Wave-shifting optical fiber reverse mode method

The invention discloses a wave-shifting optical fiber reverse molding method. The method comprises the following steps: step 1, preparing a pouring sealant; 2, eliminating bubbles in the pouring sealant; 3, pouring the de-foamed pouring sealant into a first mold bottom plate; 4, a plastic scintillat...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: ZHANG KAIJUN, HU ZHUO, LIU SIWEI, RUN GUOWEI, LI JIANGLONG, HAN HAN, HE XUNSHE, WANG HONGTAO, YANG ZHENGYU
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator ZHANG KAIJUN
HU ZHUO
LIU SIWEI
RUN GUOWEI
LI JIANGLONG
HAN HAN
HE XUNSHE
WANG HONGTAO
YANG ZHENGYU
description The invention discloses a wave-shifting optical fiber reverse molding method. The method comprises the following steps: step 1, preparing a pouring sealant; 2, eliminating bubbles in the pouring sealant; 3, pouring the de-foamed pouring sealant into a first mold bottom plate; 4, a plastic scintillator is arranged on the surface of the pouring sealant after mold reversing; 5, drying; 6, demolding, wherein a groove is formed in the surface of the demolded pouring sealant under the action of the first mold bottom plate; 7, embedding the wave-shifting optical fiber with the fixed length into the groove in the surface of the cured pouring sealant; 8, secondary glue preparation and defoaming; ninthly, the pouring sealant in the seventh step and the wave-shifting optical fiber assembly are loaded into a second mold bottom plate; 10, pouring the pouring sealant in the step 8 into a second mold bottom plate; eleventhly, secondary drying and demolding are conducted. The method is simple in step, reasonable in design, c
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116714155A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116714155A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116714155A3</originalsourceid><addsrcrecordid>eNrjZNAPTyxL1S3OyEwrycxLV8gvKMlMTsxRSMtMSi1SKEotSy0qTlXIzU8BEqklGfkpPAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMTk1L7Uk3tnP0NDM3NDE0NTU0ZgYNQAtlSrm</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Wave-shifting optical fiber reverse mode method</title><source>esp@cenet</source><creator>ZHANG KAIJUN ; HU ZHUO ; LIU SIWEI ; RUN GUOWEI ; LI JIANGLONG ; HAN HAN ; HE XUNSHE ; WANG HONGTAO ; YANG ZHENGYU</creator><creatorcontrib>ZHANG KAIJUN ; HU ZHUO ; LIU SIWEI ; RUN GUOWEI ; LI JIANGLONG ; HAN HAN ; HE XUNSHE ; WANG HONGTAO ; YANG ZHENGYU</creatorcontrib><description>The invention discloses a wave-shifting optical fiber reverse molding method. The method comprises the following steps: step 1, preparing a pouring sealant; 2, eliminating bubbles in the pouring sealant; 3, pouring the de-foamed pouring sealant into a first mold bottom plate; 4, a plastic scintillator is arranged on the surface of the pouring sealant after mold reversing; 5, drying; 6, demolding, wherein a groove is formed in the surface of the demolded pouring sealant under the action of the first mold bottom plate; 7, embedding the wave-shifting optical fiber with the fixed length into the groove in the surface of the cured pouring sealant; 8, secondary glue preparation and defoaming; ninthly, the pouring sealant in the seventh step and the wave-shifting optical fiber assembly are loaded into a second mold bottom plate; 10, pouring the pouring sealant in the step 8 into a second mold bottom plate; eleventhly, secondary drying and demolding are conducted. The method is simple in step, reasonable in design, c</description><language>chi ; eng</language><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING ; INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES ; PERFORMING OPERATIONS ; SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR ; SHAPING OR JOINING OF PLASTICS ; TRANSPORTING ; WORKING OF PLASTICS ; WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230908&amp;DB=EPODOC&amp;CC=CN&amp;NR=116714155A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25564,76547</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230908&amp;DB=EPODOC&amp;CC=CN&amp;NR=116714155A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>ZHANG KAIJUN</creatorcontrib><creatorcontrib>HU ZHUO</creatorcontrib><creatorcontrib>LIU SIWEI</creatorcontrib><creatorcontrib>RUN GUOWEI</creatorcontrib><creatorcontrib>LI JIANGLONG</creatorcontrib><creatorcontrib>HAN HAN</creatorcontrib><creatorcontrib>HE XUNSHE</creatorcontrib><creatorcontrib>WANG HONGTAO</creatorcontrib><creatorcontrib>YANG ZHENGYU</creatorcontrib><title>Wave-shifting optical fiber reverse mode method</title><description>The invention discloses a wave-shifting optical fiber reverse molding method. The method comprises the following steps: step 1, preparing a pouring sealant; 2, eliminating bubbles in the pouring sealant; 3, pouring the de-foamed pouring sealant into a first mold bottom plate; 4, a plastic scintillator is arranged on