High-content coal gasification furnace slag-based green low-carbon cementing material and preparation method thereof
The invention provides a high-content coal gasification furnace slag-based green low-carbon cementing material and a preparation method thereof, and the method specifically comprises the following steps: burning 50-55% by mass of coal gasification furnace slag at 600-800 DEG C for 30 min, and coolin...
Gespeichert in:
Hauptverfasser: | , , , , , , , , , , , , , , , , , , , , , |
---|---|
Format: | Patent |
Sprache: | chi ; eng |
Schlagworte: | |
Online-Zugang: | Volltext bestellen |
Tags: |
Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
|
container_end_page | |
---|---|
container_issue | |
container_start_page | |
container_title | |
container_volume | |
creator | ZHANG ZITAO CHEN HAOXU MA TANGDONG BAO WANLU WANG MENGMENG MA XUDONG JIA CHUNYUAN SU JIANHUA ZHANG ZHITAO LI ZHONG DING XIAOPING DING XINJIAN MEN GUANGYU YAN XIAOPING REN LIWEI JIA XIAOLONG DONG HONGNAN WEI LI LI RUIJIE DONG WEI HUI YINGXIN LUO TINGCHI |
description | The invention provides a high-content coal gasification furnace slag-based green low-carbon cementing material and a preparation method thereof, and the method specifically comprises the following steps: burning 50-55% by mass of coal gasification furnace slag at 600-800 DEG C for 30 min, and cooling to room temperature, S2, mixing 50-55% by mass of coal gasification furnace slag after high-temperature burning, 15-20% by mass of slag and 17-20% by mass of gypsum according to a mass ratio of 1: (1-2), and carrying out stirring and mixing to obtain the high-content coal gasification furnace slag-based green low-carbon cementing material. And levigating 5% of furnace slag, 3%-4% of calcium hydroxide and 1%-2% of silica fume, and putting the levigated materials into a stirrer for mixing to obtain the high-content coal gasification furnace slag-based green low-carbon cementing material. The optimal crystalline phase structure of the coal gasification furnace slag is obtained through high-temperature firing tempera |
format | Patent |
fullrecord | <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116903274A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116903274A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116903274A3</originalsourceid><addsrcrecordid>eNqNjUEKwjAQRbtxIeodxgMErBWLSylKV67cl2k6SQPpJCQjXt-AHsDV37z_3rqS3tlZ6cBCLKADerCYnXEaxQUG80qMmiB7tGrETBPYRMTgw1tpTGNhNC3l7NjCgkLJFQfyBDFRxPTVLCRzmEBmShTMtloZ9Jl2v91U-_vt2fWKYhgoxxJkkqF71PX5cmiO7ena_MN8AKJCRSA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>High-content coal gasification furnace slag-based green low-carbon cementing material and preparation method thereof</title><source>esp@cenet</source><creator>ZHANG ZITAO ; CHEN HAOXU ; MA TANGDONG ; BAO WANLU ; WANG MENGMENG ; MA XUDONG ; JIA CHUNYUAN ; SU JIANHUA ; ZHANG ZHITAO ; LI ZHONG ; DING XIAOPING ; DING XINJIAN ; MEN GUANGYU ; YAN XIAOPING ; REN LIWEI ; JIA XIAOLONG ; DONG HONGNAN ; WEI LI ; LI RUIJIE ; DONG WEI ; HUI YINGXIN ; LUO TINGCHI</creator><creatorcontrib>ZHANG ZITAO ; CHEN HAOXU ; MA TANGDONG ; BAO WANLU ; WANG MENGMENG ; MA XUDONG ; JIA CHUNYUAN ; SU JIANHUA ; ZHANG ZHITAO ; LI ZHONG ; DING XIAOPING ; DING XINJIAN ; MEN GUANGYU ; YAN XIAOPING ; REN LIWEI ; JIA XIAOLONG ; DONG HONGNAN ; WEI LI ; LI RUIJIE ; DONG WEI ; HUI YINGXIN ; LUO TINGCHI</creatorcontrib><description>The invention provides a high-content coal gasification furnace slag-based green low-carbon cementing material and a preparation method thereof, and the method specifically comprises the following steps: burning 50-55% by mass of coal gasification furnace slag at 600-800 DEG C for 30 min, and cooling to room temperature, S2, mixing 50-55% by mass of coal gasification furnace slag after high-temperature burning, 15-20% by mass of slag and 17-20% by mass of gypsum according to a mass ratio of 1: (1-2), and carrying out stirring and mixing to obtain the high-content coal gasification furnace slag-based green low-carbon cementing material. And levigating 5% of furnace slag, 3%-4% of calcium hydroxide and 1%-2% of silica fume, and putting the levigated materials into a stirrer for mixing to obtain the high-content coal gasification furnace slag-based green low-carbon cementing