High-temperature alloy GH710 alloy steel ingot for turbine disc and preparation method of high-temperature alloy GH710 alloy steel ingot

According to the high-temperature alloy GH710 alloy steel ingot for the turbine disc and the preparation method of the high-temperature alloy GH710 alloy steel ingot, raw materials comprise a component A and a component B. The component A comprises, by mass, 53%-55% of metal nickel, 17%-19% of metal...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: GAO JINGBAO, PEI BINGHONG, LUO YUANYUAN, WANG RUI, FENG XU, HE YUNHUA
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator GAO JINGBAO
PEI BINGHONG
LUO YUANYUAN
WANG RUI
FENG XU
HE YUNHUA
description According to the high-temperature alloy GH710 alloy steel ingot for the turbine disc and the preparation method of the high-temperature alloy GH710 alloy steel ingot, raw materials comprise a component A and a component B. The component A comprises, by mass, 53%-55% of metal nickel, 17%-19% of metal chromium, 14%-15.5% of metal cobalt, 1.5%-1.9% of metal tungsten, 3%-3.4% of metal molybdenum, 0.06%-0.09% of high-purity graphite blocks and the balance steel. And the component B comprises the following chemical components in percentage by mass: 2.3 to 3.8 percent of metal aluminum, 4.8 to 5.3 percent of sponge titanium, 0.075 to 0.125 percent of ferroboron, 0.05 to 0.15 percent of magnesium alloy and 0.01 to 0.03 percent of metal cerium. According to the method, vacuum induction smelting, protective atmosphere electroslag remelting and vacuum consumable remelting are adopted, the ingot shape is enlarged from phi 305 mm to phi 508 mm, the alloy ingot material rate is increased, the consumable ingot with the maxi
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116516205A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116516205A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116516205A3</originalsourceid><addsrcrecordid>eNqVjDEOwjAQBN1QIOAPxwMixaCEGkWAKyr6yCSb2JLjs2xT8AOeTYo8AKrZYnbW4qPsaIqMKSDq_Iog7Ry_6aZOslx2yoAj60fONHCkWXtaD-pt6kj7nkJE0PPdsqcJ2XBPPJD5q7wVq0G7hN3CjdhfL49GFQjcIgXdwSO3zV3KupL1oazOx1-cLwFBSto</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>High-temperature alloy GH710 alloy steel ingot for turbine disc and preparation method of high-temperature alloy GH710 alloy steel ingot</title><source>esp@cenet</source><creator>GAO JINGBAO ; PEI BINGHONG ; LUO YUANYUAN ; WANG RUI ; FENG XU ; HE YUNHUA</creator><creatorcontrib>GAO JINGBAO ; PEI BINGHONG ; LUO YUANYUAN ; WANG RUI ; FENG XU ; HE YUNHUA</creatorcontrib><description>According to the high-temperature alloy GH710 alloy steel ingot for the turbine disc and the preparation method of the high-temperature alloy GH710 alloy steel ingot, raw materials comprise a component A and a component B. The component A comprises, by mass, 53%-55% of metal nickel, 17%-19% of metal chromium, 14%-15.5% of metal cobalt, 1.5%-1.9% of metal tungsten, 3%-3.4% of metal molybdenum, 0.06%-0.09% of high-purity graphite blocks and the balance steel. And the component B comprises the following chemical components in percentage by mass: 2.3 to 3.8 percent of metal aluminum, 4.8 to 5.3 percent of sponge titanium, 0.075 to 0.125 percent of ferroboron, 0.05 to 0.15 percent of magnesium alloy and 0.01 to 0.03 percent of metal cerium. According to the method, vacuum induction smelting, protective atmosphere electroslag remelting and vacuum consumable remelting are adopted, the ingot shape is enlarged from phi 305 mm to phi 508 mm, the alloy ingot material rate is increased, the consumable ingot with the maxi</description><language>chi ; eng</language><subject>ALLOYS ; CASTING ; CASTING OF METALS ; CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES ; CHEMISTRY ; FERROUS OR NON-FERROUS ALLOYS ; METALLURGY ; PERFORMING OPERATIONS ; POWDER METALLURGY ; PRETREATMENT OF RAW MATERIALS ; PRODUCTION AND REFINING OF METALS ; TRANSPORTING ; TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230801&amp;DB=EPODOC&amp;CC=CN&amp;NR=116516205A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,777,882,25545,76296</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230801&amp;DB=EPODOC&amp;CC=CN&amp;NR=116516205A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>GAO JINGBAO</creatorcontrib><creatorcontrib>PEI BINGHONG</creatorcontrib><creatorcontrib>LUO YUANYUAN</creatorcontrib><creatorcontrib>WANG RUI</creatorcontrib><creatorcontrib>FENG XU</creatorcontrib><creatorcontrib>HE YUNHUA</creatorcontrib><title>High-temperature alloy GH710 alloy steel ingot for turbine disc and preparation method of high-temperature alloy GH710 alloy steel ingot</title><description>According to the high-temperature alloy GH710 alloy steel ingot for the turbine disc and the preparation method of the high-temperature alloy GH710 alloy steel ingot, raw materials comprise a component A and a component B. The component A comprises, by mass, 53%-55% of metal nickel, 17%-19% of metal chromium, 14%-15.5% of metal cobalt, 1.5%-1.9% of metal tungsten, 3%-3.4% of metal molybdenum, 0.06%-0.09% of high-purity graphite blocks and the balance steel. And the component B comprises the following chemical components in percentage by mass: 2.3 to 3.8 percent of metal aluminum, 4.8 to 5.3 percent of sponge titanium, 0.075 to 0.125 percent of ferroboron, 0.05 to 0.15 percent of magnesium alloy and 0.01 to 0.03 percent of metal cerium. According to the method, vacuum induction smelting, protective atmosphere electroslag remelting and vacuum consumable remelting are adopted, the ingot shape is enlarged from phi 305 mm to phi 508 mm, the alloy ingot material rate is increased, the consumable ingot with the maxi</description><subject>ALLOYS</subject><subject>CASTING</subject><subject>CASTING OF METALS</subject><subject>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</subject><subject>CHEMISTRY</subject><subject>FERROUS OR NON-FERROUS ALLOYS</subject><subject>METALLURGY</subject><subject>PERFORMING OPERATIONS</subject><subject>POWDER METALLURGY</subject><subject>PRETREATMENT OF RAW MATERIALS</subject><subject>PRODUCTION AND REFINING OF METALS</subject><subject>TRANSPORTING</subject><subject>TREATMENT OF ALLOYS OR NON-FERROUS METALS</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqVjDEOwjAQBN1QIOAPxwMixaCEGkWAKyr6yCSb2JLjs2xT8AOeTYo8AKrZYnbW4qPsaIqMKSDq_Iog7Ry_6aZOslx2yoAj60fONHCkWXtaD-pt6kj7nkJE0PPdsqcJ2XBPPJD5q7wVq0G7hN3CjdhfL49GFQjcIgXdwSO3zV3KupL1oazOx1-cLwFBSto</recordid><startdate>20230801</startdate><enddate>20230801</enddate><creator>GAO JINGBAO</creator><creator>PEI BINGHONG</creator><creator>LUO YUANYUAN</creator><creator>WANG RUI</creator><creator>FENG XU</creator><creator>HE YUNHUA</creator><scope>EVB</scope></search><sort><creationdate>20230801</creationdate><title>High-temperature alloy GH710 alloy steel ingot for turbine disc and preparation method of high-temperature alloy GH710 alloy steel ingot</title><author>GAO JINGBAO ; PEI BINGHONG ; LUO YUANYUAN ; WANG RUI ; FENG XU ; HE YUNHUA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116516205A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>ALLOYS</topic><topic>CASTING</topic><topic>CASTING OF METALS</topic><topic>CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES</topic><topic>CHEMISTRY</topic><topic>FERROUS OR NON-FERROUS ALLOYS</topic><topic>METALLURGY</topic><topic>PERFORMING OPERATIONS</topic><topic>POWDER METALLURGY</topic><topic>PRETREATMENT OF RAW MATERIALS</topic><topic>PRODUCTION AND REFINING OF METALS</topic><topic>TRANSPORTING</topic><topic>TREATMENT OF ALLOYS OR NON-FERROUS METALS</topic><toplevel>online_resources</toplevel><creatorcontrib>GAO JINGBAO</creatorcontrib><creatorcontrib>PEI BINGHONG</creatorcontrib><creatorcontrib>LUO YUANYUAN</creatorcontrib><creatorcontrib>WANG RUI</creatorcontrib><creatorcontrib>FENG XU</creatorcontrib><creatorcontrib>HE YUNHUA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>GAO JINGBAO</au><au>PEI BINGHONG</au><au>LUO YUANYUAN</au><au>WANG RUI</au><au>FENG XU</au><au>HE YUNHUA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>High-temperature alloy GH710 alloy steel ingot for turbine disc and preparation method of high-temperature alloy GH710 alloy steel ingot</title><date>2023-08-01</date><risdate>2023</risdate><abstract>According to the high-temperature alloy GH710 alloy steel ingot for the turbine disc and the preparation method of the high-temperature alloy GH710 alloy steel ingot, raw materials comprise a component A and a component B. The component A comprises, by mass, 53%-55% of metal nickel, 17%-19% of metal chromium, 14%-15.5% of metal cobalt, 1.5%-1.9% of metal tungsten, 3%-3.4% of metal molybdenum, 0.06%-0.09% of high-purity graphite blocks and the balance steel. And the component B comprises the following chemical components in percentage by mass: 2.3 to 3.8 percent of metal aluminum, 4.8 to 5.3 percent of sponge titanium, 0.075 to 0.125 percent of ferroboron, 0.05 to 0.15 percent of magnesium alloy and 0.01 to 0.03 percent of metal cerium. According to the method, vacuum induction smelting, protective atmosphere electroslag remelting and vacuum consumable remelting are adopted, the ingot shape is enlarged from phi 305 mm to phi 508 mm, the alloy ingot material rate is increased, the consumable ingot with the maxi</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116516205A
source esp@cenet
subjects ALLOYS
CASTING
CASTING OF METALS
CASTING OF OTHER SUBSTANCES BY THE SAME PROCESSES OR DEVICES
CHEMISTRY
FERROUS OR NON-FERROUS ALLOYS
METALLURGY
PERFORMING OPERATIONS
POWDER METALLURGY
PRETREATMENT OF RAW MATERIALS
PRODUCTION AND REFINING OF METALS
TRANSPORTING
TREATMENT OF ALLOYS OR NON-FERROUS METALS
title High-temperature alloy GH710 alloy steel ingot for turbine disc and preparation method of high-temperature alloy GH710 alloy steel ingot
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-20T02%3A34%3A50IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=GAO%20JINGBAO&rft.date=2023-08-01&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116516205A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true