Method for preparing calcite-rhododite solid solution through water bath co-heating and application of calcite-rhododite solid solution
The invention discloses a method for preparing a calcite-rhomboxite solid solution through water bath co-heating and application of the calcite-rhomboxite solid solution. According to the method, a calcium nitrate solution and a nickel nitrate solution are proportioned into a mixed solution accordin...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | ZHOU XINGZI YU XIAOLING NONG PEIJIE LUO FEI XU CHUNLI LIU XINGHANG ZHU YINIAN NONG XIAOKE XU FAN ZHU ZONGQIANG |
description | The invention discloses a method for preparing a calcite-rhomboxite solid solution through water bath co-heating and application of the calcite-rhomboxite solid solution. According to the method, a calcium nitrate solution and a nickel nitrate solution are proportioned into a mixed solution according to a corresponding molar ratio, and ammonium bicarbonate is used as a basic solution. The preparation method comprises the following steps: adding an ammonium bicarbonate solution into a mixed solution with a corresponding ratio, controlling the reaction temperature and the stirring speed, and adjusting the heat preservation time and the aging time, so as to obtain calcite-rhomboxite solid solutions with different molar ratios. And finally, taking a proper amount of synthesized calcite-rhomboinite solid solution series, and dissolving in three different aqueous solutions at 25 DEG C to research the dissolution, migration and transformation rules and stability of the calcite-rhomboinite solid solution nickel in th |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117446848A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117446848A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117446848A3</originalsourceid><addsrcrecordid>eNqNjLEOwjAQQ7swIOAfjg_IUBFBV1SBWGBir47k2kSKclFyFZ_Ab9MidlhsS372snpdSRxb6DlDypQw-ziAwWC8kMpTxXZKUDh4O-soniOIyzwODp4olOGB4sCwcoQyzzFawJSCN_ihuf_5uK4WPYZCm6-vqu35dG8vihJ3VBIaiiRde6vrg9b7RjfH3T_MG_iKTMo</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for preparing calcite-rhododite solid solution through water bath co-heating and application of calcite-rhododite solid solution</title><source>esp@cenet</source><creator>ZHOU XINGZI ; YU XIAOLING ; NONG PEIJIE ; LUO FEI ; XU CHUNLI ; LIU XINGHANG ; ZHU YINIAN ; NONG XIAOKE ; XU FAN ; ZHU ZONGQIANG</creator><creatorcontrib>ZHOU XINGZI ; YU XIAOLING ; NONG PEIJIE ; LUO FEI ; XU CHUNLI ; LIU XINGHANG ; ZHU YINIAN ; NONG XIAOKE ; XU FAN ; ZHU ZONGQIANG</creatorcontrib><description>The invention discloses a method for preparing a calcite-rhomboxite solid solution through water bath co-heating and application of the calcite-rhomboxite solid solution. According to the method, a calcium nitrate solution and a nickel nitrate solution are proportioned into a mixed solution according to a corresponding molar ratio, and ammonium bicarbonate is used as a basic solution. The preparation method comprises the following steps: adding an ammonium bicarbonate solution into a mixed solution with a corresponding ratio, controlling the reaction temperature and the stirring speed, and adjusting the heat preservation time and the aging time, so as to obtain calcite-rhomboxite solid solutions with different molar ratios. And finally, taking a proper amount of synthesized calcite-rhomboinite solid solution series, and dissolving in three different aqueous solutions at 25 DEG C to research the dissolution, migration and transformation rules and stability of the calcite-rhomboinite solid solution nickel in th</description><language>chi ; eng</language><subject>CHEMISTRY ; COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F ; COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS ; INORGANIC CHEMISTRY ; METALLURGY</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240126&DB=EPODOC&CC=CN&NR=117446848A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20240126&DB=EPODOC&CC=CN&NR=117446848A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHOU XINGZI</creatorcontrib><creatorcontrib>YU XIAOLING</creatorcontrib><creatorcontrib>NONG PEIJIE</creatorcontrib><creatorcontrib>LUO FEI</creatorcontrib><creatorcontrib>XU CHUNLI</creatorcontrib><creatorcontrib>LIU XINGHANG</creatorcontrib><creatorcontrib>ZHU YINIAN</creatorcontrib><creatorcontrib>NONG XIAOKE</creatorcontrib><creatorcontrib>XU FAN</creatorcontrib><creatorcontrib>ZHU ZONGQIANG</creatorcontrib><title>Method for preparing calcite-rhododite solid solution through water bath co-heating and application of calcite-rhododite solid solution</title><description>The invention discloses a method for preparing a calcite-rhomboxite solid solution through water bath co-heating and application of the calcite-rhomboxite solid solution. According to the method, a calcium nitrate solution and a nickel nitrate solution are proportioned into a mixed solution according