Method for reducing rotten steel generated in rolling process of deformed steel bar

The invention discloses a method for reducing rotten steel generated in the rolling process of deformed steel bars. A method for reducing rotten steel generated in the rolling process of deformed steel bars comprises the refining procedure, specifically, a temperature drop detection device is arrang...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DENG ZHIXUN, HOU ZEWANG, JIN RENCHUN, XU HAO, DENG BIRONG, GUO HUANGXUN, SHU CHUNYANG, LUO GANG, XU GUANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator DENG ZHIXUN
HOU ZEWANG
JIN RENCHUN
XU HAO
DENG BIRONG
GUO HUANGXUN
SHU CHUNYANG
LUO GANG
XU GUANG
description The invention discloses a method for reducing rotten steel generated in the rolling process of deformed steel bars. A method for reducing rotten steel generated in the rolling process of deformed steel bars comprises the refining procedure, specifically, a temperature drop detection device is arranged to detect the temperature drop of molten steel in a refining furnace, if the temperature drop is lower than or higher than 0.5-1.5 DEG C/min, the molten steel is heated through an automatic control system, and if the temperature drop is within 0.5-1.5 DEG C/min, the molten steel is cooled to the room temperature; if yes, the molten steel leaves the station and enters a continuous casting procedure through an automatic control system; and in the continuous casting procedure, after the molten steel is solidified and crystallized through a crystallizer, a square billet is obtained, when the pulling speed of the crystallizer is adjusted, the single-time adjustment pulling speed is controlled to be smaller than 0.3 m
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117583393A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117583393A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117583393A3</originalsourceid><addsrcrecordid>eNqNjDEOwjAQBN1QIOAPxwMoIgsBJYpANNBAHxl7EyIZn3U-_o8RPIBqi5nZqbmeoQ8O1LOQILz8mAYSVkWiokCkAQniFIHGVEmMHyMLe5RC3FNAbZ8Vf_W7k7mZ9C4WLH47M8vj4daeVsjcoWTn66V27aVpNuuttTu7t_84b1PGOGU</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for reducing rotten steel generated in rolling process of deformed steel bar</title><source>esp@cenet</source><creator>DENG ZHIXUN ; HOU ZEWANG ; JIN RENCHUN ; XU HAO ; DENG BIRONG ; GUO HUANGXUN ; SHU CHUNYANG ; LUO GANG ; XU GUANG</creator><creatorcontrib>DENG ZHIXUN ; HOU ZEWANG ; JIN RENCHUN ; XU HAO ; DENG BIRONG ; GUO HUANGXUN ; SHU CHUNYANG ; LUO GANG ; XU GUANG</creatorcontrib><description>The invention discloses a method for reducing rotten steel generated in the rolling process of deformed steel bars. A method for reducing rotten steel generated in the rolling process of deformed steel bars comprises the refining procedure, specifically, a temperature drop detection device is arranged to detect the temperature drop of molten steel in a refining furnace, if the temperature drop is lower than or higher than 0.5-1.5 DEG C/min, the molten steel is heated through an automatic control system, and if the temperature drop is within 0.5-1.5 DEG C/min, the molten steel is cooled to the room temperature; if yes, the molten steel leaves the station and enters a continuous casting procedure through an automatic control system; and in the continuous casting procedure, after the molten steel is solidified and crystallized through a crystallizer, a square billet is obtained, when the pulling speed of the crystallizer is adjusted, the single-time adjustment pulling speed is controlled to be smaller than 0.3 m</description><language>chi ; eng</language><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; PERFORMING OPERATIONS ; PUNCHING METAL ; ROLLING OF METAL ; TRANSPORTING</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240223&amp;DB=EPODOC&amp;CC=CN&amp;NR=117583393A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25544,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240223&amp;DB=EPODOC&amp;CC=CN&amp;NR=117583393A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DENG ZHIXUN</creatorcontrib><creatorcontrib>HOU ZEWANG</creatorcontrib><creatorcontrib>JIN RENCHUN</creatorcontrib><creatorcontrib>XU HAO</creatorcontrib><creatorcontrib>DENG BIRONG</creatorcontrib><creatorcontrib>GUO HUANGXUN</creatorcontrib><creatorcontrib>SHU CHUNYANG</creatorcontrib><creatorcontrib>LUO GANG</creatorcontrib><creatorcontrib>XU GUANG</creatorcontrib><title>Method for reducing rotten steel generated in rolling process