the surface of the pouring sealant after mold reversing; 5, drying; 6, demolding, wherein a groove is formed in the surface of the demolded pouring sealant under the action of the first mold bottom plate; 7, embedding the wave-shifting optical fiber with the fixed length into the groove in the surface of the cured pouring sealant; 8, secondary glue preparation and defoaming; ninthly, the pouring sealant in the seventh step and the wave-shifting optical fiber assembly are loaded into a second mold bottom plate; 10, pouring the pouring sealant in the step 8 into a second mold bottom plate; eleventhly, secondary drying and demolding are conducted. The method is simple in step, reasonable in design, c</description><subject>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</subject><subject>INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES</subject><subject>PERFORMING OPERATIONS</subject><subject>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</subject><subject>SHAPING OR JOINING OF PLASTICS</subject><subject>TRANSPORTING</subject><subject>WORKING OF PLASTICS</subject><subject>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNrjZNAPTyxL1S3OyEwrycxLV8gvKMlMTsxRSMtMSi1SKEotSy0qTlXIzU8BEqklGfkpPAysaYk5xam8UJqbQdHNNcTZQze1ID8-tbggMTk1L7Uk3tnP0NDM3NDE0NTU0ZgYNQAtlSrm</recordid><startdate>20230908</startdate><enddate>20230908</enddate><creator>ZHANG KAIJUN</creator><creator>HU ZHUO</creator><creator>LIU SIWEI</creator><creator>RUN GUOWEI</creator><creator>LI JIANGLONG</creator><creator>HAN HAN</creator><creator>HE XUNSHE</creator><creator>WANG HONGTAO</creator><creator>YANG ZHENGYU</creator><scope>EVB</scope></search><sort><creationdate>20230908</creationdate><title>Wave-shifting optical fiber reverse mode method</title><author>ZHANG KAIJUN ; HU ZHUO ; LIU SIWEI ; RUN GUOWEI ; LI JIANGLONG ; HAN HAN ; HE XUNSHE ; WANG HONGTAO ; YANG ZHENGYU</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116714155A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING</topic><topic>INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES</topic><topic>PERFORMING OPERATIONS</topic><topic>SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR</topic><topic>SHAPING OR JOINING OF PLASTICS</topic><topic>TRANSPORTING</topic><topic>WORKING OF PLASTICS</topic><topic>WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL</topic><toplevel>online_resources</toplevel><creatorcontrib>ZHANG KAIJUN</creatorcontrib><creatorcontrib>HU ZHUO</creatorcontrib><creatorcontrib>LIU SIWEI</creatorcontrib><creatorcontrib>RUN GUOWEI</creatorcontrib><creatorcontrib>LI JIANGLONG</creatorcontrib><creatorcontrib>HAN HAN</creatorcontrib><creatorcontrib>HE XUNSHE</creatorcontrib><creatorcontrib>WANG HONGTAO</creatorcontrib><creatorcontrib>YANG ZHENGYU</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>ZHANG KAIJUN</au><au>HU ZHUO</au><au>LIU SIWEI</au><au>RUN GUOWEI</au><au>LI JIANGLONG</au><au>HAN HAN</au><au>HE XUNSHE</au><au>WANG HONGTAO</au><au>YANG ZHENGYU</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Wave-shifting optical fiber reverse mode method</title><date>2023-09-08</date><risdate>2023</risdate><abstract>The invention discloses a wave-shifting optical fiber reverse molding method. The method comprises the following steps: step 1, preparing a pouring sealant; 2, eliminating bubbles in the pouring sealant; 3, pouring the de-foamed pouring sealant into a first mold bottom plate; 4, a plastic scintillator is arranged on the surface of the pouring sealant after mold reversing; 5, drying; 6, demolding, wherein a groove is formed in the surface of the demolded pouring sealant under the action of the first mold bottom plate; 7, embedding the wave-shifting optical fiber with the fixed length into the groove in the surface of the cured pouring sealant; 8, secondary glue preparation and defoaming; ninthly, the pouring sealant in the seventh step and the wave-shifting optical fiber assembly are loaded into a second mold bottom plate; 10, pouring the pouring sealant in the step 8 into a second mold bottom plate; eleventhly, secondary drying and demolding are conducted. The method is simple in step, reasonable in design, c</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116714155A
source esp@cenet
subjects AFTER-TREATMENT OF THE SHAPED PRODUCTS, e.g. REPAIRING
INDEXING SCHEME ASSOCIATED WITH SUBCLASS B29C, RELATING TO PARTICULARARTICLES
PERFORMING OPERATIONS
SHAPING OF MATERIAL IN A PLASTIC STATE, NOT OTHERWISE PROVIDEDFOR
SHAPING OR JOINING OF PLASTICS
TRANSPORTING
WORKING OF PLASTICS
WORKING OF SUBSTANCES IN A PLASTIC STATE, IN GENERAL
title Wave-shifting optical fiber reverse mode method
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2024-12-29T01%3A25%3A40IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=ZHANG%20KAIJUN&rft.date=2023-09-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116714155A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true