Slagging constituent and method for recovering electrical steel waste through slagging and remelting

The invention discloses a slagging agent and a method for recovering electrical steel waste through slagging and remelting. The slagging agent is prepared by mixing CaO powder, SiO2 powder, CaF2 powder, K2O powder and Na2O powder according to the mass ratio of (0.40-0.55): (0.45-0.60): (0.05-0.10):...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: HU SHOUTIAN, QIU GUIBAO, ZOU HONG, PENG XIAOQIAN, TIAN ZHENYUN, FAN GANGQIANG, DENG YING, TAN JIANFEN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator HU SHOUTIAN
QIU GUIBAO
ZOU HONG
PENG XIAOQIAN
TIAN ZHENYUN
FAN GANGQIANG
DENG YING
TAN JIANFEN
description The invention discloses a slagging agent and a method for recovering electrical steel waste through slagging and remelting. The slagging agent is prepared by mixing CaO powder, SiO2 powder, CaF2 powder, K2O powder and Na2O powder according to the mass ratio of (0.40-0.55): (0.45-0.60): (0.05-0.10): (0.04-0.10): (0.01-0.05). The method for recovering the electrical steel waste through slagging and remelting comprises the following steps: uniformly mixing slag former powder, putting the slag former powder into a reaction container, heating the slag former powder in an inert atmosphere until the slag former powder is completely melted, adding the electrical steel waste into the reaction container, adding a monatomic silicon ingot after the electrical steel waste is completely melted, melting the monatomic silicon ingot, uniformly stirring the monatomic silicon ingot and the monatomic silicon ingot, and keeping the temperature at 1500-1550 DEG C for 40-60 minutes, and cooling and removing a slag layer at the uppe
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117051251A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117051251A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117051251A3</originalsourceid><addsrcrecordid>eNqNjLEKwjAURbM4iPoPzw8QjFKcpShOLrqXkNymgTSvJK_6-7agu9PhwOEslXtE431IniynIkFGJCGTHPWQjh21nCnD8gt5rhBhJQdrIhUBIr3NRJIu8-g7Kr_bfMjoEWWytVq0JhZsvlyp7fXyrG87DNygDMYiQZr6rvVpX-lDpc_Hf5oPQvA_dA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Slagging constituent and method for recovering electrical steel waste through slagging and remelting</title><source>esp@cenet</source><creator>HU SHOUTIAN ; QIU GUIBAO ; ZOU HONG ; PENG XIAOQIAN ; TIAN ZHENYUN ; FAN GANGQIANG ; DENG YING ; TAN JIANFEN</creator><creatorcontrib>HU SHOUTIAN ; QIU GUIBAO ; ZOU HONG ; PENG XIAOQIAN ; TIAN ZHENYUN ; FAN GANGQIANG ; DENG YING ; TAN JIANFEN</creatorcontrib><description>The invention discloses a slagging agent and a method for recovering electrical steel waste through slagging and remelting. The slagging agent is prepared by mixing CaO powder, SiO2 powder, CaF2 powder, K2O powder and Na2O powder according to the mass ratio of (0.40-0.55): (0.45-0.60): (0.05-0.10): (0.04-0.10): (0.01-0.05). The method for recovering the electrical steel waste through slagging and remelting comprises the following steps: uniformly mixing slag former powder, putting the slag former powder into a reaction container, heating the slag former powder in an inert atmosphere until the slag former powder is completely melted, adding the electrical steel waste into the reaction container, adding a monatomic silicon ingot after the electrical steel waste is completely melted, melting the monatomic silicon ingot, uniformly stirring the monatomic silicon ingot and the monatomic silicon ingot, and keeping the temperature at 1500-1550 DEG C for 40-60 minutes, and cooling and removing a slag layer at the uppe</description><language>chi ; eng</language><subject>CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; MANUFACTURE OF IRON OR STEEL ; METALLURGY ; METALLURGY OF IRON ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231114&amp;DB=EPODOC&amp;CC=CN&amp;NR=117051251A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25542,76289</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231114&amp;DB=EPODOC&amp;CC=CN&amp;NR=117051251A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>HU SHOUTIAN</creatorcontrib><creatorcontrib>QIU GUIBAO</creatorcontrib><creatorcontrib>ZOU HONG</creatorcontrib><creatorcontrib>PENG XIAOQIAN</creatorcontrib><creatorcontrib>TIAN ZHENYUN</creatorcontrib><creatorcontrib>FAN GANGQIANG</creatorcontrib><creatorcontrib>DENG YING</creatorcontrib><creatorcontrib>TAN JIANFEN</creatorcontrib><title>Slagging constituent and method for recovering electrical steel waste through slagging and