to a corresponding molar ratio, and ammonium bicarbonate is used as a basic solution. The preparation method comprises the following steps: adding an ammonium bicarbonate solution into a mixed solution with a corresponding ratio, controlling the reaction temperature and the stirring speed, and adjusting the heat preservation time and the aging time, so as to obtain calcite-rhomboxite solid solutions with different molar ratios. And finally, taking a proper amount of synthesized calcite-rhomboinite solid solution series, and dissolving in three different aqueous solutions at 25 DEG C to research the dissolution, migration and transformation rules and stability of the calcite-rhomboinite solid solution nickel in th</description><subject>CHEMISTRY</subject><subject>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</subject><subject>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</subject><subject>INORGANIC CHEMISTRY</subject><subject>METALLURGY</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjLEOwjAQQ7swIOAfjg_IUBFBV1SBWGBir47k2kSKclFyFZ_Ab9MidlhsS372snpdSRxb6DlDypQw-ziAwWC8kMpTxXZKUDh4O-soniOIyzwODp4olOGB4sCwcoQyzzFawJSCN_ihuf_5uK4WPYZCm6-vqu35dG8vihJ3VBIaiiRde6vrg9b7RjfH3T_MG_iKTMo</recordid><startdate>20240126</startdate><enddate>20240126</enddate><creator>ZHOU XINGZI</creator><creator>YU XIAOLING</creator><creator>NONG PEIJIE</creator><creator>LUO FEI</creator><creator>XU CHUNLI</creator><creator>LIU XINGHANG</creator><creator>ZHU YINIAN</creator><creator>NONG XIAOKE</creator><creator>XU FAN</creator><creator>ZHU ZONGQIANG</creator><scope>EVB</scope></search><sort><creationdate>20240126</creationdate><title>Method for preparing calcite-rhododite solid solution through water bath co-heating and application of calcite-rhododite solid solution</title><author>ZHOU XINGZI ; YU XIAOLING ; NONG PEIJIE ; LUO FEI ; XU CHUNLI ; LIU XINGHANG ; ZHU YINIAN ; NONG XIAOKE ; XU FAN ; ZHU ZONGQIANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117446848A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CHEMISTRY</topic><topic>COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F</topic><topic>COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS</topic><topic>INORGANIC CHEMISTRY</topic><topic>METALLURGY</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHOU XINGZI</creatorcontrib><creatorcontrib>YU XIAOLING</creatorcontrib><creatorcontrib>NONG PEIJIE</creatorcontrib><creatorcontrib>LUO FEI</creatorcontrib><creatorcontrib>XU CHUNLI</creatorcontrib><creatorcontrib>LIU XINGHANG</creatorcontrib><creatorcontrib>ZHU YINIAN</creatorcontrib><creatorcontrib>NONG XIAOKE</creatorcontrib><creatorcontrib>XU FAN</creatorcontrib><creatorcontrib>ZHU ZONGQIANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHOU XINGZI</au><au>YU XIAOLING</au><au>NONG PEIJIE</au><au>LUO FEI</au><au>XU CHUNLI</au><au>LIU XINGHANG</au><au>ZHU YINIAN</au><au>NONG XIAOKE</au><au>XU FAN</au><au>ZHU ZONGQIANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for preparing calcite-rhododite solid solution through water bath co-heating and application of calcite-rhododite solid solution</title><date>2024-01-26</date><risdate>2024</risdate><abstract>The invention discloses a method for preparing a calcite-rhomboxite solid solution through water bath co-heating and application of the calcite-rhomboxite solid solution. According to the method, a calcium nitrate solution and a nickel nitrate solution are proportioned into a mixed solution according to a corresponding molar ratio, and ammonium bicarbonate is used as a basic solution. The preparation method comprises the following steps: adding an ammonium bicarbonate solution into a mixed solution with a corresponding ratio, controlling the reaction temperature and the stirring speed, and adjusting the heat preservation time and the aging time, so as to obtain calcite-rhomboxite solid solutions with different molar ratios. And finally, taking a proper amount of synthesized calcite-rhomboinite solid solution series, and dissolving in three different aqueous solutions at 25 DEG C to research the dissolution, migration and transformation rules and stability of the calcite-rhomboinite solid solution nickel in th</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN117446848A |
source | esp@cenet |
subjects | CHEMISTRY COMPOUNDS CONTAINING METALS NOT COVERED BY SUBCLASSESC01D OR C01F COMPOUNDS OF THE METALS BERYLLIUM, MAGNESIUM, ALUMINIUM,CALCIUM, STRONTIUM, BARIUM, RADIUM, THORIUM, OR OF THERARE-EARTH METALS INORGANIC CHEMISTRY METALLURGY |
title | Method for preparing calcite-rhododite solid solution through water bath co-heating and application of calcite-rhododite solid solution |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-05T10%3A46%3A31IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHOU%20XINGZI&rft.date=2024-01-26&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117446848A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |