Method for repairing electromagnetic shielding copper mesh of helicopter composite structural member

The invention belongs to the field of composite material forming, and relates to a repairing method for an electromagnetic shielding copper net of a helicopter composite material structural part. The conductive adhesive is prepared from epoxy resin, an amine curing agent and silver powder according...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WANG HAILUN, LIU WANGZI, JANG JUNGI, ZHONG JINGXING, LI WEI, CHEN CHEN, WANG DONGDONG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WANG HAILUN
LIU WANGZI
JANG JUNGI
ZHONG JINGXING
LI WEI
CHEN CHEN
WANG DONGDONG
description The invention belongs to the field of composite material forming, and relates to a repairing method for an electromagnetic shielding copper net of a helicopter composite material structural part. The conductive adhesive is prepared from epoxy resin, an amine curing agent and silver powder according to a certain mass ratio, the prepared adhesive solution is uniformly coated on the damaged part of a copper net on the surface of a part by using a spatula or a brush, and the three components are mixed and then are scraped and coated within 2 hours. And placing at normal temperature for 24-48 hours for curing. And after the glue solution is cured, carefully polishing the glued part by using 120-150-mesh abrasive paper until the surface is smooth and flat and has no obvious bulges. After the damaged part of the copper wire mesh is coated with the conductive glue solution, the copper wire mesh on the surface of the part can form continuous conduction, and the part becomes a shielding body and does not generate elect
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN117015223A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN117015223A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN117015223A3</originalsourceid><addsrcrecordid>eNqNjUEKwjAQRbtxIeodxgMItkVcS1Hc6Mp9ielvE0g6YTK9vxE8gKsP7z9462p4QB0PNLKQIBkvfp4IAVaFo5lmqLeUnUcYvo_llCAUkR3xSA7BF6QFWY6Js1dQVlmsLmJC8eIbsq1WowkZu99uqv3t-uruByTukZOxKJ2-e9b1-Vifmqa9tP84H2MBP8s</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for repairing electromagnetic shielding copper mesh of helicopter composite structural member</title><source>esp@cenet</source><creator>WANG HAILUN ; LIU WANGZI ; JANG JUNGI ; ZHONG JINGXING ; LI WEI ; CHEN CHEN ; WANG DONGDONG</creator><creatorcontrib>WANG HAILUN ; LIU WANGZI ; JANG JUNGI ; ZHONG JINGXING ; LI WEI ; CHEN CHEN ; WANG DONGDONG</creatorcontrib><description>The invention belongs to the field of composite material forming, and relates to a repairing method for an electromagnetic shielding copper net of a helicopter composite material structural part. The conductive adhesive is prepared from epoxy resin, an amine curing agent and silver powder according to a certain mass ratio, the prepared adhesive solution is uniformly coated on the damaged part of a copper net on the surface of a part by using a spatula or a brush, and the three components are mixed and then are scraped and coated within 2 hours. And placing at normal temperature for 24-48 hours for curing. And after the glue solution is cured, carefully polishing the glued part by using 120-150-mesh abrasive paper until the surface is smooth and flat and has no obvious bulges. After the damaged part of the copper wire mesh is coated with the conductive glue solution, the copper wire mesh on the surface of the part can form continuous conduction, and the part becomes a shielding body and does not generate elect</description><language>chi ; eng</language><subject>CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS ; ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR ; ELECTRICITY ; MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS ; PRINTED CIRCUITS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231107&amp;DB=EPODOC&amp;CC=CN&amp;NR=117015223A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,309,781,886,25566,76549</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231107&amp;DB=EPODOC&amp;CC=CN&amp;NR=117015223A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WANG HAILUN</creatorcontrib><creatorcontrib>LIU WANGZI</creatorcontrib><creatorcontrib>JANG JUNGI</creatorcontrib><creatorcontrib>ZHONG JINGXING</creatorcontrib><creatorcontrib>LI WEI</creatorcontrib><creatorcontrib>CHEN CHEN</creatorcontrib><creatorcontrib>WANG DONGDONG</creatorcontrib><title>Method for repairing electromagnetic shielding copper mesh of helicopter composite structural member</title><description>The invention belongs to the field of composite material forming, and relates to a repairing method for an electromagnetic