material. The optimal crystalline phase structure of the coal gasification furnace slag is obtained through high-temperature firing tempera</description><language>chi ; eng</language><subject>ARTIFICIAL STONE ; CEMENTS ; CERAMICS ; CHEMISTRY ; COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS ; CONCRETE ; LIME, MAGNESIA ; METALLURGY ; REFRACTORIES ; SLAG ; TREATMENT OF NATURAL STONE</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20231020&DB=EPODOC&CC=CN&NR=116903274A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&date=20231020&DB=EPODOC&CC=CN&NR=116903274A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHANG ZITAO</creatorcontrib><creatorcontrib>CHEN HAOXU</creatorcontrib><creatorcontrib>MA TANGDONG</creatorcontrib><creatorcontrib>BAO WANLU</creatorcontrib><creatorcontrib>WANG MENGMENG</creatorcontrib><creatorcontrib>MA XUDONG</creatorcontrib><creatorcontrib>JIA CHUNYUAN</creatorcontrib><creatorcontrib>SU JIANHUA</creatorcontrib><creatorcontrib>ZHANG ZHITAO</creatorcontrib><creatorcontrib>LI ZHONG</creatorcontrib><creatorcontrib>DING XIAOPING</creatorcontrib><creatorcontrib>DING XINJIAN</creatorcontrib><creatorcontrib>MEN GUANGYU</creatorcontrib><creatorcontrib>YAN XIAOPING</creatorcontrib><creatorcontrib>REN LIWEI</creatorcontrib><creatorcontrib>JIA XIAOLONG</creatorcontrib><creatorcontrib>DONG HONGNAN</creatorcontrib><creatorcontrib>WEI LI</creatorcontrib><creatorcontrib>LI RUIJIE</creatorcontrib><creatorcontrib>DONG WEI</creatorcontrib><creatorcontrib>HUI YINGXIN</creatorcontrib><creatorcontrib>LUO TINGCHI</creatorcontrib><title>High-content coal gasification furnace slag-based green low-carbon cementing material and preparation method thereof</title><description>The invention provides a high-content coal gasification furnace slag-based green low-carbon cementing material and a preparation method thereof, and the method specifically comprises the following steps: burning 50-55% by mass of coal gasification furnace slag at 600-800 DEG C for 30 min, and cooling to room temperature, S2, mixing 50-55% by mass of coal gasification furnace slag after high-temperature burning, 15-20% by mass of slag and 17-20% by mass of gypsum according to a mass ratio of 1: (1-2), and carrying out stirring and mixing to obtain the high-content coal gasification furnace slag-based green low-carbon cementing material. And levigating 5% of furnace slag, 3%-4% of calcium hydroxide and 1%-2% of silica fume, and putting the levigated materials into a stirrer for mixing to obtain the high-content coal gasification furnace slag-based green low-carbon cementing material. The optimal crystalline phase structure of the coal gasification furnace slag is obtained through high-temperature firing tempera</description><subject>ARTIFICIAL STONE</subject><subject>CEMENTS</subject><subject>CERAMICS</subject><subject>CHEMISTRY</subject><subject>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</subject><subject>CONCRETE</subject><subject>LIME, MAGNESIA</subject><subject>METALLURGY</subject><subject>REFRACTORIES</subject><subject>SLAG</subject><subject>TREATMENT OF NATURAL STONE</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjUEKwjAQRbtxIeodxgMErBWLSylKV67cl2k6SQPpJCQjXt-AHsDV37z_3rqS3tlZ6cBCLKADerCYnXEaxQUG80qMmiB7tGrETBPYRMTgw1tpTGNhNC3l7NjCgkLJFQfyBDFRxPTVLCRzmEBmShTMtloZ9Jl2v91U-_vt2fWKYhgoxxJkkqF71PX5cmiO7ena_MN8AKJCRSA</recordid><startdate>20231020</startdate><enddate>20231020</enddate><creator>ZHANG ZITAO</creator><creator>CHEN HAOXU</creator><creator>MA TANGDONG</creator><creator>BAO WANLU</creator><creator>WANG MENGMENG</creator><creator>MA XUDONG</creator><creator>JIA CHUNYUAN</creator><creator>SU JIANHUA</creator><creator>ZHANG ZHITAO</creator><creator>LI ZHONG</creator><creator>DING XIAOPING</creator><creator>DING XINJIAN</creator><creator>MEN GUANGYU</creator><creator>YAN XIAOPING</creator><creator>REN LIWEI</creator><creator>JIA XIAOLONG</creator><creator>DONG HONGNAN</creator><creator>WEI LI</creator><creator>LI RUIJIE</creator><creator>DONG WEI</creator><creator>HUI YINGXIN</creator><creator>LUO TINGCHI</creator><scope>EVB</scope></search><sort><creationdate>20231020</creationdate><title>High-content coal gasification furnace slag-based green low-carbon cementing material and preparation method