Micro negative pressure welding repair method for flue gas pipeline leakage

The invention relates to the technical field of smelting flue gas pipeline repair welding, and aims to provide a flue gas pipeline leakage micro-negative pressure repair welding method which comprises the following steps: S1, manufacturing a pipeline leakage micro-negative pressure repair welding de...

Ausführliche Beschreibung

Gespeichert in:
Bibliographische Detailangaben
Hauptverfasser: WU YIYUN, CAO YINQIANG, ZHENG XIAONA
Format: Patent
Sprache:chi ; eng
Schlagworte:
Online-Zugang:Volltext bestellen
Tags: Tag hinzufügen
Keine Tags, Fügen Sie den ersten Tag hinzu!
container_end_page
container_issue
container_start_page
container_title
container_volume
creator WU YIYUN
CAO YINQIANG
ZHENG XIAONA
description The invention relates to the technical field of smelting flue gas pipeline repair welding, and aims to provide a flue gas pipeline leakage micro-negative pressure repair welding method which comprises the following steps: S1, manufacturing a pipeline leakage micro-negative pressure repair welding device which comprises a smoke hood, an adjusting ball valve and two sections of straight pipes, and mounting an air pipe on the side wall of the straight pipe positioned at the rear end of the adjusting ball valve, an adjusting valve is mounted on the air pipe; s2, the pipeline leakage micro-negative-pressure welding repair device is in butt joint with a flue gas pipeline, an adjusting ball valve and an adjusting valve are opened, and the surrounding environment is in a micro-negative-pressure state; s3, the section, close to the smoke pipeline, of the smoke hood is subjected to rapid welding repair; s4, after welding repair is completed, the adjusting ball valve and the adjusting valve are closed, and the straight
format Patent
fullrecord <record><control><sourceid>epo_EVB</sourceid><recordid>TN_cdi_epo_espacenet_CN116423089A</recordid><sourceformat>XML</sourceformat><sourcesystem>PC</sourcesystem><sourcerecordid>CN116423089A</sourcerecordid><originalsourceid>FETCH-epo_espacenet_CN116423089A3</originalsourceid><addsrcrecordid>eNqNyrEKwjAQBuAsDqK-w_kAgrUidZSiCKKTeznaP_EwJuGS6uu7-ABO3_JNzeUqvUYKcFzkDUqKnEcFfeAHCY4UiUXphfKIA9moZP0IcpwpSYKXAPLgJzvMzcSyz1j8nJnl6Xhvzyuk2CEn7hFQuvZWVbvtpl43-0P9z_kCagE1eA</addsrcrecordid><sourcetype>Open Access Repository</sourcetype><iscdi>true</iscdi><recordtype>patent</recordtype></control><display><type>patent</type><title>Micro negative pressure welding repair method for flue gas pipeline leakage</title><source>esp@cenet</source><creator>WU YIYUN ; CAO YINQIANG ; ZHENG XIAONA</creator><creatorcontrib>WU YIYUN ; CAO YINQIANG ; ZHENG XIAONA</creatorcontrib><description>The invention relates to the technical field of smelting flue gas pipeline repair welding, and aims to provide a flue gas pipeline leakage micro-negative pressure repair welding method which comprises the following steps: S1, manufacturing a pipeline leakage micro-negative pressure repair welding device which comprises a smoke hood, an adjusting ball valve and two sections of straight pipes, and mounting an air pipe on the side wall of the straight pipe positioned at the rear end of the adjusting ball valve, an adjusting valve is mounted on the air pipe; s2, the pipeline leakage micro-negative-pressure welding repair device is in butt joint with a flue gas pipeline, an adjusting ball valve and an adjusting valve are opened, and the surrounding environment