Control method for full decarburization of silicon spring flat steel

The invention provides a control method for full decarburization of silicon spring flat steel, which comprises the following steps of: performing mechanical shot blasting on a continuous casting billet before heating in a furnace to remove surface oxide scale, quickly heating in the furnace at high...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LI GUOXIANG, LI GUOWANG, WU MING, YANG DONGOU, WANG YUFENG, LI WEIHAI, QIAO DONGFAN, YUAN CHANGBO, ZHU LEI, JIANG CHAO, HOU SHIYAO
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LI GUOXIANG
LI GUOWANG
WU MING
YANG DONGOU
WANG YUFENG
LI WEIHAI
QIAO DONGFAN
YUAN CHANGBO
ZHU LEI
JIANG CHAO
HOU SHIYAO
description The invention provides a control method for full decarburization of silicon spring flat steel, which comprises the following steps of: performing mechanical shot blasting on a continuous casting billet before heating in a furnace to remove surface oxide scale, quickly heating in the furnace at high temperature in an oxidizing atmosphere, respectively descaling by using high-pressure water before and after rough rolling in a rolling process, quickly passing through a structure transformation two-phase region after finish rolling, and continuously rolling to obtain the silicon spring flat steel. Burners of the heating section I and the heating section II are both closed, the temperature of the heating section III is 1250 +/-20 DEG C, and the temperature of the soaking section is 1240 +/-20 DEG C; the total time for the continuous casting billet to enter and exit from the heating furnace is less than or equal to 95 minutes, and the total heating time in the heating section III and the soaking section is controll
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116790860A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116790860A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116790860A3</originalsourceid><addsrcrecordid>eNrjZHBxzs8rKcrPUchNLcnIT1FIyy9SSCvNyVFISU1OLEoqLcqsSizJzM9TyE9TKM7MyUwGMosLijLz0hXSchJLFIpLUlNzeBhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoaGZuaWBhZmBozExagDVoTMW</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Control method for full decarburization of silicon spring flat steel</title><source>esp@cenet</source><creator>LI GUOXIANG ; LI GUOWANG ; WU MING ; YANG DONGOU ; WANG YUFENG ; LI WEIHAI ; QIAO DONGFAN ; YUAN CHANGBO ; ZHU LEI ; JIANG CHAO ; HOU SHIYAO</creator><creatorcontrib>LI GUOXIANG ; LI GUOWANG ; WU MING ; YANG DONGOU ; WANG YUFENG ; LI WEIHAI ; QIAO DONGFAN ; YUAN CHANGBO ; ZHU LEI ; JIANG CHAO ; HOU SHIYAO</creatorcontrib><description>The invention provides a control method for full decarburization of silicon spring flat steel, which comprises the following steps of: performing mechanical shot blasting on a continuous casting billet before heating in a furnace to remove surface oxide scale, quickly heating in the furnace at high temperature in an oxidizing atmosphere, respectively descaling by using high-pressure water before and after rough rolling in a rolling process, quickly passing through a structure transformation two-phase region after finish rolling, and continuously rolling to obtain the silicon spring flat steel. Burners of the heating section I and the heating section II are both closed, the temperature of the heating section III is 1250 +/-20 DEG C, and the temperature of the soaking section is 1240 +/-20 DEG C; the total time for the continuous casting billet to enter and exit from the heating furnace is less than or equal to 95 minutes, and the total heating time in the heating section III and the soaking section is controll</description><language>chi ; eng</language><subject>CHEMISTRY ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230922&amp;DB=EPODOC&amp;CC=CN&amp;NR=116790860A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230922&amp;DB=EPODOC&amp;CC=CN&amp;NR=116790860A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LI GUOXIANG</creatorcontrib><creatorcontrib>LI GUOWANG</creatorcontrib><creatorcontrib>WU MING</creatorcontrib><creatorcontrib>YANG DONGOU</creatorcontrib><creatorcontrib>WANG YUFENG</creatorcontrib><creatorcontrib>LI WEIHAI</creatorcontrib><creatorcontrib>QIAO DONGFAN</creatorcontrib><creatorcontrib>YUAN CHANGBO</creatorcontrib><creatorcontrib>ZHU LEI</creatorcontrib><creatorcontrib>JIANG CHAO</creatorcontrib><creatorcontrib>HOU SHIYAO</creatorcontrib><title>Control method for full decarburization of silicon spring flat steel</title><description>The