Preparation method of solid solution aging state Ti6Al4V alloy bar/wire

The invention belongs to the technical field of nonferrous metal material processing, and relates to a preparation method of a solid solution aging state Ti6Al4V alloy bar/wire, which comprises the following steps: 1) blank preparation: preparing a Ti6Al4V alloy bar blank with uniform transverse and...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIU XIANGHONG, SHI QI, LOU MEIQI, MA HAN, FENG YONG, WANG KAIXUAN, FU HANGTAO, DU YUXUAN, SUN XIAOPING, LI SHAOQIANG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LIU XIANGHONG
SHI QI
LOU MEIQI
MA HAN
FENG YONG
WANG KAIXUAN
FU HANGTAO
DU YUXUAN
SUN XIAOPING
LI SHAOQIANG
description The invention belongs to the technical field of nonferrous metal material processing, and relates to a preparation method of a solid solution aging state Ti6Al4V alloy bar/wire, which comprises the following steps: 1) blank preparation: preparing a Ti6Al4V alloy bar blank with uniform transverse and longitudinal tissues; (2) solution treatment is conducted, specifically, the Ti6Al4V alloy bar billet obtained in the step (1) is placed in a heat treatment furnace to be heated and subjected to heat preservation, and solution treatment and water quenching treatment are conducted; (3) aging treatment is conducted, specifically, the Ti6Al4V alloy bar blank obtained after solution treatment is placed in a heat treatment furnace to be heated and subjected to heat preservation, and aging treatment is conducted; and (4) straightening and finishing treatment is conducted, specifically, the Ti6Al4V alloy bar blank treated in the step (3) is heated, straightened and finished into a finished bar/wire, the performance of th
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116815090A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116815090A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116815090A3</originalsourceid><addsrcrecordid>eNrjZHAPKEotSCxKLMnMz1PITS3JyE9RyE9TKM7PyUwBkaVgicT0zLx0heKSxJJUhZBMM8cckzCFxJyc_EqFpMQi_fLMolQeBta0xJziVF4ozc2g6OYa4uyhm1qQH59aXJCYnJqXWhLv7GdoaGZhaGpgaeBoTIwaADCsM0w</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Preparation method of solid solution aging state Ti6Al4V alloy bar/wire</title><source>esp@cenet</source><creator>LIU XIANGHONG ; SHI QI ; LOU MEIQI ; MA HAN ; FENG YONG ; WANG KAIXUAN ; FU HANGTAO ; DU YUXUAN ; SUN XIAOPING ; LI SHAOQIANG</creator><creatorcontrib>LIU XIANGHONG ; SHI QI ; LOU MEIQI ; MA HAN ; FENG YONG ; WANG KAIXUAN ; FU HANGTAO ; DU YUXUAN ; SUN XIAOPING ; LI SHAOQIANG</creatorcontrib><description>The invention belongs to the technical field of nonferrous metal material processing, and relates to a preparation method of a solid solution aging state Ti6Al4V alloy bar/wire, which comprises the following steps: 1) blank preparation: preparing a Ti6Al4V alloy bar blank with uniform transverse and longitudinal tissues; (2) solution treatment is conducted, specifically, the Ti6Al4V alloy bar billet obtained in the step (1) is placed in a heat treatment furnace to be heated and subjected to heat preservation, and solution treatment and water quenching treatment are conducted; (3) aging treatment is conducted, specifically, the Ti6Al4V alloy bar blank obtained after solution treatment is placed in a heat treatment furnace to be heated and subjected to heat preservation, and aging treatment is conducted; and (4) straightening and finishing treatment is conducted, specifically, the Ti6Al4V alloy bar blank treated in the step (3) is heated, straightened and finished into a finished bar/wire, the performance of th</description><language>chi ; eng</language><subject>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230929&amp;DB=EPODOC&amp;CC=CN&amp;NR=116815090A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,776,881,25543,76293</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230929&amp;DB=EPODOC&amp;CC=CN&amp;NR=116815090A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIU XIANGHONG</creatorcontrib><creatorcontrib>SHI QI</creatorcontrib><creatorcontrib>LOU MEIQI</creatorcontrib><creatorcontrib>MA HAN</creatorcontrib><creatorcontrib>FENG YONG</creatorcontrib><creatorcontrib>WANG KAIXUAN</creatorcontrib><creatorcontrib>FU HANGTAO</creatorcontrib><creatorcontrib>DU YUXUAN</creatorcontrib><creatorcontrib>SUN XIAOPING</creatorcontrib><creatorcontrib>LI SHAOQIANG</creatorcontrib><title>Preparation method of solid solution aging state