgNJfkgCggvPbhEP0NXAMMyy-twTIicuVgJ5lFE0iSEnr1pxek4yxxFJrLZvaPKcbABl66ziAuKgScEjFIq_0dSYJH7uYF0tDLuMzZ-rans5P_prjSgDcmSFgDL0t6Y5dvu2O-xO7ZzmCwZ2SUQ</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of low-carbon spheroidized marine silicate and cement prepared from low-carbon spheroidized marine silicate</title><source>esp@cenet</source><creator>LUO MINGYANG ; WU YUXIANG ; WU HONG'AN ; LIU ANQI ; MA HAIJUN ; MA ZHAOMU ; SUN ZHISHENG ; WANG XINGQIN ; ZHU WENSHANG</creator><creatorcontrib>LUO MINGYANG ; WU YUXIANG ; WU HONG'AN ; LIU ANQI ; MA HAIJUN ; MA ZHAOMU ; SUN ZHISHENG ; WANG XINGQIN ; ZHU WENSHANG</creatorcontrib><description>The invention provides a preparation method of low-carbon spheroidized maritime work silicate and cement prepared from the low-carbon spheroidized maritime work silicate. The low-carbon spheroidized maritime work silicate cement has the particle size and interval accumulative distribution as follows: 13%-23% of a part with the particle size smaller than 3 microns, 50%-70% of a part with the particle size smaller than 32 microns and 8%-18% of residues on a square hole sieve with the particle size smaller than 45 microns. The invention also provides a preparation method of the low-carbon spheroidized maritime work Portland cement. The mixed material is directly fed into a novel dry-process energy-saving vertical grinder for grinding and shaping. The particle size distribution of the low-carbon spheroidized cement is optimized, the circularity is improved, the length-diameter ratio is reduced, the distribution interval of the length-diameter ratio and the circularity of particles is small, the particle size dist</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240301&amp;DB=EPODOC&amp;CC=CN&amp;NR=117623650A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76419</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240301&amp;DB=EPODOC&amp;CC=CN&amp;NR=117623650A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LUO MINGYANG</creatorcontrib><creatorcontrib>WU YUXIANG</creatorcontrib><creatorcontrib>WU HONG'AN</creatorcontrib><creatorcontrib>LIU ANQI</creatorcontrib><creatorcontrib>MA HAIJUN</creatorcontrib><creatorcontrib>MA ZHAOMU</creatorcontrib><creatorcontrib>SUN ZHISHENG</creatorcontrib><creatorcontrib>WANG XINGQIN</creatorcontrib><creatorcontrib>ZHU WENSHANG</creatorcontrib><title>Preparation method of low-carbon spheroidized marine silicate and cement prepared from low-carbon spheroidized marine silicate</title><description>The invention provides a preparation method of low-carbon spheroidized maritime work silicate and cement prepared from the low-carbon spheroidized maritime work silicate. The low-carbon spheroidized maritime work silicate cement has the particle size and interval accumulative distribution as follows: 13%-23% of a part with the particle size smaller than 3 microns, 50%-70% of a part with the particle size smaller than 32 microns and 8%-18% of residues on a square hole sieve with the particle size smaller than 45 microns. The invention also provides a preparation method of the low-carbon spheroidized maritime work Portland cement. The mixed material is directly fed into a novel dry-process energy-saving vertical grinder for grinding and shaping. The particle size distribution of the low-carbon spheroidized cement is optimized, the circularity is improved, the length-diameter ratio is reduced, the distribution interval of the length-diameter ratio and the circularity of particles is small, the particle size dist</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjEEKwjAUBbtxIeodvgcoWIt1LUVxJS7cl2_yQgNJfkgCggvPbhEP0NXAMMyy-twTIicuVgJ5lFE0iSEnr1pxek4yxxFJrLZvaPKcbABl66ziAuKgScEjFIq_0dSYJH7uYF0tDLuMzZ-rans5P_prjSgDcmSFgDL0t6Y5dvu2O-xO7ZzmCwZ2SUQ</recordid><startdate>20240301</startdate><enddate>20240301</enddate><creator>LUO MINGYANG</creator><creator>WU YUXIANG</creator><creator>WU HONG'AN</creator><creator>LIU ANQI</creator><creator>MA HAIJUN</creator><creator>MA ZHAOMU</creator><creator>SUN ZHISHENG</creator><creator>WANG XINGQIN</creator><creator>ZHU WENSHANG</creator><scope>EVB</scope></search><sort><creationdate>20240301</creationdate><title>Preparation method of low-carbon spheroidized marine silicate and cement prepared from low-carbon spheroidized marine silicate</title><author>LUO MINGYANG ; WU YUXIANG ; WU HONG'AN ; LIU ANQI ; MA HAIJUN ; MA ZHAOMU ; SUN ZHISHENG ; WANG XINGQIN ; ZHU WENSHANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117623650A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>LUO MINGYANG</creatorcontrib><creatorcontrib>WU YUXIANG</creatorcontrib><creatorcontrib>WU HONG'AN</creatorcontrib><creatorcontrib>LIU ANQI</creatorcontrib><creatorcontrib>MA HAIJUN</creatorcontrib><creatorcontrib>MA ZHAOMU</creatorcontrib><creatorcontrib>SUN ZHISHENG</creatorcontrib><creatorcontrib>WANG XINGQIN</creatorcontrib><creatorcontrib>ZHU WENSHANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LUO MINGYANG</au><au>WU YUXIANG</au><au>WU HONG'AN</au><au>LIU ANQI</au><au>MA HAIJUN</au><au>MA ZHAOMU</au><au>SUN ZHISHENG</au><au>WANG XINGQIN</au><au>ZHU WENSHANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of low-carbon spheroidized marine silicate and cement prepared from low-carbon spheroidized marine silicate</title><date>2024-03-01</date><risdate>2024</risdate><abstract>The invention provides a preparation method of low-carbon spheroidized maritime work silicate and cement prepared from the low-carbon spheroidized maritime work silicate. The low-carbon spheroidized maritime work silicate cement has the particle size and interval accumulative distribution as follows: 13%-23% of a part with the particle size smaller than 3 microns, 50%-70% of a part with the particle size smaller than 32 microns and 8%-18% of residues on a square hole sieve with the particle size smaller than 45 microns. The invention also provides a preparation method of the low-carbon spheroidized maritime work Portland cement. The mixed material is directly fed into a novel dry-process energy-saving vertical grinder for grinding and shaping. The particle size distribution of the low-carbon spheroidized cement is optimized, the circularity is improved, the length-diameter ratio is reduced, the distribution interval of the length-diameter ratio and the circularity of particles is small, the particle size dist</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117623650A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Preparation method of low-carbon spheroidized marine silicate and cement prepared from low-carbon spheroidized marine silicate
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T01%3A00%3A54IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LUO%20MINGYANG&rft.date=2024-03-01&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117623650A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true