invention provides a control method for full decarburization of silicon spring flat steel, which comprises the following steps of: performing mechanical shot blasting on a continuous casting billet before heating in a furnace to remove surface oxide scale, quickly heating in the furnace at high temperature in an oxidizing atmosphere, respectively descaling by using high-pressure water before and after rough rolling in a rolling process, quickly passing through a structure transformation two-phase region after finish rolling, and continuously rolling to obtain the silicon spring flat steel. Burners of the heating section I and the heating section II are both closed, the temperature of the heating section III is 1250 +/-20 DEG C, and the temperature of the soaking section is 1240 +/-20 DEG C; the total time for the continuous casting billet to enter and exit from the heating furnace is less than or equal to 95 minutes, and the total heating time in the heating section III and the soaking section is controll</description><subject>CHEMISTRY</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZHBxzs8rKcrPUchNLcnIT1FIyy9SSCvNyVFISU1OLEoqLcqsSizJzM9TyE9TKM7MyUwGMosLijLz0hXSchJLFIpLUlNzeBhY0xJzilN5oTQ3g6Kba4izh25qQX58anFBYnJqXmpJvLOfoaGZuaWBhZmBozExagDVoTMW</recordid><startdate>20230922</startdate><enddate>20230922</enddate><creator>LI GUOXIANG</creator><creator>LI GUOWANG</creator><creator>WU MING</creator><creator>YANG DONGOU</creator><creator>WANG YUFENG</creator><creator>LI WEIHAI</creator><creator>QIAO DONGFAN</creator><creator>YUAN CHANGBO</creator><creator>ZHU LEI</creator><creator>JIANG CHAO</creator><creator>HOU SHIYAO</creator><scope>EVB</scope></search><sort><creationdate>20230922</creationdate><title>Control method for full decarburization of silicon spring flat steel</title><author>LI GUOXIANG ; LI GUOWANG ; WU MING ; YANG DONGOU ; WANG YUFENG ; LI WEIHAI ; QIAO DONGFAN ; YUAN CHANGBO ; ZHU LEI ; JIANG CHAO ; HOU SHIYAO</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116790860A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CHEMISTRY</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>LI GUOXIANG</creatorcontrib><creatorcontrib>LI GUOWANG</creatorcontrib><creatorcontrib>WU MING</creatorcontrib><creatorcontrib>YANG DONGOU</creatorcontrib><creatorcontrib>WANG YUFENG</creatorcontrib><creatorcontrib>LI WEIHAI</creatorcontrib><creatorcontrib>QIAO DONGFAN</creatorcontrib><creatorcontrib>YUAN CHANGBO</creatorcontrib><creatorcontrib>ZHU LEI</creatorcontrib><creatorcontrib>JIANG CHAO</creatorcontrib><creatorcontrib>HOU SHIYAO</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LI GUOXIANG</au><au>LI GUOWANG</au><au>WU MING</au><au>YANG DONGOU</au><au>WANG YUFENG</au><au>LI WEIHAI</au><au>QIAO DONGFAN</au><au>YUAN CHANGBO</au><au>ZHU LEI</au><au>JIANG CHAO</au><au>HOU SHIYAO</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Control method for full decarburization of silicon spring flat steel</title><date>2023-09-22</date><risdate>2023</risdate><abstract>The invention provides a control method for full decarburization of silicon spring flat steel, which comprises the following steps of: performing mechanical shot blasting on a continuous casting billet before heating in a furnace to remove surface oxide scale, quickly heating in the furnace at high temperature in an oxidizing atmosphere, respectively descaling by using high-pressure water before and after rough rolling in a rolling process, quickly passing through a structure transformation two-phase region after finish rolling, and continuously rolling to obtain the silicon spring flat steel. Burners of the heating section I and the heating section II are both closed, the temperature of the heating section III is 1250 +/-20 DEG C, and the temperature of the soaking section is 1240 +/-20 DEG C; the total time for the continuous casting billet to enter and exit from the heating furnace is less than or equal to 95 minutes, and the total heating time in the heating section III and the soaking section is controll</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116790860A
source esp@cenet
subjects CHEMISTRY
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
title Control method for full decarburization of silicon spring flat steel
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-07T07%3A40%3A52IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LI%20GUOXIANG&rft.date=2023-09-22&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116790860A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true