is in a micro-negative-pressure state; s3, the section, close to the smoke pipeline, of the smoke hood is subjected to rapid welding repair; s4, after welding repair is completed, the adjusting ball valve and the adjusting valve are closed, and the straight</description><language>chi ; eng</language><subject>CLADDING OR PLATING BY SOLDERING OR WELDING ; CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING ; MACHINE TOOLS ; METAL-WORKING NOT OTHERWISE PROVIDED FOR ; PERFORMING OPERATIONS ; SOLDERING OR UNSOLDERING ; TRANSPORTING ; WELDING ; WORKING BY LASER BEAM</subject><creationdate>2023</creationdate><oa>free_for_read</oa><woscitedreferencessubscribed>false</woscitedreferencessubscribed></display><links><openurl>$$Topenurl_article</openurl><openurlfulltext>$$Topenurlfull_article</openurlfulltext><thumbnail>$$Tsyndetics_thumb_exl</thumbnail><linktohtml>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230714&amp;DB=EPODOC&amp;CC=CN&amp;NR=116423089A$$EHTML$$P50$$Gepo$$Hfree_for_read</linktohtml><link.rule.ids>230,308,778,883,25551,76302</link.rule.ids><linktorsrc>$$Uhttps://worldwide.espacenet.com/publicationDetails/biblio?FT=D&amp;date=20230714&amp;DB=EPODOC&amp;CC=CN&amp;NR=116423089A$$EView_record_in_European_Patent_Office$$FView_record_in_$$GEuropean_Patent_Office$$Hfree_for_read</linktorsrc></links><search><creatorcontrib>WU YIYUN</creatorcontrib><creatorcontrib>CAO YINQIANG</creatorcontrib><creatorcontrib>ZHENG XIAONA</creatorcontrib><title>Micro negative pressure welding repair method for flue gas pipeline leakage</title><description>The invention relates to the technical field of smelting flue gas pipeline repair welding, and aims to provide a flue gas pipeline leakage micro-negative pressure repair welding method which comprises the following steps: S1, manufacturing a pipeline leakage micro-negative pressure repair welding device which comprises a smoke hood, an adjusting ball valve and two sections of straight pipes, and mounting an air pipe on the side wall of the straight pipe positioned at the rear end of the adjusting ball valve, an adjusting valve is mounted on the air pipe; s2, the pipeline leakage micro-negative-pressure welding repair device is in butt joint with a flue gas pipeline, an adjusting ball valve and an adjusting valve are opened, and the surrounding environment is in a micro-negative-pressure state; s3, the section, close to the smoke pipeline, of the smoke hood is subjected to rapid welding repair; s4, after welding repair is completed, the adjusting ball valve and the adjusting valve are closed, and the straight</description><subject>CLADDING OR PLATING BY SOLDERING OR WELDING</subject><subject>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</subject><subject>MACHINE TOOLS</subject><subject>METAL-WORKING NOT OTHERWISE PROVIDED FOR</subject><subject>PERFORMING OPERATIONS</subject><subject>SOLDERING OR UNSOLDERING</subject><subject>TRANSPORTING</subject><subject>WELDING</subject><subject>WORKING BY LASER BEAM</subject><fulltext>true</fulltext><rsrctype>patent</rsrctype><creationdate>2023</creationdate><recordtype>patent</recordtype><sourceid>EVB</sourceid><recordid>eNqNyrEKwjAQBuAsDqK-w_kAgrUidZSiCKKTeznaP_EwJuGS6uu7-ABO3_JNzeUqvUYKcFzkDUqKnEcFfeAHCY4UiUXphfKIA9moZP0IcpwpSYKXAPLgJzvMzcSyz1j8nJnl6Xhvzyuk2CEn7hFQuvZWVbvtpl43-0P9z_kCagE1eA</recordid><startdate>20230714</startdate><enddate>20230714</enddate><creator>WU YIYUN</creator><creator>CAO YINQIANG</creator><creator>ZHENG