of deformed steel bar</title><description>The invention discloses a method for reducing rotten steel generated in the rolling process of deformed steel bars. A method for reducing rotten steel generated in the rolling process of deformed steel bars comprises the refining procedure, specifically, a temperature drop detection device is arranged to detect the temperature drop of molten steel in a refining furnace, if the temperature drop is lower than or higher than 0.5-1.5 DEG C/min, the molten steel is heated through an automatic control system, and if the temperature drop is within 0.5-1.5 DEG C/min, the molten steel is cooled to the room temperature; if yes, the molten steel leaves the station and enters a continuous casting procedure through an automatic control system; and in the continuous casting procedure, after the molten steel is solidified and crystallized through a crystallizer, a square billet is obtained, when the pulling speed of the crystallizer is adjusted, the single-time adjustment pulling speed is controlled to be smaller than 0.3 m</description><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>ROLLING OF METAL</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjDEOwjAQBN1QIOAPxwMoIgsBJYpANNBAHxl7EyIZn3U-_o8RPIBqi5nZqbmeoQ8O1LOQILz8mAYSVkWiokCkAQniFIHGVEmMHyMLe5RC3FNAbZ8Vf_W7k7mZ9C4WLH47M8vj4daeVsjcoWTn66V27aVpNuuttTu7t_84b1PGOGU</recordid><startdate>20240223</startdate><enddate>20240223</enddate><creator>DENG ZHIXUN</creator><creator>HOU ZEWANG</creator><creator>JIN RENCHUN</creator><creator>XU HAO</creator><creator>DENG BIRONG</creator><creator>GUO HUANGXUN</creator><creator>SHU CHUNYANG</creator><creator>LUO GANG</creator><creator>XU GUANG</creator><scope>EVB</scope></search><sort><creationdate>20240223</creationdate><title>Method for reducing rotten steel generated in rolling process of deformed steel bar</title><author>DENG ZHIXUN ; HOU ZEWANG ; JIN RENCHUN ; XU HAO ; DENG BIRONG ; GUO HUANGXUN ; SHU CHUNYANG ; LUO GANG ; XU GUANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117583393A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>ROLLING OF METAL</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>DENG ZHIXUN</creatorcontrib><creatorcontrib>HOU ZEWANG</creatorcontrib><creatorcontrib>JIN RENCHUN</creatorcontrib><creatorcontrib>XU HAO</creatorcontrib><creatorcontrib>DENG BIRONG</creatorcontrib><creatorcontrib>GUO HUANGXUN</creatorcontrib><creatorcontrib>SHU CHUNYANG</creatorcontrib><creatorcontrib>LUO GANG</creatorcontrib><creatorcontrib>XU GUANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DENG ZHIXUN</au><au>HOU ZEWANG</au><au>JIN RENCHUN</au><au>XU HAO</au><au>DENG BIRONG</au><au>GUO HUANGXUN</au><au>SHU CHUNYANG</au><au>LUO GANG</au><au>XU GUANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for reducing rotten steel generated in rolling process of deformed steel bar</title><date>2024-02-23</date><risdate>2024</risdate><abstract>The invention discloses a method for reducing rotten steel generated in the rolling process of deformed steel bars. A method for reducing rotten steel generated in the rolling process of deformed steel bars comprises the refining procedure, specifically, a temperature drop detection device is arranged to detect the temperature drop of molten steel in a refining furnace, if the temperature drop is lower than or higher than 0.5-1.5 DEG C/min, the molten steel is heated through an automatic control system, and if the temperature drop is within 0.5-1.5 DEG C/min, the molten steel is cooled to the room temperature; if yes, the molten steel leaves the station and enters a continuous casting procedure through an automatic control system; and in the continuous casting procedure, after the molten steel is solidified and crystallized through a crystallizer, a square billet is obtained, when the pulling speed of the crystallizer is adjusted, the single-time adjustment pulling speed is controlled to be smaller than 0.3 m</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117583393A
source esp@cenet
subjects MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
PERFORMING OPERATIONS
PUNCHING METAL
ROLLING OF METAL
TRANSPORTING
title Method for reducing rotten steel generated in rolling process of deformed steel bar
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-27T17%3A43%3A01IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DENG%20ZHIXUN&rft.date=2024-02-23&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117583393A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true