Weaving method of cotton-polylactic acid fiber composite fabric

The invention discloses a weaving method of a cotton-polylactic acid fiber composite fabric, which comprises the following steps: S1, warp yarns are warped into a ball warp beam with 300-600 yarns per beam at a speed of 250m/min by adopting ball warp, and the warp yarns are cotton fiber/polylactic a...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GU JIN, DENG JIANGUANG, CHEN GUICHUN, HUANG ZHUOHENG, QIN YUJUAN, QIU DIHENG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GU JIN
DENG JIANGUANG
CHEN GUICHUN
HUANG ZHUOHENG
QIN YUJUAN
QIU DIHENG
description The invention discloses a weaving method of a cotton-polylactic acid fiber composite fabric, which comprises the following steps: S1, warp yarns are warped into a ball warp beam with 300-600 yarns per beam at a speed of 250m/min by adopting ball warp, and the warp yarns are cotton fiber/polylactic acid covering yarns formed by wrapping the outside of polylactic acid fibers with cotton fibers; s2, adding a proper amount of deionized water into a finishing agent consisting of low-viscosity starch, indigo dye, amino-terminated dimethyl silicone oil, methyl isobutyl ketone, sodium hydroxide, isopropyl-ketone and glycerol to prepare a finishing solution with the concentration of 100-150g/L; and S3, adopting a size taking combined process, completing warp dyeing and sizing processes at 50-100m/min and twice dipping and twice rolling, drying with hot air at 105-120 DEG C, then re-beaming, and weaving with weft on a machine to obtain the polylactic acid fiber composite fabric. The fabric woven by the weaving method i
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117449014A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117449014A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117449014A3</originalsourceid><addsrcrecordid>eNrjZLAPT00sy8xLV8hNLcnIT1HIT1NIzi8pyc_TLcjPqcxJTC7JTFZITM5MUUjLTEotAkrmFuQXZ5akKqQlJhVlJvMwsKYl5hSn8kJpbgZFN9cQZw_d1IL8-NTigsTk1LzUknhnP0NDcxMTSwNDE0djYtQAAJfeMPY</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Weaving method of cotton-polylactic acid fiber composite fabric</title><source>esp@cenet</source><creator>GU JIN ; DENG JIANGUANG ; CHEN GUICHUN ; HUANG ZHUOHENG ; QIN YUJUAN ; QIU DIHENG</creator><creatorcontrib>GU JIN ; DENG JIANGUANG ; CHEN GUICHUN ; HUANG ZHUOHENG ; QIN YUJUAN ; QIU DIHENG</creatorcontrib><description>The invention discloses a weaving method of a cotton-polylactic acid fiber composite fabric, which comprises the following steps: S1, warp yarns are warped into a ball warp beam with 300-600 yarns per beam at a speed of 250m/min by adopting ball warp, and the warp yarns are cotton fiber/polylactic acid covering yarns formed by wrapping the outside of polylactic acid fibers with cotton fibers; s2, adding a proper amount of deionized water into a finishing agent consisting of low-viscosity starch, indigo dye, amino-terminated dimethyl silicone oil, methyl isobutyl ketone, sodium hydroxide, isopropyl-ketone and glycerol to prepare a finishing solution with the concentration of 100-150g/L; and S3, adopting a size taking combined process, completing warp dyeing and sizing processes at 50-100m/min and twice dipping and twice rolling, drying with hot air at 105-120 DEG C, then re-beaming, and weaving with weft on a machine to obtain the polylactic acid fiber composite fabric. The fabric woven by the weaving method i</description><language>chi ; eng</language><subject>DYEING LEATHER, FURS, OR SOLID MACROMOLECULAR SUBSTANCES INANY FORM ; DYEING OR PRINTING TEXTILES ; FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR ; LAUNDERING ; LOOMS ; METHODS OF WEAVING ; TEXTILES ; TREATMENT OF TEXTILES OR THE LIKE ; TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS ; WEAVING ; WOVEN FABRICS</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240126&amp;DB=EPODOC&amp;CC=CN&amp;NR=117449014A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76294</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240126&amp;DB=EPODOC&amp;CC=CN&amp;NR=117449014A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GU JIN</creatorcontrib><creatorcontrib>DENG JIANGUANG</creatorcontrib><creatorcontrib>CHEN GUICHUN</creatorcontrib><creatorcontrib>HUANG ZHUOHENG</creatorcontrib><creatorcontrib>QIN YUJUAN</creatorcontrib><creatorcontrib>QIU DIHENG</creatorcontrib><title>Weaving method of cotton-polylactic acid fiber composite fabric</title><description>The invention discloses a weaving method of a cotton-polylactic acid fiber composite fabric, which comprises the following steps: S1, warp yarns are warped into a ball warp beam with 300-600 yarns per beam at a speed of 250m/min by adopting ball warp, and the warp yarns are cotton fiber/polylactic acid covering yarns formed by wrapping the outside of polylactic acid fibers with cotton