Ti6Al4V alloy bar/wire</title><description>The invention belongs to the technical field of nonferrous metal material processing, and relates to a preparation method of a solid solution aging state Ti6Al4V alloy bar/wire, which comprises the following steps: 1) blank preparation: preparing a Ti6Al4V alloy bar blank with uniform transverse and longitudinal tissues; (2) solution treatment is conducted, specifically, the Ti6Al4V alloy bar billet obtained in the step (1) is placed in a heat treatment furnace to be heated and subjected to heat preservation, and solution treatment and water quenching treatment are conducted; (3) aging treatment is conducted, specifically, the Ti6Al4V alloy bar blank obtained after solution treatment is placed in a heat treatment furnace to be heated and subjected to heat preservation, and aging treatment is conducted; and (4) straightening and finishing treatment is conducted, specifically, the Ti6Al4V alloy bar blank treated in the step (3) is heated, straightened and finished into a finished bar/wire, the performance of th</description><subject>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHAPKEotSCxKLMnMz1PITS3JyE9RyE9TKM7PyUwBkaVgicT0zLx0heKSxJJUhZBMM8cckzCFxJyc_EqFpMQi_fLMolQeBta0xJziVF4ozc2g6OYa4uyhm1qQH59aXJCYnJqXWhLv7GdoaGZhaGpgaeBoTIwaADCsM0w</recordid><startdate>20230929</startdate><enddate>20230929</enddate><creator>LIU XIANGHONG</creator><creator>SHI QI</creator><creator>LOU MEIQI</creator><creator>MA HAN</creator><creator>FENG YONG</creator><creator>WANG KAIXUAN</creator><creator>FU HANGTAO</creator><creator>DU YUXUAN</creator><creator>SUN XIAOPING</creator><creator>LI SHAOQIANG</creator><scope>EVB</scope></search><sort><creationdate>20230929</creationdate><title>Preparation method of solid solution aging state Ti6Al4V alloy bar/wire</title><author>LIU XIANGHONG ; SHI QI ; LOU MEIQI ; MA HAN ; FENG YONG ; WANG KAIXUAN ; FU HANGTAO ; DU YUXUAN ; SUN XIAOPING ; LI SHAOQIANG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116815090A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>LIU XIANGHONG</creatorcontrib><creatorcontrib>SHI QI</creatorcontrib><creatorcontrib>LOU MEIQI</creatorcontrib><creatorcontrib>MA HAN</creatorcontrib><creatorcontrib>FENG YONG</creatorcontrib><creatorcontrib>WANG KAIXUAN</creatorcontrib><creatorcontrib>FU HANGTAO</creatorcontrib><creatorcontrib>DU YUXUAN</creatorcontrib><creatorcontrib>SUN XIAOPING</creatorcontrib><creatorcontrib>LI SHAOQIANG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIU XIANGHONG</au><au>SHI QI</au><au>LOU MEIQI</au><au>MA HAN</au><au>FENG YONG</au><au>WANG KAIXUAN</au><au>FU HANGTAO</au><au>DU YUXUAN</au><au>SUN XIAOPING</au><au>LI SHAOQIANG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Preparation method of solid solution aging state Ti6Al4V alloy bar/wire</title><date>2023-09-29</date><risdate>2023</risdate><abstract>The invention belongs to the technical field of nonferrous metal material processing, and relates to a preparation method of a solid solution aging state Ti6Al4V alloy bar/wire, which comprises the following steps: 1) blank preparation: preparing a Ti6Al4V alloy bar blank with uniform transverse and longitudinal tissues; (2) solution treatment is conducted, specifically, the Ti6Al4V alloy bar billet obtained in the step (1) is placed in a heat treatment furnace to be heated and subjected to heat preservation, and solution treatment and water quenching treatment are conducted; (3) aging treatment is conducted, specifically, the Ti6Al4V alloy bar blank obtained after solution treatment is placed in a heat treatment furnace to be heated and subjected to heat preservation, and aging treatment is conducted; and (4) straightening and finishing treatment is conducted, specifically, the Ti6Al4V alloy bar blank treated in the step (3) is heated, straightened and finished into a finished bar/wire, the performance of th</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116815090A
source esp@cenet
subjects CHANGING THE PHYSICAL STRUCTURE OF NON-FERROUS METALS ANDNON-FERROUS ALLOYS
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title Preparation method of solid solution aging state Ti6Al4V alloy bar/wire
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-24T23%3A04%3A57IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIU%20XIANGHONG&rft.date=2023-09-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116815090A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true