XIAONA</creator><scope>EVB</scope></search><sort><creationdate>20230714</creationdate><title>Micro negative pressure welding repair method for flue gas pipeline leakage</title><author>WU YIYUN ; CAO YINQIANG ; ZHENG XIAONA</author></sort><facets><frbrtype>5</frbrtype><frbrgroupid>cdi_FETCH-epo_espacenet_CN116423089A3</frbrgroupid><rsrctype>patents</rsrctype><prefilter>patents</prefilter><language>chi ; eng</language><creationdate>2023</creationdate><topic>CLADDING OR PLATING BY SOLDERING OR WELDING</topic><topic>CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING</topic><topic>MACHINE TOOLS</topic><topic>METAL-WORKING NOT OTHERWISE PROVIDED FOR</topic><topic>PERFORMING OPERATIONS</topic><topic>SOLDERING OR UNSOLDERING</topic><topic>TRANSPORTING</topic><topic>WELDING</topic><topic>WORKING BY LASER BEAM</topic><toplevel>online_resources</toplevel><creatorcontrib>WU YIYUN</creatorcontrib><creatorcontrib>CAO YINQIANG</creatorcontrib><creatorcontrib>ZHENG XIAONA</creatorcontrib><collection>esp@cenet</collection></facets><delivery><delcategory>Remote Search Resource</delcategory><fulltext>fulltext_linktorsrc</fulltext></delivery><addata><au>WU YIYUN</au><au>CAO YINQIANG</au><au>ZHENG XIAONA</au><format>patent</format><genre>patent</genre><ristype>GEN</ristype><title>Micro negative pressure welding repair method for flue gas pipeline leakage</title><date>2023-07-14</date><risdate>2023</risdate><abstract>The invention relates to the technical field of smelting flue gas pipeline repair welding, and aims to provide a flue gas pipeline leakage micro-negative pressure repair welding method which comprises the following steps: S1, manufacturing a pipeline leakage micro-negative pressure repair welding device which comprises a smoke hood, an adjusting ball valve and two sections of straight pipes, and mounting an air pipe on the side wall of the straight pipe positioned at the rear end of the adjusting ball valve, an adjusting valve is mounted on the air pipe; s2, the pipeline leakage micro-negative-pressure welding repair device is in butt joint with a flue gas pipeline, an adjusting ball valve and an adjusting valve are opened, and the surrounding environment is in a micro-negative-pressure state; s3, the section, close to the smoke pipeline, of the smoke hood is subjected to rapid welding repair; s4, after welding repair is completed, the adjusting ball valve and the adjusting valve are closed, and the straight</abstract><oa>free_for_read</oa></addata></record>
fulltext fulltext_linktorsrc
identifier
ispartof
issn
language chi ; eng
recordid cdi_epo_espacenet_CN116423089A
source esp@cenet
subjects CLADDING OR PLATING BY SOLDERING OR WELDING
CUTTING BY APPLYING HEAT LOCALLY, e.g. FLAME CUTTING
MACHINE TOOLS
METAL-WORKING NOT OTHERWISE PROVIDED FOR
PERFORMING OPERATIONS
SOLDERING OR UNSOLDERING
TRANSPORTING
WELDING
WORKING BY LASER BEAM
title Micro negative pressure welding repair method for flue gas pipeline leakage
url https://sfx.bib-bvb.de/sfx_tum?ctx_ver=Z39.88-2004&ctx_enc=info:ofi/enc:UTF-8&ctx_tim=2025-01-15T15%3A11%3A05IST&url_ver=Z39.88-2004&url_ctx_fmt=infofi/fmt:kev:mtx:ctx&rfr_id=info:sid/primo.exlibrisgroup.com:primo3-Article-epo_EVB&rft_val_fmt=info:ofi/fmt:kev:mtx:patent&rft.genre=patent&rft.au=WU%20YIYUN&rft.date=2023-07-14&rft_id=info:doi/&rft_dat=%3Cepo_EVB%3ECN116423089A%3C/epo_EVB%3E%3Curl%3E%3C/url%3E&disable_directlink=true&sfx.directlink=off&sfx.report_link=0&rft_id=info:oai/&rft_id=info:pmid/&rfr_iscdi=true