Production method of 20Cr13 stainless steel wire rod for cold heading shaft sleeve

The invention belongs to the technical field of stainless steel production, and relates to a production method of a 20Cr13 stainless steel wire rod for a cold heading shaft sleeve. According to the method, on the basis of a conventional method, the steps of smelting, rolling and annealing are furthe...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: XU XIN, LUO BIN, JI DENGPING, CHU YUNXING, LI LI, LIN SHUANGWEI
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator XU XIN
LUO BIN
JI DENGPING
CHU YUNXING
LI LI
LIN SHUANGWEI
description The invention belongs to the technical field of stainless steel production, and relates to a production method of a 20Cr13 stainless steel wire rod for a cold heading shaft sleeve. According to the method, on the basis of a conventional method, the steps of smelting, rolling and annealing are further improved, and during smelting, molten steel elements are adjusted as follows: 0.16-0.20% of C; si < = 0.40; less than or equal to 0.40% of Mn; 12.0-14.0% of Cr; 0.30% or less of Ni; 0.10% to 0.30% of Cu; the stainless steel wire rod with better surface quality and high dimensional precision is manufactured by adopting a high-speed rolling machine; and then annealing treatment is conducted in a cover type annealing furnace, and the 20Cr13 stainless steel wire rod for the cold heading shaft sleeve is obtained. Through the comprehensive action of element control, rolling speed and temperature control and the annealing process, the annealing hardness of the finished wire rod is smaller than or equal to 145 HBW, the s
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117265226A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117265226A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117265226A3</originalsourceid><addsrcrecordid>eNqNyjEKAjEQRuFtLES9w3gAwWRxrSUoViJiv4TNHxOImSUT9fpu4QGs3iu-eXO7FnavoUbO9EQN7Ig96a0pqiWpNuYEkemARJ9YQJMnz4UGTo4CrIv5QRKsryQJeGPZzLxNgtWvi2Z9Ot7NeYORe8hoB2TU3lyU2utup3V3aP8xX4PWNvM</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Production method of 20Cr13 stainless steel wire rod for cold heading shaft sleeve</title><source>esp@cenet</source><creator>XU XIN ; LUO BIN ; JI DENGPING ; CHU YUNXING ; LI LI ; LIN SHUANGWEI</creator><creatorcontrib>XU XIN ; LUO BIN ; JI DENGPING ; CHU YUNXING ; LI LI ; LIN SHUANGWEI</creatorcontrib><description>The invention belongs to the technical field of stainless steel production, and relates to a production method of a 20Cr13 stainless steel wire rod for a cold heading shaft sleeve. According to the method, on the basis of a conventional method, the steps of smelting, rolling and annealing are further improved, and during smelting, molten steel elements are adjusted as follows: 0.16-0.20% of C; si &lt; = 0.40; less than or equal to 0.40% of Mn; 12.0-14.0% of Cr; 0.30% or less of Ni; 0.10% to 0.30% of Cu; the stainless steel wire rod with better surface quality and high dimensional precision is manufactured by adopting a high-speed rolling machine; and then annealing treatment is conducted in a cover type annealing furnace, and the 20Cr13 stainless steel wire rod for the cold heading shaft sleeve is obtained. Through the comprehensive action of element control, rolling speed and temperature control and the annealing process, the annealing hardness of the finished wire rod is smaller than or equal to 145 HBW, the s</description><language>chi ; eng</language><subject>ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; PERFORMING OPERATIONS ; PUNCHING METAL ; ROLLING OF METAL ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231222&amp;DB=EPODOC&amp;CC=CN&amp;NR=117265226A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231222&amp;DB=EPODOC&amp;CC=CN&amp;NR=117265226A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>XU XIN</creatorcontrib><creatorcontrib>LUO BIN</creatorcontrib><creatorcontrib>JI DENGPING</creatorcontrib><creatorcontrib>CHU YUNXING</creatorcontrib><creatorcontrib>LI LI</creatorcontrib><creatorcontrib>LIN SHUANGWEI</creatorcontrib><title>Production method of 20Cr13 stainless steel wire rod for cold heading shaft sleeve</title><description>The