remelting</title><description>The invention discloses a slagging agent and a method for recovering electrical steel waste through slagging and remelting. The slagging agent is prepared by mixing CaO powder, SiO2 powder, CaF2 powder, K2O powder and Na2O powder according to the mass ratio of (0.40-0.55): (0.45-0.60): (0.05-0.10): (0.04-0.10): (0.01-0.05). The method for recovering the electrical steel waste through slagging and remelting comprises the following steps: uniformly mixing slag former powder, putting the slag former powder into a reaction container, heating the slag former powder in an inert atmosphere until the slag former powder is completely melted, adding the electrical steel waste into the reaction container, adding a monatomic silicon ingot after the electrical steel waste is completely melted, melting the monatomic silicon ingot, uniformly stirring the monatomic silicon ingot and the monatomic silicon ingot, and keeping the temperature at 1500-1550 DEG C for 40-60 minutes, and cooling and removing a slag layer at the uppe</description><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>MANUFACTURE OF IRON OR STEEL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjLEKwjAURbM4iPoPzw8QjFKcpShOLrqXkNymgTSvJK_6-7agu9PhwOEslXtE431IniynIkFGJCGTHPWQjh21nCnD8gt5rhBhJQdrIhUBIr3NRJIu8-g7Kr_bfMjoEWWytVq0JhZsvlyp7fXyrG87DNygDMYiQZr6rvVpX-lDpc_Hf5oPQvA_dA</recordid><startdate>20231114</startdate><enddate>20231114</enddate><creator>HU SHOUTIAN</creator><creator>QIU GUIBAO</creator><creator>ZOU HONG</creator><creator>PENG XIAOQIAN</creator><creator>TIAN ZHENYUN</creator><creator>FAN GANGQIANG</creator><creator>DENG YING</creator><creator>TAN JIANFEN</creator><scope>EVB</scope></search><sort><creationdate>20231114</creationdate><title>Slagging constituent and method for recovering electrical steel waste through slagging and remelting</title><author>HU SHOUTIAN ; QIU GUIBAO ; ZOU HONG ; PENG XIAOQIAN ; TIAN ZHENYUN ; FAN GANGQIANG ; DENG YING ; TAN JIANFEN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117051251A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>MANUFACTURE OF IRON OR STEEL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>HU SHOUTIAN</creatorcontrib><creatorcontrib>QIU GUIBAO</creatorcontrib><creatorcontrib>ZOU HONG</creatorcontrib><creatorcontrib>PENG XIAOQIAN</creatorcontrib><creatorcontrib>TIAN ZHENYUN</creatorcontrib><creatorcontrib>FAN GANGQIANG</creatorcontrib><creatorcontrib>DENG YING</creatorcontrib><creatorcontrib>TAN JIANFEN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>HU SHOUTIAN</au><au>QIU GUIBAO</au><au>ZOU HONG</au><au>PENG XIAOQIAN</au><au>TIAN ZHENYUN</au><au>FAN GANGQIANG</au><au>DENG YING</au><au>TAN JIANFEN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Slagging constituent and method for recovering electrical steel waste through slagging and remelting</title><date>2023-11-14</date><risdate>2023</risdate><abstract>The invention discloses a slagging agent and a method for recovering electrical steel waste through slagging and remelting. The slagging agent is prepared by mixing CaO powder, SiO2 powder, CaF2 powder, K2O powder and Na2O powder according to the mass ratio of (0.40-0.55): (0.45-0.60): (0.05-0.10): (0.04-0.10): (0.01-0.05). The method for recovering the electrical steel waste through slagging and remelting comprises the following steps: uniformly mixing slag former powder, putting the slag former powder into a reaction container, heating the slag former powder in an inert atmosphere until the slag former powder is completely melted, adding the electrical steel waste into the reaction container, adding a monatomic silicon ingot after the electrical steel waste is completely melted, melting the monatomic silicon ingot, uniformly stirring the monatomic silicon ingot and the monatomic silicon ingot, and keeping the temperature at 1500-1550 DEG C for 40-60 minutes, and cooling and removing a slag layer at the uppe</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117051251A
source esp@cenet
subjects CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
MANUFACTURE OF IRON OR STEEL
METALLURGY
METALLURGY OF IRON
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Slagging constituent and method for recovering electrical steel waste through slagging and remelting
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-02-09T08%3A11%3A43IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=HU%20SHOUTIAN&rft.date=2023-11-14&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117051251A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true