Ultrathin high-strength composite environment-friendly inorganic artificial stone and preparation method thereof

The invention relates to the technical field of building materials, in particular to an ultrathin high-strength composite environment-friendly inorganic artificial stone and a preparation method thereof. The inorganic artificial stone provided by the invention comprises a facing layer and a structur...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZOU CHANGGEN, ZHAO BAOJUN, YIN ZHENG, WU CHEN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZOU CHANGGEN
ZHAO BAOJUN
YIN ZHENG
WU CHEN
description The invention relates to the technical field of building materials, in particular to an ultrathin high-strength composite environment-friendly inorganic artificial stone and a preparation method thereof. The inorganic artificial stone provided by the invention comprises a facing layer and a structural layer, the facing layer mixture comprises 56-75 parts of cement, 8-12 parts of an auxiliary cementing material, 10-20 parts of active powder, 15-25 parts of 325 silicon powder, 70-80 parts of fine recycled concrete aggregate, 20-30 parts of coarse recycled concrete aggregate, 1-3 parts of a water reducing agent, 7-15 parts of water and 2-4 parts of a toughening agent; 15 parts of steel fibers are added to the structural layer mixture on the basis of the facing layer mixture. Different mixtures are adopted according to the characteristics of the facing layer and the structural layer, and the chopped steel fibers are added into the structural layer, so that the ultrathin high-strength composite environment-friendl
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116924743A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116924743A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116924743A3</originalsourceid><addsrcrecordid>eNqNzLEKwkAMgOEuDqK-Q3yADrWiOEpRnJx0LuGa9gLX5MgFwbfXwQdw-pePf1nlZ3JDjywQeYp1cSOZPELQOWthJyB5sanMJF6PxiRDegOL2oTCAdCcRw6MCYqrEKAMkI0yfr-sAjN51AE8kpGO62oxYiq0-XVVba-XR3erKWtPJWMgIe-7e9McTrv9cd-e23_MB0QDROs</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Ultrathin high-strength composite environment-friendly inorganic artificial stone and preparation method thereof</title><source>esp@cenet</source><creator>ZOU CHANGGEN ; ZHAO BAOJUN ; YIN ZHENG ; WU CHEN</creator><creatorcontrib>ZOU CHANGGEN ; ZHAO BAOJUN ; YIN ZHENG ; WU CHEN</creatorcontrib><description>The invention relates to the technical field of building materials, in particular to an ultrathin high-strength composite environment-friendly inorganic artificial stone and a preparation method thereof. The inorganic artificial stone provided by the invention comprises a facing layer and a structural layer, the facing layer mixture comprises 56-75 parts of cement, 8-12 parts of an auxiliary cementing material, 10-20 parts of active powder, 15-25 parts of 325 silicon powder, 70-80 parts of fine recycled concrete aggregate, 20-30 parts of coarse recycled concrete aggregate, 1-3 parts of a water reducing agent, 7-15 parts of water and 2-4 parts of a toughening agent; 15 parts of steel fibers are added to the structural layer mixture on the basis of the facing layer mixture. Different mixtures are adopted according to the characteristics of the facing layer and the structural layer, and the chopped steel fibers are added into the structural layer, so that the ultrathin high-strength composite environment-friendl</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231024&amp;DB=EPODOC&amp;CC=CN&amp;NR=116924743A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20231024&amp;DB=EPODOC&amp;CC=CN&amp;NR=116924743A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZOU CHANGGEN</creatorcontrib><creatorcontrib>ZHAO BAOJUN</creatorcontrib><creatorcontrib>YIN ZHENG</creatorcontrib><creatorcontrib>WU CHEN</creatorcontrib><title>Ultrathin high-strength composite environment-friendly inorganic artificial stone and preparation method thereof</title><description>The invention relates to the technical field of building materials, in particular to an ultrathin high-strength composite environment-friendly inorganic artificial stone and a preparation method thereof. The inorganic artificial stone provided by the invention comprises a facing layer and a structural layer, the facing layer mixture comprises 56-75 parts of cement, 8-12 parts of an auxiliary cementing material, 10-20 parts of active powder, 15-25 parts of 325 silicon powder, 70-80 parts of fine recycled concrete aggregate, 20-30 parts of coarse recycled concrete aggregate, 1-3 parts of a water reducing agent, 7-15 parts of water and 2-4 parts of a toughening agent; 15 parts of steel fibers are added to the structural layer mixture on the basis of the facing layer mixture. Different mixtures are adopted according to the characteristics of the facing layer and the structural layer, and the chopped steel fibers are added into the structural layer, so that the ultrathin high-strength composite environment-friendl</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNzLEKwkAMgOEuDqK-Q3yADrWiOEpRnJx0LuGa9gLX5MgFwbfXwQdw-pePf1nlZ3JDjywQeYp1cSOZPELQOWthJyB5sanMJF6PxiRDegOL2oTCAdCcRw6MCYqrEKAMkI0yfr-sAjN51AE8kpGO62oxYiq0-XVVba-XR3erKWtPJWMgIe-7e9McTrv9cd-e23_MB0QDROs</recordid><startdate>20231024</startdate><enddate>20231024</enddate><creator>ZOU CHANGGEN</creator><creator>ZHAO BAOJUN</creator><creator>YIN ZHENG</creator><creator>WU CHEN</creator><scope>EVB</scope></search><sort><creationdate>20231024</creationdate><title>Ultrathin high-strength composite environment-friendly inorganic artificial stone and preparation method thereof</title><author>ZOU CHANGGEN ; ZHAO BAOJUN ; YIN ZHENG ; WU CHEN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116924743A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>ZOU CHANGGEN</creatorcontrib><creatorcontrib>ZHAO BAOJUN</creatorcontrib><creatorcontrib>YIN ZHENG</creatorcontrib><creatorcontrib>WU CHEN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZOU CHANGGEN</au><au>ZHAO BAOJUN</au><au>YIN ZHENG</au><au>WU CHEN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Ultrathin high-strength composite environment-friendly inorganic artificial stone and preparation method thereof</title><date>2023-10-24</date><risdate>2023</risdate><abstract>The invention relates to the technical field of building materials, in particular to an ultrathin high-strength composite environment-friendly inorganic artificial stone and a preparation method thereof. The inorganic artificial stone provided by the invention comprises a facing layer and a structural layer, the facing layer mixture comprises 56-75 parts of cement, 8-12 parts of an auxiliary cementing material, 10-20 parts of active powder, 15-25 parts of 325 silicon powder, 70-80 parts of fine recycled concrete aggregate, 20-30 parts of coarse recycled concrete aggregate, 1-3 parts of a water reducing agent, 7-15 parts of water and 2-4 parts of a toughening agent; 15 parts of steel fibers are added to the structural layer mixture on the basis of the facing layer mixture. Different mixtures are adopted according to the characteristics of the facing layer and the structural layer, and the chopped steel fibers are added into the structural layer, so that the ultrathin high-strength composite environment-friendl</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116924743A
source esp@cenet
subjects ARTIFICIAL STONE
CEMENTS
CERAMICS
CHEMISTRY
COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS
CONCRETE
LIME, MAGNESIA
METALLURGY
REFRACTORIES
SLAG
TREATMENT OF NATURAL STONE
title Ultrathin high-strength composite environment-friendly inorganic artificial stone and preparation method thereof
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-19T15%3A44%3A44IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZOU%20CHANGGEN&rft.date=2023-10-24&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116924743A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true