Preparation method of TA15 titanium alloy cold-rolled pipe
The invention discloses a preparation method of a TA15 titanium alloy cold-rolled pipe. The method comprises the following steps: 1, processing a TA15 titanium alloy cast ingot into a bar billet; 2, drilling and boring the bar blank to obtain a hollow bar blank; thirdly, the hollow bar blank is slee...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | HOU ZHIMIN WU XIAODONG SU SONGLIN LI XUSHENG YANG PEI NAN LI LIN JIPIN ZHANG ZHI WANG SHA ZHANG YI REN WEINING LUO DENGCHAO ZHANG NA MA WEI LI GANG |
description | The invention discloses a preparation method of a TA15 titanium alloy cold-rolled pipe. The method comprises the following steps: 1, processing a TA15 titanium alloy cast ingot into a bar billet; 2, drilling and boring the bar blank to obtain a hollow bar blank; thirdly, the hollow bar blank is sleeved, heated, extruded, straightened and subjected to acid pickling, and an extruded pipe blank is obtained; fourthly, the extruded pipe blank is subjected to multi-pass rolling, and a rolled pipe is obtained; and 5, peeling and boring the rolled pipe to obtain the TA15 titanium alloy cold-rolled pipe. By means of equipment selection, blank preparation, rolling procedure design and parameter control, the TA15 titanium alloy pipe is successfully prepared through the cold rolling process, the quality of the TA15 titanium alloy cold-rolled pipe is guaranteed, the yield is increased, the production cost is reduced, and the preparation process is simple, easy to implement, suitable for industrial production and suitable |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117564728A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117564728A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117564728A3</originalsourceid><addsrcrecordid>eNrjZLAKKEotSCxKLMnMz1PITS3JyE9RyE9TCHE0NFUoySxJzMsszVVIzMnJr1RIzs9J0S3Kz8lJTVEoyCxI5WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hobmpmYm5kYWjsbEqAEALdEudA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of TA15 titanium alloy cold-rolled pipe</title><source>esp@cenet</source><creator>HOU ZHIMIN ; WU XIAODONG ; SU SONGLIN ; LI XUSHENG ; YANG PEI ; NAN LI ; LIN JIPIN ; ZHANG ZHI ; WANG SHA ; ZHANG YI ; REN WEINING ; LUO DENGCHAO ; ZHANG NA ; MA WEI ; LI GANG</creator><creatorcontrib>HOU ZHIMIN ; WU XIAODONG ; SU SONGLIN ; LI XUSHENG ; YANG PEI ; NAN LI ; LIN JIPIN ; ZHANG ZHI ; WANG SHA ; ZHANG YI ; REN WEINING ; LUO DENGCHAO ; ZHANG NA ; MA WEI ; LI GANG</creatorcontrib><description>The invention discloses a preparation method of a TA15 titanium alloy cold-rolled pipe. The method comprises the following steps: 1, processing a TA15 titanium alloy cast ingot into a bar billet; 2, drilling and boring the bar blank to obtain a hollow bar blank; thirdly, the hollow bar blank is sleeved, heated, extruded, straightened and subjected to acid pickling, and an extruded pipe blank is obtained; fourthly, the extruded pipe blank is subjected to multi-pass rolling, and a rolled pipe is obtained; and 5, peeling and boring the rolled pipe to obtain the TA15 titanium alloy cold-rolled pipe. By means of equipment selection, blank preparation, rolling procedure design and parameter control, the TA15 titanium alloy pipe is successfully prepared through the cold rolling process, the quality of the TA15 titanium alloy cold-rolled pipe is guaranteed, the yield is increased, the production cost is reduced, and the preparation process is simple, easy to implement, suitable for industrial production and suitable</description><language>chi ; eng</language><subject>COMBINED OPERATIONS ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; OTHER WORKING OF METAL ; PERFORMING OPERATIONS ; TRANSPORTING ; UNIVERSAL MACHINE TOOLS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240220&DB=EPODOC&CC=CN&NR=117564728A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240220&DB=EPODOC&CC=CN&NR=117564728A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HOU ZHIMIN</creatorcontrib><creatorcontrib>WU XIAODONG</creatorcontrib><creatorcontrib>SU SONGLIN</creatorcontrib><creatorcontrib>LI XUSHENG</creatorcontrib><creatorcontrib>YANG PEI</creatorcontrib><creatorcontrib>NAN LI</creatorcontrib><creatorcontrib>LIN JIPIN</creatorcontrib><creatorcontrib>ZHANG ZHI</creatorcontrib><creatorcontrib>WANG SHA</creatorcontrib><creatorcontrib>ZHANG YI</creatorcontrib><creatorcontrib>REN WEINING</creatorcontrib><creatorcontrib>LUO DENGCHAO</creatorcontrib><creatorcontrib>ZHANG NA</creatorcontrib><creatorcontrib>MA WEI</creatorcontrib><creatorcontrib>LI GANG</creatorcontrib><title>Preparation method of TA15 titanium alloy cold-rolled pipe</title><description>The invention discloses a preparation method of a TA15 titanium alloy cold-rolled pipe. The method comprises the following steps: 1, processing a TA15 titanium alloy cast ingot into a bar billet; 2, drilling and boring the bar blank to obtain a hollow bar blank; thirdly, the hollow bar blank is