Low-cost low-density high-modulus magnesium alloy and preparation method thereof

The invention provides a low-cost, low-density and high-modulus magnesium alloy and a preparation method thereof. The magnesium alloy comprises the following elements in percentage by mass: 2.5 to 5 weight percent of Al, 2 to 4 weight percent of Ca, 0.2 to 0.6 weight percent of Mn, 3.5 to 6.5 weight...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: YAO MENGLING, GAO SHIQING, ZHANG FEIYUE, WANG YANBIN, XIA XIANGSHENG, LIU PENG, LI MING, CHAI SHUXIN, WAN YUANYUAN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator YAO MENGLING
GAO SHIQING
ZHANG FEIYUE
WANG YANBIN
XIA XIANGSHENG
LIU PENG
LI MING
CHAI SHUXIN
WAN YUANYUAN
description The invention provides a low-cost, low-density and high-modulus magnesium alloy and a preparation method thereof. The magnesium alloy comprises the following elements in percentage by mass: 2.5 to 5 weight percent of Al, 2 to 4 weight percent of Ca, 0.2 to 0.6 weight percent of Mn, 3.5 to 6.5 weight percent of SiC particles and the balance of Mg and inevitable impurities. The preparation method comprises the following steps: mechanically stirring a melt, quickly adding SiC particles after the melt forms a stable vortex, continuously stirring after the SiC particles are added, so that the SiC particles are uniformly distributed in the melt, carrying out secondary dispersion on the SiC particles in the melt by adopting ultrasonic treatment, and obtaining a magnesium alloy cast ingot by adopting a mode of air cooling and then water cooling, and after homogenization treatment, three-time upsetting and three-time drawing are conducted, and extrusion deformation is conducted. According to the method, the elasticity
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117265352A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117265352A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117265352A3</originalsourceid><addsrcrecordid>eNqNyrEKwjAQgOEuDqK-w_kAGdpSnUtRHEQc3MvRXJtAkgvJBenb6-ADOP3f8G-r553fauIs4L7QFLKVFYxdjPKsiysZPC6Bsi0e0DleAYOGmChiQrEcwJMY1iCGEvG8rzYzukyHX3fV8Xp5DTdFkUfKEScKJOPwqOtzc-rarunbf54P0q430Q</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Low-cost low-density high-modulus magnesium alloy and preparation method thereof</title><source>esp@cenet</source><creator>YAO MENGLING ; GAO SHIQING ; ZHANG FEIYUE ; WANG YANBIN ; XIA XIANGSHENG ; LIU PENG ; LI MING ; CHAI SHUXIN ; WAN YUANYUAN</creator><creatorcontrib>YAO MENGLING ; GAO SHIQING ; ZHANG FEIYUE ; WANG YANBIN ; XIA XIANGSHENG ; LIU PENG ; LI MING ; CHAI SHUXIN ; WAN YUANYUAN</creatorcontrib><description>The invention provides a low-cost, low-density and high-modulus magnesium alloy and a preparation method thereof. The magnesium alloy comprises the following elements in percentage by mass: 2.5 to 5 weight percent of Al, 2 to 4 weight percent of Ca, 0.2 to 0.6 weight percent of Mn, 3.5 to 6.5 weight percent of SiC particles and the balance of Mg and inevitable impurities. The preparation method comprises the following steps: mechanically stirring a melt, quickly adding SiC particles after the melt forms a stable vortex, continuously stirring after the SiC particles are added, so that the SiC particles are uniformly distributed in the melt, carrying out secondary dispersion on the SiC particles in the melt by adopting ultrasonic treatment, and obtaining a magnesium alloy cast ingot by adopting a mode of air cooling and then water cooling, and after homogenization treatment, three-time upsetting and three-time drawing are conducted, and extrusion deformation is conducted. According to the method, the elasticity</description><language>chi ; eng</language><subject>ALLOYS ; CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; FORGE FURNACES ; FORGING ; HAMMERING ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; METALLURGY ; PERFORMING OPERATIONS ; PRESSING METAL ; PUNCHING METAL ; RIVETING ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231222&amp;DB=EPODOC&amp;CC=CN&amp;NR=117265352A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76516</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231222&amp;DB=EPODOC&amp;CC=CN&amp;NR=117265352A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>YAO MENGLING</creatorcontrib><creatorcontrib>GAO SHIQING</creatorcontrib><creatorcontrib>ZHANG FEIYUE</creatorcontrib><creatorcontrib>WANG YANBIN</creatorcontrib><creatorcontrib>XIA XIANGSHENG</creatorcontrib><creatorcontrib>LIU PENG</creatorcontrib><creatorcontrib>LI MING</creatorcontrib><creatorcontrib>CHAI SHUXIN</creatorcontrib><creatorcontrib>WAN YUANYUAN</creatorcontrib><title>Low-cost low-density high-modulus magnesium alloy and preparation method thereof</title><description>The invention provides a low-cost, low-density and high-modulus magnesium alloy and a preparation method thereof. The magnesium alloy comprises the following elements in percentage by mass: 2.5 to 5 weight percent of Al, 2 to 4 weight percent of Ca, 0.2 to 0.6 weight percent of Mn, 3.5 to 6.5 weight percent of SiC particles and the balance of Mg and inevitable impurities. The preparation method comprises the following steps: mechanically stirring a melt, quickly adding SiC particles after the melt forms a stable vortex, continuously stirring after the SiC particles are added, so that the SiC particles are uniformly distributed in the melt, carrying out secondary dispersion on the SiC particles in the melt by adopting ultrasonic treatment, and obtaining a magnesium alloy cast ingot by adopting a mode of air cooling and then water cooling, and after homogenization treatment, three-time upsetting and three-time drawing are conducted, and extrusion deformation is conducted. According to the method, the elasticity</description><subject>ALLOYS</subject><subject>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>FORGE FURNACES</subject><subject>FORGING</subject><subject>HAMMERING</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>PRESSING METAL</subject><subject>PUNCHING METAL</subject><subject>RIVETING</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEKwjAQgOEuDqK-w_kAGdpSnUtRHEQc3MvRXJtAkgvJBenb6-ADOP3f8G-r553fauIs4L7QFLKVFYxdjPKsiysZPC6Bsi0e0DleAYOGmChiQrEcwJMY1iCGEvG8rzYzukyHX3fV8Xp5DTdFkUfKEScKJOPwqOtzc-rarunbf54P0q430Q</recordid><startdate>20231222</startdate><enddate>20231222</enddate><creator>YAO MENGLING</creator><creator>GAO SHIQING</creator><creator>ZHANG FEIYUE</creator><creator>WANG YANBIN</creator><creator>XIA XIANGSHENG</creator><creator>LIU PENG</creator><creator>LI MING</creator><creator>CHAI SHUXIN</creator><creator>WAN YUANYUAN</creator><scope>EVB</scope></search><sort><creationdate>20231222</creationdate><title>Low-cost low-density high-modulus magnesium alloy and preparation method thereof</title><author>YAO MENGLING ; GAO SHIQING ; ZHANG FEIYUE ; WANG YANBIN ; XIA XIANGSHENG ; LIU PENG ; LI MING ; CHAI SHUXIN ; WAN YUANYUAN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117265352A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>ALLOYS</topic><topic>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>FORGE FURNACES</topic><topic>FORGING</topic><topic>HAMMERING</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>PRESSING METAL</topic><topic>PUNCHING METAL</topic><topic>RIVETING</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>YAO MENGLING</creatorcontrib><creatorcontrib>GAO SHIQING</creatorcontrib><creatorcontrib>ZHANG FEIYUE</creatorcontrib><creatorcontrib>WANG YANBIN</creatorcontrib><creatorcontrib>XIA XIANGSHENG</creatorcontrib><creatorcontrib>LIU PENG</creatorcontrib><creatorcontrib>LI MING</creatorcontrib><creatorcontrib>CHAI SHUXIN</creatorcontrib><creatorcontrib>WAN YUANYUAN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>YAO MENGLING</au><au>GAO SHIQING</au><au>ZHANG FEIYUE</au><au>WANG YANBIN</au><au>XIA XIANGSHENG</au><au>LIU PENG</au><au>LI MING</au><au>CHAI SHUXIN</au><au>WAN YUANYUAN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Low-cost low-density high-modulus magnesium alloy and preparation method thereof</title><date>2023-12-22</date><risdate>2023</risdate><abstract>The invention provides a low-cost, low-density and high-modulus magnesium alloy and a preparation method thereof. The magnesium alloy comprises the following elements in percentage by mass: 2.5 to 5 weight percent of Al, 2 to 4 weight percent of Ca, 0.2 to 0.6 weight percent of Mn, 3.5 to 6.5 weight percent of SiC particles and the balance of Mg and inevitable impurities. The preparation method comprises the following steps: mechanically stirring a melt, quickly adding SiC particles after the melt forms a stable vortex, continuously stirring after the SiC particles are added, so that the SiC particles are uniformly distributed in the melt, carrying out secondary dispersion on the SiC particles in the melt by adopting ultrasonic treatment, and obtaining a magnesium alloy cast ingot by adopting a mode of air cooling and then water cooling, and after homogenization treatment, three-time upsetting and three-time drawing are conducted, and extrusion deformation is conducted. According to the method, the elasticity</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117265352A
source esp@cenet
subjects ALLOYS
CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
FORGE FURNACES
FORGING
HAMMERING
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
METALLURGY
PERFORMING OPERATIONS
PRESSING METAL
PUNCHING METAL
RIVETING
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Low-cost low-density high-modulus magnesium alloy and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-20T16%3A23%3A51IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=YAO%20MENGLING&rft.date=2023-12-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117265352A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true