invention belongs to the technical field of stainless steel production, and relates to a production method of a 20Cr13 stainless steel wire rod for a cold heading shaft sleeve. According to the method, on the basis of a conventional method, the steps of smelting, rolling and annealing are further improved, and during smelting, molten steel elements are adjusted as follows: 0.16-0.20% of C; si &lt; = 0.40; less than or equal to 0.40% of Mn; 12.0-14.0% of Cr; 0.30% or less of Ni; 0.10% to 0.30% of Cu; the stainless steel wire rod with better surface quality and high dimensional precision is manufactured by adopting a high-speed rolling machine; and then annealing treatment is conducted in a cover type annealing furnace, and the 20Cr13 stainless steel wire rod for the cold heading shaft sleeve is obtained. Through the comprehensive action of element control, rolling speed and temperature control and the annealing process, the annealing hardness of the finished wire rod is smaller than or equal to 145 HBW, the s</description><subject>ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>ROLLING OF METAL</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyjEKAjEQRuFtLES9w3gAwWRxrSUoViJiv4TNHxOImSUT9fpu4QGs3iu-eXO7FnavoUbO9EQN7Ig96a0pqiWpNuYEkemARJ9YQJMnz4UGTo4CrIv5QRKsryQJeGPZzLxNgtWvi2Z9Ot7NeYORe8hoB2TU3lyU2utup3V3aP8xX4PWNvM</recordid><startdate>20231222</startdate><enddate>20231222</enddate><creator>XU XIN</creator><creator>LUO BIN</creator><creator>JI DENGPING</creator><creator>CHU YUNXING</creator><creator>LI LI</creator><creator>LIN SHUANGWEI</creator><scope>EVB</scope></search><sort><creationdate>20231222</creationdate><title>Production method of 20Cr13 stainless steel wire rod for cold heading shaft sleeve</title><author>XU XIN ; LUO BIN ; JI DENGPING ; CHU YUNXING ; LI LI ; LIN SHUANGWEI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117265226A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>ROLLING OF METAL</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>XU XIN</creatorcontrib><creatorcontrib>LUO BIN</creatorcontrib><creatorcontrib>JI DENGPING</creatorcontrib><creatorcontrib>CHU YUNXING</creatorcontrib><creatorcontrib>LI LI</creatorcontrib><creatorcontrib>LIN SHUANGWEI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>XU XIN</au><au>LUO BIN</au><au>JI DENGPING</au><au>CHU YUNXING</au><au>LI LI</au><au>LIN SHUANGWEI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Production method of 20Cr13 stainless steel wire rod for cold heading shaft sleeve</title><date>2023-12-22</date><risdate>2023</risdate><abstract>The invention belongs to the technical field of stainless steel production, and relates to a production method of a 20Cr13 stainless steel wire rod for a cold heading shaft sleeve. According to the method, on the basis of a conventional method, the steps of smelting, rolling and annealing are further improved, and during smelting, molten steel elements are adjusted as follows: 0.16-0.20% of C; si &lt; = 0.40; less than or equal to 0.40% of Mn; 12.0-14.0% of Cr; 0.30% or less of Ni; 0.10% to 0.30% of Cu; the stainless steel wire rod with better surface quality and high dimensional precision is manufactured by adopting a high-speed rolling machine; and then annealing treatment is conducted in a cover type annealing furnace, and the 20Cr13 stainless steel wire rod for the cold heading shaft sleeve is obtained. Through the comprehensive action of element control, rolling speed and temperature control and the annealing process, the annealing hardness of the finished wire rod is smaller than or equal to 145 HBW, the s</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117265226A
source esp@cenet
subjects ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
PERFORMING OPERATIONS
PUNCHING METAL
ROLLING OF METAL
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Production method of 20Cr13 stainless steel wire rod for cold heading shaft sleeve
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-24T06%3A44%3A00IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=XU%20XIN&rft.date=2023-12-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117265226A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true