thereof</title><author>ZHANG ZITAO ; CHEN HAOXU ; MA TANGDONG ; BAO WANLU ; WANG MENGMENG ; MA XUDONG ; JIA CHUNYUAN ; SU JIANHUA ; ZHANG ZHITAO ; LI ZHONG ; DING XIAOPING ; DING XINJIAN ; MEN GUANGYU ; YAN XIAOPING ; REN LIWEI ; JIA XIAOLONG ; DONG HONGNAN ; WEI LI ; LI RUIJIE ; DONG WEI ; HUI YINGXIN ; LUO TINGCHI</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116903274A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>ARTIFICIAL STONE</topic><topic>CEMENTS</topic><topic>CERAMICS</topic><topic>CHEMISTRY</topic><topic>COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS</topic><topic>CONCRETE</topic><topic>LIME, MAGNESIA</topic><topic>METALLURGY</topic><topic>REFRACTORIES</topic><topic>SLAG</topic><topic>TREATMENT OF NATURAL STONE</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHANG ZITAO</creatorcontrib><creatorcontrib>CHEN HAOXU</creatorcontrib><creatorcontrib>MA TANGDONG</creatorcontrib><creatorcontrib>BAO WANLU</creatorcontrib><creatorcontrib>WANG MENGMENG</creatorcontrib><creatorcontrib>MA XUDONG</creatorcontrib><creatorcontrib>JIA CHUNYUAN</creatorcontrib><creatorcontrib>SU JIANHUA</creatorcontrib><creatorcontrib>ZHANG ZHITAO</creatorcontrib><creatorcontrib>LI ZHONG</creatorcontrib><creatorcontrib>DING XIAOPING</creatorcontrib><creatorcontrib>DING XINJIAN</creatorcontrib><creatorcontrib>MEN GUANGYU</creatorcontrib><creatorcontrib>YAN XIAOPING</creatorcontrib><creatorcontrib>REN LIWEI</creatorcontrib><creatorcontrib>JIA XIAOLONG</creatorcontrib><creatorcontrib>DONG HONGNAN</creatorcontrib><creatorcontrib>WEI LI</creatorcontrib><creatorcontrib>LI RUIJIE</creatorcontrib><creatorcontrib>DONG WEI</creatorcontrib><creatorcontrib>HUI YINGXIN</creatorcontrib><creatorcontrib>LUO TINGCHI</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHANG ZITAO</au><au>CHEN HAOXU</au><au>MA TANGDONG</au><au>BAO WANLU</au><au>WANG MENGMENG</au><au>MA XUDONG</au><au>JIA CHUNYUAN</au><au>SU JIANHUA</au><au>ZHANG ZHITAO</au><au>LI ZHONG</au><au>DING XIAOPING</au><au>DING XINJIAN</au><au>MEN GUANGYU</au><au>YAN XIAOPING</au><au>REN LIWEI</au><au>JIA XIAOLONG</au><au>DONG HONGNAN</au><au>WEI LI</au><au>LI RUIJIE</au><au>DONG WEI</au><au>HUI YINGXIN</au><au>LUO TINGCHI</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>High-content coal gasification furnace slag-based green low-carbon cementing material and preparation method thereof</title><date>2023-10-20</date><risdate>2023</risdate><abstract>The invention provides a high-content coal gasification furnace slag-based green low-carbon cementing material and a preparation method thereof, and the method specifically comprises the following steps: burning 50-55% by mass of coal gasification furnace slag at 600-800 DEG C for 30 min, and cooling to room temperature, S2, mixing 50-55% by mass of coal gasification furnace slag after high-temperature burning, 15-20% by mass of slag and 17-20% by mass of gypsum according to a mass ratio of 1: (1-2), and carrying out stirring and mixing to obtain the high-content coal gasification furnace slag-based green low-carbon cementing material. And levigating 5% of furnace slag, 3%-4% of calcium hydroxide and 1%-2% of silica fume, and putting the levigated materials into a stirrer for mixing to obtain the high-content coal gasification furnace slag-based green low-carbon cementing material. The optimal crystalline phase structure of the coal gasification furnace slag is obtained through high-temperature firing tempera</abstract><oa>free_for_read</oa></addata></record> |
fulltext | fulltext_linktorsrc |
identifier | |
ispartof | |
issn | |
language | chi ; eng |
recordid | cdi_epo_espacenet_CN116903274A |
source | esp@cenet |
subjects | ARTIFICIAL STONE CEMENTS CERAMICS CHEMISTRY COMPOSITIONS THEREOF, e.g. MORTARS, CONCRETE OR LIKE BUILDINGMATERIALS CONCRETE LIME, MAGNESIA METALLURGY REFRACTORIES SLAG TREATMENT OF NATURAL STONE |
title | High-content coal gasification furnace slag-based green low-carbon cementing material and preparation method thereof |
url | https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-24T06%3A26%3A30IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHANG%20ZITAO&rft.date=2023-10-20&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116903274A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true |