Method for improving internal structure of heavy rail steel by adopting combined electromagnetic stirring

The invention discloses a method for improving the internal structure of heavy rail steel by adopting combined electromagnetic stirring, which comprises the following steps: 1) a square billet continuous casting machine adopts combined stirring of a crystallizer and a solidification tail end, and th...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: DIAO WANGCAI, CHEN JIANXIN, ZHANG DAXIAN, QIAN JINGQIU, HAN CHUNPENG, ZHANG XIAOFENG
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator DIAO WANGCAI
CHEN JIANXIN
ZHANG DAXIAN
QIAN JINGQIU
HAN CHUNPENG
ZHANG XIAOFENG
description The invention discloses a method for improving the internal structure of heavy rail steel by adopting combined electromagnetic stirring, which comprises the following steps: 1) a square billet continuous casting machine adopts combined stirring of a crystallizer and a solidification tail end, and the electromagnetic stirring parameter of the crystallizer is 580A/1.8 Hz; (2) under the conditions that the section is 280 mm * 380 mm and the pulling speed and the superheat degree are the same, the current of a crystallizer is 580 A and 1.8 HZ, the tail end electromagnetic stirring current is 300 A to 450 A, and the frequency is 8 HZ; according to the method for improving the internal structure of the heavy rail steel through combined electromagnetic stirring, the combined electromagnetic stirring, namely, the crystallizer electromagnetic stirring and solidification tail end electromagnetic stirring technology, is adopted, and the tail end electromagnetic stirring current is optimized; the problems of center segre
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116652135A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116652135A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116652135A3</originalsourceid><addsrcrecordid>eNqNyzEOgkAQhWEaC6PeYTyABRLoDdHYaGVPhmWASZadzTCQcHsh8QBWL3n5_n3CL7JeGmhFgYeoMnPogIORBvQwmk7OJiWQFnrCeQFF3n4iD_UC2Ei0LXEy1ByoAfLkTGXALpCxWymrruKY7Fr0I51-e0jOj_unfF4oSkVjREdrUJXvNC2K_Jpm-S37x3wBtv9Bjg</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Method for improving internal structure of heavy rail steel by adopting combined electromagnetic stirring</title><source>esp@cenet</source><creator>DIAO WANGCAI ; CHEN JIANXIN ; ZHANG DAXIAN ; QIAN JINGQIU ; HAN CHUNPENG ; ZHANG XIAOFENG</creator><creatorcontrib>DIAO WANGCAI ; CHEN JIANXIN ; ZHANG DAXIAN ; QIAN JINGQIU ; HAN CHUNPENG ; ZHANG XIAOFENG</creatorcontrib><description>The invention discloses a method for improving the internal structure of heavy rail steel by adopting combined electromagnetic stirring, which comprises the following steps: 1) a square billet continuous casting machine adopts combined stirring of a crystallizer and a solidification tail end, and the electromagnetic stirring parameter of the crystallizer is 580A/1.8 Hz; (2) under the conditions that the section is 280 mm * 380 mm and the pulling speed and the superheat degree are the same, the current of a crystallizer is 580 A and 1.8 HZ, the tail end electromagnetic stirring current is 300 A to 450 A, and the frequency is 8 HZ; according to the method for improving the internal structure of the heavy rail steel through combined electromagnetic stirring, the combined electromagnetic stirring, namely, the crystallizer electromagnetic stirring and solidification tail end electromagnetic stirring technology, is adopted, and the tail end electromagnetic stirring current is optimized; the problems of center segre</description><language>chi ; eng</language><subject>CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES ; MEASURING ; PERFORMING OPERATIONS ; PHYSICS ; POWDER METALLURGY ; TESTING ; TRANSPORTING</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230829&amp;DB=EPODOC&amp;CC=CN&amp;NR=116652135A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,780,885,25563,76418</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230829&amp;DB=EPODOC&amp;CC=CN&amp;NR=116652135A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>DIAO WANGCAI</creatorcontrib><creatorcontrib>CHEN JIANXIN</creatorcontrib><creatorcontrib>ZHANG DAXIAN</creatorcontrib><creatorcontrib>QIAN JINGQIU</creatorcontrib><creatorcontrib>HAN CHUNPENG</creatorcontrib><creatorcontrib>ZHANG XIAOFENG</creatorcontrib><title>Method for improving internal structure of heavy rail steel by adopting combined electromagnetic stirring</title><description>The invention discloses a method for improving the internal structure of heavy rail steel by adopting combined electromagnetic stirring, which comprises the following steps: 1) a square billet continuous casting machine adopts combined stirring of a crystallizer and a solidification tail end, and the electromagnetic stirring parameter of the crystallizer is 580A/1.8 Hz; (2) under the conditions that the section is 280 mm * 380 mm and the pulling speed and the superheat degree are the same, the current of a crystallizer is 580 A and 1.8 HZ, the tail end electromagnetic stirring current is 300 A to 450 A, and the frequency is 8 HZ; according to the method for improving the internal structure of the heavy rail steel through combined electromagnetic stirring, the combined electromagnetic stirring, namely, the crystallizer electromagnetic stirring and solidification tail end electromagnetic stirring technology, is adopted, and the tail end electromagnetic stirring current is optimized; the problems of center segre</description><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES</subject><subject>MEASURING</subject><subject>PERFORMING OPERATIONS</subject><subject>PHYSICS</subject><subject>POWDER METALLURGY</subject><subject>TESTING</subject><subject>TRANSPORTING</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyzEOgkAQhWEaC6PeYTyABRLoDdHYaGVPhmWASZadzTCQcHsh8QBWL3n5_n3CL7JeGmhFgYeoMnPogIORBvQwmk7OJiWQFnrCeQFF3n4iD_UC2Ei0LXEy1ByoAfLkTGXALpCxWymrruKY7Fr0I51-e0jOj_unfF4oSkVjREdrUJXvNC2K_Jpm-S37x3wBtv9Bjg</recordid><startdate>20230829</startdate><enddate>20230829</enddate><creator>DIAO WANGCAI</creator><creator>CHEN JIANXIN</creator><creator>ZHANG DAXIAN</creator><creator>QIAN JINGQIU</creator><creator>HAN CHUNPENG</creator><creator>ZHANG XIAOFENG</creator><scope>EVB</scope></search><sort><creationdate>20230829</creationdate><title>Method for improving internal structure of heavy rail steel by adopting combined electromagnetic stirring</title><author>DIAO WANGCAI ; CHEN JIANXIN ; ZHANG DAXIAN ; QIAN JINGQIU ; HAN CHUNPENG ; ZHANG XIAOFENG</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116652135A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES</topic><topic>MEASURING</topic><topic>PERFORMING OPERATIONS</topic><topic>PHYSICS</topic><topic>POWDER METALLURGY</topic><topic>TESTING</topic><topic>TRANSPORTING</topic><toplevel>online_resources</toplevel><creatorcontrib>DIAO WANGCAI</creatorcontrib><creatorcontrib>CHEN JIANXIN</creatorcontrib><creatorcontrib>ZHANG DAXIAN</creatorcontrib><creatorcontrib>QIAN JINGQIU</creatorcontrib><creatorcontrib>HAN CHUNPENG</creatorcontrib><creatorcontrib>ZHANG XIAOFENG</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>DIAO WANGCAI</au><au>CHEN JIANXIN</au><au>ZHANG DAXIAN</au><au>QIAN JINGQIU</au><au>HAN CHUNPENG</au><au>ZHANG XIAOFENG</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Method for improving internal structure of heavy rail steel by adopting combined electromagnetic stirring</title><date>2023-08-29</date><risdate>2023</risdate><abstract>The invention discloses a method for improving the internal structure of heavy rail steel by adopting combined electromagnetic stirring, which comprises the following steps: 1) a square billet continuous casting machine adopts combined stirring of a crystallizer and a solidification tail end, and the electromagnetic stirring parameter of the crystallizer is 580A/1.8 Hz; (2) under the conditions that the section is 280 mm * 380 mm and the pulling speed and the superheat degree are the same, the current of a crystallizer is 580 A and 1.8 HZ, the tail end electromagnetic stirring current is 300 A to 450 A, and the frequency is 8 HZ; according to the method for improving the internal structure of the heavy rail steel through combined electromagnetic stirring, the combined electromagnetic stirring, namely, the crystallizer electromagnetic stirring and solidification tail end electromagnetic stirring technology, is adopted, and the tail end electromagnetic stirring current is optimized; the problems of center segre</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116652135A
source esp@cenet
subjects CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
INVESTIGATING OR ANALYSING MATERIALS BY DETERMINING THEIRCHEMICAL OR PHYSICAL PROPERTIES
MEASURING
PERFORMING OPERATIONS
PHYSICS
POWDER METALLURGY
TESTING
TRANSPORTING
title Method for improving internal structure of heavy rail steel by adopting combined electromagnetic stirring
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-08T15%3A43%3A14IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=DIAO%20WANGCAI&rft.date=2023-08-29&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116652135A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true