Preparation method of large-size magnesium alloy cast ingot

The invention provides a large-size magnesium alloy cast ingot preparation method which comprises the following steps: casting an alloy melt, starting a cooling system, simultaneously monitoring the temperatures of different parts of a cast ingot mold, opening a water inlet valve, enabling the water...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YAO MENGLING, GAO SHIQING, ZHANG FEIYUE, WANG YANBIN, XIA XIANGSHENG, LIU PENG, CHEN QIANG, LI MING, CHAI SHUXIN, WAN YUANYUAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YAO MENGLING
GAO SHIQING
ZHANG FEIYUE
WANG YANBIN
XIA XIANGSHENG
LIU PENG
CHEN QIANG
LI MING
CHAI SHUXIN
WAN YUANYUAN
description The invention provides a large-size magnesium alloy cast ingot preparation method which comprises the following steps: casting an alloy melt, starting a cooling system, simultaneously monitoring the temperatures of different parts of a cast ingot mold, opening a water inlet valve, enabling the water level in a cooling chamber to rise at the speed of 80-100mm/min, closing all nozzles on the layer when the water level reaches the height of the nozzles on each layer, and cooling the cast ingot mold at the speed of 80-100mm/min. When the water level reaches the top of the cooling chamber, opening a drain valve, and quickly adjusting the water flow to enable the water inlet amount to be equal to the water discharge amount; and when the temperature of the cast ingot is lower than 200 DEG C, closing the water inlet valve, taking out the cast ingot after the water in the cooling chamber is completely discharged, washing the cast ingot with water for 3-5 minutes, and then air-cooling the cast ingot to room temperature
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117324560A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117324560A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117324560A3</originalsourceid><addsrcrecordid>eNrjZLAOKEotSCxKLMnMz1PITS3JyE9RyE9TyEksSk_VLc6sSlXITUzPSy3OLM1VSMzJya9USE4sLlHIzEvPL-FhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfHOfoaG5sZGJqZmBo7GxKgBALyxL30</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of large-size magnesium alloy cast ingot</title><source>esp@cenet</source><creator>YAO MENGLING ; GAO SHIQING ; ZHANG FEIYUE ; WANG YANBIN ; XIA XIANGSHENG ; LIU PENG ; CHEN QIANG ; LI MING ; CHAI SHUXIN ; WAN YUANYUAN</creator><creatorcontrib>YAO MENGLING ; GAO SHIQING ; ZHANG FEIYUE ; WANG YANBIN ; XIA XIANGSHENG ; LIU PENG ; CHEN QIANG ; LI MING ; CHAI SHUXIN ; WAN YUANYUAN</creatorcontrib><description>The invention provides a large-size magnesium alloy cast ingot preparation method which comprises the following steps: casting an alloy melt, starting a cooling system, simultaneously monitoring the temperatures of different parts of a cast ingot mold, opening a water inlet valve, enabling the water level in a cooling chamber to rise at the speed of 80-100mm/min, closing all nozzles on the layer when the water level reaches the height of the nozzles on each layer, and cooling the cast ingot mold at the speed of 80-100mm/min. When the water level reaches the top of the cooling chamber, opening a drain valve, and quickly adjusting the water flow to enable the water inlet amount to be equal to the water discharge amount; and when the temperature of the cast ingot is lower than 200 DEG C, closing the water inlet valve, taking out the cast ingot after the water in the cooling chamber is completely discharged, washing the cast ingot with water for 3-5 minutes, and then air-cooling the cast ingot to room temperature</description><language>chi ; eng</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; PERFORMING OPERATIONS ; POWDER METALLURGY ; TRANSPORTING</subject><creationdate>2024</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240102&amp;DB=EPODOC&amp;CC=CN&amp;NR=117324560A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20240102&amp;DB=EPODOC&amp;CC=CN&amp;NR=117324560A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YAO MENGLING</creatorcontrib><creatorcontrib>GAO SHIQING</creatorcontrib><creatorcontrib>ZHANG FEIYUE</creatorcontrib><creatorcontrib>WANG YANBIN</creatorcontrib><creatorcontrib>XIA XIANGSHENG</creatorcontrib><creatorcontrib>LIU PENG</creatorcontrib><creatorcontrib>CHEN QIANG</creatorcontrib><creatorcontrib>LI MING</creatorcontrib><creatorcontrib>CHAI SHUXIN</creatorcontrib><creatorcontrib>WAN YUANYUAN</creatorcontrib><title>Preparation method of large-size magnesium alloy cast ingot</title><description>The invention provides a large-size magnesium alloy cast ingot preparation method which comprises the following steps: casting an alloy melt, starting a cooling system, simultaneously monitoring the temperatures of different parts of a cast ingot mold, opening a water inlet valve, enabling the water level in a cooling chamber to rise at the speed of 80-100mm/min, closing all nozzles on the layer when the water level reaches the height of the nozzles on each layer, and cooling the cast ingot mold at the speed of 80-100mm/min. When the water level reaches the top of the cooling chamber, opening a drain valve, and quickly adjusting the water flow to enable the water inlet amount to be equal to the water discharge amount; and when the temperature of the cast ingot is lower than 200 DEG C, closing the water inlet valve, taking out the cast ingot after the water in the cooling chamber is completely discharged, washing the cast ingot with water for 3-5 minutes, and then air-cooling the cast ingot to room temperature</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2024</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZLAOKEotSCxKLMnMz1PITS3JyE9RyE9TyEksSk_VLc6sSlXITUzPSy3OLM1VSMzJya9USE4sLlHIzEvPL-FhYE1LzClO5YXS3AyKbq4hzh66qQX58anFBYnJqXmpJfHOfoaG5sZGJqZmBo7GxKgBALyxL30</recordid><startdate>20240102</startdate><enddate>20240102</enddate><creator>YAO MENGLING</creator><creator>GAO SHIQING</creator><creator>ZHANG FEIYUE</creator><creator>WANG YANBIN</creator><creator>XIA XIANGSHENG</creator><creator>LIU PENG</creator><creator>CHEN QIANG</creator><creator>LI MING</creator><creator>CHAI SHUXIN</creator><creator>WAN YUANYUAN</creator><scope>EVB</scope></search><sort><creationdate>20240102</creationdate><title>Preparation method of large-size magnesium alloy cast ingot</title><author>YAO MENGLING ; GAO SHIQING ; ZHANG FEIYUE ; WANG YANBIN ; XIA XIANGSHENG ; LIU PENG ; CHEN QIANG ; LI MING ; CHAI SHUXIN ; WAN YUANYUAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117324560A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2024</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>YAO MENGLING</creatorcontrib><creatorcontrib>GAO SHIQING</creatorcontrib><creatorcontrib>ZHANG FEIYUE</creatorcontrib><creatorcontrib>WANG YANBIN</creatorcontrib><creatorcontrib>XIA XIANGSHENG</creatorcontrib><creatorcontrib>LIU PENG</creatorcontrib><creatorcontrib>CHEN QIANG</creatorcontrib><creatorcontrib>LI MING</creatorcontrib><creatorcontrib>CHAI SHUXIN</creatorcontrib><creatorcontrib>WAN YUANYUAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YAO MENGLING</au><au>GAO SHIQING</au><au>ZHANG FEIYUE</au><au>WANG YANBIN</au><au>XIA XIANGSHENG</au><au>LIU PENG</au><au>CHEN QIANG</au><au>LI MING</au><au>CHAI SHUXIN</au><au>WAN YUANYUAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of large-size magnesium alloy cast ingot</title><date>2024-01-02</date><risdate>2024</risdate><abstract>The invention provides a large-size magnesium alloy cast ingot preparation method which comprises the following steps: casting an alloy melt, starting a cooling system, simultaneously monitoring the temperatures of different parts of a cast ingot mold, opening a water inlet valve, enabling the water level in a cooling chamber to rise at the speed of 80-100mm/min, closing all nozzles on the layer when the water level reaches the height of the nozzles on each layer, and cooling the cast ingot mold at the speed of 80-100mm/min. When the water level reaches the top of the cooling chamber, opening a drain valve, and quickly adjusting the water flow to enable the water inlet amount to be equal to the water discharge amount; and when the temperature of the cast ingot is lower than 200 DEG C, closing the water inlet valve, taking out the cast ingot after the water in the cooling chamber is completely discharged, washing the cast ingot with water for 3-5 minutes, and then air-cooling the cast ingot to room temperature</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117324560A
source esp@cenet
subjects CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
PERFORMING OPERATIONS
POWDER METALLURGY
TRANSPORTING
title Preparation method of large-size magnesium alloy cast ingot
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-20T16%3A28%3A12IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YAO%20MENGLING&rft.date=2024-01-02&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117324560A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true