Production method for avoiding uneven surface color of cutter steel hot-rolled plate

The invention relates to a production method for avoiding uneven surface color of a cutter steel hot-rolled plate. The process comprises the steps of smelting, continuous casting, hot rolling and cold rolling pickling. The method comprises the following steps: 1) adjusting the water spraying amount...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: LIANG JIANHUN, FANG JIANFENG, LUO JIE, LIN JIE, XIE SHUIWANG, BANG GUN, HUANG WEIWEN
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator LIANG JIANHUN
FANG JIANFENG
LUO JIE
LIN JIE
XIE SHUIWANG
BANG GUN
HUANG WEIWEN
description The invention relates to a production method for avoiding uneven surface color of a cutter steel hot-rolled plate. The process comprises the steps of smelting, continuous casting, hot rolling and cold rolling pickling. The method comprises the following steps: 1) adjusting the water spraying amount of a water spraying header at the upper part of a hot-rolled layer cold area to be large in middle and small in two sides; cleaning impurities on the surface of the steel belt by using a reverse spraying device; (2) the cold water conductivity of a hot rolling layer is smaller than 650 microseconds, and the chlorate concentration is smaller than or equal to 70 g/L; (3) cover annealing is conducted after hot rolling, gas is continuously purged before the temperature is increased to 650 DEG C, and the purge time is longer than 3 h; and 4) cold rolling pickling, wherein pickling solution concentration and pickling temperature are controlled. By adjusting the use standard of the cooling water and the water amount of th
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116713320A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116713320A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116713320A3</originalsourceid><addsrcrecordid>eNqNjLEKwjAURbM4iPoPzw8oGAs6l6I4iUP3EpIbG4h5JXnp99vBD3A6wzmcrRpemV21EjjRBzKxI8-ZzMLBhfSmmrAgUanZGwuyHFfLnmwVQaYiQKSJpckcIxzN0Qj2auNNLDj8uFPH-23oHw1mHlHm9ZQgY__U-nLVbXs-de0_zRfC5Tj9</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Production method for avoiding uneven surface color of cutter steel hot-rolled plate</title><source>esp@cenet</source><creator>LIANG JIANHUN ; FANG JIANFENG ; LUO JIE ; LIN JIE ; XIE SHUIWANG ; BANG GUN ; HUANG WEIWEN</creator><creatorcontrib>LIANG JIANHUN ; FANG JIANFENG ; LUO JIE ; LIN JIE ; XIE SHUIWANG ; BANG GUN ; HUANG WEIWEN</creatorcontrib><description>The invention relates to a production method for avoiding uneven surface color of a cutter steel hot-rolled plate. The process comprises the steps of smelting, continuous casting, hot rolling and cold rolling pickling. The method comprises the following steps: 1) adjusting the water spraying amount of a water spraying header at the upper part of a hot-rolled layer cold area to be large in middle and small in two sides; cleaning impurities on the surface of the steel belt by using a reverse spraying device; (2) the cold water conductivity of a hot rolling layer is smaller than 650 microseconds, and the chlorate concentration is smaller than or equal to 70 g/L; (3) cover annealing is conducted after hot rolling, gas is continuously purged before the temperature is increased to 650 DEG C, and the purge time is longer than 3 h; and 4) cold rolling pickling, wherein pickling solution concentration and pickling temperature are controlled. By adjusting the use standard of the cooling water and the water amount of th</description><language>chi ; eng</language><subject>CHEMICAL SURFACE TREATMENT ; CHEMISTRY ; CLEANING OR DEGREASING OF METALLIC MATERIAL BY CHEMICALMETHODS OTHER THAN ELECTROLYSIS ; COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATIONOR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL ; COATING MATERIAL WITH METALLIC MATERIAL ; COATING METALLIC MATERIAL ; DIFFUSION TREATMENT OF METALLIC MATERIAL ; GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS ; INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION INGENERAL ; MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS ; MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL ; METALLURGY ; METALLURGY OF IRON ; MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS ; PERFORMING OPERATIONS ; PUNCHING METAL ; ROLLING OF METAL ; TRANSPORTING</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230908&amp;DB=EPODOC&amp;CC=CN&amp;NR=116713320A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230908&amp;DB=EPODOC&amp;CC=CN&amp;NR=116713320A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>LIANG JIANHUN</creatorcontrib><creatorcontrib>FANG JIANFENG</creatorcontrib><creatorcontrib>LUO JIE</creatorcontrib><creatorcontrib>LIN JIE</creatorcontrib><creatorcontrib>XIE SHUIWANG</creatorcontrib><creatorcontrib>BANG GUN</creatorcontrib><creatorcontrib>HUANG WEIWEN</creatorcontrib><title>Production method for avoiding uneven surface color of cutter steel hot-rolled plate</title><description>The invention relates to a production method for avoiding uneven surface color of a cutter steel hot-rolled plate. The process comprises the steps of smelting, continuous casting, hot rolling and cold rolling pickling. The method comprises the following steps: 1) adjusting the water spraying amount of a water spraying header at the upper part of a hot-rolled layer cold area to be large in middle and small in two sides; cleaning impurities on the surface of the steel belt by using a reverse spraying device; (2) the cold water conductivity of a hot rolling layer is smaller than 650 microseconds, and the chlorate concentration is smaller than or equal to 70 g/L; (3) cover annealing is conducted after hot rolling, gas is continuously purged before the temperature is increased to 650 DEG C, and the purge time is longer than 3 h; and 4) cold rolling pickling, wherein pickling solution concentration and pickling temperature are controlled. By adjusting the use standard of the cooling water and the water amount of th</description><subject>CHEMICAL SURFACE TREATMENT</subject><subject>CHEMISTRY</subject><subject>CLEANING OR DEGREASING OF METALLIC MATERIAL BY CHEMICALMETHODS OTHER THAN ELECTROLYSIS</subject><subject>COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATIONOR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL</subject><subject>COATING MATERIAL WITH METALLIC MATERIAL</subject><subject>COATING METALLIC MATERIAL</subject><subject>DIFFUSION TREATMENT OF METALLIC MATERIAL</subject><subject>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</subject><subject>INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION INGENERAL</subject><subject>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</subject><subject>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</subject><subject>METALLURGY</subject><subject>METALLURGY OF IRON</subject><subject>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</subject><subject>PERFORMING OPERATIONS</subject><subject>PUNCHING METAL</subject><subject>ROLLING OF METAL</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNjLEKwjAURbM4iPoPzw8oGAs6l6I4iUP3EpIbG4h5JXnp99vBD3A6wzmcrRpemV21EjjRBzKxI8-ZzMLBhfSmmrAgUanZGwuyHFfLnmwVQaYiQKSJpckcIxzN0Qj2auNNLDj8uFPH-23oHw1mHlHm9ZQgY__U-nLVbXs-de0_zRfC5Tj9</recordid><startdate>20230908</startdate><enddate>20230908</enddate><creator>LIANG JIANHUN</creator><creator>FANG JIANFENG</creator><creator>LUO JIE</creator><creator>LIN JIE</creator><creator>XIE SHUIWANG</creator><creator>BANG GUN</creator><creator>HUANG WEIWEN</creator><scope>EVB</scope></search><sort><creationdate>20230908</creationdate><title>Production method for avoiding uneven surface color of cutter steel hot-rolled plate</title><author>LIANG JIANHUN ; FANG JIANFENG ; LUO JIE ; LIN JIE ; XIE SHUIWANG ; BANG GUN ; HUANG WEIWEN</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116713320A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CHEMICAL SURFACE TREATMENT</topic><topic>CHEMISTRY</topic><topic>CLEANING OR DEGREASING OF METALLIC MATERIAL BY CHEMICALMETHODS OTHER THAN ELECTROLYSIS</topic><topic>COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATIONOR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL</topic><topic>COATING MATERIAL WITH METALLIC MATERIAL</topic><topic>COATING METALLIC MATERIAL</topic><topic>DIFFUSION TREATMENT OF METALLIC MATERIAL</topic><topic>GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS</topic><topic>INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION INGENERAL</topic><topic>MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS</topic><topic>MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL</topic><topic>METALLURGY</topic><topic>METALLURGY OF IRON</topic><topic>MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS</topic><topic>PERFORMING OPERATIONS</topic><topic>PUNCHING METAL</topic><topic>ROLLING OF METAL</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>LIANG JIANHUN</creatorcontrib><creatorcontrib>FANG JIANFENG</creatorcontrib><creatorcontrib>LUO JIE</creatorcontrib><creatorcontrib>LIN JIE</creatorcontrib><creatorcontrib>XIE SHUIWANG</creatorcontrib><creatorcontrib>BANG GUN</creatorcontrib><creatorcontrib>HUANG WEIWEN</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>LIANG JIANHUN</au><au>FANG JIANFENG</au><au>LUO JIE</au><au>LIN JIE</au><au>XIE SHUIWANG</au><au>BANG GUN</au><au>HUANG WEIWEN</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Production method for avoiding uneven surface color of cutter steel hot-rolled plate</title><date>2023-09-08</date><risdate>2023</risdate><abstract>The invention relates to a production method for avoiding uneven surface color of a cutter steel hot-rolled plate. The process comprises the steps of smelting, continuous casting, hot rolling and cold rolling pickling. The method comprises the following steps: 1) adjusting the water spraying amount of a water spraying header at the upper part of a hot-rolled layer cold area to be large in middle and small in two sides; cleaning impurities on the surface of the steel belt by using a reverse spraying device; (2) the cold water conductivity of a hot rolling layer is smaller than 650 microseconds, and the chlorate concentration is smaller than or equal to 70 g/L; (3) cover annealing is conducted after hot rolling, gas is continuously purged before the temperature is increased to 650 DEG C, and the purge time is longer than 3 h; and 4) cold rolling pickling, wherein pickling solution concentration and pickling temperature are controlled. By adjusting the use standard of the cooling water and the water amount of th</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116713320A
source esp@cenet
subjects CHEMICAL SURFACE TREATMENT
CHEMISTRY
CLEANING OR DEGREASING OF METALLIC MATERIAL BY CHEMICALMETHODS OTHER THAN ELECTROLYSIS
COATING BY VACUUM EVAPORATION, BY SPUTTERING, BY ION IMPLANTATIONOR BY CHEMICAL VAPOUR DEPOSITION, IN GENERAL
COATING MATERIAL WITH METALLIC MATERIAL
COATING METALLIC MATERIAL
DIFFUSION TREATMENT OF METALLIC MATERIAL
GENERAL DEVICES FOR HEAT TREATMENT OF FERROUS OR NON-FERROUSMETALS OR ALLOYS
INHIBITING CORROSION OF METALLIC MATERIAL OR INCRUSTATION INGENERAL
MAKING METAL MALLEABLE BY DECARBURISATION, TEMPERING OR OTHERTREATMENTS
MECHANICAL METAL-WORKING WITHOUT ESSENTIALLY REMOVINGMATERIAL
METALLURGY
METALLURGY OF IRON
MODIFYING THE PHYSICAL STRUCTURE OF FERROUS METALS
PERFORMING OPERATIONS
PUNCHING METAL
ROLLING OF METAL
TRANSPORTING
title Production method for avoiding uneven surface color of cutter steel hot-rolled plate
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T22%3A39%3A33IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=LIANG%20JIANHUN&rft.date=2023-09-08&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116713320A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true