sleeved, heated, extruded, straightened and subjected to acid pickling, and an extruded pipe blank is obtained; fourthly, the extruded pipe blank is subjected to multi-pass rolling, and a rolled pipe is obtained; and 5, peeling and boring the rolled pipe to obtain the TA15 titanium alloy cold-rolled pipe. By means of equipment selection, blank preparation, rolling procedure design and parameter control, the TA15 titanium alloy pipe is successfully prepared through the cold rolling process, the quality of the TA15 titanium alloy cold-rolled pipe is guaranteed, the yield is increased, the production cost is reduced, and the preparation process is simple, easy to implement, suitable for industrial production and suitable</description><subject>COMBINED OPERATIONS</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>OTHER WORKING OF METAL</subject><subject>PERFORMING OPERATIONS</subject><subject>TRANSPORTING</subject><subject>UNIVERSAL MACHINE TOOLS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAKKEotSCxKLMnMz1PITS3JyE9RyE9TCHE0NFUoySxJzMsszVVIzMnJr1RIzs9J0S3Kz8lJTVEoyCxI5WFgTUvMKU7lhdLcDIpuriHOHrqpBfnxqcUFicmpeakl8c5-hobmpmYm5kYWjsbEqAEALdEudA</recordid><startdate>20240220</startdate><enddate>20240220</enddate><creator>HOU ZHIMIN</creator><creator>WU XIAODONG</creator><creator>SU SONGLIN</creator><creator>LI XUSHENG</creator><creator>YANG PEI</creator><creator>NAN LI</creator><creator>LIN JIPIN</creator><creator>ZHANG ZHI</creator><creator>WANG SHA</creator><creator>ZHANG YI</creator><creator>REN WEINING</creator><creator>LUO DENGCHAO</creator><creator>ZHANG NA</creator><creator>MA WEI</creator><creator>LI GANG</creator><scope>EVB</scope></search><sort><creationdate>20240220</creationdate><title>Preparation method of TA15 titanium alloy cold-rolled pipe</title><author>HOU ZHIMIN ; WU XIAODONG ; SU SONGLIN ; LI XUSHENG ; YANG PEI ; NAN LI ; LIN JIPIN ; ZHANG ZHI ; WANG SHA ; ZHANG YI ; REN WEINING ; LUO DENGCHAO ; ZHANG NA ; MA WEI ; LI GANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117564728A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>COMBINED OPERATIONS</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>OTHER WORKING OF METAL</topic><topic>PERFORMING OPERATIONS</topic><topic>TRANSPORTING</topic><topic>UNIVERSAL MACHINE TOOLS</topic><toplevel>online_resources</toplevel><creatorcontrib>HOU ZHIMIN</creatorcontrib><creatorcontrib>WU XIAODONG</creatorcontrib><creatorcontrib>SU SONGLIN</creatorcontrib><creatorcontrib>LI XUSHENG</creatorcontrib><creatorcontrib>YANG PEI</creatorcontrib><creatorcontrib>NAN LI</creatorcontrib><creatorcontrib>LIN JIPIN</creatorcontrib><creatorcontrib>ZHANG ZHI</creatorcontrib><creatorcontrib>WANG SHA</creatorcontrib><creatorcontrib>ZHANG YI</creatorcontrib><creatorcontrib>REN WEINING</creatorcontrib><creatorcontrib>LUO DENGCHAO</creatorcontrib><creatorcontrib>ZHANG NA</creatorcontrib><creatorcontrib>MA WEI</creatorcontrib><creatorcontrib>LI GANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HOU ZHIMIN</au><au>WU XIAODONG</au><au>SU SONGLIN</au><au>LI XUSHENG</au><au>YANG PEI</au><au>NAN LI</au><au>LIN JIPIN</au><au>ZHANG ZHI</au><au>WANG SHA</au><au>ZHANG YI</au><au>REN WEINING</au><au>LUO DENGCHAO</au><au>ZHANG NA</au><au>MA WEI</au><au>LI GANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of TA15 titanium alloy cold-rolled pipe</title><date>2024-02-20</date><risdate>2024</risdate><abstract>The invention discloses a preparation method of a TA15 titanium alloy cold-rolled pipe. The method comprises the following steps: 1, processing a TA15 titanium alloy cast ingot into a bar billet; 2, drilling and boring the bar blank to obtain a hollow bar blank; thirdly, the hollow bar blank is sleeved, heated, extruded, straightened and subjected to acid pickling, and an extruded pipe blank is obtained; fourthly, the extruded pipe blank is subjected to multi-pass rolling, and a rolled pipe is obtained; and 5, peeling and boring the rolled pipe to obtain the TA15 titanium alloy cold-rolled pipe. By means of equipment selection, blank preparation, rolling procedure design and parameter control, the TA15 titanium alloy pipe is successfully prepared through the cold rolling process, the quality of the TA15 titanium alloy cold-rolled pipe is guaranteed, the yield is increased, the production cost is reduced, and the preparation process is simple, easy to implement, suitable for industrial production and suitable</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN117564728A |
source | esp@cenet |
subjects | COMBINED OPERATIONS MACHINE TOOLS METAL-WORKING NOT OTHERWISE PROVIDED FOR OTHER WORKING OF METAL PERFORMING OPERATIONS TRANSPORTING UNIVERSAL MACHINE TOOLS |
title | Preparation method of TA15 titanium alloy cold-rolled pipe |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-13T14%3A31%3A58IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HOU%20ZHIMIN&rft.date=2024-02-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117564728A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |