Multi-element boron-free high-temperature brazing filler metal and seal welding application method
The invention designs a multi-element boron-free high-temperature brazing filler metal, which comprises the following chemical components in percentage by weight: 5.5 to 7.5 percent of Al, 5.0 to 7.0 percent of Ti, 12.0 to 16.0 percent of Cr, 4.0 to 8.0 percent of Co, 4.0 to 7.0 percent of Nb, 2.0 t...