fibers; s2, adding a proper amount of deionized water into a finishing agent consisting of low-viscosity starch, indigo dye, amino-terminated dimethyl silicone oil, methyl isobutyl ketone, sodium hydroxide, isopropyl-ketone and glycerol to prepare a finishing solution with the concentration of 100-150g/L; and S3, adopting a size taking combined process, completing warp dyeing and sizing processes at 50-100m/min and twice dipping and twice rolling, drying with hot air at 105-120 DEG C, then re-beaming, and weaving with weft on a machine to obtain the polylactic acid fiber composite fabric. The fabric woven by the weaving method i</description><subject>DYEING LEATHER, FURS, OR SOLID MACROMOLECULAR SUBSTANCES INANY FORM</subject><subject>DYEING OR PRINTING TEXTILES</subject><subject>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</subject><subject>LAUNDERING</subject><subject>LOOMS</subject><subject>METHODS OF WEAVING</subject><subject>TEXTILES</subject><subject>TREATMENT OF TEXTILES OR THE LIKE</subject><subject>TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</subject><subject>WEAVING</subject><subject>WOVEN FABRICS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAPT00sy8xLV8hNLcnIT1HIT1NIzi8pyc_TLcjPqcxJTC7JTFZITM5MUUjLTEotAkrmFuQXZ5akKqQlJhVlJvMwsKYl5hSn8kJpbgZFN9cQZw_d1IL8-NTigsTk1LzUknhnP0NDcxMTSwNDE0djYtQAAJfeMPY</recordid><startdate>20240126</startdate><enddate>20240126</enddate><creator>GU JIN</creator><creator>DENG JIANGUANG</creator><creator>CHEN GUICHUN</creator><creator>HUANG ZHUOHENG</creator><creator>QIN YUJUAN</creator><creator>QIU DIHENG</creator><scope>EVB</scope></search><sort><creationdate>20240126</creationdate><title>Weaving method of cotton-polylactic acid fiber composite fabric</title><author>GU JIN ; DENG JIANGUANG ; CHEN GUICHUN ; HUANG ZHUOHENG ; QIN YUJUAN ; QIU DIHENG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117449014A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>DYEING LEATHER, FURS, OR SOLID MACROMOLECULAR SUBSTANCES INANY FORM</topic><topic>DYEING OR PRINTING TEXTILES</topic><topic>FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR</topic><topic>LAUNDERING</topic><topic>LOOMS</topic><topic>METHODS OF WEAVING</topic><topic>TEXTILES</topic><topic>TREATMENT OF TEXTILES OR THE LIKE</topic><topic>TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS</topic><topic>WEAVING</topic><topic>WOVEN FABRICS</topic><toplevel>online_resources</toplevel><creatorcontrib>GU JIN</creatorcontrib><creatorcontrib>DENG JIANGUANG</creatorcontrib><creatorcontrib>CHEN GUICHUN</creatorcontrib><creatorcontrib>HUANG ZHUOHENG</creatorcontrib><creatorcontrib>QIN YUJUAN</creatorcontrib><creatorcontrib>QIU DIHENG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GU JIN</au><au>DENG JIANGUANG</au><au>CHEN GUICHUN</au><au>HUANG ZHUOHENG</au><au>QIN YUJUAN</au><au>QIU DIHENG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Weaving method of cotton-polylactic acid fiber composite fabric</title><date>2024-01-26</date><risdate>2024</risdate><abstract>The invention discloses a weaving method of a cotton-polylactic acid fiber composite fabric, which comprises the following steps: S1, warp yarns are warped into a ball warp beam with 300-600 yarns per beam at a speed of 250m/min by adopting ball warp, and the warp yarns are cotton fiber/polylactic acid covering yarns formed by wrapping the outside of polylactic acid fibers with cotton fibers; s2, adding a proper amount of deionized water into a finishing agent consisting of low-viscosity starch, indigo dye, amino-terminated dimethyl silicone oil, methyl isobutyl ketone, sodium hydroxide, isopropyl-ketone and glycerol to prepare a finishing solution with the concentration of 100-150g/L; and S3, adopting a size taking combined process, completing warp dyeing and sizing processes at 50-100m/min and twice dipping and twice rolling, drying with hot air at 105-120 DEG C, then re-beaming, and weaving with weft on a machine to obtain the polylactic acid fiber composite fabric. The fabric woven by the weaving method i</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117449014A
source esp@cenet
subjects DYEING LEATHER, FURS, OR SOLID MACROMOLECULAR SUBSTANCES INANY FORM
DYEING OR PRINTING TEXTILES
FLEXIBLE MATERIALS NOT OTHERWISE PROVIDED FOR
LAUNDERING
LOOMS
METHODS OF WEAVING
TEXTILES
TREATMENT OF TEXTILES OR THE LIKE
TREATMENT, NOT PROVIDED FOR ELSEWHERE IN CLASS D06, OF FIBRES, THREADS, YARNS,FABRICS, FEATHERS, OR FIBROUS GOODS MADE FROM SUCH MATERIALS
WEAVING
WOVEN FABRICS
title Weaving method of cotton-polylactic acid fiber composite fabric
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-22T01%3A07%3A17IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GU%20JIN&rft.date=2024-01-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117449014A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true