shielding copper net of a helicopter composite material structural part. The conductive adhesive is prepared from epoxy resin, an amine curing agent and silver powder according to a certain mass ratio, the prepared adhesive solution is uniformly coated on the damaged part of a copper net on the surface of a part by using a spatula or a brush, and the three components are mixed and then are scraped and coated within 2 hours. And placing at normal temperature for 24-48 hours for curing. And after the glue solution is cured, carefully polishing the glued part by using 120-150-mesh abrasive paper until the surface is smooth and flat and has no obvious bulges. After the damaged part of the copper wire mesh is coated with the conductive glue solution, the copper wire mesh on the surface of the part can form continuous conduction, and the part becomes a shielding body and does not generate elect</description><subject>CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS</subject><subject>ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR</subject><subject>ELECTRICITY</subject><subject>MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS</subject><subject>PRINTED CIRCUITS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjUEKwjAQRbtxIeodxgMItkVcS1Hc6Mp9ielvE0g6YTK9vxE8gKsP7z9462p4QB0PNLKQIBkvfp4IAVaFo5lmqLeUnUcYvo_llCAUkR3xSA7BF6QFWY6Js1dQVlmsLmJC8eIbsq1WowkZu99uqv3t-uruByTukZOxKJ2-e9b1-Vifmqa9tP84H2MBP8s</recordid><startdate>20231107</startdate><enddate>20231107</enddate><creator>WANG HAILUN</creator><creator>LIU WANGZI</creator><creator>JANG JUNGI</creator><creator>ZHONG JINGXING</creator><creator>LI WEI</creator><creator>CHEN CHEN</creator><creator>WANG DONGDONG</creator><scope>EVB</scope></search><sort><creationdate>20231107</creationdate><title>Method for repairing electromagnetic shielding copper mesh of helicopter composite structural member</title><author>WANG HAILUN ; LIU WANGZI ; JANG JUNGI ; ZHONG JINGXING ; LI WEI ; CHEN CHEN ; WANG DONGDONG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN117015223A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS</topic><topic>ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR</topic><topic>ELECTRICITY</topic><topic>MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS</topic><topic>PRINTED CIRCUITS</topic><toplevel>online_resources</toplevel><creatorcontrib>WANG HAILUN</creatorcontrib><creatorcontrib>LIU WANGZI</creatorcontrib><creatorcontrib>JANG JUNGI</creatorcontrib><creatorcontrib>ZHONG JINGXING</creatorcontrib><creatorcontrib>LI WEI</creatorcontrib><creatorcontrib>CHEN CHEN</creatorcontrib><creatorcontrib>WANG DONGDONG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WANG HAILUN</au><au>LIU WANGZI</au><au>JANG JUNGI</au><au>ZHONG JINGXING</au><au>LI WEI</au><au>CHEN CHEN</au><au>WANG DONGDONG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for repairing electromagnetic shielding copper mesh of helicopter composite structural member</title><date>2023-11-07</date><risdate>2023</risdate><abstract>The invention belongs to the field of composite material forming, and relates to a repairing method for an electromagnetic shielding copper net of a helicopter composite material structural part. The conductive adhesive is prepared from epoxy resin, an amine curing agent and silver powder according to a certain mass ratio, the prepared adhesive solution is uniformly coated on the damaged part of a copper net on the surface of a part by using a spatula or a brush, and the three components are mixed and then are scraped and coated within 2 hours. And placing at normal temperature for 24-48 hours for curing. And after the glue solution is cured, carefully polishing the glued part by using 120-150-mesh abrasive paper until the surface is smooth and flat and has no obvious bulges. After the damaged part of the copper wire mesh is coated with the conductive glue solution, the copper wire mesh on the surface of the part can form continuous conduction, and the part becomes a shielding body and does not generate elect</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN117015223A
source esp@cenet
subjects CASINGS OR CONSTRUCTIONAL DETAILS OF ELECTRIC APPARATUS
ELECTRIC TECHNIQUES NOT OTHERWISE PROVIDED FOR
ELECTRICITY
MANUFACTURE OF ASSEMBLAGES OF ELECTRICAL COMPONENTS
PRINTED CIRCUITS
title Method for repairing electromagnetic shielding copper mesh of helicopter composite structural member
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-18T13%3A00%3A26IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WANG%20HAILUN&rft.date=2023-11-07&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN117015223A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true